EN 10297-2 1.4547 Seamless Stainless Steel Tube
What is EN 10297-2 1.4547 Seamless Stainless Steel Tube
If the purchase file still names only a commercial alias such as 254 SMO / S31254 without a product standard, the mill cannot know whether general-purpose seamless acceptance or pressure-tube acceptance applies. EN 10297-2 plus steel number 1.4547 (X1CrNiMoCuN20-18-7) selects seamless tube for mechanical and general engineering. 1.4547 is the EN 10297-2 6Mo superaustenitic seamless number — not a casual dual of 1.4439 or 904L. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Mill path for 1.4547: specialty seamless OD on mill enquiry. SHH STEEL can produce and supply X1CrNiMoCuN20-18-7 under EN 10297-2 1.4547 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties.
On the shop floor people still say “254 SMO / S31254 tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4547, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service. Typical duties include seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties. Design caution: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work. Caution thread: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work.
EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4547: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Inside this seamless general-purpose series, compare EN 10297-2 1.4529, EN 10297-2 1.4539, EN 10297-2 1.4439, EN 10297-2 1.4410. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4547.
Chemical Composition of EN 10297-2 1.4547
Cast window focus for 1.4547: Every 1.4547 heat under EN 10297-2 must meet the cast (ladle) analysis for X1CrNiMoCuN20-18-7 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 254 SMO / S31254 is body text only. Corrosion thread: ~6% Mo plus Cu and N for severe pitting/crevice chloride environments.
The composition table that follows lists public BSSA EN 10297-2 cast limits for 1.4547 / X1CrNiMoCuN20-18-7. Treat secondary web catalogues as non-contractual; the purchased EN 10297-2:2005 text wins if anything conflicts. Ranges are shown where the standard publishes min/max rather than a single maximum. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
| Steel | C | Si | Mn | P | S | Cr | Mo | Ni | Cu | N |
|---|---|---|---|---|---|---|---|---|---|---|
| 1.4547 / X1CrNiMoCuN20-18-7 | ≤0.020 | ≤0.70 | ≤1.00 | ≤0.030 | ≤0.010 | 19.5–20.5 | 6.0–7.0 | 17.5–18.5 | 0.50–1.00 | 0.18–0.25 |
Mechanical Properties of EN 10297-2 1.4547
Ambient floors focus for 1.4547: Table mechanical floors for 1.4547 / X1CrNiMoCuN20-18-7 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 300 MPa, Rp1.0 min 340 MPa, Rm min 650 MPa, longitudinal elongation min 35%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Family: austenitic corrosion-resisting. Caution thread: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 300 | 340 | 650 min | 35 | 30 | Yes |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4547 / X1CrNiMoCuN20-18-7. Guideline solution/anneal band (Annex B): 1140–1200 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4547
Seamless route narrative for 1.4547: EN 10297-2 does not offer a welded route for 1.4547. Tube in X1CrNiMoCuN20-18-7 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Annex A process-route symbols for seamless 1.4547 include HFD (hot finished, heat treated, descaled), CFD (cold finished, heat treated, descaled), CFA (cold finished bright annealed), CFG (ground), and CFP (polished). Combinations may be agreed at enquiry. Weld thread: matching 6Mo fillers; nickel over-alloyed consumables common; rapid cool from solution anneal.
For austenitic 1.4547, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4547 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1140–1200 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4547. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4547: specialty seamless OD on mill enquiry. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties.
Dimensions and Tolerances for EN 10297-2 1.4547
Dimensional order line for 1.4547: Order EN 10297-2 1.4547 by outside diameter D and wall thickness T for steel name X1CrNiMoCuN20-18-7. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Specialty seamless od on mill enquiry. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties.
Length supply for 1.4547 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Size hint for 1.4547: specialty seamless OD on mill enquiry. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Equivalent Grades for EN 10297-2 1.4547
Equivalence talk for 1.4547 starts with X1CrNiMoCuN20-18-7: 1.4547 / X1CrNiMoCuN20-18-7 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 254 SMO / S31254 appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4529, 1.4539, 1.4439, 1.4410. Hook for buyers still using only the 254 SMO / S31254 alias: lock EN 10297-2 1.4547 on the order line. Caution thread: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work.
Heat Treatment and Delivery Condition for EN 10297-2 1.4547
Austenitic 1.4547 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1140–1200 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching 6Mo fillers; nickel over-alloyed consumables common; rapid cool from solution anneal.
Fabrication HT reminder for 1.4547 (+AT): Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4547, restore the delivery condition agreed on the order before corrosive or load-bearing service. Delivery framing on the certificate for 1.4547 should match +AT. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Corrosion Resistance of EN 10297-2 1.4547
Corrosion behaviour of EN 10297-2 1.4547 tracks its austenitic corrosion-resisting balance: ~6% Mo plus Cu and N for severe pitting/crevice chloride environments. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work Corrosion thread: ~6% Mo plus Cu and N for severe pitting/crevice chloride environments.
For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4547 is filed as austenitic corrosion-resisting — pick tests that match that filing. Family filing for 1.4547 is austenitic corrosion-resisting. Caution thread: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work.
Applications of EN 10297-2 1.4547 Tube
Applications of EN 10297-2 1.4547 tube centre on mechanical and general engineering rather than PED pressure shells: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties. Role summary: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties.
