EN 10297-2 1.4876 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4876 Seamless Stainless Steel Tube

EN 10297-2 1.4876 / X10NiCrAlTi32-21 seamless stainless general-purpose tube (800H / Alloy 800-class), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 170 MPa, Rm min 450 MPa, A long. min 28%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4876 / X10NiCrAlTi32-21 (800H / Alloy 800-class — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4876 Seamless Stainless Steel Tube

Mechanical and general engineering projects that need seamless stainless tube under a European product standard look to EN 10297-2:2005 — Part 2 of EN 10297 — rather than a PED pressure Part 5 page or an ASTM tubing habit alone. 1.4876 / X10NiCrAlTi32-21 sits in the austenitic heat-resisting tables. 1.4876 is the EN 10297-2 heat-resisting home for X10NiCrAlTi32-21 — lock whether 800 vs 800H carbon practice is required on the order text. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Mill path for 1.4876: specialty heat-service seamless OD. SHH STEEL can make and supply EN 10297-2 1.4876 / X10NiCrAlTi32-21 as seamless general-purpose tube across specialty heat-service seamless OD, solution annealed or annealed/QT as the grade tables require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Use thread: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families.

On the shop floor people still say “800H / Alloy 800-class tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4876, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service. Typical duties include petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families. Design caution: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558. Caution thread: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558.

Scope discipline matters: 1.4876 under EN 10297-2 is seamless general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Role reminder for 1.4876: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Inside this seamless general-purpose series, compare EN 10297-2 1.4558, EN 10297-2 1.4854, EN 10297-2 1.4845. Hub: EN 10297-2. Related pressure seamless chemistry page: EN 10216-5 1.4558.

Chemical Composition of EN 10297-2 1.4876

Cast window focus for 1.4876: Every 1.4876 heat under EN 10297-2 must meet the cast (ladle) analysis for X10NiCrAlTi32-21 in the austenitic heat-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 800H / Alloy 800-class is body text only. Corrosion thread: high Ni-Cr with Ti-Al for oxidising and many petrochemical heat duties.

For 1.4876 / X10NiCrAlTi32-21, the following chem table is the public EN 10297-2 window SHH STEEL uses at enquiry. Product-analysis Options, when taken, apply the standard’s permitted deviations rather than inventing tighter shop limits. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Steel C Si Mn P S Cr Ni Ti Al
1.4876 / X10NiCrAlTi32-21 ≤0.12 ≤1.00 ≤2.00 ≤0.030 ≤0.015 19.0–23.0 30.0–34.0 0.15–0.60 0.15–0.60

Mechanical Properties of EN 10297-2 1.4876

Ambient floors focus for 1.4876: Table mechanical floors for 1.4876 / X10NiCrAlTi32-21 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 170 MPa, Rp1.0 min 210 MPa, Rm min 450 MPa, longitudinal elongation min 28%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Family: austenitic heat-resisting. Caution thread: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 170 210 450 min 28 30 –

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4876 / X10NiCrAlTi32-21. Guideline solution/anneal band (Annex B): 1050–1150 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4876

Seamless route narrative for 1.4876: EN 10297-2 does not offer a welded route for 1.4876. Tube in X10NiCrAlTi32-21 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Annex A process-route symbols for seamless 1.4876 include HFD (hot finished, heat treated, descaled), CFD (cold finished, heat treated, descaled), CFA (cold finished bright annealed), CFG (ground), and CFP (polished). Combinations may be agreed at enquiry. Weld thread: matching Alloy 800-class fillers; solution anneal after hot work as required.

For austenitic 1.4876, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4876 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1050–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

When dual documentation against EN 10216-5 is requested for the same 1.4876 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 1.4876: specialty heat-service seamless OD. Use thread: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families.

Dimensions and Tolerances for EN 10297-2 1.4876

Dimensional order line for 1.4876: Dimensional orders for 1.4876 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Specialty heat-service seamless od. Use thread: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families.

Length supply for 1.4876 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Size hint for 1.4876: specialty heat-service seamless OD. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Equivalent Grades for EN 10297-2 1.4876

Equivalence talk for 1.4876 starts with X10NiCrAlTi32-21: 1.4876 / X10NiCrAlTi32-21 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 800H / Alloy 800-class appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4558, 1.4854, 1.4845. Hook for buyers still using only the 800H / Alloy 800-class alias: lock EN 10297-2 1.4876 on the order line. Caution thread: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558.

Heat Treatment and Delivery Condition for EN 10297-2 1.4876

Austenitic 1.4876 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1050–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching Alloy 800-class fillers; solution anneal after hot work as required.

Fabrication HT reminder for 1.4876 (+AT): For 1.4876, purchasers who need verified IGC after fabrication should say so with the applicable Option and method (EN ISO 3651-2 framing). Mill +AT or +A of the tube does not automatically clear a fabricator’s as-welded joint without procedure control. Delivery framing on the certificate for 1.4876 should match +AT. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Corrosion Resistance of EN 10297-2 1.4876

Corrosion behaviour of EN 10297-2 1.4876 tracks its austenitic heat-resisting balance: high Ni-Cr with Ti-Al for oxidising and many petrochemical heat duties. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558 Corrosion thread: high Ni-Cr with Ti-Al for oxidising and many petrochemical heat duties.

Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4558, 1.4854, 1.4845 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4876 is austenitic heat-resisting. Caution thread: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558.

Applications of EN 10297-2 1.4876 Tube

Applications of EN 10297-2 1.4876 tube centre on mechanical and general engineering rather than PED pressure shells: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families. Role summary: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families.

Typical BOM language pairs EN 10297-2 1.4876 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “800H / Alloy 800-class” substitutions do not creep in. Primary application sketch: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Weldability of EN 10297-2 1.4876

1.4876 / X10NiCrAlTi32-21 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching Alloy 800-class fillers; solution anneal after hot work as required. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching Alloy 800-class fillers; solution anneal after hot work as required.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558 Filler/shop note for 1.4876: matching Alloy 800-class fillers; solution anneal after hot work as required. Caution thread: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558.

Surface Finishes for EN 10297-2 1.4876

Finish selection for 1.4876 on Annex A: For 1.4876, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 800H / Alloy 800-class, but the finish symbol still belongs on the EN 10297-2 line. Use thread: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families.

Transit protection for 1.4876 is sized to the Annex A finish: heavier wrap for CFA/CFG/CFP, standard export wrap for HFD/CFD. Open-deck ocean exposure without wrap is refused on bright tube. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Inspection and Testing for EN 10297-2 1.4876

Inspection lot framing for 1.4876 in austenitic heat-resisting: SHH STEEL EN 10204 3.1 documents for 1.4876 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4876 heat identity intact from cast through bundle tag. Weld thread: matching Alloy 800-class fillers; solution anneal after hot work as required.

Purchasers who need witness points on 1.4876 should say so at enquiry. Routine mill inspection still records cast chemistry, tensile results, delivery condition, and dimensions; witness adds scheduling, not a different chemistry table. Use thread: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families.

Packaging and Shipping for EN 10297-2 1.4876

Dispatch note for 1.4876 (800H / Alloy 800-class body alias only): Export packing for 1.4876 / X10NiCrAlTi32-21 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavy HFD bundles use spacers to stop fretting in transit. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Marking and identity for 1.4876: For 1.4876, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Finish-sensitive packing for 1.4876 follows the Annex A symbol on the order. Use thread: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families.

Ocean containers loaded with 1.4876 use desiccant and sealed wrap when the route or season warrants it. Inland deliveries may omit container desiccant but never omit end caps on precision OD. Caution thread: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558.

Why Choose SHH STEEL

Why 1.4876 with SHH STEEL — role: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service. SHH STEEL can produce and supply X10NiCrAlTi32-21 as EN 10297-2 1.4876 seamless tube with honest scope boundaries. General engineering seamless acceptance is what this page sells; pressure, welded-pressure, and welded-general-purpose sisters are separate standards with separate MTCs. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Grade advice stays practical for 1.4876. If the duty needs a sister chemistry, we point to 1.4558, 1.4854, 1.4845. Design caution for this number: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558 Technical clarification on QT level, cold- versus hot-finished rows, or duplex thin-wall footnotes happens before acknowledgement. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558.

Supply Capability

For 1.4876, SHH STEEL can produce and supply seamless tube in the X10NiCrAlTi32-21 analysis with the Annex A finish you name. Lead time tracks hollow stock and heat-treatment slots; Stock / Available sizes below helps size the first RFQ. Use thread: petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4876 / X10NiCrAlTi32-21
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Available sizes for 1.4876 follow seamless general-purpose practice: specialty heat-service seamless OD. Dual size lists against sister grades are welcome on one enquiry sheet. Duty thread: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.

Dual documentation talk for 1.4876 versus 1.4558, 1.4854, 1.4845 is fine at enquiry — each steel number still needs its own cast compliance. SHH STEEL can produce and supply staged deliveries by size priority. Weld thread: matching Alloy 800-class fillers; solution anneal after hot work as required.

FAQ

What is EN 10297-2 1.4876 seamless stainless steel tube used for?
EN 10297-2 1.4876 (X10NiCrAlTi32-21) is seamless tube for mechanical and general engineering — petrochemical furnace-adjacent tubing, steam-hydrocarbon reformer-adjacent mechanical parts, and high-temp process lines naming Alloy 800/800H chemistry families. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service.
Is EN 10297-2 1.4876 the same as EN 10216-5 1.4876?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4876 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4876 / X10NiCrAlTi32-21?
Delivery framing for 1.4876 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1050–1150 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4876?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4876 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4876 compare with sister grades 1.4558, 1.4854, 1.4845?
1.4876 / X10NiCrAlTi32-21 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4558, 1.4854, 1.4845. Design caution: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558 Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4876 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching Alloy 800-class fillers; solution anneal after hot work as required. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4876?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4876?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4876 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty heat-service seamless OD. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 800H / Alloy 800-class belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 800H / Alloy 800-class in body text and BOM notes, but lock EN 10297-2 and 1.4876 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4876?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: C/Ti/Al windows and heat-resisting Table 9 apply — distinguish from corrosion-resisting 1.4558 Sister pointers: 1.4558, 1.4854, 1.4845. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4876 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4876 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4876 (X10NiCrAlTi32-21) is seamless stainless tube for mechanical and general engineering — Alloy 800-class austenitic heat-resisting seamless tube with Ti-Al for high-temperature mechanical service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4558, 1.4854, 1.4845. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X