GOST 22178 VT5-1 Titanium Sheet | Ti-Al-Sn Alloy (BT5-1)

GOST 22178 VT5-1 titanium sheet is Ti-Al-Sn alloy (BT5-1) supplied annealed. It is specified for 735 MPa minimum tensile strength and 15% minimum elongation. Typical uses include elevated-temperature welded sheet structures. Equivalents are confirmed against the ordered edition. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
GOST 22178 VT5-1 titanium sheet, VT5-1 titanium sheet, Ti-Al-Sn alloy (BT5-1) sheet, GOST 22178 titanium plate, GOST 22178 VT5-1 titanium strip
Equivalent Grades:
UNS R54520, ASTM B265 Gr.6, ASME SB-265 Gr.6, GB/T TA7, 3.7115
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is GOST 22178 VT5-1 titanium sheet?

GOST 22178 VT5-1 titanium sheet is made to GOST 22178, the interstate standard for sheets of titanium and titanium alloys. VT5-1 is a Ti-Al-Sn all-alpha alloy (about 5% aluminium, 2.5% tin) comparable in role to ASTM Grade 6 and the Chinese TA7. It is weldable and keeps strength at elevated and cryogenic temperatures.

This is an alpha or near-alpha titanium alloy. Aluminium (and in some grades tin or zirconium) strengthens the alpha phase, while only small amounts of beta stabilisers such as manganese, molybdenum or vanadium are present. Such alloys keep good weldability and creep strength at elevated temperature, are normally used annealed, and respond little to strengthening heat treatment.

Its typical density of about 4.48 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

Russian designations follow the original VT (BT in Cyrillic) and OT naming. VT1-00 and VT1-0 are unalloyed titanium, OT4 grades are Ti-Al-Mn alloys, and VT5-1, VT6, VT14 and VT20 are structural alloys used widely in aerospace sheet work.

SHH STEEL handles VT5-1 sheet enquiries within its range of titanium alloy plates and sheets, checking the ordered GOST 22178 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 6, ASME SB-265 Grade 6, GB/T 3621 TA7.

Material specification for GOST 22178 VT5-1

GOST 22178 is the interstate standard for sheets of titanium and titanium alloys. It covers sheets from 0.3 to 10.5 mm thick, sets sizes, tolerances, surface quality groups and mechanical properties, and refers chemical composition to GOST 19807 or OST 1 90013. Because the standard covers sheet, this page uses the term titanium sheet.

Ordering item GOST 22178 basis
Standard GOST 22178-76 with its amendments; state the revision required
Grade VT5-1 (Ti-Al-Sn Alloy (BT5-1))
Size range for this grade 0.8–10.5 mm thick
Condition Annealed
Surface finish Ordinary or high surface finish; improved flatness on request
Designation example Sheet VT5-1 5 × 1000 × 1500 GOST 22178-76
Certificate Quality document with chemistry and test results

Width and length tolerances are plus-only: up to +10 mm on width for sheets up to 1500 mm long and up to +20 mm on length for sheets up to 2000 mm long. Order the grade, thickness, width, length, surface finish group and flatness class.

Many Russian aerospace orders cite OST 1 90013 for chemistry or add supplementary technical conditions to GOST 22178. If the drawing names such documents, list them on the order, because they can change impurity limits, test frequency and acceptance criteria. When sheet is bought for use outside the CIS, agree in advance whether a GOST certificate alone is acceptable or a cross-reference to another standard is required.

Chemical composition of GOST 22178 VT5-1

Composition follows GOST 19807 for the grade. Single values are maximums; titanium is the balance.

Element Limit, %
Nitrogen (N) 0.05 max
Carbon (C) 0.10 max
Hydrogen (H) 0.015 max
Iron (Fe) 0.30 max
Oxygen (O) 0.15 max
Aluminium (Al) 4.3–6.0
Vanadium (V) 1.0 max
Tin (Sn) 2.0–3.0
Zirconium (Zr) 0.30 max
Silicon (Si) 0.12 max
Other impurities, total 0.30 max
Titanium (Ti) Balance

Alloying ranges are wider than in some Western specifications, so a sheet can meet GOST 19807 and still fall outside another standard’s range. Where an order cites both GOST and another standard, both sets of limits must be satisfied.

Mechanical properties of GOST 22178 VT5-1

The values below are the requirements for VT5-1 sheet in the annealed condition.

Sheet thickness, mm (condition) Tensile strength, MPa Elongation, min, %
0.8–1.2 735 min 15
>1.2–1.8 735 min 12
>1.8–6.0 735 min 10
6.0–10.5 735 min 8

GOST 22178 sets minimum tensile strength and elongation; yield strength is not specified and can be agreed separately. Tests are made on transverse specimens. The bend test is made around a mandrel, and the sheet must reach the minimum angle below without cracks.

Sheet thickness, mm Bend angle, min
0.8–1.2 60°
>1.2–1.8 50°
>1.8–10.5 40°

Where sheets are quenched and aged, the properties of heat-treated samples are agreed when ordering.

Delivery condition, finish and marking

GOST 22178 sheets are supplied with an ordinary or high surface finish. Light dressing of surface defects is allowed within the depth limits of the standard, and the angles of the sheet must stay within the flatness requirement for the ordered class.

