ASTM A265 SA516 Gr.70 + Alloy 20 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Alloy 20 clad plate bonds niobium-stabilized alloy 20 (UNS N08020) to a carbon steel pressure vessel base. Its nickel, copper and molybdenum resist sulfuric acid and chloride stress corrosion cracking. SHH STEEL produces it by explosion bonding with shear and UT tests as ordered.
Keywords
Alloy 20 clad plate, alloy 20 clad steel plate, ASTM A265 alloy 20, SA516 Gr.70 + N08020, sulfuric acid clad plate
Equivalent Grades:
ASME SA-265, JIS G3602, NB/T 47002.2 (by agreement); alloy 20 = N08020 / 2.4660 / 20Cb-3
Share:
General Description
Material Specification
Base and Cladding Materials
Bonding Methods
Chemical Composition
Mechanical Properties
Heat Treatment
Tolerances
Available Sizes
Weldability
Applications
Testing and Certification
Equivalent Material Grade
Why choose Us
FAQ
Conclusion

What is ASTM A265 SA516 Gr.70 + Alloy 20 nickel alloy clad plate?

ASTM A265 SA516 Gr.70 + Alloy 20 nickel alloy clad plate is a composite plate in which alloy 20 (UNS N08020, often called Carpenter 20 or 20Cb-3), an iron-nickel-chromium alloy with copper, molybdenum and niobium, is metallurgically bonded to an SA516 Grade 70 carbon steel base. The steel carries the pressure; the alloy 20 face resists sulfuric acid. It is ordered to ASTM A265 or ASME SA-265.

It is written SA516 Gr.70 + N08020 or SA516 Gr.70 + alloy 20 with the thickness pair, for example 3 + 20 mm. Alloy 20 was developed for sulfuric acid: its 32 to 38 % nickel resists chloride stress corrosion cracking, copper and molybdenum resist the acid itself, and niobium stabilizes it against sensitization during welding.

Strictly, alloy 20 is a high-nickel stainless alloy rather than a nickel-base alloy, but ASTM places it in the nickel alloy plate specification B463, which is one of the cladding standards A265 accepts.

SHH STEEL can produce alloy 20 clad plate by explosion bonding and certifies each plate to the A265 tests on the order. Other claddings are listed under nickel alloy clad plates.

ASTM A265 / ASME SA-265 requirements for Alloy 20 clad plate

ASTM A265 covers plate of a carbon or low-alloy steel base with nickel or a nickel-base alloy integrally and continuously bonded to one or both faces. It is written mainly for pressure vessels but may be used in other structural applications where corrosion resistance is needed. ASME publishes it as SA-265, identical with ASTM A265-12(2019).

Item Requirement for SA516 Gr.70 + Alloy 20
Cladding B463 / SB-463 UNS N08020 (alloy 20)
Other permitted claddings Alloys of B127, B162, B168, B333, B409, B424, B443, B463, B463, B582, B625, or others agreed
Base steel SA516 Grade 70; the standard allows pressure vessel or general structural steels (A20/A20M or A6/A6M)
Product size “Plate” means 3/16 in (4.8 mm) and over in thickness and over 10 in (254 mm) wide
Bond strength 140 MPa (20 000 psi) minimum shear, or three bond bend tests, when the purchaser requires them
Bond integrity Visual below 10 mm total; ultrasonic to A578/A578M procedures at 10 mm and over; Class 1, 3 or 5
Clad surface As-rolled, blasted (descaled and pickled) or 100 % conditioned, unless otherwise specified
Marking Per A20 or A6 for the base, plus the alloy designation and the specification number

A complete order line reads: “Clad plate to ASME SA-265, cladding SB-463 UNS N08020, 3 mm minimum; base SA-516 Grade 70, 20 mm minimum; Class 1 bond quality, 100 % UT (S12); shear test required; simulated PWHT per S3.” State whether the cladding counts toward design strength or is corrosion allowance only.

SA516 Gr.70 base and Alloy 20 cladding

A265 certifies each layer to its own specification: the cladding to ASTM B463 and the base to ASTM A516 / ASME SA-516. The pairing puts an expensive corrosion alloy only on the wetted face.

