EN 10297-2 1.4529 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4529 Seamless Stainless Steel Tube

EN 10297-2 1.4529 / X1NiCrMoCuN25-20-7 seamless stainless general-purpose tube (6Mo / N08926), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 270 MPa, Rm min 600 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4529 / X1NiCrMoCuN25-20-7 (6Mo / N08926 — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4529 Seamless Stainless Steel Tube

Mechanical and general engineering projects that need seamless stainless tube under a European product standard look to EN 10297-2:2005 — Part 2 of EN 10297 — rather than a PED pressure Part 5 page or an ASTM tubing habit alone. 1.4529 / X1NiCrMoCuN25-20-7 sits in the austenitic corrosion-resisting tables. When the material list says N08926 or 1.4529, EN 10297-2 is the seamless general-purpose home — do not silently substitute 1.4547 without approval. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Mill path for 1.4529: specialty seamless OD. SHH STEEL can produce and supply X1NiCrMoCuN25-20-7 under EN 10297-2 1.4529 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified.

On the shop floor people still say “6Mo / N08926 tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4529, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel. Typical duties include severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified. Design caution: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order. Caution thread: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order.

Scope discipline matters: 1.4529 under EN 10297-2 is seamless general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Role reminder for 1.4529: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Inside this seamless general-purpose series, compare EN 10297-2 1.4547, EN 10297-2 1.4539, EN 10297-2 1.4563. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4529.

Chemical Composition of EN 10297-2 1.4529

Cast window focus for 1.4529: Buying 6Mo / N08926-family seamless tube without locking 1.4529 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X1NiCrMoCuN25-20-7; highlight elements for this grade include C ≤0.020, Cr 19.0–21.0, Ni 24.0–26.0, Mo 6.0–7.0, N 0.15–0.25, Cu 0.50–1.50. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 6Mo / N08926 is body text only. Corrosion thread: 6% Mo plus high Ni, Cu, N for aggressive halide and acid-chloride media.

Below is the BSSA-sourced EN 10297-2 chemistry window for 1.4529 (X1NiCrMoCuN25-20-7). Maxima apply unless a band is printed. SHH STEEL quotes against this window and reports actual cast values on the EN 10204 document — not a rewritten catalogue paraphrase. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Steel C Si Mn P S Cr Mo Ni Cu N
1.4529 / X1NiCrMoCuN25-20-7 ≤0.020 ≤0.50 ≤1.00 ≤0.030 ≤0.010 19.0–21.0 6.0–7.0 24.0–26.0 0.50–1.50 0.15–0.25

Mechanical Properties of EN 10297-2 1.4529

Ambient floors focus for 1.4529: Ambient mechanical properties for EN 10297-2 1.4529 follow Tables 6–9 by family. For this grade the delivery-condition floors to watch are: Rp0.2 min 270 MPa, Rp1.0 min 310 MPa, Rm min 600 MPa, longitudinal elongation min 35%. Intergranular corrosion resistance per EN ISO 3651-2 is tabulated where applicable — see the IGC column on the mechanical table below. Family: austenitic corrosion-resisting. Caution thread: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 270 310 600 min 35 — Yes

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4529 / X1NiCrMoCuN25-20-7. Guideline solution/anneal band (Annex B): 1120–1180 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4529

Seamless route narrative for 1.4529: EN 10297-2 does not offer a welded route for 1.4529. Tube in X1NiCrMoCuN25-20-7 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Order EN 10297-2 1.4529 with an Annex A surface/process symbol — HFD or CFD for metallically clean descaled tube, CFA when bright-annealed OD is required, CFG/CFP when ground or polished roughness is written into the purchase order. Weld thread: matching 6Mo/high-Ni fillers; high solution-anneal practice.

For austenitic 1.4529, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4529 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1120–1180 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4529. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4529: specialty seamless OD. Use thread: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified.

Dimensions and Tolerances for EN 10297-2 1.4529

Dimensional order line for 1.4529: Order EN 10297-2 1.4529 by outside diameter D and wall thickness T for steel name X1NiCrMoCuN25-20-7. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Specialty seamless od. Use thread: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified.

Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4529: specialty seamless OD. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Equivalent Grades for EN 10297-2 1.4529

Equivalence talk for 1.4529 starts with X1NiCrMoCuN25-20-7: 1.4529 / X1NiCrMoCuN25-20-7 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 6Mo / N08926 appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4547, 1.4539, 1.4563. Hook for buyers still using only the 6Mo / N08926 alias: lock EN 10297-2 1.4529 on the order line. Caution thread: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order.

Heat Treatment and Delivery Condition for EN 10297-2 1.4529

Austenitic 1.4529 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1120–1180 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching 6Mo/high-Ni fillers; high solution-anneal practice.

Fabrication HT reminder for 1.4529 (+AT): Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4529, restore the delivery condition agreed on the order before corrosive or load-bearing service. Delivery framing on the certificate for 1.4529 should match +AT. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Corrosion Resistance of EN 10297-2 1.4529

Corrosion behaviour of EN 10297-2 1.4529 tracks its austenitic corrosion-resisting balance: 6% Mo plus high Ni, Cu, N for aggressive halide and acid-chloride media. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order Corrosion thread: 6% Mo plus high Ni, Cu, N for aggressive halide and acid-chloride media.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4529 is filed as austenitic corrosion-resisting — pick tests that match that filing. Family filing for 1.4529 is austenitic corrosion-resisting. Caution thread: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order.

