API 5L Grade B PSL2 Steel Plate | Line Pipe Plate PSL2
What is API 5L Grade B PSL2 steel plate?
API 5L Grade B PSL2 covers plate intended for line pipe manufactured to API Spec 5L (46th Edition) / ISO 3183. PSL2 Grade B adds max YS 450 MPa, max TS 655 MPa, Y/T max 0.93 (D>323.9 mm), CE limits and mandatory CVN. Delivery may be R, N, Q or M as ordered in the steel name (BR/BN/BQ/BM).
API 5L is a pipe specification; these product pages describe plate feedstock ordered to the same grade chemistry and mechanical package for welded-pipe mills (LSAW, HFW and related). State PSL, delivery letter (PSL2), dimensions, CVN/DWTT temperature and any Annex H/G/J requirements on the purchase order.
China mill-direct supply with EN 10204 3.1 (or 3.2) MTC and optional third-party inspection. Category hubs: API 5L · Pipeline Steel Plates.
Sibling / related grades: API 5L X42 PSL2 · API 5L X46 PSL2 · API 5L X52 PSL2 · API 5L X56 PSL2 · API 5L X60 PSL2 · API 5L X65 PSL2 · API 5L X70 PSL2 · API 5L X80 PSL2 · API 5L Grade B PSL1 · GB/T 21237 L245M.
Material Specification for API 5L Grade B PSL2
| Parameter | Specification |
|---|---|
| Standard | API Spec 5L (46th Edition) / ISO 3183; confirm ordered edition on the MTC |
| Grade | L245 / Grade B (+ delivery letter) |
| PSL / annex | PSL2 |
| Product form | Plate for welded line-pipe manufacture (LSAW / HFW and related) |
| Thickness relevance | Chemistry tables cited for t ≤ 25.0 mm; for t > 25.0 mm composition as agreed. Plate thickness for pipe mills typically about 6-40 mm; thicker by mill inquiry. Confirm on PO/MTC. |
| Width / length | Per mill capability and pipe-mill nesting; cut-to-size on request |
| Delivery condition | R/N/Q/M as ordered in steel name |
| Surface | As-rolled or shot blasted |
| Edge | Mill edge or cut edge |
| Certification | EN 10204 3.1 / 3.2 |
| Density | 7.85 g/cm³ |
Chemical Composition of API 5L Grade B PSL2 by delivery letter (heat and product analysis)
Limits below are from API 5L Table 5 for PSL2 pipe with t ≤ 25.0 mm. Values apply to heat (melt) and product analyses in one table. For t > 25.0 mm, composition shall be as agreed. Footnote letters match the standard.
| Element / CE | BR | BN | BQ | BM |
|---|---|---|---|---|
| C max (%) | 0.24 | 0.24 | 0.18 | 0.22 |
| Si max (%) | 0.40 | 0.40 | 0.45 | 0.45 |
| Mn max (%) | 1.20 | 1.20 | 1.40 | 1.20 |
| P max (%) | 0.03 | 0.03 | 0.03 | 0.03 |
| S max (%) | 0.01 | 0.01 | 0.01 | 0.01 |
| V max (%) | c | c | 0.05 | 0.05 |
| Nb max (%) | c | c | 0.05 | 0.05 |
| Ti max (%) | 0.04 | 0.04 | 0.04 | 0.04 |
| CEIIW max | 0.43 | 0.43 | 0.43 | 0.43 |
| CEPcm max | 0.25 | 0.25 | 0.25 | 0.25 |
Footnotes (API 5L Table 5): c unless otherwise agreed Nb+V ≤ 0.06%; d Nb+V+Ti ≤ 0.15%; g unless otherwise agreed Nb+V+Ti ≤ 0.15%; other Cu/Ni/Cr/Mo caps per footnotes e/h/i. CEIIW applies if product-analysis C > 0.12%; CEPcm if C ≤ 0.12%. Carbon-manganese trade-off footnote applies within stated caps. No intentional B (residual ≤ 0.001%) except where footnote j applies on higher grades.
