KR AH40 shipbuilding steel plate to Korean Register (KR) rules, stacked hull plates

KR RA40 Shipbuilding Steel Plate

KR RA40 (KR RA40) higher-strength hull structural steel plate, yield 390 N/mm², tensile 510–650 N/mm², Charpy at 0 °C, stamped KR RA40 with Korean Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
KR RA40 steel plate, KR AH40 steel plate, KR RA40 shipbuilding steel plate, KR RA40 marine plate, AH40 hull steel, Korean Register AH40 plate, RA/RD/RE/RF 40 marine plate, Korean Register Rules Pt 2 hull steel
Equivalent Grades:
ASTM A131 Grade AH40; ABS AH40; DNV NV A40; LR AH40; BV AH40; NK KA40; CCS A40 / AH40; RINA Grade AH40; GB 712 Grade AH40
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

KR RA40 (KR RA40) shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

Korean Register writes its 0 °C higher-strength hull steel as KR RA40 — official KR designation RA40, not “AH40”. KR Rules for the Classification of Steel Ships, Pt 2, keep the IACS UR W11 numbers, but the R prefix replaces the H used by ABS, CCS and DNV; on a KR certificate you will read RA40. Strength level 40 means minimum yield 390 N/mm², tensile 510–650 N/mm² and elongation 20 % min. (A5). The letter A fixes Charpy V-notch testing at 0 °C. In commercial enquiries it is called KR RA40 shipbuilding steel plate; “KR AH40” is a common but unofficial way of writing it.

Equivalent grades: KR RA40 ≈ ASTM A131 Grade AH40 ≈ ABS AH40 ≈ DNV NV A40 ≈ LR AH40 ≈ BV AH40 ≈ CCS A40 / AH40 ≈ NK KA40 ≈ RINA AH40 ≈ GB 712 Grade AH40 (all class-approved, stamped by the issuing society).

KR RA40 is selected when the scantling needs the 40 yield band and the KR material class assigns 0 °C toughness. Ordinary-strength KR RA–RE stay at 235 N/mm² and cannot replace RA40 without a drawing change. In the KR ladder for strength 40: RA40 0 °C → RD40 −20 °C → RE40 −40 °C → RF40 −60 °C; within the A letter, RA32 → RA36 → RA40-style steps raise yield from 315 to 355 to 390 N/mm².

Plates that pass mill tests under KR survey are stamped with the KR mark and RA40 (stencils sometimes add the IACS form AH40 for the yard; plus Z or U where through-thickness or ultrasonic requirements apply) and are supplied with a mill certificate the KR Surveyor endorses. SHH STEEL supplies KR RA40 from Chinese mills that hold KR works approval for the grade, from stock in common sizes or from a mill rolling cycle, with KR survey arranged at the mill.

KR RA40 plate: specification summary

ItemKR RA40 / RA40 data
Rule basisKR Rules Pt 2; IACS UR W11 higher-strength Grade AH40 (KR Rules Pt 2 paragraph cross-refs UNCERTAIN without local KR Rules text)
Official KR designationRA40 (R prefix = KR rolled hull steel); IACS / ABS-style equivalent AH40 — write RA40 on KR-class POs
Related product standardASTM A131/A131M Grade AH40 — product standard only; not KR class approval
Strength levelhigher strength 40, yield 390 N/mm² min., tensile 510–650 N/mm²
Toughness classAH / R → Charpy at 0 °C
Plate thickness primarily coveredup to 100 mm under IACS UR W11 scope for plates; greater thickness by special consideration (see UNCERTAIN)
Deoxidationkilled, fine grain practice (UR W11)
Impact testCharpy V at 0 °C; frequency and supply condition per UR W11 / KR Rules Pt 2 tables
MarkingKR RA40 / KR RA40; plus Z / U / TM where ordered and qualified
TMCP Ceq (indicative UR W11 / industry practice)≤ 0.40 % for t ≤ 50 mm; ≤ 0.42 % for 50 < t ≤ 100 mm (TM steels) — confirm on mill approval / PO
Thickness toleranceIACS UR W13 as adopted by KR (minus tolerance commonly 0.3 mm class — confirm on PO; see UNCERTAIN)
Certificatemill certificate endorsed by the KR Surveyor; EN 10204 3.1 / 3.2 on request

Size range. Common market thicknesses for RA40 are about 6–80 mm (heavier plates available as per mill approval), widths 1500–3500 mm. Exact maximum thickness for a given delivery condition is as per standard and mill certificate / KR works approval. Ask for confirmation above 100 mm.

