API 5L X60MS PSL2 Sour Service Steel Plate | Annex H Sour Service Plate
What is API 5L X60MS PSL2 steel plate?
API 5L X60MS PSL2 covers plate intended for line pipe manufactured to API Spec 5L (46th Edition) / ISO 3183. X60MS raises Mn/V/Nb allowances versus X52MS while keeping C max 0.10% and S max 0.002% (welded). Pcm max 0.21. Use when design needs X60 strength in wet H2S service under NACE MR0175/ISO 15156 selection rules.
API 5L is a pipe specification; these product pages describe plate feedstock ordered to the same grade chemistry and mechanical package for welded-pipe mills (LSAW, HFW and related). State PSL, delivery letter (PSL2), dimensions, CVN/DWTT temperature and any Annex H/G/J requirements on the purchase order.
China mill-direct supply with EN 10204 3.1 (or 3.2) MTC and optional third-party inspection. Category hubs: API 5L · Pipeline Steel Plates.
Sibling / related grades: API 5L X52MS · API 5L X65MS · API 5L X70MS · API 5L X60 PSL2 · GB/T 21237 L415M.
Material Specification for API 5L X60MS PSL2
| Parameter | Specification |
|---|---|
| Standard | API Spec 5L (46th Edition) / ISO 3183; confirm ordered edition on the MTC |
| Grade | L415MS / X60MS |
| PSL / annex | PSL2 + Annex H (sour) |
| Product form | Plate for welded line-pipe manufacture (LSAW / HFW and related) |
| Thickness relevance | Chemistry tables cited for t ≤ 25.0 mm; for t > 25.0 mm composition as agreed. Plate thickness for pipe mills typically about 6-40 mm; thicker by mill inquiry. Confirm on PO/MTC. |
| Width / length | Per mill capability and pipe-mill nesting; cut-to-size on request |
| Delivery condition | M (TMCP) sour welded; Annex H |
| Surface | As-rolled or shot blasted |
| Edge | Mill edge or cut edge |
| Certification | EN 10204 3.1 / 3.2 |
| Density | 7.85 g/cm³ |
Chemical Composition of API 5L X60MS (Annex H, heat and product analysis)
Annex H Table H.1 limits for welded X60MS with t ≤ 25.0 mm. Limits apply to heat and product analyses (one table). For t > 25.0 mm, composition as agreed.
| Element / CE | X60MS (welded) |
|---|---|
| C max (%) | 0.10 |
| Si max (%) | 0.45 |
| Mn max (%) | 1.45 |
| P max (%) | 0.020 |
| S max (%) | 0.002 e |
| V max (%) | 0.08 |
| Nb max (%) | 0.08 |
| Ti max (%) | 0.06 |
| CEIIW max | – |
| CEPcm max | 0.21 |
Footnote e: S max may be increased to ≤ 0.008% for SMLS and, if agreed, ≤ 0.006% for welded pipe. Other Annex H footnotes: Al total ≤ 0.060%; N ≤ 0.012%; Al/N ≥ 2:1 (not for Ti-killed); Cu ≤ 0.35% (≤ 0.10% if agreed); Ni ≤ 0.30%; Cr ≤ 0.30%; Mo ≤ 0.15% (≤ 0.35% if agreed on higher MS); B ≤ 0.0005%; Ca ≤ 0.006%; Ca/S ≥ 1.5 when Ca added and S > 0.0015%. Nb+V+Ti ≤ 0.15% where footnote g applies. Mn may rise 0.05% per 0.01% C below max, up to +0.20% Mn.
Mechanical Properties of API 5L X60MS
Annex H Table H.2 tensile requirements for X60MS. Y/T max 0.93 for D > 323.9 mm.
| Grade | Yield Rt0.5 | Tensile Rm | Y/T max |
|---|---|---|---|
| L415MS / X60MS | 415-565 MPa | 520-760 MPa | 0.93 |
Elongation Af per API 5L equation. HIC, hardness and (if agreed) SSC requirements in Annex H apply in addition to PSL2 CVN/DWTT.
