EN 10297-2 1.4833 Seamless Stainless Steel Tube
What is EN 10297-2 1.4833 Seamless Stainless Steel Tube
Mechanical and general engineering projects that need seamless stainless tube under a European product standard look to EN 10297-2:2005 — Part 2 of EN 10297 — rather than a PED pressure Part 5 page or an ASTM tubing habit alone. 1.4833 / X12CrNi23-13 sits in the austenitic heat-resisting tables. Shop “309S tube” for heat service maps to EN 10297-2 1.4833 in the heat-resisting set — not to a corrosion-resisting 18-8 page. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Mill path for 1.4833: heat-service seamless OD, HFD/CFD common. SHH STEEL can produce and supply EN 10297-2 1.4833 seamless stainless steel tube — hot-finished or cold-finished on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, hydrostatic, eddy current, ultrasonic, and related NDT Options). Use thread: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases.
On the shop floor people still say “309S tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4833, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty. Typical duties include furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases. Design caution: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice. Caution thread: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice.
EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4833: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Inside this seamless general-purpose series, compare EN 10297-2 1.4845, EN 10297-2 1.4878, EN 10297-2 1.4835. Hub: EN 10297-2.
Chemical Composition of EN 10297-2 1.4833
Cast window focus for 1.4833: Every 1.4833 heat under EN 10297-2 must meet the cast (ladle) analysis for X12CrNi23-13 in the austenitic heat-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 309S is body text only. Corrosion thread: oxidation resistance of 309-class heat-resisting austenitic practice.
Chemical limits for 1.4833 / X12CrNi23-13 under EN 10297-2 appear in the table underneath. Source priority is BSSA’s EN 10297-2 article cross-checked to the 2005 grade list. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
| Steel | C | Si | Mn | P | S | Cr | Ni | N |
|---|---|---|---|---|---|---|---|---|
| 1.4833 / X12CrNi23-13 | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.015 | 22.0–24.0 | 12.0–14.0 | ≤0.11 |
Mechanical Properties of EN 10297-2 1.4833
Ambient floors focus for 1.4833: Table mechanical floors for 1.4833 / X12CrNi23-13 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 210 MPa, Rp1.0 min 250 MPa, Rm min 500 MPa, longitudinal elongation min 33%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Family: austenitic heat-resisting. Caution thread: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 210 | 250 | 500 min | 33 | 35 | – |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4833 / X12CrNi23-13. Guideline solution/anneal band (Annex B): 1050–1150 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4833
Seamless route narrative for 1.4833: EN 10297-2 does not offer a welded route for 1.4833. Tube in X12CrNi23-13 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Seamless manufacture for 1.4833 finishes through hot- or cold-finished routes. Pick HFD/CFD for descaled engineering surfaces, CFA for bright anneal, and CFG or CFP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Weld thread: 309-class fillers; solution anneal guidance 1050–1150 °C.
For austenitic 1.4833, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4833 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1050–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4833. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4833: heat-service seamless OD, HFD/CFD common. Use thread: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases.
Dimensions and Tolerances for EN 10297-2 1.4833
Dimensional order line for 1.4833: Order EN 10297-2 1.4833 by outside diameter D and wall thickness T for steel name X12CrNi23-13. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Heat-service seamless od, hfd/cfd common. Use thread: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases.
For precision mechanical duty on 1.4833, cold-finished CFA/CFD routes are the usual conversation; heavier structural or heat-service walls may stay hot-finished HFD. Agree eccentricity and straightness when the assembly stack-up is tight. Size hint for 1.4833: heat-service seamless OD, HFD/CFD common. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Equivalent Grades for EN 10297-2 1.4833
Equivalence talk for 1.4833 starts with X12CrNi23-13: 1.4833 / X12CrNi23-13 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 309S appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4845, 1.4878, 1.4835. Hook for buyers still using only the 309S alias: lock EN 10297-2 1.4833 on the order line. Caution thread: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice.
Heat Treatment and Delivery Condition for EN 10297-2 1.4833
Austenitic 1.4833 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1050–1150 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: 309-class fillers; solution anneal guidance 1050–1150 °C.
