API 5L X70 PSL1 Steel Plate | API 5L Pipeline Steel - SHH STEEL

API 5L X70 PSL1 Steel Plate | Line Pipe Plate PSL1

API 5L X70 PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L485/X70: specified minimum yield 485 MPa (70,300 psi) and minimum tensile 570 MPa (82,700 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies X70 PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.
Equivalent Grades:
ISO 3183 L485; GB/T 21237 L485 PSL1 talk; EN 10208 / EN ISO 3183 related designations. Sibling API 5L pages under https://www.steelspecs.com/products-item/api-5l/. Confirm against project specs.
Heat Treatment
Manufacturer option unless ordered: as-rolled, normalizing rolled, thermomechanical rolled/formed, normalizing formed, normalized, normalized and tempered; Q&T for SMLS only if agreed (Grade B+).
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
PSL / toughness / sour guidance
Equivalent Material Grade
X70 PSL1 vs related grades
Why choose Us
Our Service
FAQ
Conclusion

What is API 5L X70 PSL1 steel plate?

API 5L X70 PSL1 covers plate intended for line pipe manufactured to API Spec 5L (46th Edition) / ISO 3183. X70 (L485) is the top strength class in standard PSL1. Plate for X70 pipe is typically microalloyed; when sour service or fracture arrest is required, move to PSL2 X70 or Annex H X70MS.

API 5L is a pipe specification; these product pages describe plate feedstock ordered to the same grade chemistry and mechanical package for welded-pipe mills (LSAW, HFW and related). State PSL, delivery letter (PSL2), dimensions, CVN/DWTT temperature and any Annex H/G/J requirements on the purchase order.

China mill-direct supply with EN 10204 3.1 (or 3.2) MTC and optional third-party inspection. Category hubs: API 5L · Pipeline Steel Plates.

Sibling / related grades: API 5L Grade A PSL1 · API 5L Grade B PSL1 · API 5L X42 PSL1 · API 5L X46 PSL1 · API 5L X52 PSL1 · API 5L X56 PSL1 · API 5L X60 PSL1 · API 5L X65 PSL1 · API 5L X70 PSL2 · GB/T 21237 L485.

Material Specification for API 5L X70 PSL1

Parameter Specification
Standard API Spec 5L (46th Edition) / ISO 3183; confirm ordered edition on the MTC
Grade L485 / X70
PSL / annex PSL1
Product form Plate for welded line-pipe manufacture (LSAW / HFW and related)
Thickness relevance Chemistry tables cited for t ≤ 25.0 mm; for t > 25.0 mm composition as agreed. Plate thickness for pipe mills typically about 6-40 mm; thicker by mill inquiry. Confirm on PO/MTC.
Width / length Per mill capability and pipe-mill nesting; cut-to-size on request
Delivery condition Manufacturer option unless specified (see Heat Treatment chip); report condition on MTC
Surface As-rolled or shot blasted
Edge Mill edge or cut edge
Certification EN 10204 3.1 / 3.2
Density 7.85 g/cm³

Chemical Composition of API 5L X70 PSL1 (heat and product analysis)

Limits below are from API 5L Table 4 for PSL1 pipe with t ≤ 25.0 mm (0.984 in.). The same maxima apply to heat (melt) and product analyses (shown in one table). For t > 25.0 mm, composition shall be as agreed. Always verify the mill test certificate before fabrication or substitution.

Item Seamless Welded
C max (%) 0.28 0.26
Mn max (%) 1.40 1.65
P max (%) 0.030
S max (%) 0.030

C/Mn unless otherwise agreed; Nb+V+Ti<=0.15% unless otherwise agreed. Cu ≤ 0.50%; Ni ≤ 0.50%; Cr ≤ 0.50%; Mo ≤ 0.15% (Table 4 footnotes). Carbon-manganese trade-off footnote applies (for each 0.01% C below max, Mn may rise 0.05% within the stated grade caps). No deliberate boron; residual B ≤ 0.001%.