Delivery Conditions for API 5L X60MS PSL2
Annex H sour TMCP welded route (MS). Delivery condition M (thermomechanical); Q/N sour variants exist in Annex H but this page covers the MS (welded TMCP) track.
Annex H also defines NS and QS sour variants. This page focuses on the MS (thermomechanical, welded) track named in the plan. Do not mix MS chemistry with standard M chemistry on one heat.
Weldability of API 5L X60MS PSL2
Sour-service X60MS welding must keep weld and HAZ hardness within Annex H limits (<=250 HV10 / 22 HRC in exposed zones; if agreed and t>9 mm, the OD-row alternative <=275 HV10 / 26 HRC may apply where the weld cap is not exposed to sour fluid). Select consumables qualified for sour service, control heat input, and avoid hard spots larger than 50 mm in any direction (Annex H hard-spot rules). HIC-tested plate does not by itself qualify the girth weld for SSC; procedure qualification and, if ordered, SSC testing remain separate. Prefer low-hydrogen SAW/GMAW wires agreed with the welding engineer for LSAW longitudinal seams and field girth welds.
Related grades: API 5L X52MS · API 5L X65MS · API 5L X70MS · API 5L X60 PSL2
Dimensional Tolerances for API 5L X60MS PSL2
Dimensional tolerances for plate follow the plate producer’s dimensional standard and the pipe mill’s order (thickness, width, flatness, edge camber). API 5L Tables 10/11 govern finished pipe OD and wall, not the plate as such. State plate tolerance class on the purchase order when nesting for LSAW.
Ultrasonic inspection of plate for laminar imperfections is commonly specified for sour (Annex H) and large-OD gas pipe; agree coverage and acceptance (e.g. related to Annex K practice) on the order.
Applications and service limits for API 5L X60MS PSL2
Typical use: plate for Annex H sour-service welded pipe in wet H2S production and transmission systems selected under NACE MR0175/ISO 15156. X60MS targets HIC-resistant TMCP feedstock. Used when wall-thickness optimization needs X60 strength in a sour envelope without stepping to X65MS cost and welding hardness control. Confirm partial pressure of H2S, pH, chloride, design hardness limits and whether SSC qualification is required with the end user. Do not treat standard X60M plate as sour-qualified without Annex H chemistry and testing.
- Plate for Annex H sour-service LSAW / HFW line pipe (X60MS)
- Wet H2S production, gathering and transmission lines selected under NACE MR0175/ISO 15156
- Projects specifying HIC-tested TMCP plate with hardness control
- Bends and fittings only when the sour qualification package covers them
Related pages: API 5L · Pipeline Steel Plates · API 5L X52MS · API 5L X65MS · API 5L X70MS · API 5L X60 PSL2
Annex H sour-service guidance for X60MS
Annex H applies only to PSL2 pipe ordered for sour service. PSL1 shall not be ordered to Annex H. The steel name ends with S (e.g. X60MS = thermomechanical + sour).
HIC/SWC (NACE TM0284, Solution A unless agreed otherwise): CSR ≤ 2%, CLR ≤ 15%, CTR ≤ 5% (average of three sections per specimen).
Hardness: Pipe body / weld / HAZ hardness <=250 HV10 or 22 HRC (alternative OD-row limit <=275 HV10 or 26 HRC if agreed and t>9 mm).
SSC testing is by agreement for manufacturing-procedure qualification (Table H.3). End-user selection still follows NACE MR0175/ISO 15156 for the actual H2S environment.
Chemistry for welded X60MS (t ≤ 25.0 mm): C ≤ 0.10%, S ≤ 0.002%, Pcm ≤ 0.21. For t > 25.0 mm, composition is as agreed with Table H.1 amended as appropriate.
