EN 10297-2 1.4835 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4835 Seamless Stainless Steel Tube

EN 10297-2 1.4835 / X9CrNiSiNCe21-11-2 seamless stainless general-purpose tube (253MA), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 310 MPa, Rm min 650 MPa, A long. min 37%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4835 / X9CrNiSiNCe21-11-2 (253MA — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4835 Seamless Stainless Steel Tube

EN 10297-2 covers seamless stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4835 is the austenitic heat-resisting grade X9CrNiSiNCe21-11-2, commercially discussed as 253MA. When the enquiry names 253MA seamless tube for general engineering heat service, EN 10297-2 1.4835 is the steel number that belongs on the order. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Mill path for 1.4835: heat-service seamless OD on specialty mill programmes. SHH STEEL can make and supply EN 10297-2 1.4835 / X9CrNiSiNCe21-11-2 as seamless general-purpose tube across heat-service seamless OD on specialty mill programmes, solution annealed or annealed/QT as the grade tables require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Use thread: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA.

On the shop floor people still say “253MA tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4835, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service. Typical duties include furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA. Design caution: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute. Caution thread: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute.

Do not treat an EN 10297-2 1.4835 MTC as automatic clearance for pressure equipment — Part 5 of EN 10216 is the pressure seamless home. Likewise, welded pressure tube lives under EN 10217-7, which is a different product form and test regime. Match the product standard to the duty before dual-marking talk begins. Role reminder for 1.4835: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Inside this seamless general-purpose series, compare EN 10297-2 1.4854, EN 10297-2 1.4833, EN 10297-2 1.4845. Hub: EN 10297-2.

Chemical Composition of EN 10297-2 1.4835

Cast window focus for 1.4835: Buying 253MA-family seamless tube without locking 1.4835 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X9CrNiSiNCe21-11-2; highlight elements for this grade include C 0.05–0.12, Cr 20.0–22.0, Ni 10.0–12.0, N 0.12–0.20, Si 1.40–2.50, Ce 0.03–0.08. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 253MA is body text only. Corrosion thread: rare-earth + Si for improved oxidation/spallation resistance in many furnace atmospheres.

Below is the BSSA-sourced EN 10297-2 chemistry window for 1.4835 (X9CrNiSiNCe21-11-2). Maxima apply unless a band is printed. SHH STEEL quotes against this window and reports actual cast values on the EN 10204 document — not a rewritten catalogue paraphrase. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Steel C Si Mn P S Cr Ni N Ce
1.4835 / X9CrNiSiNCe21-11-2 0.05–0.12 1.40–2.50 ≤1.00 ≤0.045 ≤0.015 20.0–22.0 10.0–12.0 0.12–0.20 0.03–0.08

Mechanical Properties of EN 10297-2 1.4835

Ambient floors focus for 1.4835: Ambient mechanical properties for EN 10297-2 1.4835 follow Tables 6–9 by family. For this grade the delivery-condition floors to watch are: Rp0.2 min 310 MPa, Rp1.0 min 350 MPa, Rm min 650 MPa, longitudinal elongation min 37%. Intergranular corrosion resistance per EN ISO 3651-2 is tabulated where applicable — see the IGC column on the mechanical table below. Family: austenitic heat-resisting. Caution thread: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 310 350 650 min 37 40 –

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4835 / X9CrNiSiNCe21-11-2. Guideline solution/anneal band (Annex B): 1020–1120 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4835

Seamless route narrative for 1.4835: EN 10297-2 does not offer a welded route for 1.4835. Tube in X9CrNiSiNCe21-11-2 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Order EN 10297-2 1.4835 with an Annex A surface/process symbol — HFD or CFD for metallically clean descaled tube, CFA when bright-annealed OD is required, CFG/CFP when ground or polished roughness is written into the purchase order. Weld thread: matching 253MA-class fillers; control heat input and Ce-bearing consumable availability.

For austenitic 1.4835, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4835 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1020–1120 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4835. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4835: heat-service seamless OD on specialty mill programmes. Use thread: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA.

Dimensions and Tolerances for EN 10297-2 1.4835

Dimensional order line for 1.4835: SHH STEEL aligns OD × wall, tolerance class, and process-route symbol for 1.4835 / X9CrNiSiNCe21-11-2 before rolling or drawing slots are locked. Heat-service seamless od on specialty mill programmes. Use thread: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA.

Length supply for 1.4835 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Size hint for 1.4835: heat-service seamless OD on specialty mill programmes. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Equivalent Grades for EN 10297-2 1.4835

Equivalence talk for 1.4835 starts with X9CrNiSiNCe21-11-2: 1.4835 / X9CrNiSiNCe21-11-2 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 253MA appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4854, 1.4833, 1.4845. Hook for buyers still using only the 253MA alias: lock EN 10297-2 1.4835 on the order line. Caution thread: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute.

Heat Treatment and Delivery Condition for EN 10297-2 1.4835

Austenitic 1.4835 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1020–1120 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching 253MA-class fillers; control heat input and Ce-bearing consumable availability.

Fabrication HT reminder for 1.4835 (+AT): For 1.4835, purchasers who need verified IGC after fabrication should say so with the applicable Option and method (EN ISO 3651-2 framing). Mill +AT or +A of the tube does not automatically clear a fabricator’s as-welded joint without procedure control. Delivery framing on the certificate for 1.4835 should match +AT. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Corrosion Resistance of EN 10297-2 1.4835

Corrosion behaviour of EN 10297-2 1.4835 tracks its austenitic heat-resisting balance: rare-earth + Si for improved oxidation/spallation resistance in many furnace atmospheres. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute Corrosion thread: rare-earth + Si for improved oxidation/spallation resistance in many furnace atmospheres.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4835 is filed as austenitic heat-resisting — pick tests that match that filing. Family filing for 1.4835 is austenitic heat-resisting. Caution thread: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute.

Applications of EN 10297-2 1.4835 Tube

Applications of EN 10297-2 1.4835 tube centre on mechanical and general engineering rather than PED pressure shells: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA. Role summary: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA.

Skip 1.4835 when the specification locks a different family — for example forcing ferritic 1.4835 into severe chloride process duty, or forcing a free-machining grade into welded corrosive service. Sister conversation inside EN 10297-2: 1.4854, 1.4833, 1.4845. Primary application sketch: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Weldability of EN 10297-2 1.4835

1.4835 / X9CrNiSiNCe21-11-2 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching 253MA-class fillers; control heat input and Ce-bearing consumable availability. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching 253MA-class fillers; control heat input and Ce-bearing consumable availability.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute Filler/shop note for 1.4835: matching 253MA-class fillers; control heat input and Ce-bearing consumable availability. Caution thread: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute.

Surface Finishes for EN 10297-2 1.4835

Finish selection for 1.4835 on Annex A: Interior Ra limits, electropolish, or special protection for X9CrNiSiNCe21-11-2 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4835 when the mill can measure and report the finish. Alias reminder: commercial talk may say 253MA, but the finish symbol still belongs on the EN 10297-2 line. Use thread: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA.

Storage guidance for 1.4835: keep bundles off bare concrete in coastal yards, avoid chloride-bearing tarps against CFA OD, and leave end caps fitted until fabrication. Special export crate liners are available when the packing note asks for them. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Inspection and Testing for EN 10297-2 1.4835

Inspection lot framing for 1.4835 in austenitic heat-resisting: SHH STEEL EN 10204 3.1 documents for 1.4835 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4835 heat identity intact from cast through bundle tag. Weld thread: matching 253MA-class fillers; control heat input and Ce-bearing consumable availability.

Technological tests on 1.4835 follow the order matrix — they are not assumed. IGC, when required, cites EN ISO 3651-2. Stencil or inkjet marking stays light on polished OD so the finish remains acceptable after receipt inspection. Use thread: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA.

Packaging and Shipping for EN 10297-2 1.4835

Dispatch note for 1.4835 (253MA body alias only): Finished EN 10297-2 1.4835 (X9CrNiSiNCe21-11-2) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Marking and identity for 1.4835: Marking typically includes manufacturer identity, dimensions, EN 10297-2, steel name or number 1.4835, cast/code, inspection mark, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging CFA/CFP surfaces. Finish-sensitive packing for 1.4835 follows the Annex A symbol on the order. Use thread: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA.

Packing lists for 1.4835 map bundle IDs to heats and sizes so receiving inspection can clear documents without unpacking every crate. Damaged wrap discovered at destination is reported with photos before the material is issued to fabrication. Caution thread: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10297-2 1.4835 seamless stainless steel tube. Why 1.4835 with SHH STEEL — role: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service. Choose SHH STEEL for EN 10297-2 1.4835 when you need a mill partner who will not blur EN 10297-2 with EN 10216-5 or EN 10217-7 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

Grade advice stays practical for 1.4835. If the duty needs a sister chemistry, we point to 1.4854, 1.4833, 1.4845. Design caution for this number: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute Quotes state scope boundaries in plain language so purchasing and engineering share the same acceptance standard. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute.

Supply Capability

Supply capability for EN 10297-2 1.4835 / X9CrNiSiNCe21-11-2 starts with your OD × wall list and delivery-condition choice. SHH STEEL can produce and supply against that list with EN 10204 3.1 documents; the Stock / Available sizes block frames enquiry sizes rather than a public warehouse catalogue. Use thread: furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4835 / X9CrNiSiNCe21-11-2
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Available sizes conversation for 1.4835 starts with your OD × wall matrix. Typical note: heat-service seamless OD on specialty mill programmes. Send preferred delivery condition (+A / +AT / +QT as applicable) and any eddy-current or hydrostatic Options with the size list. Duty thread: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.

On 1.4835, Options and sister duals (1.4854, 1.4833, 1.4845) belong on the same enquiry as the size list. SHH STEEL can produce and supply production heats after a short pilot when forming or polish trials are required. Weld thread: matching 253MA-class fillers; control heat input and Ce-bearing consumable availability.

FAQ

What is EN 10297-2 1.4835 seamless stainless steel tube used for?
EN 10297-2 1.4835 (X9CrNiSiNCe21-11-2) is seamless tube for mechanical and general engineering — furnace rollers adjacent tubing, heat-treatment fixtures, and high-temp process mechanical lines naming 253MA. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service.
Is EN 10297-2 1.4835 the same as EN 10216-5 1.4835?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4835 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4835 / X9CrNiSiNCe21-11-2?
Delivery framing for 1.4835 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1020–1120 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4835?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4835 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4835 compare with sister grades 1.4854, 1.4833, 1.4845?
1.4835 / X9CrNiSiNCe21-11-2 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4854, 1.4833, 1.4845. Design caution: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4835 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching 253MA-class fillers; control heat input and Ce-bearing consumable availability. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4835?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4835?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4835 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: heat-service seamless OD on specialty mill programmes. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 253MA belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 253MA in body text and BOM notes, but lock EN 10297-2 and 1.4835 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4835?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: Ce and Si ranges are mandatory on cast analysis — commodity 309/310 is not a silent substitute Sister pointers: 1.4854, 1.4833, 1.4845. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4835 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4835 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4835 (X9CrNiSiNCe21-11-2) is seamless stainless tube for mechanical and general engineering — Ce-Si-N microalloyed austenitic heat-resisting seamless tube (253MA-class) for high-temperature oxidising service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4854, 1.4833, 1.4845. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X