PSL1 does not mandate CE(IIW)/Pcm. If the order needs CE caps, specify PSL2.

Mechanical Properties of API 5L X70 PSL1

API 5L Table 6 tensile requirements for PSL1 pipe body (SMLS and welded). PSL1 specifies minima only (no max YS/TS, no Y/T).

Grade Yield Rt0.5 min Tensile Rm min Elongation Af
L485 / X70 ≥ 485 MPa (70,300 psi) ≥ 570 MPa (82,700 psi) Per API 5L equation (Af from U and Axc); see standard

Weld-seam tensile min equals body tensile min for this grade. Intermediate grades follow Table 6 footnotes.

CVN and DWTT are not mandatory for PSL1 unless agreed on the purchase order.

Delivery Conditions for API 5L X70 PSL1

Manufacturer option unless ordered: as-rolled, normalizing rolled, thermomechanical rolled/formed, normalizing formed, normalized, normalized and tempered; Q&T for SMLS only if agreed (Grade B+).

For PSL1 the manufacturer may select the delivery condition unless the purchase order fixes it. Report the actual condition on the MTC. Normalizing or TMCP is often used when toughness is agreed even under PSL1.

Weldability of API 5L X70 PSL1

Higher-strength PSL1 X70 plate is often microalloyed. Control heat input to protect HAZ toughness even though CVN is not mandatory under PSL1 unless the order adds it. Do not substitute PSL2 welding procedures without reviewing CE and delivery condition.

Related grades: API 5L Grade A PSL1 · API 5L Grade B PSL1 · API 5L X42 PSL1 · API 5L X46 PSL1 · API 5L X52 PSL1 · API 5L X56 PSL1 · API 5L X60 PSL1 · API 5L X65 PSL1 · API 5L X70 PSL2

Dimensional Tolerances for API 5L X70 PSL1

Dimensional tolerances for plate follow the plate producer’s dimensional standard and the pipe mill’s order (thickness, width, flatness, edge camber). API 5L Tables 10/11 govern finished pipe OD and wall, not the plate as such. State plate tolerance class on the purchase order when nesting for LSAW.

Ultrasonic inspection of plate for laminar imperfections is commonly specified for sour (Annex H) and large-OD gas pipe; agree coverage and acceptance (e.g. related to Annex K practice) on the order.

Applications and service limits for API 5L X70 PSL1

Typical use: plate for welded line pipe (LSAW, HFW) and related fittings ordered to API 5L PSL1 X70. Common in low-to-moderate severity onshore oil, gas and water lines where the project specification does not require PSL2 toughness or CE caps. Not suitable for Annex H sour service (Annex H is PSL2 only).

  • Plate for LSAW / HFW line pipe to API 5L / ISO 3183
  • Oil and gas onshore transmission and gathering (per PSL / annex)
  • Water and utility pipelines when API 5L grade is specified
  • Bends and fittings made from matching plate when approved

Related pages: API 5L · Pipeline Steel Plates · API 5L Grade A PSL1 · API 5L Grade B PSL1 · API 5L X42 PSL1 · API 5L X46 PSL1 · API 5L X52 PSL1 · API 5L X56 PSL1 · API 5L X60 PSL1 · API 5L X65 PSL1 · API 5L X70 PSL2

PSL1 vs PSL2 selection for X70

PSL1 is the baseline product specification level. It does not require carbon-equivalent limits, maximum yield/tensile caps, or mandatory Charpy testing. Choose PSL1 X70 when the project specification explicitly allows PSL1 and fracture-toughness / CE control are handled elsewhere or are not required.

