EN 10297-2 1.4424 Seamless Stainless Steel Tube
What is EN 10297-2 1.4424 Seamless Stainless Steel Tube
EN 10297-2 covers seamless stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4424 is the austenitic-ferritic (duplex) grade X2CrNiMoSi18-5-3, commercially discussed as Si duplex / S31500-class. 1.4424 is a specialty Si duplex in EN 10297-2 — do not auto-quote 2205 when the enquiry locks this steel number. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Mill path for 1.4424: specialty seamless OD; solution anneal ~975–1050 °C guidance. SHH STEEL can produce and supply X2CrNiMoSi18-5-3 under EN 10297-2 1.4424 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3.
On the shop floor people still say “Si duplex / S31500-class tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4424, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon. Typical duties include specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3. Design caution: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462. Caution thread: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462.
EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4424: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Inside this seamless general-purpose series, compare EN 10297-2 1.4462, EN 10297-2 1.4362, EN 10297-2 1.4404. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4424.
Chemical Composition of EN 10297-2 1.4424
Cast window focus for 1.4424: Cast analysis for EN 10297-2 1.4424 follows the X2CrNiMoSi18-5-3 limits published for this standard’s corrosion- or heat-resisting tables. Key windows on a typical certificate include C ≤0.030, Cr 18.0–19.0, Ni 4.5–5.2, Mo 2.50–3.00, N 0.05–0.10, Si 1.40–2.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias Si duplex / S31500-class is body text only. Corrosion thread: duplex with Si for selected media; verify corrosion data for the actual process.
For 1.4424 / X2CrNiMoSi18-5-3, the following chem table is the public EN 10297-2 window SHH STEEL uses at enquiry. Product-analysis Options, when taken, apply the standard’s permitted deviations rather than inventing tighter shop limits. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
| Steel | C | Si | Mn | P | S | Cr | Mo | Ni | N |
|---|---|---|---|---|---|---|---|---|---|
| 1.4424 / X2CrNiMoSi18-5-3 | ≤0.030 | 1.40–2.00 | 1.20–2.00 | ≤0.035 | ≤0.015 | 18.0–19.0 | 2.50–3.00 | 4.5–5.2 | 0.05–0.10 |
Mechanical Properties of EN 10297-2 1.4424
Ambient floors focus for 1.4424: Table mechanical floors for 1.4424 / X2CrNiMoSi18-5-3 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 480 MPa, Rp1.0 min 490 MPa, Rm min 700 MPa, longitudinal elongation min 30%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Family: duplex (austenitic-ferritic). Caution thread: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 480 | 490 | 700 min | 30 | 30 | Yes |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4424 / X2CrNiMoSi18-5-3. Guideline solution/anneal band (Annex B): 975–1050 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4424
Seamless route narrative for 1.4424: EN 10297-2 1.4424 is seamless only — pierced or extruded hollows are hot-worked and may be cold-finished to size before heat treatment. Duplex X2CrNiMoSi18-5-3 needs controlled thermomechanical history so the ferrite–austenite balance lands in the ordered window after +AT. Seamless manufacture for 1.4424 finishes through hot- or cold-finished routes. Pick HFD/CFD for descaled engineering surfaces, CFA for bright anneal, and CFG or CFP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Weld thread: duplex practice adapted to Si-bearing chemistry; filler selection by agreement.
For duplex 1.4424, solution annealing and rapid cooling are part of the product story, not an optional cosmetic step. Ferritic 1.4424 ships annealed (+A). Annex B points at roughly 975–1050 °C with water or air cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. NDT Options (eddy current, ultrasonic, leak or hydrostatic) are selected on the order; they are not a substitute for correct duplex heat treatment. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Optional tests under EN 10297-2 for 1.4424 include leak testing, hydrostatic testing, and NDT such as eddy current or ultrasonic methods agreed at enquiry. SHH STEEL records the Options actually performed on the inspection document — we do not claim a test that was not run. Size context for 1.4424: specialty seamless OD; solution anneal ~975–1050 °C guidance. Use thread: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3.