  • Condition: Annealed
  • Surface: ordinary or high surface finish group, as ordered
  • Flatness: normal or improved, as ordered
  • Marking and packing: grade, heat, sheet size and standard number, with protection for transport

The alloy is supplied annealed; stress relieving after forming or welding is agreed with the purchaser. Mechanical tests are made on 10% of the sheets in a lot, but not fewer than one sheet, and the lot is accepted or retested on the results.

Welding and fabrication of VT5-1 titanium sheet

VT5-1 is weldable by gas tungsten arc, plasma arc, electron beam and laser processes, provided the weld zone is fully shielded from air.

  • Use trailing shields and back purging until the weld cools below about 400 °C
  • Use matching or engineer-approved filler metal and qualified procedures
  • Clean joints and filler wire; remove oil, moisture and iron contamination
  • Consider post-weld stress relief for highly restrained or precision parts, as agreed in the procedure

Room-temperature formability is lower than for CP titanium. Moderate bends can be cold formed with generous radii, but severe shapes are normally hot formed or creep formed.

Machining needs sharp carbide tools, rigid set-ups, low cutting speeds and generous coolant, because titanium alloys conduct heat poorly and the heat stays at the cutting edge. Avoid dwelling, which work-hardens the surface, and keep fine chips away from ignition sources.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

GOST 22178 sets thickness tolerances in Table 1 by thickness and width, and flatness and corner-gap limits in Table 5 by grade and flatness class. Width tolerance is up to +10 mm for sheets up to 1500 mm long and +15 mm above that; length tolerance is +20 mm up to 2000 mm and +25 mm above.

Order the thickness, width, length, surface finish group and flatness class. Theoretical sheet mass is based on 4.50 g/cm³ for VT1-00 and VT1-0, with conversion factors for the alloys. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of VT5-1 titanium sheet

Typical uses of VT5-1 sheet include:

  • Elevated-temperature welded sheet structures
  • Cryogenic tanks and components
  • Engine casings and ducting
  • Heat-exposed formed parts

As with all titanium, the alloy is not suited to hydrofluoric acid, fluoride-bearing media, dry chlorine or red fuming nitric acid. High-aluminium alloys can be sensitive to hot-salt stress corrosion, and maximum service temperatures depend on the alloy and design code. The design engineer must confirm suitability for the actual service.

When selecting VT5-1, compare it with VT6, VT6S, VT14. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare VT5-1 with other GOST 22178 grades

The grades below are the closest neighbours of VT5-1 in GOST 22178. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
VT5-1 735 MPa min (>1.8–6.0 mm) — 10% Ti-5Al-2.5Sn alpha alloy
VT6 885 MPa min (1.0–10.5 mm) — 8% Ti-6Al-4V alpha-beta
VT6S 835 MPa min (1.0–6.0 mm) — 12% Ti-6Al-4V lower-interstitial variant
VT14 885 MPa min (0.8–5.0 mm) — 8% Ti-4.5Al-3Mo-1V heat-treatable
VT20 930 MPa min (>1.8–4.0 mm) — 10% Ti-6Al-2Zr-1Mo-1V near-alpha

Alpha and near-alpha alloys trade formability for strength and elevated-temperature performance. Compare the full requirements, not only tensile strength, before changing grade.

GOST 22178 VT5-1 equivalent grades

The designations below are commonly compared with GOST 22178 VT5-1. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to GOST 22178 VT5-1
ASTM B265 Grade 6 Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 6 ASME Code version of the ASTM grade; ordered for pressure equipment
GB/T 3621 TA7 Close equivalent; confirm grade name and limits in the ordered edition
UNS R54520 Same unified number as ASTM Grade 6
DIN / EN material number 3.7115 (TiAl5Sn2.5) Close equivalent

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for VT5-1 titanium sheet

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to GOST 22178 VT5-1 sheet with the surface finish group and flatness you need
  • Certificates are checked against GOST 19807 chemistry, tensile strength, elongation and bend angle
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for GOST 22178 VT5-1 sheet

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material GOST 22178 VT5-1, revision
Product form Sheet 0.3–10.5 mm; surface finish group and flatness class
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Bend test, any quenched-and-aged tests where applicable
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Why is GOST 22178 VT5-1 called sheet rather than plate?
GOST 22178 covers sheets from 0.3 to 10.5 mm thick. Thicker plate in Russian grades is ordered to other GOST or OST documents, so this page uses the term sheet.
What is the tensile strength of GOST 22178 VT5-1 titanium sheet?
The requirement is 735 MPa minimum. Minimum elongation is 15%. Values apply to the condition and thickness range stated in the standard.
What is VT5-1 mainly used for?
Typical uses include elevated-temperature welded sheet structures, cryogenic tanks and components and engine casings and ducting. The design engineer should confirm the grade for the actual service.
What thickness range applies to GOST 22178 VT5-1?
For this grade the standard lists 0.8–10.5 mm thick. Width and length depend on thickness, so confirm the full sheet size against the standard's size table when ordering.
What should I send for a quotation?
Send GOST 22178 VT5-1, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for GOST 22178 VT5-1 titanium sheet

GOST 22178 VT5-1 is Ti-Al-Sn alloy (BT5-1) specified for 735 MPa minimum tensile strength and 15% minimum elongation in the annealed condition. Typical uses include elevated-temperature welded sheet structures and cryogenic tanks and components.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the GOST 22178 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X