Applications of EN 10297-2 1.4529 Tube

Applications of EN 10297-2 1.4529 tube centre on mechanical and general engineering rather than PED pressure shells: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified. Role summary: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified.

It is the wrong first choice when a welded product form is mandatory (use EN 10296-2 or EN 10217-7 as applicable), when PED pressure seamless acceptance is locked to EN 10216-5 alone, or when the medium clearly needs a sister such as 1.4547. Primary application sketch: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Weldability of EN 10297-2 1.4529

1.4529 / X1NiCrMoCuN25-20-7 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching 6Mo/high-Ni fillers; high solution-anneal practice. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching 6Mo/high-Ni fillers; high solution-anneal practice.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order Filler/shop note for 1.4529: matching 6Mo/high-Ni fillers; high solution-anneal practice. Caution thread: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order.

Surface Finishes for EN 10297-2 1.4529

Finish selection for 1.4529 on Annex A: For 1.4529, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 6Mo / N08926, but the finish symbol still belongs on the EN 10297-2 line. Use thread: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified.

Storage guidance for 1.4529: keep bundles off bare concrete in coastal yards, avoid chloride-bearing tarps against CFA OD, and leave end caps fitted until fabrication. Special export crate liners are available when the packing note asks for them. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Inspection and Testing for EN 10297-2 1.4529

Inspection lot framing for 1.4529 in austenitic corrosion-resisting: NDT intensity on 1.4529 is Option-driven under EN 10297-2 — eddy current, ultrasonic, leak, or hydrostatic methods are selected at enquiry. That is a different framing from EN 10216-5 TC1/TC2 pressure categories; copy the Options you need. Keep 1.4529 heat identity intact from cast through bundle tag. Weld thread: matching 6Mo/high-Ni fillers; high solution-anneal practice.

Technological tests on 1.4529 follow the order matrix — they are not assumed. IGC, when required, cites EN ISO 3651-2. Stencil or inkjet marking stays light on polished OD so the finish remains acceptable after receipt inspection. Use thread: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified.

Packaging and Shipping for EN 10297-2 1.4529

Dispatch note for 1.4529 (6Mo / N08926 body alias only): Finished EN 10297-2 1.4529 (X1NiCrMoCuN25-20-7) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Marking and identity for 1.4529: For 1.4529, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Finish-sensitive packing for 1.4529 follows the Annex A symbol on the order. Use thread: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified.

Packing lists for 1.4529 map bundle IDs to heats and sizes so receiving inspection can clear documents without unpacking every crate. Damaged wrap discovered at destination is reported with photos before the material is issued to fabrication. Caution thread: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10297-2 1.4529 seamless stainless steel tube. Why 1.4529 with SHH STEEL — role: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel. Choose SHH STEEL for EN 10297-2 1.4529 when you need a mill partner who will not blur EN 10297-2 with EN 10216-5 or EN 10217-7 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

Grade advice stays practical for 1.4529. If the duty needs a sister chemistry, we point to 1.4547, 1.4539, 1.4563. Design caution for this number: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order Quotes state scope boundaries in plain language so purchasing and engineering share the same acceptance standard. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order.

Supply Capability

Supply capability for EN 10297-2 1.4529 / X1NiCrMoCuN25-20-7 starts with your OD × wall list and delivery-condition choice. SHH STEEL can produce and supply against that list with EN 10204 3.1 documents; the Stock / Available sizes block frames enquiry sizes rather than a public warehouse catalogue. Use thread: severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4529 / X1NiCrMoCuN25-20-7
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Available sizes conversation for 1.4529 starts with your OD × wall matrix. Typical note: specialty seamless OD. Send preferred delivery condition (+A / +AT / +QT as applicable) and any eddy-current or hydrostatic Options with the size list. Duty thread: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.

On 1.4529, Options and sister duals (1.4547, 1.4539, 1.4563) belong on the same enquiry as the size list. SHH STEEL can produce and supply production heats after a short pilot when forming or polish trials are required. Weld thread: matching 6Mo/high-Ni fillers; high solution-anneal practice.

FAQ

What is EN 10297-2 1.4529 seamless stainless steel tube used for?
EN 10297-2 1.4529 (X1NiCrMoCuN25-20-7) is seamless tube for mechanical and general engineering — severe chloride and acid-chloride mechanical lines where N08926 chemistry is specified. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel.
Is EN 10297-2 1.4529 the same as EN 10216-5 1.4529?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4529 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4529 / X1NiCrMoCuN25-20-7?
Delivery framing for 1.4529 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1120–1180 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4529?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4529 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4529 compare with sister grades 1.4547, 1.4539, 1.4563?
1.4529 / X1NiCrMoCuN25-20-7 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4547, 1.4539, 1.4563. Design caution: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4529 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching 6Mo/high-Ni fillers; high solution-anneal practice. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4529?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4529?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4529 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty seamless OD. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 6Mo / N08926 belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 6Mo / N08926 in body text and BOM notes, but lock EN 10297-2 and 1.4529 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4529?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: transverse elongation not tabulated the same way as some sisters — check Table 7 footnotes on the order Sister pointers: 1.4547, 1.4539, 1.4563. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4529 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4529 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4529 (X1NiCrMoCuN25-20-7) is seamless stainless tube for mechanical and general engineering — 6Mo high-Ni superaustenitic seamless tube (N08926-class) parallel to 1.4547 with higher nickel. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4547, 1.4539, 1.4563. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X