EN 10297-2 1.4429 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4429 Seamless Stainless Steel Tube

EN 10297-2 1.4429 / X2CrNiMoN17-13-3 seamless stainless general-purpose tube (316LN), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 295 MPa, Rm min 580 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4429 / X2CrNiMoN17-13-3 (316LN — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4429 Seamless Stainless Steel Tube

EN 10297-2 covers seamless stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4429 is the austenitic corrosion-resisting grade X2CrNiMoN17-13-3, commercially discussed as 316LN. When 1.4404’s proof floor is short but the medium still wants Mo austenitic seamless tube, 1.4429 is the EN 10297-2 nitrogen path. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Mill path for 1.4429: same OD conversation as 1.4404 with higher Rp/Rm on the MTC. SHH STEEL can make and supply EN 10297-2 1.4429 / X2CrNiMoN17-13-3 as seamless general-purpose tube across same OD conversation as 1.4404 with higher Rp/Rm on the MTC, solution annealed or annealed/QT as the grade tables require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects.

On the shop floor people still say “316LN tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4429, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. Typical duties include higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects. Design caution: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up. Caution thread: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up.

Scope discipline matters: 1.4429 under EN 10297-2 is seamless general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Role reminder for 1.4429: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Inside this seamless general-purpose series, compare EN 10297-2 1.4435, EN 10297-2 1.4404, EN 10297-2 1.4439, EN 10297-2 1.4311. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4429. ASTM/ASME related product pages (not interchangeable by default): A269 TP316L.

Chemical Composition of EN 10297-2 1.4429

Cast window focus for 1.4429: Buying 316LN-family seamless tube without locking 1.4429 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X2CrNiMoN17-13-3; highlight elements for this grade include C ≤0.030, Cr 16.5–18.5, Ni 11.0–15.0, Mo 2.50–3.00, N 0.12–0.22, Si ≤1.00. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 316LN is body text only. Corrosion thread: Mo plus nitrogen; pitting resistance above lean 316L with interstitial strengthening.

The composition table that follows lists public BSSA EN 10297-2 cast limits for 1.4429 / X2CrNiMoN17-13-3. Treat secondary web catalogues as non-contractual; the purchased EN 10297-2:2005 text wins if anything conflicts. Ranges are shown where the standard publishes min/max rather than a single maximum. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Steel C Si Mn P S Cr Mo Ni N
1.4429 / X2CrNiMoN17-13-3 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 16.5–18.5 2.50–3.00 11.0–15.0 0.12–0.22

Mechanical Properties of EN 10297-2 1.4429

Ambient floors focus for 1.4429: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4429 order. General-purpose Table values for this number read: Rp0.2 min 295 MPa, Rp1.0 min 330 MPa, Rm min 580 MPa, longitudinal elongation min 35%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic corrosion-resisting. Caution thread: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 295 330 580 min 35 30 Yes

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4429 / X2CrNiMoN17-13-3. Guideline solution/anneal band (Annex B): 1040–1120 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4429

Seamless route narrative for 1.4429: EN 10297-2 does not offer a welded route for 1.4429. Tube in X2CrNiMoN17-13-3 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Seamless manufacture for 1.4429 finishes through hot- or cold-finished routes. Pick HFD/CFD for descaled engineering surfaces, CFA for bright anneal, and CFG or CFP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Weld thread: match Mo-N austenitic fillers; protect nitrogen level in weld metal.

For austenitic 1.4429, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4429 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1040–1120 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Optional tests under EN 10297-2 for 1.4429 include leak testing, hydrostatic testing, and NDT such as eddy current or ultrasonic methods agreed at enquiry. SHH STEEL records the Options actually performed on the inspection document — we do not claim a test that was not run. Size context for 1.4429: same OD conversation as 1.4404 with higher Rp/Rm on the MTC. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects.

Dimensions and Tolerances for EN 10297-2 1.4429

Dimensional order line for 1.4429: Dimensional orders for 1.4429 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Same od conversation as 1.4404 with higher rp/rm on the mtc. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects.

For precision mechanical duty on 1.4429, cold-finished CFA/CFD routes are the usual conversation; heavier structural or heat-service walls may stay hot-finished HFD. Agree eccentricity and straightness when the assembly stack-up is tight. Size hint for 1.4429: same OD conversation as 1.4404 with higher Rp/Rm on the MTC. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Equivalent Grades for EN 10297-2 1.4429

Equivalence talk for 1.4429 starts with X2CrNiMoN17-13-3: 1.4429 / X2CrNiMoN17-13-3 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 316LN appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4435, 1.4404, 1.4439, 1.4311. Hook for buyers still using only the 316LN alias: lock EN 10297-2 1.4429 on the order line. Caution thread: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up.

Heat Treatment and Delivery Condition for EN 10297-2 1.4429

Austenitic 1.4429 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1040–1120 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: match Mo-N austenitic fillers; protect nitrogen level in weld metal.

Fabrication HT reminder for 1.4429 (+AT): Hot-working temperature bands in Annex B for X2CrNiMoN17-13-3 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4429 should match +AT. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Corrosion Resistance of EN 10297-2 1.4429

Corrosion behaviour of EN 10297-2 1.4429 tracks its austenitic corrosion-resisting balance: Mo plus nitrogen; pitting resistance above lean 316L with interstitial strengthening. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up Corrosion thread: Mo plus nitrogen; pitting resistance above lean 316L with interstitial strengthening.

Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4435, 1.4404, 1.4439, 1.4311 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4429 is austenitic corrosion-resisting. Caution thread: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up.

