ASTM A240 Type 410 Stainless Steel Sheet & Plate | 410 / UNS S41000 - SHH STEEL

ASTM A240 Type 410 Stainless Steel Sheet Plate

ASTM A240 Type 410 /UNS S41000 is a martensitic stainless steel containing approximately 12% chromium. It can be heat-treated to high hardness and strength while offering moderate corrosion resistance. Globally supplied by SHH STEEL.
Equivalent Grades:
UNS S41000 / EN 1.4006 / JIS SUS410 / GB 12Cr13
Product form:
Plate, Sheet, Coil, Strip, Foil, Shim, Circle, Ring
Surface:
No.1, 2B, 2D, BA, No.4, HL, 8K Mirror, Hairline
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

ASTM A240 Type 410 Stainless Steel Sheet & Plate | 410 / UNS S41000 - SHH STEEL

As a professional stainless steel supplier, SHH STEEL is pleased to present ASTM A240 Type 410 Stainless Steel Sheet and Plate. Also known as SS410 or UNS S41000, this grade is a basic martensitic stainless steel containing 11.5–13.5% chromium.

Type 410 is hardenable by heat treatment and can achieve high strength and hardness while providing moderate corrosion resistance in mildly corrosive environments. It is magnetic in both the annealed and hardened conditions. SHH STEEL supplies ASTM A240 Type 410 in both sheet and plate forms, covering thicknesses from 0.5 mm to 100 mm, with widths up to 2000–2500 mm and lengths up to 12000 mm. Custom sizes and surface finishes are available.

The material is typically delivered in the annealed condition with full Mill Test Certificates (EN 10204 3.1). Heat treatment (hardening and tempering) can be performed according to customer requirements. Whether for thin sheet fabrication or heavy plate applications, SHH STEEL provides consistent quality for engineering, valve, pump and general industrial projects worldwide.

Material Specification

ASTM A240 Type 410 stainless steel sheet and plate are manufactured in accordance with ASTM A240/A240M and ASME SA-240.

Specification Element Requirement SHH STEEL Compliance
Primary Standard ASTM A240 / ASME SA-240 Type 410 Full compliance
UNS Designation S41000 Confirmed
Product Form Sheet and Plate Both available
Thickness Range 0.5 mm – 100 mm Custom sizes available
Width / Length Up to 2000–2500 mm / 12000 mm Custom fabrication supported
Surface Finish 2B, No.1, BA, HL Multiple options
Heat Treatment Condition Annealed (hardenable) Standard supply condition
Certification EN 10204 3.1 / 3.2 Available

Chemical Composition

The chemical composition of ASTM A240 Type 410 is designed for hardenability and moderate corrosion resistance.

Element Content (%) Standard Limit Role
Carbon (C) 0.08 – 0.15 0.08 – 0.15 Enables hardening by heat treatment
Manganese (Mn) ≤ 1.00 1.00 max Deoxidation and strength
Phosphorus (P) ≤ 0.040 0.040 max Impurity control
Sulfur (S) ≤ 0.030 0.030 max Cleanliness
Silicon (Si) ≤ 1.00 1.00 max Deoxidation
Chromium (Cr) 11.5 – 13.5 11.5 – 13.5 Corrosion resistance
Nickel (Ni) ≤ 0.75 0.75 max —

Mechanical Properties

In the annealed condition, ASTM A240 Type 410 provides good formability. Higher strength and hardness can be achieved by hardening and tempering.

Property Value (Annealed) Test Method
Tensile Strength ≥ 450 – 515 MPa ASTM A370
Yield Strength (0.2% Offset) ≥ 205 – 290 MPa ASTM A370
Elongation in 50 mm ≥ 20% ASTM A370
Hardness ≤ 217 HB / ≤ 96 HRB ASTM E10/E18
Density 7.65 – 7.75 g/cm³ —

After hardening and tempering, hardness can typically reach 38–45 HRC depending on the heat treatment parameters.

Delivery Conditions

SHH STEEL supplies ASTM A240 Type 410 primarily in the annealed condition. Detailed capabilities by surface finish are as follows:

2B Finish (Cold-rolled, annealed, pickled and skin-passed)

  • Typical thickness range: 0.5 mm – 6.0 mm
  • Maximum width: up to 1500–2000 mm depending on thickness
  • Preferred for applications requiring a smooth surface and good formability.

No.1 Finish (Hot-rolled, annealed and pickled)

  • Typical thickness range: 3.0 mm – 100 mm
  • Maximum width: up to 2000–2500 mm
  • Standard finish for heavy plates used in engineering components and structural applications.