Dimensions and Tolerances for EN 10297-2 1.4424
Dimensional order line for 1.4424: Dimensional orders for 1.4424 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Specialty seamless od; solution anneal ~975–1050 °c guidance. Use thread: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3.
For precision mechanical duty on 1.4424, cold-finished CFA/CFD routes are the usual conversation; heavier structural or heat-service walls may stay hot-finished HFD. Agree eccentricity and straightness when the assembly stack-up is tight. Size hint for 1.4424: specialty seamless OD; solution anneal ~975–1050 °C guidance. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Equivalent Grades for EN 10297-2 1.4424
Equivalence talk for 1.4424 starts with X2CrNiMoSi18-5-3: 1.4424 / X2CrNiMoSi18-5-3 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias Si duplex / S31500-class appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4462, 1.4362, 1.4404. Hook for buyers still using only the Si duplex / S31500-class alias: lock EN 10297-2 1.4424 on the order line. Caution thread: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462.
Heat Treatment and Delivery Condition for EN 10297-2 1.4424
Ferritic 1.4424 ships annealed (+A). Annex B points at roughly 975–1050 °C with water or air cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Weld thread: duplex practice adapted to Si-bearing chemistry; filler selection by agreement.
Fabrication HT reminder for 1.4424 (+AT): Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4424, restore the delivery condition agreed on the order before corrosive or load-bearing service. Delivery framing on the certificate for 1.4424 should match +AT. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Corrosion Resistance of EN 10297-2 1.4424
Corrosion behaviour of EN 10297-2 1.4424 tracks its austenitic-ferritic (duplex) balance: duplex with Si for selected media; verify corrosion data for the actual process. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462 Corrosion thread: duplex with Si for selected media; verify corrosion data for the actual process.
For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4424 is filed as austenitic-ferritic (duplex) — pick tests that match that filing. Family filing for 1.4424 is duplex (austenitic-ferritic). Caution thread: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462.
Applications of EN 10297-2 1.4424 Tube
Applications of EN 10297-2 1.4424 tube centre on mechanical and general engineering rather than PED pressure shells: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3. Role summary: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3.
It is the wrong first choice when a welded product form is mandatory (use EN 10296-2 or EN 10217-7 as applicable), when PED pressure seamless acceptance is locked to EN 10216-5 alone, or when the medium clearly needs a sister such as 1.4462. Primary application sketch: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Weldability of EN 10297-2 1.4424
1.4424 / X2CrNiMoSi18-5-3 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: duplex practice adapted to Si-bearing chemistry; filler selection by agreement. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: duplex practice adapted to Si-bearing chemistry; filler selection by agreement.
When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Filler/shop note for 1.4424: duplex practice adapted to Si-bearing chemistry; filler selection by agreement. Caution thread: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462.
Surface Finishes for EN 10297-2 1.4424
Finish selection for 1.4424 on Annex A: For 1.4424, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say Si duplex / S31500-class, but the finish symbol still belongs on the EN 10297-2 line. Use thread: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3.
Transit protection for 1.4424 is sized to the Annex A finish: heavier wrap for CFA/CFG/CFP, standard export wrap for HFD/CFD. Open-deck ocean exposure without wrap is refused on bright tube. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Inspection and Testing for EN 10297-2 1.4424
Inspection lot framing for 1.4424 in duplex (austenitic-ferritic): NDT intensity on 1.4424 is Option-driven under EN 10297-2 — eddy current, ultrasonic, leak, or hydrostatic methods are selected at enquiry. That is a different framing from EN 10216-5 TC1/TC2 pressure categories; copy the Options you need. Keep 1.4424 heat identity intact from cast through bundle tag. Weld thread: duplex practice adapted to Si-bearing chemistry; filler selection by agreement.
Purchasers who need witness points on 1.4424 should say so at enquiry. Routine mill inspection still records cast chemistry, tensile results, delivery condition, and dimensions; witness adds scheduling, not a different chemistry table. Use thread: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3.