Skip 1.4547 when the specification locks a different family — for example forcing ferritic 1.4547 into severe chloride process duty, or forcing a free-machining grade into welded corrosive service. Sister conversation inside EN 10297-2: 1.4529, 1.4539, 1.4439, 1.4410. Primary application sketch: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Weldability of EN 10297-2 1.4547
1.4547 / X1CrNiMoCuN20-18-7 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching 6Mo fillers; nickel over-alloyed consumables common; rapid cool from solution anneal. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching 6Mo fillers; nickel over-alloyed consumables common; rapid cool from solution anneal.
Filler selection should match or over-alloy the base X1CrNiMoCuN20-18-7 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, martensitic, duplex, or heat-resisting — not a single shop habit. Filler/shop note for 1.4547: matching 6Mo fillers; nickel over-alloyed consumables common; rapid cool from solution anneal. Caution thread: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work.
Surface Finishes for EN 10297-2 1.4547
Finish selection for 1.4547 on Annex A: For 1.4547, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 254 SMO / S31254, but the finish symbol still belongs on the EN 10297-2 line. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties.
Protective agreements for 1.4547 cover sleeved bright tube, desiccant in sealed crates on long ocean routes, and dry indoor storage after arrival. Polished CFP surfaces ship with non-metallic rub strips so bundle-to-bundle contact cannot print fretting marks. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Inspection and Testing for EN 10297-2 1.4547
Inspection lot framing for 1.4547 in austenitic corrosion-resisting: SHH STEEL EN 10204 3.1 documents for 1.4547 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4547 heat identity intact from cast through bundle tag. Weld thread: matching 6Mo fillers; nickel over-alloyed consumables common; rapid cool from solution anneal.
When EN ISO 3651-2 IGC is ordered on 1.4547, the method letter and acceptance sit on the Option line and the MTC. Hardness, flattening, ring expanding, or drift tests run only when invoked. Marking carries manufacturer identity, OD × wall, EN 10297-2, 1.4547 or the steel name, cast/code, and inspection correlation. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties.
Packaging and Shipping for EN 10297-2 1.4547
Dispatch note for 1.4547 (254 SMO / S31254 body alias only): Finished EN 10297-2 1.4547 (X1CrNiMoCuN20-18-7) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Marking and identity for 1.4547: When cut lengths and special ends are part of the 1.4547 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Finish-sensitive packing for 1.4547 follows the Annex A symbol on the order. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties.
Bundle cards for 1.4547 repeat the heat identity used on the EN 10204 3.1 certificate. SHH STEEL can email packing photos before sailing when the project file needs them, and will re-pack if a bright finish shows transit rub before handover. Caution thread: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work.
Why Choose SHH STEEL
Why 1.4547 with SHH STEEL — role: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service. SHH STEEL can produce and supply EN 10297-2 1.4547 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “254 SMO / S31254 tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Grade advice stays practical for 1.4547. If the duty needs a sister chemistry, we point to 1.4529, 1.4539, 1.4439, 1.4410. Design caution for this number: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work We answer medium questions with sister pointers rather than overselling a single chemistry. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work.
Supply Capability
SHH STEEL can produce and supply EN 10297-2 1.4547 seamless tube to the edition, delivery condition, Annex A symbol, and Options on your enquiry. Capability and Stock / Available sizes notes below are a first-pass map for X1CrNiMoCuN20-18-7, not a promise of frozen tonnage. Use thread: seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4547 / X1CrNiMoCuN20-18-7 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Stock / Available sizes for EN 10297-2 1.4547: enquiry band commonly spans instrumentation-to-process OD with walls suited to this grade. This is not a frozen SKU tonnage table — heat availability of X1CrNiMoCuN20-18-7 and finishing slots for the Annex A symbol set the real promise date. Size context: specialty seamless OD on mill enquiry. Duty thread: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
Cut lengths, bevels or special ends, IGC Options, and dual RFQs against 1.4529, 1.4539, 1.4439, 1.4410 are routine for 1.4547. Catalogue charts only sanity-check OD × wall — contractual acceptance stays with EN 10297-2. SHH STEEL can produce and supply pilot lengths when the schedule allows. Weld thread: matching 6Mo fillers; nickel over-alloyed consumables common; rapid cool from solution anneal.
FAQ
-
What is EN 10297-2 1.4547 seamless stainless steel tube used for?
- EN 10297-2 1.4547 (X1CrNiMoCuN20-18-7) is seamless tube for mechanical and general engineering — seawater cooling mechanical lines, flue-gas and scrubber-adjacent tubing, and halide process duties. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service.
-
Is EN 10297-2 1.4547 the same as EN 10216-5 1.4547?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4547 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4547 / X1CrNiMoCuN20-18-7?
- Delivery framing for 1.4547 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1140–1200 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4547?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4547 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4547 compare with sister grades 1.4529, 1.4539, 1.4439?
- 1.4547 / X1CrNiMoCuN20-18-7 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4529, 1.4539, 1.4439. Design caution: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4547 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching 6Mo fillers; nickel over-alloyed consumables common; rapid cool from solution anneal. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4547?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4547?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4547 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty seamless OD on mill enquiry. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 254 SMO / S31254 belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 254 SMO / S31254 in body text and BOM notes, but lock EN 10297-2 and 1.4547 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4547?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: solution-anneal band is high (1140–1200 °C guidance) — fabricator HT must match; do not under-anneal after hot work Sister pointers: 1.4529, 1.4539, 1.4439. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4547 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4547 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4547 (X1CrNiMoCuN20-18-7) is seamless stainless tube for mechanical and general engineering — 6Mo superaustenitic seamless tube (254 SMO-class) for severe seawater and halide mechanical service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4529, 1.4539, 1.4439. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.