API 5L X52MS PSL2 Sour Service Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X52MS PSL2 Sour Service Steel Plate | Annex H Sour Service Plate

API 5L X52MS PSL2 sour-service steel plate meets API 5L Annex H for PSL2 pipe ordered for wet H2S service. Designation L360MS/X52MS: yield 360-530 MPa, tensile 460-760 MPa, TMCP welded route. HIC acceptance and hardness limits apply; SSC testing by agreement. SHH STEEL supplies X52MS plate for sour LSAW programmes with EN 10204 3.1 (or 3.2) mill test certificates.
Equivalent Grades:
ISO 3183 Annex H L360MS; related QS/NS sour variants in Annex H; NACE MR0175/ISO 15156 selection context. Sibling MS pages under https://www.steelspecs.com/products-item/api-5l/. Confirm against project specs.
Heat Treatment
Annex H sour TMCP welded route (MS). Delivery condition M (thermomechanical); Q/N sour variants exist in Annex H but this page covers the MS (welded TMCP) track.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Atmospheric exposure guidance
Equivalent Material Grade
X52MS vs X52 / sibling MS
Why choose Us
Our Service
FAQ
Conclusion

What is API 5L X52MS PSL2 steel plate?

API 5L X52MS PSL2 covers plate intended for line pipe manufactured to API Spec 5L (46th Edition) / ISO 3183. X52MS is Annex H thermomechanical welded sour-service plate/pipe steel. Ultra-low S (max 0.002% unless raised by agreement), Pcm max 0.20, and mandatory HIC (CSR/CLR/CTR) distinguish it from standard X52M.

API 5L is a pipe specification; these product pages describe plate feedstock ordered to the same grade chemistry and mechanical package for welded-pipe mills (LSAW, HFW and related). State PSL, delivery letter (PSL2), dimensions, CVN/DWTT temperature and any Annex H/G/J requirements on the purchase order.

China mill-direct supply with EN 10204 3.1 (or 3.2) MTC and optional third-party inspection. Category hubs: API 5L · Pipeline Steel Plates.

Sibling / related grades: API 5L X60MS · API 5L X65MS · API 5L X70MS · API 5L X52 PSL2 · GB/T 21237 L360M.

Material Specification for API 5L X52MS PSL2

Parameter Specification
Standard API Spec 5L (46th Edition) / ISO 3183; confirm ordered edition on the MTC
Grade L360MS / X52MS
PSL / annex PSL2 + Annex H (sour)
Product form Plate for welded line-pipe manufacture (LSAW / HFW and related)
Thickness relevance Chemistry tables cited for t ≤ 25.0 mm; for t > 25.0 mm composition as agreed. Plate thickness for pipe mills typically about 6-40 mm; thicker by mill inquiry. Confirm on PO/MTC.
Width / length Per mill capability and pipe-mill nesting; cut-to-size on request
Delivery condition M (TMCP) sour welded; Annex H
Surface As-rolled or shot blasted
Edge Mill edge or cut edge
Certification EN 10204 3.1 / 3.2
Density 7.85 g/cm³

Chemical Composition of API 5L X52MS (Annex H, heat and product analysis)

Annex H Table H.1 limits for welded X52MS with t ≤ 25.0 mm. Limits apply to heat and product analyses (one table). For t > 25.0 mm, composition as agreed.

Element / CE X52MS (welded)
C max (%) 0.10
Si max (%) 0.45
Mn max (%) 1.45
P max (%) 0.020
S max (%) 0.002 e
V max (%) 0.05
Nb max (%) 0.06
Ti max (%) 0.04
CEIIW max –
CEPcm max 0.20

Footnote e: S max may be increased to ≤ 0.008% for SMLS and, if agreed, ≤ 0.006% for welded pipe. Other Annex H footnotes: Al total ≤ 0.060%; N ≤ 0.012%; Al/N ≥ 2:1 (not for Ti-killed); Cu ≤ 0.35% (≤ 0.10% if agreed); Ni ≤ 0.30%; Cr ≤ 0.30%; Mo ≤ 0.15% (≤ 0.35% if agreed on higher MS); B ≤ 0.0005%; Ca ≤ 0.006%; Ca/S ≥ 1.5 when Ca added and S > 0.0015%. Nb+V+Ti ≤ 0.15% where footnote g applies. Mn may rise 0.05% per 0.01% C below max, up to +0.20% Mn.