Packaging and Shipping for EN 10297-2 1.4424
Dispatch note for 1.4424 (Si duplex / S31500-class body alias only): Export packing for 1.4424 / X2CrNiMoSi18-5-3 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavy HFD bundles use spacers to stop fretting in transit. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Marking and identity for 1.4424: Marking typically includes manufacturer identity, dimensions, EN 10297-2, steel name or number 1.4424, cast/code, inspection mark, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging CFA/CFP surfaces. Finish-sensitive packing for 1.4424 follows the Annex A symbol on the order. Use thread: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3.
Ocean containers loaded with 1.4424 use desiccant and sealed wrap when the route or season warrants it. Inland deliveries may omit container desiccant but never omit end caps on precision OD. Caution thread: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462.
Why Choose SHH STEEL
Why 1.4424 with SHH STEEL — role: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon. SHH STEEL can produce and supply X2CrNiMoSi18-5-3 as EN 10297-2 1.4424 seamless tube with honest scope boundaries. General engineering seamless acceptance is what this page sells; pressure, welded-pressure, and welded-general-purpose sisters are separate standards with separate MTCs. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Grade advice stays practical for 1.4424. If the duty needs a sister chemistry, we point to 1.4462, 1.4362, 1.4404. Design caution for this number: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462 Technical clarification on QT level, cold- versus hot-finished rows, or duplex thin-wall footnotes happens before acknowledgement. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462.
Supply Capability
For 1.4424, SHH STEEL can produce and supply seamless tube in the X2CrNiMoSi18-5-3 analysis with the Annex A finish you name. Lead time tracks hollow stock and heat-treatment slots; Stock / Available sizes below helps size the first RFQ. Use thread: specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4424 / X2CrNiMoSi18-5-3 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Available sizes for 1.4424 follow seamless general-purpose practice: specialty seamless OD; solution anneal ~975–1050 °C guidance. Dual size lists against sister grades are welcome on one enquiry sheet. Duty thread: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
Dual documentation talk for 1.4424 versus 1.4462, 1.4362, 1.4404 is fine at enquiry — each steel number still needs its own cast compliance. SHH STEEL can produce and supply staged deliveries by size priority. Weld thread: duplex practice adapted to Si-bearing chemistry; filler selection by agreement.
FAQ
-
What is EN 10297-2 1.4424 seamless stainless steel tube used for?
- EN 10297-2 1.4424 (X2CrNiMoSi18-5-3) is seamless tube for mechanical and general engineering — specialty chemical mechanical lines and European specs that name X2CrNiMoSi18-5-3. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon.
-
Is EN 10297-2 1.4424 the same as EN 10216-5 1.4424?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4424 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4424 / X2CrNiMoSi18-5-3?
- Delivery framing for 1.4424 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 975–1050 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4424?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4424 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4424 compare with sister grades 1.4462, 1.4362, 1.4404?
- 1.4424 / X2CrNiMoSi18-5-3 is filed as duplex (austenitic-ferritic). Typical sisters discussed on the same RFQ are 1.4462, 1.4362, 1.4404. Design caution: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462 Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4424 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: duplex practice adapted to Si-bearing chemistry; filler selection by agreement. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4424?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4424?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4424 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty seamless OD; solution anneal ~975–1050 °C guidance. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias Si duplex / S31500-class belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use Si duplex / S31500-class in body text and BOM notes, but lock EN 10297-2 and 1.4424 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4424?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what duplex (austenitic-ferritic) practice can defend for the temperature and stress state. Caution for this number: narrower Ni window and Si range — confirm cast analysis; not a drop-in for 1.4462 Sister pointers: 1.4462, 1.4362, 1.4404. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4424 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4424 is filed as duplex (austenitic-ferritic). If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4424 (X2CrNiMoSi18-5-3) is seamless stainless tube for mechanical and general engineering — Si-bearing duplex seamless tube for specialised mechanical duty needing duplex strength with elevated silicon. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4462, 1.4362, 1.4404. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.