ASTM A240 UNS S44600 Stainless Steel Sheet
What is ASTM A240 UNS S44600 Stainless Steel Sheet?
Equivalent grades: UNS S44600 ≈ EN 1.4749 X18CrN28 (nearest) ≈ GB/T 16Cr25N (S12550) ≈ JIS SUH446.
UNS S44600 is a high-chromium ferritic grade. S44600 (Type 446) is a 25Cr ferritic steel with the highest scaling resistance of the ferritic grades, up to about 1100 °C in air, and good resistance to sulfur-bearing gases where nickel grades suffer. It has low ductility at room temperature and is prone to 475 °C embrittlement and sigma formation in long service, so it is used mainly for heat.
ASTM A240/A240M covers chromium, chromium-nickel and chromium-manganese-nickel stainless steel plate, sheet and strip for pressure vessels and general applications. Under ASTM A480, sheet is flat material under 5.00 mm thick and 600 mm or more wide, so UNS S44600 sheet is a cold-rolled 2B/2D product in thin gauges and a hot-rolled, annealed and pickled No.1 product toward the 4.75 mm end.
This page sets out the ASTM A240/A240M requirements for UNS S44600 sheet: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.
UNS S44600 sheet: specification summary
| Item | UNS S44600 data |
|---|---|
| Standard | ASTM A240/A240M; general requirements ASTM A480/A480M |
| ASME counterpart | SA-240 (ordered for ASME Code construction) |
| Product form (A480) | sheet: under 5.00 mm thick, 600 mm and wider; plate 5.00 mm and over |
| Typical gauges | 0.5–3.0 mm cold-rolled 2B/2D; 3.0–4.75 mm hot-rolled No.1 |
| Widths | 1000, 1219, 1250, 1500 mm; slit coil to order |
| Lengths | 2000, 2438, 2500, 3000 mm or cut to size |
| Finishes | No.1, 2D, 2B; BA and No.4 by agreement |
| Required tests | heat analysis, tension test, hardness (and bend where the grade requires it) |
| Certificates | EN 10204 3.1; 3.2 with third-party witness on request |
| Grade family | ferritic |
Size range. Sheet is normally cold rolled from about 0.3–0.5 mm up to 3 mm and hot rolled from about 3 mm to just under 5 mm. Coil widths of 1000, 1219, 1250 and 1500 mm are standard; slitting and cut-to-length lines produce narrower strip and exact lengths. Sheets thinner than 0.5 mm or wider than 1500 mm should be confirmed before ordering. UNS S44600 is a specialty grade made by a limited number of mills in campaign rolling. Stock covers the common sizes listed below; for project quantities or unusual sizes, plan for a mill campaign and reserve the heat early.
Chemical composition of UNS S44600 (ASTM A240/A240M)
| Element | wt % |
|---|---|
| C | 0.20 max |
| Si | 1.00 max |
| Mn | 1.50 max |
| P | 0.040 max |
| S | 0.030 max |
| Cr | 23.0–27.0 |
| Ni | 0.75 max |
| N | 0.25 max |
Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.
Low carbon and nitrogen, together with titanium and/or niobium where specified, are what make modern ferritic grades weldable. Check that the stabiliser content on the certificate meets the formula in the standard for the actual C and N.
Mechanical properties of UNS S44600 sheet
| Condition / thickness | Tensile strength, min | Yield strength 0.2 %, min | Elongation in 50 mm, min | Hardness, max |
|---|---|---|---|---|
| all thicknesses | 515 MPa (75 ksi) | 275 MPa (40 ksi) | 20 % | 217 HBW / 96 HRB |
The minimum proof strength is 275 MPa. Ferritic grades have lower elongation than austenitic grades and work-harden less, which helps in stretch forming but limits deep drawing. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.
