Product Showcase
API 5L Carbon Steel Plates
SHH STEEL offers API 5L steel plate compliant Grade B/X42/X52/X60/X70 seamless/welded line pipes. API 5L specifies carbon steel pipes for oil/gas pipeline transportation with high strength and toughness. Sour service options, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
API 5L X52MS PSL2 Sour Service Steel Plate | Annex H Sour Service Plate
API 5L X52MS PSL2 sour-service steel plate meets API 5L Annex H for PSL2 pipe ordered for wet H2S service. Designation L360MS/X52MS: yield 360-530 MPa, tensile 460-760 MPa, TMCP welded route. HIC acceptance and hardness limits apply; SSC testing by agreement. SHH STEEL supplies X52MS plate for sour LSAW programmes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L X52 PSL2 Steel Plate | Line Pipe Plate PSL2
API 5L X52 PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L360/X52: yield 360-530 MPa, tensile 460-760 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (N/Q/M). CE and CVN are mandatory. SHH STEEL supplies X52 PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L X52 PSL1 Steel Plate | Line Pipe Plate PSL1
API 5L X52 PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L360/X52: specified minimum yield 360 MPa (52,200 psi) and minimum tensile 460 MPa (66,700 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies X52 PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L X46 PSL2 Steel Plate | Line Pipe Plate PSL2
API 5L X46 PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L320/X46: yield 320-525 MPa, tensile 435-655 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (N/Q/M). CE and CVN are mandatory. SHH STEEL supplies X46 PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L X46 PSL1 Steel Plate | Line Pipe Plate PSL1
API 5L X46 PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L320/X46: specified minimum yield 320 MPa (46,400 psi) and minimum tensile 435 MPa (63,100 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies X46 PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L X42 PSL2 Steel Plate | Line Pipe Plate PSL2
API 5L X42 PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L290/X42: yield 290-495 MPa, tensile 415-655 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (R/N/Q/M). CE and CVN are mandatory. SHH STEEL supplies X42 PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L X42 PSL1 Steel Plate | Line Pipe Plate PSL1
API 5L X42 PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L290/X42: specified minimum yield 290 MPa (42,100 psi) and minimum tensile 415 MPa (60,200 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies X42 PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L Grade B PSL2 Steel Plate | Line Pipe Plate PSL2
API 5L Grade B PSL2 is carbon / HSLA plate for welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 2. Designation L245/Grade B: yield 245-450 MPa, tensile 415-655 MPa, Y/T max 0.93 (D > 323.9 mm). Delivery condition ordered in the steel name (R/N/Q/M). CE and CVN are mandatory. SHH STEEL supplies Grade B PSL2 plate for LSAW/HFW routes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L Grade B PSL1 Steel Plate | Line Pipe Plate PSL1
API 5L Grade B PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L245/Grade B: specified minimum yield 245 MPa (35,500 psi) and minimum tensile 415 MPa (60,200 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies Grade B PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.View More -
API 5L Grade A PSL1 Steel Plate | Line Pipe Plate PSL1
API 5L Grade A PSL1 is carbon steel plate for manufacture of welded line pipe under API Spec 5L (46th Edition) / ISO 3183, product specification level 1. Designation L210/Grade A: specified minimum yield 210 MPa (30,500 psi) and minimum tensile 335 MPa (48,600 psi). PSL1 does not mandate CE limits, max YS/TS or Charpy testing unless agreed. SHH STEEL supplies Grade A PSL1 plate for LSAW/HFW pipe routes with EN 10204 3.1 (or 3.2) mill test certificates.View More
API 5L Carbon Steel Plates
Pipeline Steel Plates
SHH STEEL, a premier Pipeline Steel Plates exporter, produces and exports pipeline steel plates for oil, gas, and water transport systems. Our plates, like API 5L X70, offer high strength and corrosion resistance, meeting API standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Trust SHH STEEL for oil and gas steel plates and custom pipeline infrastructure solutions.
Pipeline Steel Plates
X