EN 10297-2 1.4854 Seamless Stainless Steel Tube
What is EN 10297-2 1.4854 Seamless Stainless Steel Tube
Mechanical and general engineering projects that need seamless stainless tube under a European product standard look to EN 10297-2:2005 — Part 2 of EN 10297 — rather than a PED pressure Part 5 page or an ASTM tubing habit alone. 1.4854 / X6NiCrSiNCe35-25 sits in the austenitic heat-resisting tables. When the material list locks 353MA seamless tube, EN 10297-2 1.4854 is the steel number — confirm patented-grade supply path at enquiry. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
Mill path for 1.4854: specialty heat-service seamless OD. SHH STEEL can produce and supply X6NiCrSiNCe35-25 under EN 10297-2 1.4854 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
On the shop floor people still say “353MA tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4854, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service. Typical duties include demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA. Design caution: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310. Caution thread: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310.
Do not treat an EN 10297-2 1.4854 MTC as automatic clearance for pressure equipment — Part 5 of EN 10216 is the pressure seamless home. Likewise, welded pressure tube lives under EN 10217-7, which is a different product form and test regime. Match the product standard to the duty before dual-marking talk begins. Role reminder for 1.4854: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
Inside this seamless general-purpose series, compare EN 10297-2 1.4835, EN 10297-2 1.4876, EN 10297-2 1.4845. Hub: EN 10297-2.
Chemical Composition of EN 10297-2 1.4854
Cast window focus for 1.4854: Buying 353MA-family seamless tube without locking 1.4854 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X6NiCrSiNCe35-25; highlight elements for this grade include C 0.04–0.08, Cr 24.0–26.0, Ni 34.0–36.0, N 0.12–0.20, Si 1.20–2.00, Ce 0.03–0.08. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 353MA is body text only. Corrosion thread: rare-earth + high Ni-Cr-Si for severe oxidising heat environments.
Cast chemistry for seamless 1.4854 must land inside X6NiCrSiNCe35-25 limits. The table is transcribed from public BSSA EN 10297-2 data for quick comparison with sister grades; always re-check the paid standard when a dispute arises. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
| Steel | C | Si | Mn | P | S | Cr | Ni | N | Ce |
|---|---|---|---|---|---|---|---|---|---|
| 1.4854 / X6NiCrSiNCe35-25 | 0.04–0.08 | 1.20–2.00 | ≤2.00 | ≤0.040 | ≤0.015 | 24.0–26.0 | 34.0–36.0 | 0.12–0.20 | 0.03–0.08 |
Mechanical Properties of EN 10297-2 1.4854
Ambient floors focus for 1.4854: Table mechanical floors for 1.4854 / X6NiCrSiNCe35-25 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 300 MPa, Rp1.0 min 340 MPa, Rm min 650 MPa, longitudinal elongation min 40%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Family: austenitic heat-resisting. Caution thread: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 300 | 340 | 650 min | 40 | 40 | – |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4854 / X6NiCrSiNCe35-25. Guideline solution/anneal band (Annex B): 1100–1150 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4854
Seamless route narrative for 1.4854: EN 10297-2 does not offer a welded route for 1.4854. Tube in X6NiCrSiNCe35-25 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Order EN 10297-2 1.4854 with an Annex A surface/process symbol — HFD or CFD for metallically clean descaled tube, CFA when bright-annealed OD is required, CFG/CFP when ground or polished roughness is written into the purchase order. Weld thread: matching 353MA-class fillers; high solution-anneal band ~1100–1150 °C.
For austenitic 1.4854, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4854 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1100–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
When dual documentation against EN 10216-5 is requested for the same 1.4854 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 1.4854: specialty heat-service seamless OD. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Dimensions and Tolerances for EN 10297-2 1.4854
Dimensional order line for 1.4854: Order EN 10297-2 1.4854 by outside diameter D and wall thickness T for steel name X6NiCrSiNCe35-25. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Specialty heat-service seamless od. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Length supply for 1.4854 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Size hint for 1.4854: specialty heat-service seamless OD. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
Equivalent Grades for EN 10297-2 1.4854
Equivalence talk for 1.4854 starts with X6NiCrSiNCe35-25: 1.4854 / X6NiCrSiNCe35-25 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 353MA appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4835, 1.4876, 1.4845. Hook for buyers still using only the 353MA alias: lock EN 10297-2 1.4854 on the order line. Caution thread: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310.
Heat Treatment and Delivery Condition for EN 10297-2 1.4854
Austenitic 1.4854 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1100–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching 353MA-class fillers; high solution-anneal band ~1100–1150 °C.
Fabrication HT reminder for 1.4854 (+AT): Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4854, restore the delivery condition agreed on the order before corrosive or load-bearing service. Delivery framing on the certificate for 1.4854 should match +AT. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
Corrosion Resistance of EN 10297-2 1.4854
Corrosion behaviour of EN 10297-2 1.4854 tracks its austenitic heat-resisting balance: rare-earth + high Ni-Cr-Si for severe oxidising heat environments. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310 Corrosion thread: rare-earth + high Ni-Cr-Si for severe oxidising heat environments.
Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4835, 1.4876, 1.4845 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4854 is austenitic heat-resisting. Caution thread: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310.