Why Alloy 20 is chosen

Alloy 20 contains 32.0 to 38.0 % nickel, 19.0 to 21.0 % chromium, 2.0 to 3.0 % molybdenum and 3.0 to 4.0 % copper, with niobium of at least 8 times the carbon content up to 1.00 % and iron as the balance. Carbon is limited to 0.07 %.

Copper and molybdenum together make alloy 20 resistant to sulfuric acid over a wide concentration range at moderate temperatures, where 316L corrodes too quickly. The high nickel content raises resistance to chloride stress corrosion cracking well above that of 300-series stainless steels.

Niobium ties up carbon so that the heat-affected zones of welds are not sensitized. That is important in clad plate, where the cladding cannot be solution annealed after fabrication.

SA516 Grade 70 base steel

ASME SA516 Grade 70 is the usual base: a carbon-manganese vessel plate with 485 to 620 MPa tensile and 260 MPa minimum yield, available normalized and impact tested. Outside ASME work it is bought as ASTM A516 Grade 70. For high-temperature hydrogen or creep service, a Cr-Mo base such as ASTM A387 Grade 11 Class 2 can replace it.

Claddings for sulfuric acid service compared

Cladding Mo, % Cr, % Best fit
Alloy 20 (N08020) 2.0 – 3.0 19.0 – 21.0 Sulfuric acid, moderate temperatures; Cu-bearing
904L (N08904) 4.0 – 5.0 19.0 – 23.0 Sulfuric acid with chlorides
Alloy 825 (N08825) 2.5 – 3.5 19.5 – 23.5 Sulfuric and phosphoric acid, higher Ni
Alloy C-276 (N10276) 15.0 – 17.0 14.5 – 16.5 Hot, contaminated mixed acids

Design notes for alloy 20 clad plate

Alloy 20 is usually treated as corrosion allowance. Pick it by corrosion data for the actual acid concentration and temperature: sulfuric acid corrosion rates change sharply with both, and the margin between alloy 20, 904L and 825 is narrow in some ranges.

Alloy 20 is a common choice for pickling tanks, acid coolers and storage of hot, dilute to medium-strength sulfuric acid, and for chemical vessels where the medium contains both sulfuric acid and chlorides at modest levels.

How Alloy 20 clad plate is made

Explosion bonding is the main manufacturing route for nickel alloy clad plate, because it joins alloys of very different strength and melting behaviour without melting either one. Roll bonding is also possible for some nickel alloys and plate sizes, and weld overlay is the alternative for shapes that cannot be clad as plate.

Explosion bonding

The Alloy 20 sheet is positioned above the SA516 plate with a controlled gap and covered with explosive. The detonation accelerates the cladding onto the base at an oblique angle; surface oxides are jetted away and the metals bond in the solid state with a wavy interface. There is no dilution, so the cladding chemistry at the surface is exactly that of the sheet. A265 permits the cladding to be made from several sheets welded together for plates wider than the available alloy sheet, with that welding qualified to ASME Section IX.

Clad plate or weld overlay?

Alloy 20 weld overlay is possible but rarely economic for large areas, and dilution from the steel lowers its copper and nickel at the surface. An explosion bonded alloy 20 clad plate gives full-chemistry alloy across the whole surface.

Chemical composition of Alloy 20 cladding and SA516 Gr.70 base

The chemical composition is certified layer by layer by the clad plate manufacturer: the cladding to ASTM B463 and the base to SA-516.

Alloy 20 cladding (UNS N08020), heat analysis

Element Alloy 20 (UNS N08020), % (ASTM B463)
Nickel (Ni) 32.0 – 38.0
Chromium (Cr) 19.0 – 21.0
Molybdenum (Mo) 2.0 – 3.0
Copper (Cu) 3.0 – 4.0
Niobium (Nb) 8 × C min, 1.00 max
Carbon (C) 0.07 max
Manganese (Mn) 2.0 max
Silicon (Si) 1.0 max
Phosphorus (P) 0.045 max
Sulfur (S) 0.035 max
Iron (Fe) Balance

The limits are those of ASTM B463 for UNS N08020; confirm the current edition before quoting single elements. Check carbon and niobium together on the sheet certificate so the stabilization ratio can be confirmed.

