ASTM A871 Grade 60 Steel Plate | A871/A871M Weathering Plate
What is ASTM A871 Grade 60 steel plate?
ASTM A871/A871M Grade 60 covers HSLA plate for tubular structures and poles (or other suitable applications) with atmospheric corrosion resistance substantially better than carbon structural steels with or without copper addition. When properly exposed to the atmosphere, this steel can be used bare (unpainted) for many applications. Atmospheric corrosion resistance: Guide G101 corrosion-resistance index ≥ 6.0.
Two strength grades are defined: Grade 60 and Grade 65. Chemistry may follow Type I, Type II or Type IV heat-analysis packages. Delivery condition is selected so the ordered mechanical properties are met: as-rolled, normalized or quenched and tempered.
SHH STEEL is a China mill-direct source for A871 weathering plate, with EN 10204 3.1 (or 3.2) mill test certificates and optional third-party inspection. Category hubs: ASTM A871/A871M · Weathering Steel Plates. (Note: the A871 hub may need creating at publish time.)
Sibling grade: ASTM A871 Grade 65. Related weathering pages: ASTM A588 Grade A · ASTM A709 Grade 50W · EN 10025-5 S355J2W · Corten B · GB/T 4171 Q355NH · ASTM A242 Type 1 · JIS G3125 SPA-H.
Material Specification for ASTM A871 Grade 60
| Parameter | Specification |
|---|---|
| Standard | ASTM A871/A871M (Primary reference ASTM A871/A871M-20; confirm ordered edition on the MTC) |
| Grade | Grade 60 |
| Chemistry type | Type I / Type II / Type IV (as ordered) |
| Family | HSLA plate with atmospheric corrosion resistance (poles / tubular structures) |
| Product form | Plate (hot-rolled; coil-to-plate when agreed and fully tested) |
| Thickness window | Typical published tensile window about 0.138-2.00 in [3.5-50.8 mm]; thicker plate by mill inquiry. Confirm ordered thickness on the PO and MTC. |
| SHH supply focus | About 6-50 mm plate (confirm availability for thinner / thicker) |
| Width / length | Width about 1500-3000 mm; length cut-to-size on request |
| Delivery condition | As-rolled, normalized, or quenched and tempered as required to meet the specified mechanical properties. Fine-grain practice. |
| Corrosion evidence | Atmospheric corrosion resistance: Guide G101 corrosion-resistance index ≥ 6.0. |
| Surface | As-rolled or shot blasted |
| Edge | Mill edge or cut edge |
| Dimensional standard | ASTM A6/A6M |
| Certification | EN 10204 3.1 / 3.2 |
| Density | 7.85 g/cm³ |
Chemical Composition of ASTM A871 Grade 60 (Types I / II / IV)
Heat (ladle) analysis limits below follow common ASTM A871/A871M Type I / Type II / Type IV packages used for Grade 60 and Grade 65. Always verify the mill test certificate and ordered type before fabrication or substitution. Atmospheric corrosion resistance: Guide G101 corrosion-resistance index ≥ 6.0.
| Element | Type I | Type II | Type IV |
|---|---|---|---|
| C | ≤0.19 | ≤0.20 | ≤0.17 |
| Mn | 0.80-1.35 | 0.75-1.35 | 0.50-1.20 |
| P | ≤0.030 | ≤0.030 | ≤0.030 |
| S | ≤0.030 | ≤0.030 | ≤0.030 |
| Si | 0.30-0.65 | 0.15-0.50 | 0.25-0.50 |
| Ni | ≤0.40 | ≤0.50 | ≤0.40 |
| Cr | 0.40-0.70 | 0.40-0.70 | 0.40-0.70 |
| Cu | 0.25-0.40 | 0.20-0.40 | 0.30-0.50 |
| V | 0.02-0.10 | 0.01-0.10 | – |
| Mo | – | – | ≤0.10 |
| Nb (Cb) | – | – | 0.005-0.05 |
Type I / II use vanadium micro-alloying; Type IV uses columbium (niobium) with optional molybdenum. Do not mix type chemistries on one heat without mill agreement. Product-analysis tolerances follow ASTM A6 practice as applicable.