KR RA40 (KR RA40) chemical composition (heat and product analysis)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C0.18 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateAH/DH/EH group
Mn0.90–1.60 (AH ≤12.5 mm may be 0.70 min.)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateAH ≤12.5 mm may use 0.70 % Mn min.
Si0.10–0.50numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatemin. waived if acid-soluble Al ≥ 0.015 %
P0.035 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
S0.035 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Al (acid soluble) min.0.015 min. acid-soluble (or total Al per UR W11 fine-grain practice)numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificategrain refining
Nb0.02–0.05 when used singlynumeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatewhen used singly; combined minima in UR W11
V0.05–0.10 when used singlynumeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatewhen used singly
Ti0.02 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificateneed not be reported unless intentionally added
Cu0.35 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Cr0.20 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Ni0.40 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
Mo0.08 max.numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificate
N—numeric tolerance not tabulated in KR Rules (Part 2) – agree on order / mill certificatenot specified as a max in AH/DH/EH column

Product (check) analysis column: KR Rules (Part 2) specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Source: IACS UR W11 higher-strength chemistry tables (ladle samples), adopted by Korean Register for KR RA40 in Rules for the Classification of Steel Ships Pt 2 (KR paragraph numbers UNCERTAIN). The full grain-refining and residual set (Al, Nb, V, Ti, Cu, Cr, Ni, Mo, N) is shown so you can check every row on the certificate. AH/DH/EH share one chemistry column; FH is tighter on C, P, S and adds N control with higher Ni allowance. Toughness is differentiated by impact temperature and supply routes, not by separate C/Mn caps within AH/DH/EH. Product (check) analysis numeric tolerances are not tabulated in UR W11; when required, agree tolerances at enquiry. TMCP steels must also meet the applicable Ceq / Pcm limits on the mill approval — ask for Ceq on the certificate.

KR RA40 tensile properties

PropertyRequirement (IACS UR W11)
Tensile strength Rm510–650 N/mm²
Yield strength ReH390 N/mm² min.
Elongation A520 % min.
Impact test temperature0 °C

Alternative flat-specimen elongations by thickness (indicative UR W11 / industry table for strength 40):

Thickness (mm)≤5>5–10>10–15>15–20>20–25>25–30>30–40>40–50
Elongation min. %1214151617181920

Same tensile band applies to A/AH, D/DH, E/EH and F/FH 40; only impact temperature and chemistry group (FH vs AH/DH/EH) change across the letter.

KR RA40: Charpy at 0 °C and supply condition

ThicknessLong. avg. at 0 °CTrans. avg. at 0 °C
t ≤ 50 mm39 J26 J
50 < t ≤ 70 mm46 J31 J
70 < t ≤ 100 mm55 J37 J

Source: IACS UR W11 impact table for higher-strength Grade AH40 (full-size; either direction acceptable unless specified). Energies rise with thickness — a 60 mm plate must meet higher values than a 20 mm plate at the same 0 °C. Condition of supply and impact lot size depend on grain-refining practice and thickness (AR/CR/N/TM/QT as permitted). For TMCP RA40, respect Ceq caps ≈ 0.40 % (t≤50) / 0.42 % (50

Thickness tolerance and surface condition

Korean Register applies IACS UR W13 thickness tolerances unless the PO states otherwise (often 0.3 mm minus class — confirm on PO; see UNCERTAIN). Plus/flatness/width/length per agreed standard (ASTM A6, EN 10029 or GB/T 709). Surface quality per EN 10163 or equivalent accepted by KR; state primer/surface class on receipt if needed.