Product analysis of the cladding is made only when the purchaser asks for it, and the results must meet the cladding specification. For wet chemical analysis A265 asks the laboratory to discard all base metal plus 40 % of the cladding thickness from the bonded side, up to 1.6 mm, so that iron from the steel does not distort the result; spectrometric samples are taken on the centre line of the cladding.

SA516 Grade 70 base steel

Element SA516 Gr.70 heat analysis, % SA516 Gr.70 product analysis, %
Carbon (C), 12.5 mm and under 0.27 max 0.27 max
Carbon (C), over 12.5 to 50 mm 0.28 max 0.28 max
Carbon (C), over 50 to 100 mm 0.30 max 0.30 max
Carbon (C), over 100 mm 0.31 max 0.31 max
Manganese (Mn) 0.85 – 1.20 0.79 – 1.30
Phosphorus (P) 0.025 max 0.025 max
Sulfur (S) 0.025 max 0.025 max
Silicon (Si) 0.15 – 0.40 0.13 – 0.45
Iron (Fe) Balance Balance

Carbon, phosphorus and sulfur limits apply to heat and product analysis alike. For each 0.01 % carbon below the maximum, the manganese maximum may rise by 0.06 %, up to 1.50 % by heat analysis and 1.60 % by product analysis.

Mechanical properties and bond strength

A265 tests the tensile properties, the bond strength and the bond integrity of the plate in its delivered condition.

Tensile test

Condition Tensile test Acceptance
Composite 38 mm and under, base minimum tensile 485 MPa or less and minimum yield 275 MPa or less Full-thickness composite specimen Base minimum up to base maximum plus 35 MPa
Composite over 38 mm, or stronger base Base steel only All base steel tensile requirements
Cladding for corrosion allowance only Cladding need not be included All base steel tensile requirements

Properties of the two layers

Property Alloy 20 cladding (ASTM B463) SA516 Gr.70 base
Tensile strength 551 MPa min 485 – 620 MPa
Yield strength (0.2 % offset) 241 MPa min 260 MPa min
Elongation 30 % min 21 % min in 50 mm; 17 % min in 200 mm
Hardness Not specified for clad plate Not specified

A 3 + 20 mm plate is tested full thickness, with the composite between 485 and 655 MPa. Alloy 20 is similar in strength to SA516 Gr.70, so the composite result is close to that of the base alone.

Shear and bend tests

When required, the minimum shear strength between cladding and base is 20 000 psi (140 MPa), with at least 1.9 mm of cladding on the specimen and one test per plate as rolled. As an alternative, three bond bend tests through 180° with the cladding in compression are made; at least two must show no more than 50 % separation on either edge.

Ultrasonic bond quality

Class Largest single unbonded area Total unbonded area
Class 1 25 mm (1 in) longest dimension 1 % of clad surface
Class 3 75 mm (3 in) longest dimension 3 % of clad surface
Class 5 58 cm² (9 in²) 5 % of clad surface

The class must be listed on the order; when none is given, plates may be supplied as Class 5. Scanning extent is the manufacturer’s choice unless 100 % coverage, Supplementary Requirement S12, is ordered. Acid service vessels with alloy 20 cladding are commonly ordered Class 1 or Class 3; tube sheets Class 1 with 100 % coverage.

Heat treatment of Alloy 20 clad plate

A265 does not impose a single heat treatment. Unless the cladding or base specification requires a specific treatment, or the purchaser and manufacturer agree otherwise, the clad plate is furnished in a condition appropriate for the cladding alloy, the base metal, or both.

SA516 Gr.70 + alloy 20 plate is usually delivered as-clad and flattened, with the alloy sheet in the stabilized annealed condition before bonding. A solution anneal of the clad plate after bonding is not practical because of its effect on the steel.

Niobium stabilization means normal PWHT cycles of the carbon steel do not sensitize the cladding. Simulate the cycle on S3 coupons when the vessel is heat treated.

If the vessel will be post-weld heat treated, order Supplementary Requirement S3 so the test coupons see a simulated PWHT, and state temperature, holding time and number of cycles.

Thickness tolerances and surface finish

Cladding, base and total thickness may each be ordered as minimum or nominal values.