Applications of EN 10297-2 1.4854 Tube
Applications of EN 10297-2 1.4854 tube centre on mechanical and general engineering rather than PED pressure shells: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA. Role summary: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Skip 1.4854 when the specification locks a different family — for example forcing ferritic 1.4854 into severe chloride process duty, or forcing a free-machining grade into welded corrosive service. Sister conversation inside EN 10297-2: 1.4835, 1.4876, 1.4845. Primary application sketch: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
Weldability of EN 10297-2 1.4854
1.4854 / X6NiCrSiNCe35-25 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching 353MA-class fillers; high solution-anneal band ~1100–1150 °C. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching 353MA-class fillers; high solution-anneal band ~1100–1150 °C.
When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Filler/shop note for 1.4854: matching 353MA-class fillers; high solution-anneal band ~1100–1150 °C. Caution thread: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310.
Surface Finishes for EN 10297-2 1.4854
Finish selection for 1.4854 on Annex A: For 1.4854, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 353MA, but the finish symbol still belongs on the EN 10297-2 line. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Agree any site-storage constraints for 1.4854 at enquiry. Long inland dwell in winter road-salt regions needs sealed wrap even when ocean freight is not involved. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
Inspection and Testing for EN 10297-2 1.4854
Inspection lot framing for 1.4854 in austenitic heat-resisting: NDT intensity on 1.4854 is Option-driven under EN 10297-2 — eddy current, ultrasonic, leak, or hydrostatic methods are selected at enquiry. That is a different framing from EN 10216-5 TC1/TC2 pressure categories; copy the Options you need. Keep 1.4854 heat identity intact from cast through bundle tag. Weld thread: matching 353MA-class fillers; high solution-anneal band ~1100–1150 °C.
Acceptance marks on 1.4854 reference the inspection lot. If a piece is cut after delivery, retain the marked end or transfer the heat identity under the fabricator’s quality system so traceability survives the saw. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Packaging and Shipping for EN 10297-2 1.4854
Dispatch note for 1.4854 (353MA body alias only): SHH STEEL ships EN 10297-2 1.4854 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled HFD/CFD engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
Marking and identity for 1.4854: When cut lengths and special ends are part of the 1.4854 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Finish-sensitive packing for 1.4854 follows the Annex A symbol on the order. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
Project freight for 1.4854 can be staged by installation sequence when the packing list names priority bundles. That staging is agreed before the saw schedule locks. Caution thread: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310.
Why Choose SHH STEEL
Why 1.4854 with SHH STEEL — role: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service. SHH STEEL can produce and supply X6NiCrSiNCe35-25 as EN 10297-2 1.4854 seamless tube with honest scope boundaries. General engineering seamless acceptance is what this page sells; pressure, welded-pressure, and welded-general-purpose sisters are separate standards with separate MTCs. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
Grade advice stays practical for 1.4854. If the duty needs a sister chemistry, we point to 1.4835, 1.4876, 1.4845. Design caution for this number: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310 Export document packs are assembled to match the heat tags on the bundles you will receive. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310.
Supply Capability
SHH STEEL can produce and supply EN 10297-2 1.4854. SHH STEEL’s EN 10297-2 1.4854 offering is make-to-order seamless tube in X6NiCrSiNCe35-25. We can produce and supply cut lengths and standard mill lengths. Use the Stock / Available sizes map as a planning aid, then confirm live availability on the quote. Use thread: demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4854 / X6NiCrSiNCe35-25 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Stock / Available sizes note for 1.4854: bring the OD × wall list early. Context: specialty heat-service seamless OD. Bright CFA and polished CFP may add finishing lead time versus descaled CFD/HFD. Duty thread: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
When 1.4854 shares a project with 1.4835, 1.4876, 1.4845, keep separate heat identity tags. SHH STEEL can produce and supply coordinated size lists so fabrication receives matched OD bands without mixed certificates. Weld thread: matching 353MA-class fillers; high solution-anneal band ~1100–1150 °C.
FAQ
-
What is EN 10297-2 1.4854 seamless stainless steel tube used for?
- EN 10297-2 1.4854 (X6NiCrSiNCe35-25) is seamless tube for mechanical and general engineering — demanding furnace and heat-treatment equipment tubing, and high-temp process mechanical lines naming 353MA. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service.
-
Is EN 10297-2 1.4854 the same as EN 10216-5 1.4854?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4854 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4854 / X6NiCrSiNCe35-25?
- Delivery framing for 1.4854 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1100–1150 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4854?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4854 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4854 compare with sister grades 1.4835, 1.4876, 1.4845?
- 1.4854 / X6NiCrSiNCe35-25 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4835, 1.4876, 1.4845. Design caution: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310 Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4854 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching 353MA-class fillers; high solution-anneal band ~1100–1150 °C. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4854?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4854?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4854 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty heat-service seamless OD. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 353MA belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 353MA in body text and BOM notes, but lock EN 10297-2 and 1.4854 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4854?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: patented grade footnote; Ce and Si mandatory — not a silent dual of 1.4835 or commodity 310 Sister pointers: 1.4835, 1.4876, 1.4845. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4854 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4854 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4854 (X6NiCrSiNCe35-25) is seamless stainless tube for mechanical and general engineering — Ce-Si-N microalloyed high-Ni austenitic heat-resisting seamless tube (353MA-class) for severe high-temperature service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4835, 1.4876, 1.4845. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.