EN 10297-2 1.4439 Seamless Stainless Steel Tube
What is EN 10297-2 1.4439 Seamless Stainless Steel Tube
If the purchase file still names only a commercial alias such as 317LMN without a product standard, the mill cannot know whether general-purpose seamless acceptance or pressure-tube acceptance applies. EN 10297-2 plus steel number 1.4439 (X2CrNiMoN17-13-5) selects seamless tube for mechanical and general engineering. 1.4439 sits in EN 10297-2 for buyers who need more Mo than 1.4435 without jumping straight to 6Mo 1.4547/1.4529. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Mill path for 1.4439: specialty seamless OD on enquiry. SHH STEEL can produce and supply EN 10297-2 1.4439 seamless stainless steel tube — hot-finished or cold-finished on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, hydrostatic, eddy current, ultrasonic, and related NDT Options). Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry.
On the shop floor people still say “317LMN tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4439, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys. Typical duties include severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry. Design caution: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits. Caution thread: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits.
Scope discipline matters: 1.4439 under EN 10297-2 is seamless general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Role reminder for 1.4439: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Inside this seamless general-purpose series, compare EN 10297-2 1.4435, EN 10297-2 1.4429, EN 10297-2 1.4539, EN 10297-2 1.4547. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4439. ASTM/ASME related product pages (not interchangeable by default): A269 TP316L.
Chemical Composition of EN 10297-2 1.4439
Cast window focus for 1.4439: Buying 317LMN-family seamless tube without locking 1.4439 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X2CrNiMoN17-13-5; highlight elements for this grade include C ≤0.030, Cr 16.5–18.5, Ni 12.5–14.5, Mo 4.0–5.0, N 0.12–0.22, Si ≤1.00. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 317LMN is body text only. Corrosion thread: high Mo plus nitrogen for aggressive chloride pitting/crevice environments within austenitic scope.
Use the table as a working cast-analysis checklist for 1.4439 (X2CrNiMoN17-13-5). It mirrors public BSSA EN 10297-2 figures for buyer convenience; contractual acceptance still cites the edition named on the purchase order. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
| Steel | C | Si | Mn | P | S | Cr | Mo | Ni | N |
|---|---|---|---|---|---|---|---|---|---|
| 1.4439 / X2CrNiMoN17-13-5 | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.015 | 16.5–18.5 | 4.0–5.0 | 12.5–14.5 | 0.12–0.22 |
Mechanical Properties of EN 10297-2 1.4439
Ambient floors focus for 1.4439: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4439 order. General-purpose Table values for this number read: Rp0.2 min 285 MPa, Rp1.0 min 315 MPa, Rm min 580 MPa, longitudinal elongation min 35%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic corrosion-resisting. Caution thread: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 285 | 315 | 580 min | 35 | 30 | Yes |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4439 / X2CrNiMoN17-13-5. Guideline solution/anneal band (Annex B): 1060–1140 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4439
Seamless route narrative for 1.4439: EN 10297-2 does not offer a welded route for 1.4439. Tube in X2CrNiMoN17-13-5 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Order EN 10297-2 1.4439 with an Annex A surface/process symbol — HFD or CFD for metallically clean descaled tube, CFA when bright-annealed OD is required, CFG/CFP when ground or polished roughness is written into the purchase order. Weld thread: matching high-Mo N-bearing fillers; high solution-anneal band after heavy fabrication.
For austenitic 1.4439, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4439 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1060–1140 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Optional tests under EN 10297-2 for 1.4439 include leak testing, hydrostatic testing, and NDT such as eddy current or ultrasonic methods agreed at enquiry. SHH STEEL records the Options actually performed on the inspection document — we do not claim a test that was not run. Size context for 1.4439: specialty seamless OD on enquiry. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry.
Dimensions and Tolerances for EN 10297-2 1.4439
Dimensional order line for 1.4439: Order EN 10297-2 1.4439 by outside diameter D and wall thickness T for steel name X2CrNiMoN17-13-5. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Specialty seamless od on enquiry. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry.
Length supply for 1.4439 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Size hint for 1.4439: specialty seamless OD on enquiry. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Equivalent Grades for EN 10297-2 1.4439
Equivalence talk for 1.4439 starts with X2CrNiMoN17-13-5: 1.4439 / X2CrNiMoN17-13-5 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 317LMN appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4435, 1.4429, 1.4539, 1.4547. Hook for buyers still using only the 317LMN alias: lock EN 10297-2 1.4439 on the order line. Caution thread: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits.
Heat Treatment and Delivery Condition for EN 10297-2 1.4439
Austenitic 1.4439 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1060–1140 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: matching high-Mo N-bearing fillers; high solution-anneal band after heavy fabrication.
Fabrication HT reminder for 1.4439 (+AT): Hot-working temperature bands in Annex B for X2CrNiMoN17-13-5 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4439 should match +AT. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Corrosion Resistance of EN 10297-2 1.4439
Corrosion behaviour of EN 10297-2 1.4439 tracks its austenitic corrosion-resisting balance: high Mo plus nitrogen for aggressive chloride pitting/crevice environments within austenitic scope. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits Corrosion thread: high Mo plus nitrogen for aggressive chloride pitting/crevice environments within austenitic scope.
SHH STEEL does not invent PREN, CPT, or CCT marketing digits for 1.4439. When a purchaser supplies a qualified corrosion dossier, we match chemistry and delivery condition to that dossier; otherwise we stay with tabulated standard facts and plain-language family guidance. Family filing for 1.4439 is austenitic corrosion-resisting. Caution thread: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits.