Item ASTM A265 requirement
Ordered to minimum thickness Cladding, base and total not below the ordered minimums
Nominal: base steel or total 0.3 mm under
Nominal: cladding 0.8 mm under
Over-tolerance of the total Greater of 3 mm or 10 % of the ordered total, provided each minimum is met
Width, length, flatness A20/A20M or A6/A6M, as appropriate for the base

Order the alloy 20 cladding to a minimum thickness, typically 3 mm for pressure vessels. Sulfuric acid service often needs a larger corrosion allowance than chloride service, so 4 mm and over is common on acid storage and coolers.

Stock sizes and thickness combinations of Alloy 20 clad plate

SA516 Gr.70 + Alloy 20 clad plate is ordered by cladding plus base thickness, width and length. SHH STEEL keeps common sizes in stock or produces them quickly, and any other pair inside the production range can be made to order.

Cladding + base, mm Total, mm Typical use
2 + 10 12 Pickling tanks
3 + 12 15 Acid storage
3 + 16 19 Acid coolers and shells
3 + 20 23 Pressure vessels
4 + 25 29 Reactors
4 + 30 34 Heads
5 + 40 45 Tube sheets
6 + 50 56 Clad tube sheets
Dimension Production range
Cladding thickness 2 mm to 20 mm (thicker by explosion bonding on request)
Base steel thickness 6 mm to 200 mm
Total thickness 8 mm to 220 mm
Width 1000 mm to 3000 mm; wider by explosion bonding with welded cladding
Length 2000 mm to 12000 mm
Discs and blanks Round tube sheet blanks and head blanks cut to drawing
Location China

For nickel alloys, the cladding is usually 2 to 6 mm because of alloy cost; tube sheets take thicker layers so that tube-to-tubesheet welds stay inside the alloy.

Welding SA516 Gr.70 + Alloy 20 clad plate

Clad joints are welded in two parts: a carbon steel weld for strength, then a nickel alloy overlay that restores the Alloy 20 face. Carbon steel filler must not reach the cladding.

  1. Prepare the joint to the qualified procedure, usually bevelled from the steel side with the cladding cut back from the root.
  2. Weld the SA516 Gr.70 with matching carbon steel filler.
  3. Back-gouge the clad side to sound weld metal.
  4. Overlay the carbon steel weld with E320LR / ER320LR matching filler, or with a higher-alloy nickel filler such as ERNiCrMo-3 where the procedure calls for it, in two or more layers.
  5. Clean the finished overlay; nickel alloys are not normally pickled like stainless steel, but heat tint and slag must be removed.

Alloy 20 weld metal is fully austenitic and can hot crack; keep heat input low, use stringer beads and keep the joint clean. The low-residual E320LR filler was developed to reduce that risk.

Remove heat tint after welding; in sulfuric acid service, tinted zones can corrode faster than the plate.

Procedures and welders are qualified to ASME Section IX, which A265 also requires for welded cladding and for cladding repairs. Repairs are checked by liquid penetrant and reported on the certificate.

Applications of Alloy 20 clad plate

Alloy 20 clad plate is used in sulfuric acid and related duties where 316L corrodes too quickly and a full nickel-base alloy is not needed.

  • Sulfuric acid storage tanks, coolers and process vessels.
  • Steel pickling tanks and heating coils housings.
  • Phosphate fertilizer equipment.
  • Synthetic rubber and plastics process vessels.
  • Pharmaceutical and fine chemical reactors.
  • Explosives and solvents production equipment.

Limits of alloy 20 cladding

Alloy 20 is not intended for hot concentrated hydrochloric acid or strong oxidizing chlorides, where Ni-Cr-Mo alloys are needed. In hot, concentrated sulfuric acid, check corrosion data carefully; other alloys may be better.

Testing and certification

The A265 certificate reports the chemical analysis of both layers, the Section 7 test results, the bond quality class and any additional tests on the order.

Test or document Basis Frequency / note
Chemical analysis of both layers SA-516 and ASTM B463 Each heat; product analysis (S2) if ordered
Tensile test A265 and the base specification Each plate as rolled
Shear test or three bond bend tests A265 When specified
Ultrasonic bond inspection A578/A578M procedures, Class 1/3/5 10 mm and thicker; 100 % with S12
Charpy V-notch impact Supplementary Requirement S5 When ordered for the base
Simulated PWHT of coupons Supplementary Requirement S3 When the vessel is heat treated
Corrosion test of cladding Agreed method When ordered
Penetrant test of cladding repairs A265 Section 14 Each repair, reported with location and procedure
Mill test certificate EN 10204 3.1; 3.2 with third-party inspection on request Each plate or lot

If your project does not accept weld repairs of the cladding, or wants to approve them first, state that restriction on the order; A265 lists it as a purchaser option.

