API 5L

Product Showcase

API 5L Carbon Steel Plates

SHH STEEL offers API 5L steel plate compliant Grade B/X42/X52/X60/X70 seamless/welded line pipes. API 5L specifies carbon steel pipes for oil/gas pipeline transportation with high strength and toughness. Sour service options, certified quality, competitive prices, customizable. Trust SHH STEEL!

API 5L X80 PSL2 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X80 PSL2 Steel Plate | Line Pipe Plate PSL2

API 5L X80 PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L555/X80: yield 555-705 MPa, tensile 625-825 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (Q/M). CE and CVN are mandatory. SHH STEEL supplies X80 PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X70MS PSL2 Sour Service Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X70MS PSL2 Sour Service Steel Plate | Annex H Sour Service Plate

API 5L X70MS PSL2 sour-service steel plate meets API 5L Annex H for PSL2 pipe ordered for wet H2S service. Designation L485MS/X70MS: yield 485-635 MPa, tensile 570-760 MPa, TMCP welded route. HIC acceptance and hardness limits apply; SSC testing by agreement. SHH STEEL supplies X70MS plate for sour LSAW programmes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X70 PSL2 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X70 PSL2 Steel Plate | Line Pipe Plate PSL2

API 5L X70 PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L485/X70: yield 485-635 MPa, tensile 570-760 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (Q/M). CE and CVN are mandatory. SHH STEEL supplies X70 PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X70 PSL1 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X70 PSL1 Steel Plate | Line Pipe Plate PSL1

API 5L X70 PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L485/X70: specified minimum yield 485 MPa (70,300 psi) and minimum tensile 570 MPa (82,700 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies X70 PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X65MS PSL2 Sour Service Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X65MS PSL2 Sour Service Steel Plate | Annex H Sour Service Plate

API 5L X65MS PSL2 sour-service steel plate meets API 5L Annex H for PSL2 pipe ordered for wet H2S service. Designation L450MS/X65MS: yield 450-600 MPa, tensile 535-760 MPa, TMCP welded route. HIC acceptance and hardness limits apply; SSC testing by agreement. SHH STEEL supplies X65MS plate for sour LSAW programmes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X65 PSL2 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X65 PSL2 Steel Plate | Line Pipe Plate PSL2

API 5L X65 PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L450/X65: yield 450-600 MPa, tensile 535-760 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (Q/M). CE and CVN are mandatory. SHH STEEL supplies X65 PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X65 PSL1 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X65 PSL1 Steel Plate | Line Pipe Plate PSL1

API 5L X65 PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L450/X65: specified minimum yield 450 MPa (65,300 psi) and minimum tensile 535 MPa (77,600 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies X65 PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X60MS PSL2 Sour Service Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X60MS PSL2 Sour Service Steel Plate | Annex H Sour Service Plate

API 5L X60MS PSL2 sour-service steel plate meets API 5L Annex H for PSL2 pipe ordered for wet H2S service. Designation L415MS/X60MS: yield 415-565 MPa, tensile 520-760 MPa, TMCP welded route. HIC acceptance and hardness limits apply; SSC testing by agreement. SHH STEEL supplies X60MS plate for sour LSAW programmes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X60 PSL2 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X60 PSL2 Steel Plate | Line Pipe Plate PSL2

API 5L X60 PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L415/X60: yield 415-565 MPa, tensile 520-760 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (N/Q/M). CE and CVN are mandatory. SHH STEEL supplies X60 PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X60 PSL1 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X60 PSL1 Steel Plate | Line Pipe Plate PSL1

API 5L X60 PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L415/X60: specified minimum yield 415 MPa (60,200 psi) and minimum tensile 520 MPa (75,400 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies X60 PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X56 PSL2 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X56 PSL2 Steel Plate | Line Pipe Plate PSL2

API 5L X56 PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L390/X56: yield 390-545 MPa, tensile 490-760 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (N/Q/M). CE and CVN are mandatory. SHH STEEL supplies X56 PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More
API 5L X56 PSL1 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X56 PSL1 Steel Plate | Line Pipe Plate PSL1

API 5L X56 PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L390/X56: specified minimum yield 390 MPa (56,600 psi) and minimum tensile 490 MPa (71,100 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies X56 PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.
View More

Pipeline Steel Plates

SHH STEEL, a premier Pipeline Steel Plates exporter, produces and exports pipeline steel plates for oil, gas, and water transport systems. Our plates, like API 5L X70, offer high strength and corrosion resistance, meeting API standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Trust SHH STEEL for oil and gas steel plates and custom pipeline infrastructure solutions.

Pipeline Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X