Applications of EN 10297-2 1.4439 Tube
Applications of EN 10297-2 1.4439 tube centre on mechanical and general engineering rather than PED pressure shells: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry. Role summary: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry.
Typical BOM language pairs EN 10297-2 1.4439 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “317LMN” substitutions do not creep in. Primary application sketch: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Weldability of EN 10297-2 1.4439
1.4439 / X2CrNiMoN17-13-5 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching high-Mo N-bearing fillers; high solution-anneal band after heavy fabrication. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching high-Mo N-bearing fillers; high solution-anneal band after heavy fabrication.
When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Filler/shop note for 1.4439: matching high-Mo N-bearing fillers; high solution-anneal band after heavy fabrication. Caution thread: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits.
Surface Finishes for EN 10297-2 1.4439
Finish selection for 1.4439 on Annex A: For 1.4439, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 317LMN, but the finish symbol still belongs on the EN 10297-2 line. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry.
If 1.4439 will sit in a humid warehouse before use, ask for sealed wrap and humidity indicators on the packing list. Carbon-steel dunnage never contacts the stainless OD — timber or plastic separators are the default. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Inspection and Testing for EN 10297-2 1.4439
Inspection lot framing for 1.4439 in austenitic corrosion-resisting: SHH STEEL EN 10204 3.1 documents for 1.4439 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a hydrostatic or eddy-current line unless that Option was executed. Keep 1.4439 heat identity intact from cast through bundle tag. Weld thread: matching high-Mo N-bearing fillers; high solution-anneal band after heavy fabrication.
For 1.4439, dimensional inspection covers OD, wall, length, and agreed out-of-roundness/eccentricity. IGC and NDT Options appear as separate certificate lines. Correlation numbers link pieces to the EN 10204 3.1 file without opening every crate. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry.
Packaging and Shipping for EN 10297-2 1.4439
Dispatch note for 1.4439 (317LMN body alias only): Finished EN 10297-2 1.4439 (X2CrNiMoN17-13-5) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Marking and identity for 1.4439: Marking typically includes manufacturer identity, dimensions, EN 10297-2, steel name or number 1.4439, cast/code, inspection mark, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging CFA/CFP surfaces. Finish-sensitive packing for 1.4439 follows the Annex A symbol on the order. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry.
SHH STEEL closes the packing note for 1.4439 only after caps, wrap, and tags match the Annex A finish and the cut-length list. Shortages or mixed walls are corrected in the warehouse — not discovered at the jobsite. Caution thread: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits.
Why Choose SHH STEEL
Why 1.4439 with SHH STEEL — role: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys. SHH STEEL can produce and supply X2CrNiMoN17-13-5 as EN 10297-2 1.4439 seamless tube with honest scope boundaries. General engineering seamless acceptance is what this page sells; pressure, welded-pressure, and welded-general-purpose sisters are separate standards with separate MTCs. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
Grade advice stays practical for 1.4439. If the duty needs a sister chemistry, we point to 1.4435, 1.4429, 1.4539, 1.4547. Design caution for this number: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits Mill slots are planned against the Annex A symbol you order — bright and polished finishes are not assumed. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits.
Supply Capability
SHH STEEL can produce and supply EN 10297-2 1.4439. EN 10297-2 1.4439 supply from SHH STEEL covers hot- and cold-finished seamless routes for X2CrNiMoN17-13-5. We can produce and supply to the mechanical floors of the ordered delivery condition. The Stock / Available sizes section is the enquiry checklist. Use thread: severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4439 / X2CrNiMoN17-13-5 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
For 1.4439, treat the size table as an RFQ aid. Context: specialty seamless OD on enquiry. Confirm tolerance class and Annex A symbol so CFD/CFA slots are not confused with HFD on the acknowledgement. Duty thread: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
For 1.4439, ask early about cut-to-length packages and NDT Options. Peer mill size charts are indicative only. SHH STEEL can produce and supply the ordered Annex A finish once the acknowledgement locks OD × wall. Sisters often discussed: 1.4435, 1.4429, 1.4539, 1.4547. Weld thread: matching high-Mo N-bearing fillers; high solution-anneal band after heavy fabrication.
FAQ
-
What is EN 10297-2 1.4439 seamless stainless steel tube used for?
- EN 10297-2 1.4439 (X2CrNiMoN17-13-5) is seamless tube for mechanical and general engineering — severe chloride process mechanical lines, pulp-adjacent utilities, and duties naming 317LMN chemistry. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys.
-
Is EN 10297-2 1.4439 the same as EN 10216-5 1.4439?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4439 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4439 / X2CrNiMoN17-13-5?
- Delivery framing for 1.4439 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1060–1140 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4439?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4439 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4439 compare with sister grades 1.4435, 1.4429, 1.4539?
- 1.4439 / X2CrNiMoN17-13-5 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4435, 1.4429, 1.4539. Design caution: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4439 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching high-Mo N-bearing fillers; high solution-anneal band after heavy fabrication. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4439?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4439?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4439 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty seamless OD on enquiry. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 317LMN belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 317LMN in body text and BOM notes, but lock EN 10297-2 and 1.4439 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4439?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: not automatic dual with 1.4547 — Mo and Ni windows differ; confirm PREN-type thinking against the actual medium without inventing digits Sister pointers: 1.4435, 1.4429, 1.4539. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4439 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4439 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4439 (X2CrNiMoN17-13-5) is seamless stainless tube for mechanical and general engineering — 5%Mo nitrogen-bearing austenitic seamless tube (317LMN-class) bridging commodity 316L and 6Mo alloys. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4435, 1.4429, 1.4539. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.