KR RA40 plate stock in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
61800 / 20006000 / 8000AR / CR / N / TM100+ tChina
81800 / 20008000 / 12000AR / CR / N / TM200+ tChina
102000 / 22008000 / 12000AR / CR / N / TM200+ tChina
122000 / 2200 / 250012000AR / CR / N / TM200+ tChina
142000 / 220012000AR / CR / N / TM100+ tChina
162000 / 250012000AR / CR / N / TM200+ tChina
202000 / 250012000AR / CR / N / TM100+ tChina
252200 / 250012000AR / CR / N / TM100+ tChina
30220010000 / 12000AR / CR / N / TM100+ tChina
40220010000AR / CR / N / TM50+ tChina
5022008000 / 10000AR / CR / N / TM50+ tChina

Quantities are approximate and change daily (indicative — confirm before booking); all stock plates carry KR RA40 marking and KR-endorsed mill certificates when sold as KR class plate. Sizes outside the table (for example 3000 mm width, 60–100 mm thickness, or fixed lengths for a cutting plan) are produced in the next mill rolling cycle, typically 3–6 weeks including KR survey. Send your size list and we will reply with what is in stock and what must be rolled.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and KR stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

KR RA40 equivalents in other rules and standards

Standard / societyDesignationComment
KR (Korean Register)KR RA40this page; official KR designation RA40 (IACS AH40); stamped under KR survey
GB 712GB 712 Grade AH40Chinese product standard; not class approval by itself
ASTM A131/A131MASTM A131/A131M Grade AH40A131 lists AH–FH 32/36/40; product standard only
ABSABS AH40IACS UR W11 higher-strength; live product page
DNVDNV NV A40IACS UR W11; live product page
LRLR AH40 / LR/AH40IACS UR W11; live product page
BVBV AH40IACS UR W11; live product page
NK (ClassNK)NK KA40ClassNK KA40
CCSCCS A40 / AH40IACS UR W11; live CCS product page
RINARINA Grade AH40confirm exact designation per RINA rules
Structural (indicative)EN 10025-2 S355JR / S355J2land structural; no class marking

These are comparisons, not substitutions. Multi-class stamps (KR + ABS / DNV / LR / BV) require joint survey before rolling. Other KR siblings in the 40 band are linked via KR until each product page is live.

KR RA40 vs other KR hull grades

Pick RA40 when the drawing specifies higher-strength grade AH40 (KR writes AH40 as RA40). Do not substitute ordinary Grade A/B unless the designer recalculates scantlings — yield differs (390 vs 235). Within the 40 band, letter choice is toughness: A/AH 0 °C → D/DH −20 °C → E/EH −40 °C → F/FH −60 °C. Within the AH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².

For yields above 390 N/mm² KR moves to extra-high strength (IACS UR W16): RA43…RF70, numbered by ABS-style yield class (420 → 43 … 690 → 70; UNCERTAIN vs local KR text) rather than CCS/DNV AH420 or BV A420.

When KR RA40 is the right choice: typical uses are higher-strength hull girder plating (deck, bottom, side shell) of bulk carriers, tankers and container ships in normal service where 0 °C toughness suffices. The Charpy temperature (0 °C) is fixed by the letter, and the strength by the number (ReH 390 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing.

Applications, cutting and welding of KR RA40

Typical uses: higher-strength hull girder plating (deck, bottom, side shell) of bulk carriers, tankers and container ships in normal service where 0 °C toughness suffices; weight-saving vs ordinary-strength plate in large tankers, bulkers and container ships built to KR class. See offshore platform steel plates when primary offshore grades apply.

Welding: higher-strength hull steels need approved higher-strength consumables matched to 0 °C weld-metal toughness; preheat and heat input follow the approved WPS and often track Ceq/Pcm from the mill certificate. TMCP RA40 must respect the Ceq caps noted above. Cutting by oxy-fuel/plasma/laser is routine; thick FH plate may need hydrogen control — follow mill recommendations.

Processing notes for KR RA40: cold forming is routine within normal shipyard radii. Line heating and fairing of TMCP plate should stay within the temperature limits recommended by the mill, because overheating can reduce the strength gained in controlled rolling. Check the delivery condition on the certificate before planning hot forming.

Certificates, KR survey and third-party inspection

Every plate is tested and marked at the mill under Korean Register survey; the mill certificate lists heat number, ladle chemistry, Ceq where applicable, tensile results (ReH ≥ 390 N/mm², Rm 510–650 N/mm², A ≥ 20 %), Charpy at 0 °C, delivery condition and plate numbers, endorsed by the Surveyor. Optional EN 10204 3.2, UT (U), Z-direction, multi-class with ABS/DNV/LR/BV.

On receipt: verify KR RA40 (or KR RA40) stamp, 0 °C impact data, energies for the delivered thickness band, thickness within UR W13 / PO tolerance, KR Surveyor endorsement present — not a mill-only certificate.

Charpy acceptance for KR RA40 by thickness (IACS UR W11; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
t ≤ 500 °C3926
50 < t ≤ 700 °C4631
70 < t ≤ 1000 °C5537

If UT or 3.2 was ordered, check the UT report and inspector’s plate list as well.

Common mistakes when ordering KR RA40 (KR RA40)

  • Ordering “KR 40” without the letter — toughness class missing
  • Writing AH40 (ABS/CCS style) on a KR PO without stating KR RA40 — the KR certificate and stamp read RA40
  • Accepting ordinary-strength Grade A/B certificates for a RA40 PO
  • Accepting a AH40 certificate from another society (or a product-standard paper) where KR RA40 is specified
  • Ignoring TMCP Ceq caps on TM plate
  • Substituting a different letter (e.g. AH for AH) without drawing approval
  • Coil-cut plate without coil approval
  • Missing KR endorsement on the MTC
  • Writing DNV NV A40 or LR/AH40 on a KR-class PO without arranging that society’s survey

Write the KR grade (RA40), delivery condition, impact temperature and certificate type into the PO.

Sourcing KR RA40: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateKR-approved mills only; traceable KR RA40 stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mixed sizes / gradesRA40 combined with KR Grade A/B/D/E or other A–FH sizes in one container
Lead time visibilityweekly photo updates from dedicated coordinator
Prep before shipcutting, bevelling, drilling, machining in our workshop

How to order KR RA40 plate

Specify KR RA40 (KR RA40), delivery condition (AR/CR/N/TM/QT as applicable), thickness × width × length × qty, Z/U, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to KR Rules for the Classification of Steel Ships, Pt 2, Grade RA40 (KR RA40), delivery condition [AR/CR/N/TM/QT], 20 × 2500 × 12000 mm, 30 pcs, marked KR RA40, certificate endorsed by KR Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].”