Corrosion resistance of UNS S44600: PREN and limits
Ferritic stainless steels contain chromium but little or no nickel, so they are magnetic, cheaper and less sensitive to nickel price swings. They have good resistance to chloride stress-corrosion cracking, lower thermal expansion and higher thermal conductivity than austenitic grades, which helps in thermal cycling. Stabilisation with titanium and/or niobium ties up carbon and nitrogen and protects welds against intergranular corrosion.
The limits are toughness and formability in heavy sections: ferritic grades have a ductile-to-brittle transition, grain growth in the weld zone, and 475 °C embrittlement in the higher-chromium grades. They are therefore supplied mainly as sheet and light plate, and they are welded with low heat input.
How UNS S44600 compares with related grades
| Grade | Cr | Ni | Mo | N | PREN (min) | YS / Rp0.2 min, MPa |
|---|---|---|---|---|---|---|
| UNS S44600 | 23.0–27.0 | 0.75 max | — | 0.25 max | 23.0 | 275 |
| UNS S44100 | 17.5–19.5 | 1.00 max | — | 0.030 max | 17.5 | 241 |
| UNS S43940 | 17.5–18.5 | — | — | — | 17.5 | 250 |
| UNS S44100 | 17.5–19.5 | 1.00 max | — | 0.030 max | 17.5 | 241 |
| UNS S43940 | 17.5–18.5 | — | — | — | 17.5 | 250 |
Choose UNS S44600 when nickel-free cost, thermal-cycling behaviour or resistance to chloride stress-corrosion cracking matters more than toughness in heavy sections. It is not a good choice for heavy welded plate or for cryogenic service.
The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.
Heat treatment and delivery condition of UNS S44600
Heat treatment: anneal 760–1040 °C, rapid cooling.
Ferritic grades are annealed and cooled rapidly or in air; they are not hardenable by quenching. Avoid long holding in the 400–550 °C range, which causes 475 °C embrittlement in higher-chromium grades.
Surface finishes for UNS S44600 sheet
No.1 is hot-rolled, annealed and pickled, used for the 3–4.75 mm end of the sheet range. 2D is a dull cold-rolled, annealed and pickled finish that holds lubricant in deep drawing. 2B adds a light skin pass for a smoother, brighter surface and is the normal base for polishing. BA (bright annealed) and No.4 brushed finishes are available for many austenitic and ferritic grades by agreement. For highly alloyed grades, cold-rolled thin gauges are produced by fewer mills, so confirm the finish and gauge range before you fix a design.
Dimensions, tolerances and flatness
Thickness, width, length, flatness and camber tolerances follow ASTM A480/A480M. Cold-rolled sheet has tighter thickness tolerances than hot-rolled No.1 sheet. Higher-strength grades show more residual stress after slitting and laser cutting, so for laser blanks or long panels specify flatness and, where needed, tension-levelled material. Edge condition (mill or slit edge) and PVC film on one side should be stated on the order.
Ordering notes for A240 sheet. A240 refers to ASTM A480 for everything that is not grade-specific: definitions of sheet, strip and plate, dimensional tolerances, finishes, marking, retests and certification. A purchase order that says only “A240 S44600” therefore leaves several choices to the mill. State the finish (2B, 2D or No.1), the thickness tolerance basis, whether coil, slit coil or cut lengths are wanted, and whether the certificate must also show SA-240. If the sheet will be formed into vessel heads or pressure parts, say so, because some grades need specific heat-treatment records and supplementary tests that are only reported when requested. For export, also state the edition year if your specification fixes one; most mills certify to the current edition by default.
UNS S44600 sheet stock in China
| Thickness (mm) | Width (mm) | Length (mm) | Finish | Approx. quantity | Location |
|---|---|---|---|---|---|
| 0.5 | 1000 / 1219 | 2000 / 2438 | 2B | 100+ t | China |
| 0.8 | 1219 | 2438 | 2B | 100+ t | China |
| 1.0 | 1219 / 1250 | 2438 / 2500 | 2B | 100+ t | China |
| 1.5 | 1219 / 1500 | 2438 / 3000 | 2B | 100+ t | China |
| 2.0 | 1219 / 1500 | 2438 / 3000 | 2B | 100+ t | China |
| 3.0 | 1500 | 3000 | 2B / No.1 | 100+ t | China |
| 4.0 | 1500 | 3000 / 6000 | No.1 | 100+ t | China |
Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.