Seamless pipe with t > 20.0 mm: CE limits shall be as agreed.
Mechanical Properties of API 5L Grade B PSL2
API 5L Table 7 tensile requirements for PSL2 pipe body. Y/T max 0.93 applies when D > 323.9 mm (12.750 in).
| Grade | Yield Rt0.5 | Tensile Rm | Y/T max | Delivery |
|---|---|---|---|---|
| L245 / Grade B | 245-450 MPa | 415-655 MPa | 0.93 | R/N/Q/M |
Elongation Af follows the API 5L equation based on specified min tensile U and test-piece area Axc. Weld-seam tensile min equals body tensile min.
CVN: mandatory for PSL2 pipe body (Table 8 at 0 °C or agreed lower T). Weld and HAZ CVN required for welded pipe. DWTT: PSL2 welded pipe per 9.9 (average shear area ≥ 85%).
Delivery Conditions for API 5L Grade B PSL2
PSL2 steel-name suffixes: R (as-rolled); N (normalized / normalizing rolled); Q (quenched and tempered); M (thermomechanical rolled (TMCP)). Ordered as part of the steel name (e.g. X65M).
PSL2 delivery condition is part of the ordered steel name and cannot be left open. Example markings: Grade BN, Grade BQ, Grade BM, Grade BR. Plate must match the letter on the PO.
Weldability of API 5L Grade B PSL2
PSL2 B carries mandatory CE(IIW)/Pcm limits (Table 5) that guide preheat and consumable selection. Delivery condition (R/N/Q/M) changes hardenability and HAZ response: TMCP (M) plate usually needs careful heat-input caps; Q&T (Q) plate needs HAZ toughness verification. Use low-hydrogen processes and a qualified WPS matched to the ordered steel name.
Related grades: API 5L X42 PSL2 · API 5L X46 PSL2 · API 5L X52 PSL2 · API 5L X56 PSL2 · API 5L X60 PSL2 · API 5L X65 PSL2 · API 5L X70 PSL2 · API 5L X80 PSL2 · API 5L Grade B PSL1
Dimensional Tolerances for API 5L Grade B PSL2
Dimensional tolerances for plate follow the plate producer’s dimensional standard and the pipe mill’s order (thickness, width, flatness, edge camber). API 5L Tables 10/11 govern finished pipe OD and wall, not the plate as such. State plate tolerance class on the purchase order when nesting for LSAW.
Ultrasonic inspection of plate for laminar imperfections is commonly specified for sour (Annex H) and large-OD gas pipe; agree coverage and acceptance (e.g. related to Annex K practice) on the order.
Applications and service limits for API 5L Grade B PSL2
Typical use: plate for PSL2 welded line pipe on oil and gas transmission systems that require CVN, CE control and capped Y/T. Large-OD LSAW is the main plate consumer for B. Add Annex G when ductile-fracture arrest is specified; use MS grades for wet H2S.
- Plate for LSAW / HFW line pipe to API 5L / ISO 3183
- Oil and gas onshore transmission and gathering (per PSL / annex)
- Water and utility pipelines when API 5L grade is specified
- Bends and fittings made from matching plate when approved
Related pages: API 5L · Pipeline Steel Plates · API 5L X42 PSL2 · API 5L X46 PSL2 · API 5L X52 PSL2 · API 5L X56 PSL2 · API 5L X60 PSL2 · API 5L X65 PSL2 · API 5L X70 PSL2 · API 5L X80 PSL2 · API 5L Grade B PSL1
Toughness, DWTT and CE guidance for Grade B PSL2
Full-size body CVN min average typically 27 J (20 ft·lbf) at 0 °C for D up to 762 mm in grades ≤ X60; larger diameters rise to 40 J. Confirm Table 8 row for the ordered OD.
