EN 10297-2 1.4558 Seamless Stainless Steel Tube
What is EN 10297-2 1.4558 Seamless Stainless Steel Tube
If the purchase file still names only a commercial alias such as 800 / Alloy 800-class (low-C Ti-Al) without a product standard, the mill cannot know whether general-purpose seamless acceptance or pressure-tube acceptance applies. EN 10297-2 plus steel number 1.4558 (X2NiCrAlTi32-20) selects seamless tube for mechanical and general engineering. 1.4558 sits in the corrosion-resisting austenitic tables of EN 10297-2 — confirm whether the enquiry actually wants heat-resisting 1.4876 before dual-marking. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Mill path for 1.4558: specialty seamless OD; solution anneal ~950–1050 °C guidance. SHH STEEL can make and supply EN 10297-2 1.4558 / X2NiCrAlTi32-20 as seamless general-purpose tube across specialty seamless OD; solution anneal ~950–1050 °C guidance, solution annealed or annealed/QT as the grade tables require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Use thread: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone.
On the shop floor people still say “800 / Alloy 800-class (low-C Ti-Al) tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4558, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose. Typical duties include chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone. Design caution: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes. Caution thread: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes.
EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4558: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Inside this seamless general-purpose series, compare EN 10297-2 1.4876, EN 10297-2 1.4335, EN 10297-2 1.4845. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4558.
Chemical Composition of EN 10297-2 1.4558
Cast window focus for 1.4558: Buying 800 / Alloy 800-class (low-C Ti-Al)-family seamless tube without locking 1.4558 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X2NiCrAlTi32-20; highlight elements for this grade include C ≤0.030, Cr 20.0–23.0, Ni 32.0–35.0, Ti 8×C–0.60, Al 0.15–0.45, Si ≤0.70. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 800 / Alloy 800-class (low-C Ti-Al) is body text only. Corrosion thread: high Ni-Cr with Ti-Al for many chemical and elevated aqueous duties within corrosion-resisting scope.
Chemical limits for 1.4558 / X2NiCrAlTi32-20 under EN 10297-2 appear in the table underneath. Source priority is BSSA’s EN 10297-2 article cross-checked to the 2005 grade list. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
| Steel | C | Si | Mn | P | S | Cr | Ni | Ti | Al |
|---|---|---|---|---|---|---|---|---|---|
| 1.4558 / X2NiCrAlTi32-20 | ≤0.030 | ≤0.70 | ≤1.00 | ≤0.020 | ≤0.015 | 20.0–23.0 | 32.0–35.0 | 8×C–0.60 | 0.15–0.45 |
Mechanical Properties of EN 10297-2 1.4558
Ambient floors focus for 1.4558: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4558 order. General-purpose Table values for this number read: Rp0.2 min 180 MPa, Rp1.0 min 210 MPa, Rm min 450 MPa, longitudinal elongation min 35%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic corrosion-resisting. Caution thread: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 180 | 210 | 450 min | 35 | — | – |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4558 / X2NiCrAlTi32-20. Guideline solution/anneal band (Annex B): 950–1050 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4558
Seamless route narrative for 1.4558: EN 10297-2 does not offer a welded route for 1.4558. Tube in X2NiCrAlTi32-20 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Seamless manufacture for 1.4558 finishes through hot- or cold-finished routes. Pick HFD/CFD for descaled engineering surfaces, CFA for bright anneal, and CFG or CFP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Weld thread: matching high-Ni austenitic fillers; control Ti/Al burn-off.
For austenitic 1.4558, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4558 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 950–1050 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Optional tests under EN 10297-2 for 1.4558 include leak testing, hydrostatic testing, and NDT such as eddy current or ultrasonic methods agreed at enquiry. SHH STEEL records the Options actually performed on the inspection document — we do not claim a test that was not run. Size context for 1.4558: specialty seamless OD; solution anneal ~950–1050 °C guidance. Use thread: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone.
Dimensions and Tolerances for EN 10297-2 1.4558
Dimensional order line for 1.4558: SHH STEEL aligns OD × wall, tolerance class, and process-route symbol for 1.4558 / X2NiCrAlTi32-20 before rolling or drawing slots are locked. Specialty seamless od; solution anneal ~950–1050 °c guidance. Use thread: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone.
For precision mechanical duty on 1.4558, cold-finished CFA/CFD routes are the usual conversation; heavier structural or heat-service walls may stay hot-finished HFD. Agree eccentricity and straightness when the assembly stack-up is tight. Size hint for 1.4558: specialty seamless OD; solution anneal ~950–1050 °C guidance. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Equivalent Grades for EN 10297-2 1.4558
Equivalence talk for 1.4558 starts with X2NiCrAlTi32-20: 1.4558 / X2NiCrAlTi32-20 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 800 / Alloy 800-class (low-C Ti-Al) appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4876, 1.4335, 1.4845. Hook for buyers still using only the 800 / Alloy 800-class (low-C Ti-Al) alias: lock EN 10297-2 1.4558 on the order line. Caution thread: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes.
Heat Treatment and Delivery Condition for EN 10297-2 1.4558
Austenitic 1.4558 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 950–1050 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching high-Ni austenitic fillers; control Ti/Al burn-off.
Fabrication HT reminder for 1.4558 (+AT): Hot-working temperature bands in Annex B for X2NiCrAlTi32-20 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4558 should match +AT. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Corrosion Resistance of EN 10297-2 1.4558
Corrosion behaviour of EN 10297-2 1.4558 tracks its austenitic corrosion-resisting balance: high Ni-Cr with Ti-Al for many chemical and elevated aqueous duties within corrosion-resisting scope. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes Corrosion thread: high Ni-Cr with Ti-Al for many chemical and elevated aqueous duties within corrosion-resisting scope.
Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4876, 1.4335, 1.4845 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4558 is austenitic corrosion-resisting. Caution thread: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes.
Applications of EN 10297-2 1.4558 Tube
Applications of EN 10297-2 1.4558 tube centre on mechanical and general engineering rather than PED pressure shells: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone. Role summary: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone.
Skip 1.4558 when the specification locks a different family — for example forcing ferritic 1.4558 into severe chloride process duty, or forcing a free-machining grade into welded corrosive service. Sister conversation inside EN 10297-2: 1.4876, 1.4335, 1.4845. Primary application sketch: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Weldability of EN 10297-2 1.4558
1.4558 / X2NiCrAlTi32-20 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching high-Ni austenitic fillers; control Ti/Al burn-off. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching high-Ni austenitic fillers; control Ti/Al burn-off.
For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes Filler/shop note for 1.4558: matching high-Ni austenitic fillers; control Ti/Al burn-off. Caution thread: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes.
Surface Finishes for EN 10297-2 1.4558
Finish selection for 1.4558 on Annex A: For 1.4558, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 800 / Alloy 800-class (low-C Ti-Al), but the finish symbol still belongs on the EN 10297-2 line. Use thread: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone.
During delivery of 1.4558, SHH STEEL can add edge guards, VCI paper, or sealed PE wrap when the enquiry lists them. Descaled engineering finishes still need caps; bright and polished finishes need full OD sleeve protection. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Inspection and Testing for EN 10297-2 1.4558
Inspection lot framing for 1.4558 in austenitic corrosion-resisting: Specific inspection applies to EN 10297-2 1.4558 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Keep 1.4558 heat identity intact from cast through bundle tag. Weld thread: matching high-Ni austenitic fillers; control Ti/Al burn-off.
Inspection documents for 1.4558 list every Optional test that actually ran. Surrogate “typical” NDT language is never printed. Tube marking repeats the steel number 1.4558 so warehouse staff cannot confuse sister heats in the same bundle bay. Use thread: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone.
Packaging and Shipping for EN 10297-2 1.4558
Dispatch note for 1.4558 (800 / Alloy 800-class (low-C Ti-Al) body alias only): Export packing for 1.4558 / X2NiCrAlTi32-20 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavy HFD bundles use spacers to stop fretting in transit. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Marking and identity for 1.4558: For 1.4558, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Finish-sensitive packing for 1.4558 follows the Annex A symbol on the order. Use thread: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone.
For 1.4558, export documentation includes packing list, certificate, and any third-party release notes agreed at order. Heat segregation rules stay in force when multiple steel numbers share a container. Caution thread: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes.
Why Choose SHH STEEL
Why 1.4558 with SHH STEEL — role: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose. SHH STEEL can produce and supply EN 10297-2 1.4558 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “800 / Alloy 800-class (low-C Ti-Al) tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Grade advice stays practical for 1.4558. If the duty needs a sister chemistry, we point to 1.4876, 1.4335, 1.4845. Design caution for this number: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes If the file later becomes PED pressure seamless, we help retarget EN 10216-5 rather than relabeling a general-purpose MTC. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes.
Supply Capability
SHH STEEL can produce and supply EN 10297-2 1.4558. Ask SHH STEEL for EN 10297-2 1.4558 when you need seamless general-purpose X2NiCrAlTi32-20 with named Options. We can produce and supply trial lengths or production heats once OD, wall, finish symbol, and test Options are clear. See Stock / Available sizes below. Use thread: chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4558 / X2NiCrAlTi32-20 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Enquiry stock map — EN 10297-2 1.4558 / X2NiCrAlTi32-20: specialty seamless OD; solution anneal ~950–1050 °C guidance. SHH STEEL will mark which rows can roll on current hollows versus which need a fresh heat. No invented warehouse tonnages appear on this page. Duty thread: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
Sister comparisons for 1.4558 usually include 1.4876, 1.4335, 1.4845. Dimensional acceptance remains the EN 10297-2 order text, not a peer brochure. SHH STEEL can produce and supply mixed sister bundles when heats and finishes align. Weld thread: matching high-Ni austenitic fillers; control Ti/Al burn-off.
FAQ
-
What is EN 10297-2 1.4558 seamless stainless steel tube used for?
- EN 10297-2 1.4558 (X2NiCrAlTi32-20) is seamless tube for mechanical and general engineering — chemical process mechanical lines needing high Ni-Cr stability, and duties adjacent to Alloy 800 thinking without jumping to heat-resisting 1.4876 alone. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose.
-
Is EN 10297-2 1.4558 the same as EN 10216-5 1.4558?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4558 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4558 / X2NiCrAlTi32-20?
- Delivery framing for 1.4558 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 950–1050 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4558?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4558 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4558 compare with sister grades 1.4876, 1.4335, 1.4845?
- 1.4558 / X2NiCrAlTi32-20 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4876, 1.4335, 1.4845. Design caution: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4558 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching high-Ni austenitic fillers; control Ti/Al burn-off. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4558?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4558?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4558 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty seamless OD; solution anneal ~950–1050 °C guidance. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 800 / Alloy 800-class (low-C Ti-Al) belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 800 / Alloy 800-class (low-C Ti-Al) in body text and BOM notes, but lock EN 10297-2 and 1.4558 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4558?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: distinguish from heat-resisting 1.4876 — different C/Ti/Al windows and Table 9 vs Table 7 homes Sister pointers: 1.4876, 1.4335, 1.4845. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4558 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4558 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4558 (X2NiCrAlTi32-20) is seamless stainless tube for mechanical and general engineering — low-C Ti-Al bearing 32Ni-20Cr austenitic seamless tube in the Alloy 800 chemistry neighbourhood for corrosion-resisting general purpose. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4876, 1.4335, 1.4845. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.