Packing and logistics. Sheet is packed on wooden or steel pallets with interleaving paper or PVC film, edge protectors and waterproof wrapping, typically 2–3 t per pallet. Coil is packed eye-to-wall or eye-to-sky with steel bands. We consolidate mixed grades and sizes into one container and send loading photos with the shipping documents.
UNS S44600 equivalents in other standards
| Standard | Designation | Comment |
|---|---|---|
| EN | 1.4749 X18CrN28 | nearest grade only; limits differ, check before substituting |
| GB/T | 16Cr25N (S12550) | same alloy family and limits closely matched; compare each limit on the certificate |
| JIS | SUH446 | same alloy family and limits closely matched; compare each limit on the certificate |
Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.
Related grades by alloy family
Ferritic
Nickel-free, magnetic grades for heat and mild corrosion: A240 S43000, A240 S43932, A240 S44400, A240 S40920, A240 S40910, A240 S40930, 1.4509 plate, 1.4512 plate, 1.4016 plate, 1.4510 plate, A240 S44100, A240 S43940.
Austenitic
General-purpose austenitic grades for comparison: 1.4303 plate.
Same grade, other specification
Applications, forming and welding of UNS S44600
Typical uses: furnace parts, burner nozzles, glass-mould parts, heat exchangers for sulfurous flue gases, and annealing boxes.
Ferritic sheet is formed cold; heavy gauges should be warmed to 100–200 °C before bending in cold weather. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a stabilised ferritic filler such as ER409Nb or ER430LNb, or an austenitic ER309L where weld ductility matters more than matching expansion. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.
Welding practice. Use low heat input and avoid preheat above about 200 °C to limit grain growth in the HAZ. Stabilised grades do not need post-weld heat treatment for corrosion resistance. Thin sheet is commonly joined by GTAW, plasma, laser or resistance welding. Cold forming should be done above room temperature for thicker gauges to avoid brittle fracture.
Certificates, testing and receiving inspection
Every delivery carries a mill certificate to ASTM A480/A480M with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: intergranular corrosion testing (ASTM A763 or equivalent), bend test, hardness, and PMI. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.
On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.
Common mistakes when specifying UNS S44600
- Ordering heavy plate for welded pressure parts, where toughness is limited.
- Assuming all ferritic grades are stabilised; check Ti and Nb on the certificate.
- Using a ferritic grade in hot chloride solutions without checking pitting resistance.
Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.
Sourcing UNS S44600: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Toughness of heavy gauges | thickness range agreed; bend tests on the heat |
| Weld-zone grain growth | low-heat-input welding advice and stabilised filler |
| Small quantities across many sizes | mixed thicknesses and grades combined in one shipment |
| Cutting and edge preparation | in-house shearing, plasma, laser and waterjet cutting, bevelling |
| Delivery delays | weekly production and shipping updates with photos |
How to order UNS S44600 sheet
State the standard and edition (ASTM A240/A240M), the grade (UNS S44600), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.
FAQ
-
Can I use A240 S44600 sheet for ASME Code equipment?
- Only if it is certified to SA-240 as well. Most mills dual-certify A240/SA-240; tell us when the sheet is for Code construction and we will supply dual-marked material with the certificate stating both.
-
Is UNS S44600 equivalent to EN 1.4749 X18CrN28?
- They are the nearest match, but limits differ; check each element and the property table before substituting.
-
Is UNS S44600 magnetic?
- Yes. Ferritic grades are magnetic in all conditions.
-
Can I order small quantities or cut sizes?
- Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
-
Which certificates and tests can you provide?
- Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.
Conclusion
UNS S44600 sheet should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.