FAQ

What sizes and minimum order quantity can you supply for KR RA40 (KR RA40) plate?
IACS UR W11 lists AH40 plate primarily up to 100 mm; thicker plate needs special KR consideration. Most enquiries we receive for RA40 are 8–60 mm thick, 1800–3000 mm wide and 6000–12000 mm long. Popular sizes can come from China stock carrying the KR RA40 marking, with no fixed minimum. A mill rolling for a special width, thickness above roughly 60 mm or a Z-grade normally needs a minimum quantity per size, which we confirm per order. We can combine several sizes, or RA40 with other hull grades, to reach a rolling or container quantity.
How is KR RA40 certified, and can you arrange EN 10204 3.2 or dual-class with ABS/DNV/LR/BV?
Every plate is made by a KR-approved mill under Korean Register survey. It is die-stamped or stencilled KR RA40 / KR RA40 with the heat or plate number, and the mill test certificate is endorsed by the KR Surveyor. The certificate gives the ladle chemistry, the tensile results (ReH ≥ 390 N/mm², Rm 510–650 N/mm², A ≥ 20 %), the Charpy results at 0 °C, the delivery condition and the plate identity. An ASTM A131 or GB 712 certificate for AH40 alone is not KR class approval. If your contract asks for EN 10204 3.2, we arrange it before rolling. Dual or multi-class (KR + ABS, DNV, LR or BV) must be booked before testing. 3.2 cannot be added after testing, so please state it on the enquiry.
What is the impact test temperature and energy for KR RA40, and do thickness limits apply?
KR RA40 is tested at 0 °C. Required average energies (longitudinal/transverse, J min.) under IACS UR W11 rise with thickness: ≤50 mm 39/26; 50–70 mm 46/31; 70–100 mm 55/37. This matters when you order thick RA40: a 60 mm plate must meet higher values than a 20 mm plate at the same 0 °C. The test lot size and the permitted delivery condition (AR, CR, N, TM or QT) follow the UR W11 / KR Rules Pt 2 supply table. Above 100 mm, agree data positions and energies with KR. Results are as per standard and mill certificate.
What welding and preheat guidance applies to KR RA40?
KR RA40 needs higher-strength welding consumables approved for 0 °C weld-metal toughness. For TMCP plate, Ceq is commonly capped near 0.40 % (t ≤ 50 mm) and 0.42 % (50 < t ≤ 100 mm) under UR W11 practice; above 100 mm it is agreed at mill approval. N or AR plate of the same grade may have a higher actual Ceq, so the delivery condition affects how easy the plate is to weld. Preheat, interpass temperature and heat input must follow your KR-approved WPS. We send the mill certificate’s ladle analysis and Ceq before shipment so the welding engineer can confirm the procedure qualifies. We do not give generic preheat temperatures.
What is the delivery time for KR RA40 plate?
Stock sizes of KR RA40 can usually be cut, inspected and loaded in about 7–15 days. Mill-rolled orders typically take about 3–6 weeks plus inspection, depending on thickness, delivery condition and the mill schedule. These are commercial estimates, confirmed with each quote. If 3.2 witness or multi-class survey is required, we book the inspector when we place the mill order so testing is not delayed. A dedicated coordinator sends weekly progress photos until the bill of lading is issued.
Which payment terms do you accept for KR RA40, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the KR RA40 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance. With L/C, payment is tied to the presented documents. For first orders we can start with a smaller trial lot. The proforma invoice shows the grade (KR RA40 / KR RA40), sizes and certificate type.
Why does KR write RA40 instead of AH40, and what are the equivalent grades?
Korean Register uses an R prefix for rolled hull steels, so the IACS UR W11 grade AH40 appears in KR Rules and on KR certificates as RA40. Our title uses the official RA40; AH40 is the familiar cross-society name. KR RA40 corresponds to ASTM A131/A131M Grade AH40, ABS AH40, DNV NV A40, LR AH40 / LR/AH40, BV AH40, NK KA40, CCS A40 / AH40, RINA Grade AH40 (confirm RINA designation per rules), and GB 712 Grade AH40. All share yield 390 N/mm², tensile 510–650 N/mm² and a Charpy test at 0 °C under IACS UR W11. Even so, a plate is only accepted by the society whose stamp and certificate it carries. Order KR RA40 for KR class, or ask for multi-class when one stock must serve several projects. GB 712 or A131 certificates alone do not replace the KR RA40 stamp.
Can you cut, bevel or machine KR RA40 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut RA40 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the KR RA40 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. Shot blasting and shop primer are available on request. See SHH STEEL for our processing capabilities.

Conclusion

KR RA40 / KR RA40 is higher-strength hull steel under KR Rules for the Classification of Steel Ships, Pt 2 and IACS UR W11: yield 390 N/mm², tensile 510–650 N/mm², Charpy at 0 °C, marking KR RA40. AH40 is the cross-society name for the same IACS grade, but only the KR RA40 stamp and KR-endorsed certificate are accepted for KR class. Lock on the order: delivery condition, impact lot size, TMCP Ceq if TM, product analysis if needed, multi-class and 3.2.

SHH STEEL supplies KR RA40 plate rolled by Chinese mills that hold Korean Register works approval for the grade, so every plate carries the KR RA40 stamp and a Surveyor-endorsed certificate traceable to its heat. Common thicknesses are available from stock; other sizes are scheduled into the mill rolling cycle with KR survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, LR or another agency) and joint certification with ABS, DNV, LR, BV, NK, KR or RINA.

We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or KR RA40 mixed with KR RA/RB/RD/RE or other RA–RF 32/36/40 sizes, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.

Request a quotation: send SHH STEEL the grade (KR RA40 / KR RA40), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X