Mechanical Properties of ASTM A871 Grade 60
Tensile requirements for ASTM A871 Grade 60. Tension tests are typically transverse. For plates wider than 24 in [600 mm], elongation may be reduced by two percentage points; further adjustments follow ASTM A6.
| Grade | Yield min | Tensile min | Elongation in 2 in [50 mm] | Elongation in 8 in [200 mm] |
|---|---|---|---|---|
| Grade 60 | ≥60 ksi [≥415 MPa] | ≥75 ksi [≥520 MPa] | ≥18% | ≥16% |
Charpy V-notch impact testing is part of A871 mechanical practice; temperature and energy levels follow the purchase order / ASTM A6 supplementary requirements. A common published practice is longitudinal average ≥15 ft-lbf [20 J] at -20 °F [-29 °C]; always confirm the ordered CVN package on the MTC.
Sibling strength class: ASTM A871 Grade 65 (YS ≥65 ksi / TS ≥80 ksi).
Density is approximately 7.85 g/cm³.
Delivery Conditions for ASTM A871 Grade 60
As-rolled, normalized, or quenched and tempered as required to meet the specified mechanical properties. Fine-grain practice.
Hot-rolled weathering plates for poles are often supplied as-rolled when the strength package allows. Normalizing or quenching and tempering is used when thickness, toughness or the ordered mechanical package requires it. SHH STEEL supplies the delivery condition named on the order and reports it on the MTC.
Weldability of ASTM A871 Grade 60
Grade 60 is an HSLA weathering plate. When the steel is to be welded, use procedures suitable for the grade, chemistry type, thickness and intended service (see ASTM A6 Appendix X3 weldability guidance). Common processes include SMAW, GMAW and SAW. Prefer low-hydrogen consumables and consumables selected for weathering service when bare weld exposure is intended.
Preheat and interpass follow thickness, carbon equivalent, joint restraint and the approved WPS. Matching or undermatching filler must be chosen so weld-metal atmospheric behaviour and strength meet the design intent. Q&T heats need extra care on heat input and HAZ toughness.
Related fabrication pages: S355J2W · Q355NH · A588 Grade A.
Dimensional Tolerances for ASTM A871 Grade 60
Dimensional tolerances for A871 plate follow ASTM A6/A6M unless the order cites another dimensional agreement. Flatness, width and length classes should be stated on the purchase order for pole and tubular fabrication packages.
Respect the ordered thickness window and delivery condition. Coil-to-plate product is only A871-qualified after all required processing, inspection and testing are completed.
Applications and service limits for ASTM A871 Grade 60
Typical applications for Grade 60:
- Transmission and lighting poles
- Tubular structures and mast sections
- Outdoor structural members where higher yield than A588-class plate is specified
- RFQs that cite ASTM A871 Grade 60 / Grade 65 weathering plate
The self-protecting patina can lower long-term maintenance versus painted carbon steel in many rural and industrial atmospheres. It is not a universal coating substitute: sheltered pockets that stay wet, aggressive chloride splash, and continuous immersion often need coating or another material.
Related pages: Grade 65 · A588 Grade A · A709 50W · S355J2W · Corten B · Q355NH · A242 Type 1 · Weathering Steel Plates.
Atmospheric exposure guidance for ASTM A871 Grade 60
Bare Grade 60 is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.
| Environment | Typical fit for bare A871 plate | Note |
|---|---|---|
| Rural / mild industrial | Usually suitable | Needs wet/dry cycles for patina |
| Urban / general industrial | Often suitable | Check local pollution and design details |
| Coastal / marine splash with moderate chloride | Use with caution | May need coating, higher-Ni practice, or another grade |
| Sheltered pockets that stay wet | Not preferred bare | Design out traps or coat locally |
| Continuous immersion / aggressive chloride | Not recommended bare | Select coated carbon steel or another material |
Equivalent and related grades for ASTM A871 Grade 60
These grades are commonly compared with ASTM A871 Grade 60. They are approximate, not automatic substitutes. Match chemistry type, mechanical properties, toughness, thickness limits and the project specification before replacing one grade with another.
| Standard / family | Grade | Relation | Product page |
|---|---|---|---|
| ASTM A871/A871M | Grade 60 | This page | – |
| ASTM A871/A871M | Grade 65 | Sibling strength class | Grade 65 |
| ASTM | A588 / A709 50W | Related weathering role; usually lower yield class | A588 Gr.A · A709 50W |
| EN 10025-5 | S355J2W / S355J0W / S355K2W | Approximate W-family talk | S355J2W · S355J0W · S355K2W |
| Commercial | Corten B | Common purchasing talk | Corten B |
| GB/T 4171 | Q355NH / Q415NH | Related NH talk; confirm strength class | Q355NH · Q415NH |
| ASTM | A242 Type 1 / Type 2 | High-P / lower-P A242 tracks | A242 Type 1 · A242 Type 2 |
| JIS G3125 | SPA-H | High-P sheet/plate talk (different form focus) | SPA-H |
| Category | A871 / weathering hubs | Family navigation | ASTM A871/A871M · Weathering Steel Plates |
ASTM A871 Grade 60 vs Grade 65 vs A588 / S355J2W (selection aid)
These grades are often discussed together in purchasing. They are related weathering steels, not automatic substitutes.
| Item | Grade 60 | Grade 65 | A588 / S355J2W talk |
|---|---|---|---|
| Yield class | ≥60 ksi | ≥65 ksi | Typically 50 ksi / 355 MPa class |
| Primary use talk | Poles / tubular HSLA plate | Poles / tubular HSLA plate | Bridges / general weathering structures |
| Chemistry | Type I / II / IV | Type I / II / IV | Per A588 / EN edition |
| G101 | ≥ 6.0 | ≥ 6.0 | Per each standard |
| Pages | This page | Grade 65 | A588 · S355J2W |
Why choose SHH STEEL for ASTM A871 Grade 60
- China mill-direct supply of ASTM A871/A871M Grade 60 weathering plate
- EN 10204 3.1 mill test certificates; 3.2 and third-party inspection (SGS, TUV, BV, ABS) on request
- Type I / Type II / Type IV chemistry packages as ordered; G101 index documented
- Cutting, beveling and shot blasting available to shorten fabrication lead time
- Sibling coverage: ASTM A871 Grade 65 · hub ASTM A871/A871M · parent Weathering Steel Plates
- International near-equivalents when the project cites other standards: ASTM A588 Grade A · EN 10025-5 S355J2W · Corten B · GB/T 4171 Q355NH · ASTM A242 Type 1 · JIS G3125 SPA-H
Supply, cutting and inspection for ASTM A871 Grade 60
| Item | SHH STEEL supply note |
|---|---|
| Thickness | About 6-50 mm focus; confirm thinner / thicker against A871 window and mill practice |
| Size | Width about 1500-3000 mm; length cut-to-size on request |
| Delivery condition | As-rolled / normalized / quenched and tempered as ordered |
| Chemistry type | Type I / Type II / Type IV as ordered |
| Processing | Cutting, beveling, shot blasting available |
| Mill certificate | EN 10204 3.1 standard; 3.2 on request |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Grade (Grade 60), chemistry type, thickness × width × length, quantity, delivery condition, CVN package, inspection level |
FAQ
-
What is the difference between A871 Grade 60 and Grade 65?
- Grade 60 targets ≥60 ksi yield / ≥75 ksi tensile. Grade 65 targets ≥65 ksi yield / ≥80 ksi tensile. See Grade 65 for the sibling page.
-
What chemistry types are available?
- Type I, Type II and Type IV heat-analysis packages. All support the G101 index ≥ 6.0 requirement when correctly produced.
-
Is A871 the same as A588 or Corten B?
- Not automatically. A871 is a higher-strength pole/tubular plate specification. It is often compared with A588, Corten B and S355J2W, but substitution needs project approval and MTC review.
-
Can A871 be used bare (unpainted)?
- Yes, when properly exposed to the atmosphere, A871 steel can be used bare for many applications. Sheltered wet pockets, aggressive chlorides and immersion still need design review or coating.
-
What delivery conditions are allowed?
- As-rolled, normalized, or quenched and tempered as required to meet the specified mechanical properties. Confirm the condition on the order and MTC.
Request a quotation
Send ASTM A871 Grade 60, chemistry type (I / II / IV), thickness × width × length, quantity, delivery condition (AR / normalized / Q&T), CVN package and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: ASTM A871/A871M · Grade 65 · Weathering Steel Plates · A588 Grade A · S355J2W · Structural Steel Plates