Applications of EN 10297-2 1.4429 Tube

Applications of EN 10297-2 1.4429 tube centre on mechanical and general engineering rather than PED pressure shells: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects. Role summary: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects.

Typical BOM language pairs EN 10297-2 1.4429 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “316LN” substitutions do not creep in. Primary application sketch: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Weldability of EN 10297-2 1.4429

1.4429 / X2CrNiMoN17-13-3 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: match Mo-N austenitic fillers; protect nitrogen level in weld metal. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: match Mo-N austenitic fillers; protect nitrogen level in weld metal.

When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Filler/shop note for 1.4429: match Mo-N austenitic fillers; protect nitrogen level in weld metal. Caution thread: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up.

Surface Finishes for EN 10297-2 1.4429

Finish selection for 1.4429 on Annex A: For 1.4429, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 316LN, but the finish symbol still belongs on the EN 10297-2 line. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects.

Protective agreements for 1.4429 cover sleeved bright tube, desiccant in sealed crates on long ocean routes, and dry indoor storage after arrival. Polished CFP surfaces ship with non-metallic rub strips so bundle-to-bundle contact cannot print fretting marks. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Inspection and Testing for EN 10297-2 1.4429

Inspection lot framing for 1.4429 in austenitic corrosion-resisting: NDT intensity on 1.4429 is Option-driven under EN 10297-2 — eddy current, ultrasonic, leak, or hydrostatic methods are selected at enquiry. That is a different framing from EN 10216-5 TC1/TC2 pressure categories; copy the Options you need. Keep 1.4429 heat identity intact from cast through bundle tag. Weld thread: match Mo-N austenitic fillers; protect nitrogen level in weld metal.

When EN ISO 3651-2 IGC is ordered on 1.4429, the method letter and acceptance sit on the Option line and the MTC. Hardness, flattening, ring expanding, or drift tests run only when invoked. Marking carries manufacturer identity, OD × wall, EN 10297-2, 1.4429 or the steel name, cast/code, and inspection correlation. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects.

Packaging and Shipping for EN 10297-2 1.4429

Dispatch note for 1.4429 (316LN body alias only): Finished EN 10297-2 1.4429 (X2CrNiMoN17-13-3) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Marking and identity for 1.4429: When cut lengths and special ends are part of the 1.4429 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Finish-sensitive packing for 1.4429 follows the Annex A symbol on the order. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects.

Bundle cards for 1.4429 repeat the heat identity used on the EN 10204 3.1 certificate. SHH STEEL can email packing photos before sailing when the project file needs them, and will re-pack if a bright finish shows transit rub before handover. Caution thread: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10297-2 1.4429 seamless stainless steel tube. Why 1.4429 with SHH STEEL — role: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. Choose SHH STEEL for EN 10297-2 1.4429 when you need a mill partner who will not blur EN 10297-2 with EN 10216-5 or EN 10217-7 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Grade advice stays practical for 1.4429. If the duty needs a sister chemistry, we point to 1.4435, 1.4404, 1.4439, 1.4311. Design caution for this number: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up We answer medium questions with sister pointers rather than overselling a single chemistry. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up.

Supply Capability

SHH STEEL can produce and supply EN 10297-2 1.4429 seamless tube to the edition, delivery condition, Annex A symbol, and Options on your enquiry. Capability and Stock / Available sizes notes below are a first-pass map for X2CrNiMoN17-13-3, not a promise of frozen tonnage. Use thread: higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4429 / X2CrNiMoN17-13-3
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes for EN 10297-2 1.4429: enquiry band commonly spans instrumentation-to-process OD with walls suited to this grade. This is not a frozen SKU tonnage table — heat availability of X2CrNiMoN17-13-3 and finishing slots for the Annex A symbol set the real promise date. Size context: same OD conversation as 1.4404 with higher Rp/Rm on the MTC. Duty thread: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.

Cut lengths, bevels or special ends, IGC Options, and dual RFQs against 1.4435, 1.4404, 1.4439, 1.4311 are routine for 1.4429. Catalogue charts only sanity-check OD × wall — contractual acceptance stays with EN 10297-2. SHH STEEL can produce and supply pilot lengths when the schedule allows. Weld thread: match Mo-N austenitic fillers; protect nitrogen level in weld metal.

FAQ

What is EN 10297-2 1.4429 seamless stainless steel tube used for?
EN 10297-2 1.4429 (X2CrNiMoN17-13-3) is seamless tube for mechanical and general engineering — higher-design-stress chemical utilities, nitrogen-specified 316L-family lines, and wall optimisation projects. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty.
Is EN 10297-2 1.4429 the same as EN 10216-5 1.4429?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4429 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4429 / X2CrNiMoN17-13-3?
Delivery framing for 1.4429 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1040–1120 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4429?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4429 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4429 compare with sister grades 1.4435, 1.4404, 1.4439?
1.4429 / X2CrNiMoN17-13-3 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4435, 1.4404, 1.4439. Design caution: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4429 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: match Mo-N austenitic fillers; protect nitrogen level in weld metal. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4429?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4429?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4429 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: same OD conversation as 1.4404 with higher Rp/Rm on the MTC. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 316LN belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 316LN in body text and BOM notes, but lock EN 10297-2 and 1.4429 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4429?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: higher strength does not remove chloride SCC limits — duplex remains the usual SCC step-up Sister pointers: 1.4435, 1.4404, 1.4439. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4429 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4429 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4429 (X2CrNiMoN17-13-3) is seamless stainless tube for mechanical and general engineering — nitrogen-strengthened Mo austenitic seamless tube (316LN-class) for higher proof strength in chloride-bearing mechanical duty. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4435, 1.4404, 1.4439. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *