EN 10297-2 1.4410 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4410 Seamless Stainless Steel Tube

EN 10297-2 1.4410 / X2CrNiMoN25-7-4 seamless stainless general-purpose tube (2507 / superduplex), duplex (austenitic-ferritic), cast analysis per EN table, ambient Rp0.2 min 550 MPa, Rm min 800 MPa, A long. min 20%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4410 / X2CrNiMoN25-7-4 (2507 / superduplex — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4410 Seamless Stainless Steel Tube

EN 10297-2:2005 (BS EN 10297-2:2005) is the European product standard for seamless circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10216-5, and not for welded general-purpose tube under EN 10296-2. Steel number 1.4410 is listed as X2CrNiMoN25-7-4 in the austenitic-ferritic (duplex) set. EN 10297-2 1.4410 is superduplex seamless for general engineering — when PED pressure governs, pair or switch to EN 10216-5 1.4410. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Mill path for 1.4410: specialty seamless OD on mill programme. SHH STEEL can produce and supply X2CrNiMoN25-7-4 under EN 10297-2 1.4410 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines.

On the shop floor people still say “2507 / superduplex tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4410, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength. Typical duties include seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines. Design caution: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS. Caution thread: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS.

Scope discipline matters: 1.4410 under EN 10297-2 is seamless general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Role reminder for 1.4410: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Inside this seamless general-purpose series, compare EN 10297-2 1.4501, EN 10297-2 1.4462, EN 10297-2 1.4507, EN 10297-2 1.4547. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4410. ASTM/ASME related product pages (not interchangeable by default): A789 S32750.

Chemical Composition of EN 10297-2 1.4410

Cast window focus for 1.4410: Buying 2507 / superduplex-family seamless tube without locking 1.4410 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X2CrNiMoN25-7-4; highlight elements for this grade include C ≤0.030, Cr 24.0–26.0, Ni 6.0–8.0, Mo 3.0–4.5, N 0.24–0.35, Si ≤1.00. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 2507 / superduplex is body text only. Corrosion thread: superduplex PREN-type performance for severe seawater and halide duties — no invented PREN digits in copy.

Chemical limits for 1.4410 / X2CrNiMoN25-7-4 under EN 10297-2 appear in the table underneath. Source priority is BSSA’s EN 10297-2 article cross-checked to the 2005 grade list. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Steel C Si Mn P S Cr Mo Ni N
1.4410 / X2CrNiMoN25-7-4 ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.015 24.0–26.0 3.0–4.5 6.0–8.0 0.24–0.35

Mechanical Properties of EN 10297-2 1.4410

Ambient floors focus for 1.4410: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4410 order. General-purpose Table values for this number read: Rp0.2 min 550 MPa, Rp1.0 min 640 MPa, Rm min 800 MPa, longitudinal elongation min 20%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: duplex (austenitic-ferritic). Caution thread: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 550 640 800 min 20 20 Yes

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4410 / X2CrNiMoN25-7-4. Guideline solution/anneal band (Annex B): 1040–1120 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4410

Seamless route narrative for 1.4410: EN 10297-2 1.4410 is seamless only — pierced or extruded hollows are hot-worked and may be cold-finished to size before heat treatment. Duplex X2CrNiMoN25-7-4 needs controlled thermomechanical history so the ferrite–austenite balance lands in the ordered window after +AT. Annex A process-route symbols for seamless 1.4410 include HFD (hot finished, heat treated, descaled), CFD (cold finished, heat treated, descaled), CFA (cold finished bright annealed), CFG (ground), and CFP (polished). Combinations may be agreed at enquiry. Weld thread: superduplex fillers; strict heat input, interpass, and ferrite control.

For duplex 1.4410, solution annealing and rapid cooling are part of the product story, not an optional cosmetic step. Ferritic 1.4410 ships annealed (+A). Annex B points at roughly 1040–1120 °C with water or air cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. NDT Options (eddy current, ultrasonic, leak or hydrostatic) are selected on the order; they are not a substitute for correct duplex heat treatment. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Optional tests under EN 10297-2 for 1.4410 include leak testing, hydrostatic testing, and NDT such as eddy current or ultrasonic methods agreed at enquiry. SHH STEEL records the Options actually performed on the inspection document — we do not claim a test that was not run. Size context for 1.4410: specialty seamless OD on mill programme. Use thread: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines.

Dimensions and Tolerances for EN 10297-2 1.4410

Dimensional order line for 1.4410: Dimensional orders for 1.4410 name OD × wall, length tolerance, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Specialty seamless od on mill programme. Use thread: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines.

For precision mechanical duty on 1.4410, cold-finished CFA/CFD routes are the usual conversation; heavier structural or heat-service walls may stay hot-finished HFD. Agree eccentricity and straightness when the assembly stack-up is tight. Size hint for 1.4410: specialty seamless OD on mill programme. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Equivalent Grades for EN 10297-2 1.4410

Equivalence talk for 1.4410 starts with X2CrNiMoN25-7-4: 1.4410 / X2CrNiMoN25-7-4 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 2507 / superduplex appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4501, 1.4462, 1.4507, 1.4547. Hook for buyers still using only the 2507 / superduplex alias: lock EN 10297-2 1.4410 on the order line. Caution thread: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS.

Heat Treatment and Delivery Condition for EN 10297-2 1.4410

Ferritic 1.4410 ships annealed (+A). Annex B points at roughly 1040–1120 °C with water or air cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Weld thread: superduplex fillers; strict heat input, interpass, and ferrite control.

Fabrication HT reminder for 1.4410 (+AT): Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4410, restore the delivery condition agreed on the order before corrosive or load-bearing service. Delivery framing on the certificate for 1.4410 should match +AT. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Corrosion Resistance of EN 10297-2 1.4410

Corrosion behaviour of EN 10297-2 1.4410 tracks its austenitic-ferritic (duplex) balance: superduplex PREN-type performance for severe seawater and halide duties — no invented PREN digits in copy. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS Corrosion thread: superduplex PREN-type performance for severe seawater and halide duties — no invented PREN digits in copy.

Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4501, 1.4462, 1.4507, 1.4547 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4410 is duplex (austenitic-ferritic). Caution thread: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS.

Applications of EN 10297-2 1.4410 Tube

Applications of EN 10297-2 1.4410 tube centre on mechanical and general engineering rather than PED pressure shells: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines. Role summary: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines.

It is the wrong first choice when a welded product form is mandatory (use EN 10296-2 or EN 10217-7 as applicable), when PED pressure seamless acceptance is locked to EN 10216-5 alone, or when the medium clearly needs a sister such as 1.4501. Primary application sketch: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Weldability of EN 10297-2 1.4410

1.4410 / X2CrNiMoN25-7-4 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: superduplex fillers; strict heat input, interpass, and ferrite control. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: superduplex fillers; strict heat input, interpass, and ferrite control.

Filler selection should match or over-alloy the base X2CrNiMoN25-7-4 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, martensitic, duplex, or heat-resisting — not a single shop habit. Filler/shop note for 1.4410: superduplex fillers; strict heat input, interpass, and ferrite control. Caution thread: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS.

Surface Finishes for EN 10297-2 1.4410

Finish selection for 1.4410 on Annex A: Interior Ra limits, electropolish, or special protection for X2CrNiMoN25-7-4 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4410 when the mill can measure and report the finish. Alias reminder: commercial talk may say 2507 / superduplex, but the finish symbol still belongs on the EN 10297-2 line. Use thread: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines.

During delivery of 1.4410, SHH STEEL can add edge guards, VCI paper, or sealed PE wrap when the enquiry lists them. Descaled engineering finishes still need caps; bright and polished finishes need full OD sleeve protection. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Inspection and Testing for EN 10297-2 1.4410

Inspection lot framing for 1.4410 in duplex (austenitic-ferritic): SHH STEEL EN 10204 3.1 documents for 1.4410 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4410 heat identity intact from cast through bundle tag. Weld thread: superduplex fillers; strict heat input, interpass, and ferrite control.

Inspection documents for 1.4410 list every Optional test that actually ran. Surrogate “typical” NDT language is never printed. Tube marking repeats the steel number 1.4410 so warehouse staff cannot confuse sister heats in the same bundle bay. Use thread: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines.

Packaging and Shipping for EN 10297-2 1.4410

Dispatch note for 1.4410 (2507 / superduplex body alias only): Finished EN 10297-2 1.4410 (X2CrNiMoN25-7-4) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Marking and identity for 1.4410: Marking typically includes manufacturer identity, dimensions, EN 10297-2, steel name or number 1.4410, cast/code, inspection mark, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging CFA/CFP surfaces. Finish-sensitive packing for 1.4410 follows the Annex A symbol on the order. Use thread: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines.

For 1.4410, export documentation includes packing list, certificate, and any third-party release notes agreed at order. Heat segregation rules stay in force when multiple steel numbers share a container. Caution thread: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS.

Why Choose SHH STEEL

Why 1.4410 with SHH STEEL — role: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength. SHH STEEL can produce and supply EN 10297-2 1.4410 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “2507 / superduplex tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Grade advice stays practical for 1.4410. If the duty needs a sister chemistry, we point to 1.4501, 1.4462, 1.4507, 1.4547. Design caution for this number: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS If the file later becomes PED pressure seamless, we help retarget EN 10216-5 rather than relabeling a general-purpose MTC. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS.

Supply Capability

SHH STEEL can produce and supply EN 10297-2 1.4410. Ask SHH STEEL for EN 10297-2 1.4410 when you need seamless general-purpose X2CrNiMoN25-7-4 with named Options. We can produce and supply trial lengths or production heats once OD, wall, finish symbol, and test Options are clear. See Stock / Available sizes below. Use thread: seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4410 / X2CrNiMoN25-7-4
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Enquiry stock map — EN 10297-2 1.4410 / X2CrNiMoN25-7-4: specialty seamless OD on mill programme. SHH STEEL will mark which rows can roll on current hollows versus which need a fresh heat. No invented warehouse tonnages appear on this page. Duty thread: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.

Sister comparisons for 1.4410 usually include 1.4501, 1.4462, 1.4507, 1.4547. Dimensional acceptance remains the EN 10297-2 order text, not a peer brochure. SHH STEEL can produce and supply mixed sister bundles when heats and finishes align. Weld thread: superduplex fillers; strict heat input, interpass, and ferrite control.

FAQ

What is EN 10297-2 1.4410 seamless stainless steel tube used for?
EN 10297-2 1.4410 (X2CrNiMoN25-7-4) is seamless tube for mechanical and general engineering — seawater systems, oil-and-gas-adjacent mechanical tubing, and aggressive chloride process lines. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength.
Is EN 10297-2 1.4410 the same as EN 10216-5 1.4410?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4410 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4410 / X2CrNiMoN25-7-4?
Delivery framing for 1.4410 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1040–1120 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4410?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4410 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4410 compare with sister grades 1.4501, 1.4462, 1.4507?
1.4410 / X2CrNiMoN25-7-4 is filed as duplex (austenitic-ferritic). Typical sisters discussed on the same RFQ are 1.4501, 1.4462, 1.4507. Design caution: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4410 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: superduplex fillers; strict heat input, interpass, and ferrite control. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4410?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4410?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4410 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty seamless OD on mill programme. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 2507 / superduplex belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 2507 / superduplex in body text and BOM notes, but lock EN 10297-2 and 1.4410 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4410?
Move when chloride pitting, crevice attack, or SCC risk exceeds what duplex (austenitic-ferritic) practice can defend for the temperature and stress state. Caution for this number: patented grade footnote; fabrication and HT windows are tighter than 2205 — use qualified duplex WPS Sister pointers: 1.4501, 1.4462, 1.4507. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4410 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4410 is filed as duplex (austenitic-ferritic). If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4410 (X2CrNiMoN25-7-4) is seamless stainless tube for mechanical and general engineering — superduplex seamless tube (2507-class) for severe chloride mechanical service needing high strength. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4501, 1.4462, 1.4507. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X