Mechanical Properties of API 5L X52MS

Annex H Table H.2 tensile requirements for X52MS. Y/T max 0.93 for D > 323.9 mm.

Grade Yield Rt0.5 Tensile Rm Y/T max
L360MS / X52MS 360-530 MPa 460-760 MPa 0.93

Elongation Af per API 5L equation. HIC, hardness and (if agreed) SSC requirements in Annex H apply in addition to PSL2 CVN/DWTT.

Delivery Conditions for API 5L X52MS PSL2

Annex H sour TMCP welded route (MS). Delivery condition M (thermomechanical); Q/N sour variants exist in Annex H but this page covers the MS (welded TMCP) track.

Annex H also defines NS and QS sour variants. This page focuses on the MS (thermomechanical, welded) track named in the plan. Do not mix MS chemistry with standard M chemistry on one heat.

Weldability of API 5L X52MS PSL2

Sour-service X52MS welding must keep weld and HAZ hardness within Annex H limits (<=250 HV10 / 22 HRC in exposed zones; if agreed and t>9 mm, the OD-row alternative <=275 HV10 / 26 HRC may apply where the weld cap is not exposed to sour fluid). Select consumables qualified for sour service, control heat input, and avoid hard spots larger than 50 mm in any direction (Annex H hard-spot rules). HIC-tested plate does not by itself qualify the girth weld for SSC; procedure qualification and, if ordered, SSC testing remain separate. Prefer low-hydrogen SAW/GMAW wires agreed with the welding engineer for LSAW longitudinal seams and field girth welds.

Related grades: API 5L X60MS · API 5L X65MS · API 5L X70MS · API 5L X52 PSL2

Dimensional Tolerances for API 5L X52MS PSL2

Dimensional tolerances for plate follow the plate producer’s dimensional standard and the pipe mill’s order (thickness, width, flatness, edge camber). API 5L Tables 10/11 govern finished pipe OD and wall, not the plate as such. State plate tolerance class on the purchase order when nesting for LSAW.

Ultrasonic inspection of plate for laminar imperfections is commonly specified for sour (Annex H) and large-OD gas pipe; agree coverage and acceptance (e.g. related to Annex K practice) on the order.

Applications and service limits for API 5L X52MS PSL2

Typical use: plate for Annex H sour-service welded pipe in wet H2S production and transmission systems selected under NACE MR0175/ISO 15156. X52MS targets HIC-resistant TMCP feedstock. Often chosen for gathering lines and moderate-pressure sour transmission where X52 strength is enough and cleanliness/HIC dominate the RFQ. Confirm partial pressure of H2S, pH, chloride, design hardness limits and whether SSC qualification is required with the end user. Do not treat standard X52M plate as sour-qualified without Annex H chemistry and testing.

  • Plate for Annex H sour-service LSAW / HFW line pipe (X52MS)
  • Wet H2S production, gathering and transmission lines selected under NACE MR0175/ISO 15156
  • Projects specifying HIC-tested TMCP plate with hardness control
  • Bends and fittings only when the sour qualification package covers them

Related pages: API 5L · Pipeline Steel Plates · API 5L X60MS · API 5L X65MS · API 5L X70MS · API 5L X52 PSL2

Annex H sour-service guidance for X52MS

Annex H applies only to PSL2 pipe ordered for sour service. PSL1 shall not be ordered to Annex H. The steel name ends with S (e.g. X52MS = thermomechanical + sour).

HIC/SWC (NACE TM0284, Solution A unless agreed otherwise): CSR ≤ 2%, CLR ≤ 15%, CTR ≤ 5% (average of three sections per specimen).

Hardness: Pipe body / weld / HAZ hardness <=250 HV10 or 22 HRC (alternative OD-row limit <=275 HV10 or 26 HRC if agreed and t>9 mm).

SSC testing is by agreement for manufacturing-procedure qualification (Table H.3). End-user selection still follows NACE MR0175/ISO 15156 for the actual H2S environment.