Equivalent standards and grades

Other standards describe the same product with their own test levels; use them to cross-check, not to substitute without review.

Standard Scope Bond shear requirement
ASTM A265 / ASME SA-265 Nickel and nickel-base alloy-clad steel plate 140 MPa min, when specified
JIS G3602 Nickel and nickel alloy clad steels Per JIS G3602
NB/T 47002.2 Clad plate for pressure equipment, nickel-steel Per NB/T 47002.2
Layer ASTM / ASME UNS EN / W.Nr. JIS GB
Cladding B463 / SB-463 UNS N08020 (alloy 20) UNS N08020 2.4660 (NiCr20CuMo) — —
Base A516 / SA-516 Grade 70 K02700 P355GH (approx.) SGV480 (approx.) GB/T 713 Q345R (approx.)

Chinese projects order nickel-steel clad plate under NB/T 47002.2 and Japanese projects under JIS G3602; confirm that the cladding grade is listed in the edition cited or agree it. Treat these as close equivalents and verify against the design code.

Why order Alloy 20 clad plate from SHH STEEL

SHH STEEL is a clad plate manufacturer in China supplying nickel alloy clad plate to chemical and acid plant fabricators. For alloy 20 clad plate we keep the sheet certificates, including carbon and niobium, with the clad plate report.

  • We check the enquiry against ASTM A265 and flag missing items: cladding specification, bond class, shear test, PWHT simulation.
  • We quote cladding and base thicknesses separately, as minimum or nominal.
  • The nickel alloy sheet and the base plate come with traceable mill certificates; UT maps are supplied when 100 % coverage is ordered.
  • Tube sheet discs and head blanks can be cut to drawing.

FAQ

Is alloy 20 clad plate ordered to ASTM A265?
Yes. A265 (or ASME SA-265) lists B463, the alloy 20 plate specification, among its cladding standards.
Why use alloy 20 for sulfuric acid?
Its copper and molybdenum resist sulfuric acid over a wide concentration range, and its high nickel resists chloride stress corrosion cracking.
Which filler metal is used for alloy 20 clad plate?
E320LR or ER320LR, or a nickel-base filler such as ERNiCrMo-3 where the procedure calls for it.
Alloy 20 or 904L cladding?
Both serve sulfuric acid. 904L has more molybdenum for chlorides; alloy 20 has copper and niobium and more nickel. Choose by corrosion data for the medium.
Is ASME SA-265 the same as ASTM A265?
Yes in content. ASME publishes A265 as SA-265 in Section II Part A, identical with ASTM A265-12(2019). Order SA-265 for ASME Code vessels.
What is the HS code for nickel alloy clad plate?
Nickel alloy clad steel plate on a non-alloy steel base, 600 mm or wider, is commonly declared under HS 7210.90, flat-rolled products of iron or non-alloy steel, clad, plated or coated, other. The clad plate HS code depends on the base steel and width: narrower or alloy-steel-base plates fall under other headings, so confirm with your customs broker.
What should I send for a quotation?
ASTM A265 or ASME SA-265, Alloy 20 cladding thickness and specification, base grade and thickness, width, length or drawing, quantity, UT class and coverage, shear or bend test, heat treatment and PWHT simulation, and certificate type.

Request a quotation for ASTM A265 SA516 Gr.70 + Alloy 20 Nickel Alloy Clad Plate

ASTM A265 SA516 Gr.70 + Alloy 20 nickel alloy clad plate combines B463 alloy 20 with an SA516 Grade 70 base, explosion bonded, with 140 MPa minimum shear when specified and ultrasonic bond quality Class 1, 3 or 5. It is the clad solution for sulfuric acid storage, coolers and process vessels.

Send the thickness pair, plate size or drawing, quantity, tests and certificate type to SHH STEEL, or compare other claddings on our nickel alloy clad plates page. Availability, testing and delivery are confirmed with each quotation.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X