DWTT (PSL2 welded pipe, 9.9): average shear fracture area >= 85% at 0 °C (or agreed lower temperature). For t > 25.4 mm, DWTT acceptance is by agreement. Annex G adds ductile-fracture-arrest requirements when ordered (marking suffix G).
Carbon equivalent: use CEIIW when product-analysis C > 0.12%; use CEPcm when C ≤ 0.12%. Tabulated maxima for this grade’s delivery variants are in the chemistry section (typically CEIIW 0.43 / Pcm 0.25 unless footnote says as agreed).
Y/T max 0.93 applies for D > 323.9 mm. Delivery letters allowed: R/N/Q/M.
Equivalent and related grades for API 5L Grade B PSL2
These designations are commonly compared with API 5L Grade B PSL2. They are approximate, not automatic substitutes. Match PSL, delivery letter, chemistry, toughness, sour testing and the project specification before replacing one grade with another.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| API Spec 5L (46th Edition) / ISO 3183 | L245 / Grade B (+ delivery letter) | This page | – |
| GB/T 21237 | L245M PSL2 | Approximate CN TMCP talk | GB/T 21237 L245M |
| ISO 3183 | Aligned with API 5L | Same technical content family | API 5L hub |
| Category | API 5L / Pipeline hubs | Navigation | API 5L · Pipeline Steel Plates |
API 5L Grade B PSL2 vs PSL1 / related (selection aid)
Selection aid only. Not automatic substitutes.
| Item | Grade B PSL2 | Grade B PSL1 | X42 PSL2 |
|---|---|---|---|
| YS | 245-450 MPa | ≥ 245 MPa | 290-495 MPa |
| Delivery | R/N/Q/M | Manufacturer option | Delivery R/N/Q/M |
| CE / CVN | Mandatory | Not mandatory | Per page |
| Pages | This page | API 5L Grade B PSL1 | API 5L X42 PSL2 |
Why choose SHH STEEL for API 5L Grade B PSL2
- China mill-direct supply of API 5L Grade B PSL2 plate for LSAW/HFW pipe programmes
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- PSL, delivery letter and Annex H/G options documented on the MTC as ordered
- Cutting, beveling and shot blasting available to shorten pipe-mill preparation
- Family coverage: API 5L hub · Pipeline Steel Plates
- Related planned CN plate track: GB/T 21237 pages under the pipeline plan
Supply, cutting and inspection for API 5L Grade B PSL2
| Item | SHH STEEL supply note |
|---|---|
| Thickness | Typical plate for pipe mills about 6-40 mm; thicker by mill inquiry; confirm on PO |
| Size | Width/length per mill and nesting; cut-to-size on request |
| Delivery condition | R/N/Q/M as ordered in steel name |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Grade (L245 / Grade B (+ delivery letter)), PSL, delivery letter, thickness × width × length, quantity, CVN/DWTT temperature, Annex H/G if any, inspection level |
FAQ
-
What delivery letters are allowed for Grade B PSL2?
- R/N/Q/M. The letter is part of the steel name on the order and MTC.
-
What is the Y/T limit?
- Max 0.93 for D > 323.9 mm (Table 7).
-
Are CVN and DWTT required?
- CVN is mandatory for PSL2 (Table 8). DWTT applies to PSL2 welded pipe per clause 9.9 (shear area ≥ 85%). Temperatures default to 0 °C unless a lower temperature is agreed.
-
When do I need Grade BMS?
- Annex H MS grades exist for X52/X60/X65/X70; X80 sour is outside this plate batch.
-
Is ISO 3183 identical?
- It is the aligned international standard. Cite the ordered edition on the PO/MTC.
Request a quotation
Send API 5L Grade B PSL2 (include delivery letter / Annex H needs), thickness × width × length, quantity, CVN/DWTT temperature, UT level and any inspection requirement. Mill availability, certification scope and a quotation will be returned.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097