Other Finishes

  • BA (Bright Annealed) and HL (Hairline) available on request in limited thickness ranges.

Protective PVC film can be applied on one or both sides. Precision cutting (plasma, laser or waterjet) and closer dimensional tolerances are available upon request. Hardening and tempering heat treatment can be arranged according to customer specifications.

Tolerances

Dimensional tolerances for ASTM A240 Type 410 sheet and plate follow ASTM A480/A480M.

  • Thickness tolerances vary by product form and thickness.
  • Width tolerance is typically +6 mm / 0 mm.
  • Length tolerance for cut-to-length material is normally +10 mm / 0 mm.
  • Flatness is controlled according to ASTM A480; improved flatness can be supplied for precision fabrication.
  • Edge conditions include mill edge, slit edge, sheared edge or plasma/laser cut edge according to customer preference.

Tighter tolerances can be arranged for special projects.

Weldability

ASTM A240 Type 410 can be welded, but requires care due to its martensitic nature. Preheating (typically 150–250°C) and post-weld heat treatment (tempering) are often recommended to avoid cracking and restore ductility.

Matching or similar filler metals (e.g., ER410) or austenitic fillers (such as ER309L) may be used depending on the application. Controlled heat input and proper interpass temperature management are important. Welding procedures should be qualified according to the specific service requirements.

Equivalent Material Grades

Grade Standard Designation
Type 410 ASTM A240 / ASME SA-240 —
UNS S41000 Unified Numbering System —
1.4006 EN 10088 X12Cr13
SUS410 JIS G4304 / G4305 —
12Cr13 / 1Cr13 GB/T 20878 / GB/T 4237 Chinese National Standard
X12Cr13 DIN / EN —

Applications

ASTM A240 Type 410 is widely used where moderate corrosion resistance combined with high strength or hardness is required. Typical applications are shown below with relevant keywords:

Application Area Typical Components / Uses (Keywords)
Valves & Pumps Valve components, pump shafts, impellers – A240 410 Valve Pump
Cutlery & Kitchenware Knives, blades, utensils – A240 410 Cutlery
Petrochemical & Refining Refinery equipment, fasteners – A240 410 Petrochemical
General Engineering Shafts, spindles, bolts, nuts, springs – A240 410 Engineering
Mining & Mineral Processing Wear parts, screens – A240 410 Mining
Automotive & Machinery Components requiring strength and moderate corrosion resistance – A240 410 Automotive
Heat Treatment Equipment Parts requiring hardenability – A240 410 Heat Treatment

Why Choose SHH STEEL

SHH STEEL maintains long-term strategic cooperation with major Chinese stainless steel mills and acts as a first-level (primary) agent for these mills. This direct partnership enables us to offer competitive pricing advantages, faster delivery times and consistent quality assurance that many intermediate traders cannot match.

All ASTM A240 Type 410 material is sourced from reputable Chinese mills under strict quality control, supplied with complete Mill Test Certificates, and supported by our professional export team. Customers benefit from reliable supply, short lead times, technical support and cost-effective solutions for engineering and industrial applications worldwide.

FAQ

What is the main characteristic of Type 410 compared with 304 or 316?
Type 410 is a martensitic stainless steel that can be hardened by heat treatment to achieve high strength and hardness. Types 304 and 316 are austenitic and non-hardenable by heat treatment. Type 410 has lower corrosion resistance than 304/316 but higher attainable strength.
Is Type 410 magnetic?
Yes. Type 410 is magnetic in both the annealed and hardened conditions.
What are the equivalent grades of ASTM A240 Type 410?
Common equivalents include UNS S41000, EN 1.4006 (X12Cr13), JIS SUS410 and Chinese 12Cr13 (1Cr13).
What is the density of ASTM A240 Type 410?
Approximately 7.65 – 7.75 g/cm³.
Can Type 410 be heat treated?
Yes. Type 410 is hardenable by quenching and tempering. Maximum hardness typically reaches 38–45 HRC depending on the heat treatment cycle.

Conclusion

ASTM A240 Type 410 Stainless Steel Sheet and Plate from SHH STEEL provide a cost-effective combination of moderate corrosion resistance and high attainable strength through heat treatment. With strict quality control, flexible sizing options, competitive pricing through direct mill partnerships and professional global export service, we deliver trusted solutions for valves, pumps, cutlery, engineering and industrial applications worldwide.

Contact SHH STEEL today for your ASTM A240 Type 410 requirements.

Keywords: ASTM A240 410, ASTM A240 Type 410, 410 stainless steel plate, 410 stainless steel sheet, SS410, UNS S41000, 1.4006, SUS410, martensitic stainless steel plate

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X