Topic PSL1 PSL2
Max YS / TS Not specified Specified (Table 7)
Y/T ratio Not controlled Max 0.93 for D > 323.9 mm (higher grades differ)
CE(IIW) / Pcm Not mandatory Mandatory (Table 5)
CVN Only if agreed Mandatory (Table 8)
DWTT (welded) Only if agreed Required per 9.9 (shear area >= 85% at 0 °C or agreed lower T)
Sour Annex H Not applicable Required for …S / …MS grades

If the RFQ mentions CVN, CE, Y/T or H2S, move to the matching PSL2 or MS page rather than upgrading PSL1 by note alone.

Equivalent and related grades for API 5L X70 PSL1

These designations are commonly compared with API 5L X70 PSL1. They are approximate, not automatic substitutes. Match PSL, delivery letter, chemistry, toughness, sour testing and the project specification before replacing one grade with another.

Standard / family Grade Relation Product page
API Spec 5L (46th Edition) / ISO 3183 L485 / X70 This page –
GB/T 21237 L485 PSL1 Approximate CN plate talk GB/T 21237 L485
ISO 3183 Aligned with API 5L Same technical content family API 5L hub
Category API 5L / Pipeline hubs Navigation API 5L · Pipeline Steel Plates

API 5L X70 PSL1 vs PSL2 / neighbors (selection aid)

Selection aid only. Not automatic substitutes.

Item X70 PSL1 X70 PSL2 X65 PSL1
YS ≥ 485 MPa 485-635 MPa ≥ 450 MPa
TS ≥ 570 MPa 570-760 MPa ≥ 535 MPa
CE / CVN Not mandatory Mandatory Not mandatory
Pages This page API 5L X70 PSL2 API 5L X65 PSL1

Why choose SHH STEEL for API 5L X70 PSL1

  • China mill-direct supply of API 5L X70 PSL1 plate for LSAW/HFW pipe programmes
  • EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
  • PSL, delivery letter and Annex H/G options documented on the MTC as ordered
  • Cutting, beveling and shot blasting available to shorten pipe-mill preparation
  • Family coverage: API 5L hub · Pipeline Steel Plates
  • Related planned CN plate track: GB/T 21237 pages under the pipeline plan

Supply, cutting and inspection for API 5L X70 PSL1

Item SHH STEEL supply note
Thickness Typical plate for pipe mills about 6-40 mm; thicker by mill inquiry; confirm on PO
Size Width/length per mill and nesting; cut-to-size on request
Delivery condition Manufacturer option unless specified (see Heat Treatment chip); report condition on MTC
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs Grade (L485 / X70), PSL, delivery letter, thickness × width × length, quantity, CVN/DWTT temperature, Annex H/G if any, inspection level

FAQ

What is API 5L X70 PSL1?
PSL1 line-pipe / plate feedstock grade L485/X70 with min YS 485 MPa and min TS 570 MPa. CE and CVN are not mandatory unless agreed.
Should I order PSL2 instead?
Yes when the project needs CE caps, max YS/TS, Y/T control, mandatory CVN or sour service. See the matching PSL2 page when listed under API 5L.
Is this the same as ISO 3183?
ISO 3183 is the aligned international text. Order language may cite either; confirm the edition on the MTC.
Can PSL1 be used for sour service?
No. Annex H shall not be applied to PSL1. Use MS/QS/NS PSL2 grades.
What thickness can be supplied?
Per mill practice and order; chemistry tables assume t ≤ 25.0 mm unless composition is agreed for thicker plate. Typical pipe-mill plate is about 6-40 mm.

Request a quotation

Send API 5L X70 PSL1 (include delivery letter / Annex H needs), thickness × width × length, quantity, CVN/DWTT temperature, UT level and any inspection requirement. Mill availability, certification scope and a quotation will be returned.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: API 5L · Pipeline Steel Plates · API 5L Grade A PSL1 · API 5L Grade B PSL1 · API 5L X42 PSL1 · API 5L X46 PSL1 · API 5L X52 PSL1 · API 5L X56 PSL1 · API 5L X60 PSL1 · API 5L X65 PSL1 · API 5L X70 PSL2

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X