Plate UT for laminar imperfections is commonly ordered with Annex H (see purchaser options H.2). Agree coverage, acceptance and whether extended end zones apply. Calcium treatment practice (Ca/S) matters for HIC; do not change ladle practice mid-order without re-qualification.
| Annex H check | Typical order note |
|---|---|
| HIC | CSR ≤ 2% / CLR ≤ 15% / CTR ≤ 5% (Solution A) unless agreed otherwise |
| Hardness | ≤ 250 HV10 / 22 HRC body-weld-HAZ (OD-row alternative if agreed) |
| SSC | By agreement for MPQ |
| PSL1 | Not permitted for Annex H |
Equivalent and related grades for API 5L X60MS PSL2
These designations are commonly compared with API 5L X60MS PSL2. They are approximate, not automatic substitutes. Match PSL, delivery letter, chemistry, toughness, sour testing and the project specification before replacing one grade with another.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| API Spec 5L (46th Edition) / ISO 3183 | L415MS / X60MS | This page | – |
| GB/T 21237 | L415M | Related TMCP (not automatic sour) | GB/T 21237 L415M |
| NACE / ISO | MR0175 / ISO 15156 | Environment selection (not a grade) | – |
| ISO 3183 | Aligned with API 5L | Same technical content family | API 5L hub |
| Category | API 5L / Pipeline hubs | Navigation | API 5L · Pipeline Steel Plates |
API 5L X60MS vs X60 PSL2 / sibling MS (selection aid)
Selection aid only. MS is not a drop-in for standard M without sour testing.
| Item | X60MS | X60 PSL2 | X52MS |
|---|---|---|---|
| YS | 415-565 MPa | 415-565 MPa | 360-530 MPa |
| S max (welded) | 0.002% | 0.015% | 0.002% |
| Pcm max | 0.21 | 0.25 (typical Table 5) | 0.20 |
| HIC | Mandatory Annex H | Not by default | Mandatory Annex H |
| Pages | This page | API 5L X60 PSL2 | API 5L X52MS |
Why choose SHH STEEL for API 5L X60MS PSL2
- China mill-direct supply of API 5L X60MS PSL2 plate for LSAW/HFW pipe programmes
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- PSL, delivery letter and Annex H/G options documented on the MTC as ordered
- Cutting, beveling and shot blasting available to shorten pipe-mill preparation
- Family coverage: API 5L hub · Pipeline Steel Plates
- Related planned CN plate track: GB/T 21237 pages under the pipeline plan
Supply, cutting and inspection for API 5L X60MS PSL2
| Item | SHH STEEL supply note |
|---|---|
| Thickness | Typical plate for pipe mills about 6-40 mm; thicker by mill inquiry; confirm on PO |
| Size | Width/length per mill and nesting; cut-to-size on request |
| Delivery condition | M (TMCP) sour welded; Annex H |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Grade (L415MS / X60MS), PSL, delivery letter, thickness × width × length, quantity, CVN/DWTT temperature, Annex H/G if any, inspection level |
FAQ
-
What does MS mean in X60MS?
- M = thermomechanical delivery; S = Annex H sour service. Welded TMCP sour track.
-
What HIC limits apply?
- CSR ≤ 2%, CLR ≤ 15%, CTR ≤ 5% in Solution A unless alternative media/criteria are agreed.
-
Is SSC testing mandatory?
- SSC is by agreement for manufacturing procedure qualification (Table H.3). Environment selection remains per NACE MR0175/ISO 15156.
-
Can I use standard X60M plate for sour service?
- Not without meeting Annex H chemistry, HIC, hardness and order requirements. See API 5L X60 PSL2 for the non-sour track.
-
What is Pcm for X60MS?
- CEPcm max 0.21 (Table H.1, welded).
Request a quotation
Send API 5L X60MS PSL2 (include delivery letter / Annex H needs), thickness × width × length, quantity, CVN/DWTT temperature, UT level and any inspection requirement. Mill availability, certification scope and a quotation will be returned.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097