Product Showcase
EN 10208-2 Carbon Steel Plates
SHH STEEL offers EN 10208-2-compliant L245MB/L290NB/L360NB low-alloy steel pipes. EN 10208-2 specifies seamless/welded pipes for sour service pipeline transportation. Corrosion-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
EN 10208-2 L555QB Steel Plate | Q&T Pipeline Plate
EN 10208-2 L555QB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (quenched and tempered; steel number 1.8957). Pipe-body yield Rt0.5 555-675 MPa with Rm ≥ 625 MPa and yield ratio ≤0.90 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L555MB Steel Plate | TMCP Pipeline Plate
EN 10208-2 L555MB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (thermomechanically rolled; steel number 1.8978). Pipe-body yield Rt0.5 555-675 MPa with Rm ≥ 625 MPa and yield ratio ≤0.90 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L485QB Steel Plate | Q&T Pipeline Plate
EN 10208-2 L485QB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (quenched and tempered; steel number 1.8955). Pipe-body yield Rt0.5 485-605 MPa with Rm ≥ 570 MPa and yield ratio ≤0.90 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L485MB Steel Plate | TMCP Pipeline Plate
EN 10208-2 L485MB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (thermomechanically rolled; steel number 1.8977). Pipe-body yield Rt0.5 485-605 MPa with Rm ≥ 570 MPa and yield ratio ≤0.90 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L450QB Steel Plate | Q&T Pipeline Plate
EN 10208-2 L450QB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (quenched and tempered; steel number 1.8952). Pipe-body yield Rt0.5 450-570 MPa with Rm ≥ 535 MPa and yield ratio ≤0.90 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L450MB Steel Plate | TMCP Pipeline Plate
EN 10208-2 L450MB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (thermomechanically rolled; steel number 1.8975). Pipe-body yield Rt0.5 450-570 MPa with Rm ≥ 535 MPa and yield ratio ≤0.87 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L415QB Steel Plate | Q&T Pipeline Plate
EN 10208-2 L415QB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (quenched and tempered; steel number 1.8947). Pipe-body yield Rt0.5 415-565 MPa with Rm ≥ 520 MPa and yield ratio ≤0.88 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L415NB Steel Plate | Normalized Pipeline Plate
EN 10208-2 L415NB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (normalized or normalizing formed; steel number 1.8972). Pipe-body yield Rt0.5 415-565 MPa with Rm ≥ 520 MPa and yield ratio ≤0.85 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L415MB Steel Plate | TMCP Pipeline Plate
EN 10208-2 L415MB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (thermomechanically rolled; steel number 1.8973). Pipe-body yield Rt0.5 415-565 MPa with Rm ≥ 520 MPa and yield ratio ≤0.85 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L360QB Steel Plate | Q&T Pipeline Plate
EN 10208-2 L360QB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (quenched and tempered; steel number 1.8948). Pipe-body yield Rt0.5 360-510 MPa with Rm ≥ 460 MPa and yield ratio ≤0.88 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L360NB Steel Plate | Normalized Pipeline Plate
EN 10208-2 L360NB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (normalized or normalizing formed; steel number 1.0582). Pipe-body yield Rt0.5 360-510 MPa with Rm ≥ 460 MPa and yield ratio ≤0.85 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More -
EN 10208-2 L360MB Steel Plate | TMCP Pipeline Plate
EN 10208-2 L360MB is a requirement-class B pipeline steel grade under EN 10208-2:2009 (thermomechanically rolled; steel number 1.0578). Pipe-body yield Rt0.5 360-510 MPa with Rm ≥ 460 MPa and yield ratio ≤0.85 on the pipe product. SHH STEEL supplies pipeline steel plate for line-pipe forming to EN 10208 grade requirements; confirm plate-as-feedstock scope, testing and documentation at quotation. EN 10204 3.1 (or 3.2) mill test certificates are available as ordered.View More
EN 10208-2 Carbon Steel Plates
Pipeline Steel Plates
SHH STEEL, a premier Pipeline Steel Plates exporter, produces and exports pipeline steel plates for oil, gas, and water transport systems. Our plates, like API 5L X70, offer high strength and corrosion resistance, meeting API standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Trust SHH STEEL for oil and gas steel plates and custom pipeline infrastructure solutions.
Pipeline Steel Plates
X