Chemistry for welded X52MS (t ≤ 25.0 mm): C ≤ 0.10%, S ≤ 0.002%, Pcm ≤ 0.20. For t > 25.0 mm, composition is as agreed with Table H.1 amended as appropriate.

Plate UT for laminar imperfections is commonly ordered with Annex H (see purchaser options H.2). Agree coverage, acceptance and whether extended end zones apply. Calcium treatment practice (Ca/S) matters for HIC; do not change ladle practice mid-order without re-qualification.

Annex H check Typical order note
HIC CSR ≤ 2% / CLR ≤ 15% / CTR ≤ 5% (Solution A) unless agreed otherwise
Hardness ≤ 250 HV10 / 22 HRC body-weld-HAZ (OD-row alternative if agreed)
SSC By agreement for MPQ
PSL1 Not permitted for Annex H

Equivalent and related grades for API 5L X52MS PSL2

These designations are commonly compared with API 5L X52MS PSL2. They are approximate, not automatic substitutes. Match PSL, delivery letter, chemistry, toughness, sour testing and the project specification before replacing one grade with another.

Standard / family Grade Relation Product page
API Spec 5L (46th Edition) / ISO 3183 L360MS / X52MS This page –
GB/T 21237 L360M Related TMCP (not automatic sour) GB/T 21237 L360M
NACE / ISO MR0175 / ISO 15156 Environment selection (not a grade) –
ISO 3183 Aligned with API 5L Same technical content family API 5L hub
Category API 5L / Pipeline hubs Navigation API 5L · Pipeline Steel Plates

API 5L X52MS vs X52 PSL2 / sibling MS (selection aid)

Selection aid only. MS is not a drop-in for standard M without sour testing.

Item X52MS X52 PSL2 X60MS
YS 360-530 MPa 360-530 MPa 415-565 MPa
S max (welded) 0.002% 0.015% 0.002%
Pcm max 0.20 0.25 (typical Table 5) 0.21
HIC Mandatory Annex H Not by default Mandatory Annex H
Pages This page API 5L X52 PSL2 API 5L X60MS

Why choose SHH STEEL for API 5L X52MS PSL2

  • China mill-direct supply of API 5L X52MS PSL2 plate for LSAW/HFW pipe programmes
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • PSL, delivery letter and Annex H/G options documented on the MTC as ordered
  • Cutting, beveling and shot blasting available to shorten pipe-mill preparation
  • Family coverage: API 5L hub · Pipeline Steel Plates
  • Related planned CN plate track: GB/T 21237 pages under the pipeline plan

Supply, cutting and inspection for API 5L X52MS PSL2

Item SHH STEEL supply note
Thickness Typical plate for pipe mills about 6-40 mm; thicker by mill inquiry; confirm on PO
Size Width/length per mill and nesting; cut-to-size on request
Delivery condition M (TMCP) sour welded; Annex H
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs Grade (L360MS / X52MS), PSL, delivery letter, thickness × width × length, quantity, CVN/DWTT temperature, Annex H/G if any, inspection level

FAQ

What does MS mean in X52MS?
M = thermomechanical delivery; S = Annex H sour service. Welded TMCP sour track.
What HIC limits apply?
CSR ≤ 2%, CLR ≤ 15%, CTR ≤ 5% in Solution A unless alternative media/criteria are agreed.
Is SSC testing mandatory?
SSC is by agreement for manufacturing procedure qualification (Table H.3). Environment selection remains per NACE MR0175/ISO 15156.
Can I use standard X52M plate for sour service?
Not without meeting Annex H chemistry, HIC, hardness and order requirements. See API 5L X52 PSL2 for the non-sour track.
What is Pcm for X52MS?
CEPcm max 0.20 (Table H.1, welded).

Request a quotation

Send API 5L X52MS PSL2 (include delivery letter / Annex H needs), thickness × width × length, quantity, CVN/DWTT temperature, UT level and any inspection requirement. Mill availability, certification scope and a quotation will be returned.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: API 5L · Pipeline Steel Plates · API 5L X60MS · API 5L X65MS · API 5L X70MS · API 5L X52 PSL2

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X