Fabrication HT reminder for 1.4833 (+AT): Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4833, restore the delivery condition agreed on the order before corrosive or load-bearing service. Delivery framing on the certificate for 1.4833 should match +AT. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Corrosion Resistance of EN 10297-2 1.4833
Corrosion behaviour of EN 10297-2 1.4833 tracks its austenitic heat-resisting balance: oxidation resistance of 309-class heat-resisting austenitic practice. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice Corrosion thread: oxidation resistance of 309-class heat-resisting austenitic practice.
For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4833 is filed as austenitic heat-resisting — pick tests that match that filing. Family filing for 1.4833 is austenitic heat-resisting. Caution thread: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice.
Applications of EN 10297-2 1.4833 Tube
Applications of EN 10297-2 1.4833 tube centre on mechanical and general engineering rather than PED pressure shells: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases. Role summary: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases.
Typical BOM language pairs EN 10297-2 1.4833 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “309S” substitutions do not creep in. Primary application sketch: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Weldability of EN 10297-2 1.4833
1.4833 / X12CrNi23-13 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: 309-class fillers; solution anneal guidance 1050–1150 °C. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: 309-class fillers; solution anneal guidance 1050–1150 °C.
When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Filler/shop note for 1.4833: 309-class fillers; solution anneal guidance 1050–1150 °C. Caution thread: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice.
Surface Finishes for EN 10297-2 1.4833
Finish selection for 1.4833 on Annex A: Surface finish on EN 10297-2 1.4833 is carried by the Annex A symbol: descaled HFD/CFD for general mechanical tube, bright-annealed CFA for cleaner OD appearance, and ground CFG or polished CFP when roughness is agreed at enquiry. Carbon-steel strapping must not contact the stainless surface. Alias reminder: commercial talk may say 309S, but the finish symbol still belongs on the EN 10297-2 line. Use thread: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases.
During delivery of 1.4833, SHH STEEL can add edge guards, VCI paper, or sealed PE wrap when the enquiry lists them. Descaled engineering finishes still need caps; bright and polished finishes need full OD sleeve protection. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Inspection and Testing for EN 10297-2 1.4833
Inspection lot framing for 1.4833 in austenitic heat-resisting: Specific inspection applies to EN 10297-2 1.4833 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Keep 1.4833 heat identity intact from cast through bundle tag. Weld thread: 309-class fillers; solution anneal guidance 1050–1150 °C.
Inspection documents for 1.4833 list every Optional test that actually ran. Surrogate “typical” NDT language is never printed. Tube marking repeats the steel number 1.4833 so warehouse staff cannot confuse sister heats in the same bundle bay. Use thread: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases.
Packaging and Shipping for EN 10297-2 1.4833
Dispatch note for 1.4833 (309S body alias only): Finished EN 10297-2 1.4833 (X12CrNi23-13) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Marking and identity for 1.4833: For 1.4833, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Finish-sensitive packing for 1.4833 follows the Annex A symbol on the order. Use thread: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases.
For 1.4833, export documentation includes packing list, certificate, and any third-party release notes agreed at order. Heat segregation rules stay in force when multiple steel numbers share a container. Caution thread: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice.
Why Choose SHH STEEL
SHH STEEL can produce and supply EN 10297-2 1.4833 seamless stainless steel tube. Why 1.4833 with SHH STEEL — role: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty. Choose SHH STEEL for EN 10297-2 1.4833 when you need a mill partner who will not blur EN 10297-2 with EN 10216-5 or EN 10217-7 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Grade advice stays practical for 1.4833. If the duty needs a sister chemistry, we point to 1.4845, 1.4878, 1.4835. Design caution for this number: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice If the file later becomes PED pressure seamless, we help retarget EN 10216-5 rather than relabeling a general-purpose MTC. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice.
Supply Capability
SHH STEEL can produce and supply EN 10297-2 1.4833. Ask SHH STEEL for EN 10297-2 1.4833 when you need seamless general-purpose X12CrNi23-13 with named Options. We can produce and supply trial lengths or production heats once OD, wall, finish symbol, and test Options are clear. See Stock / Available sizes below. Use thread: furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4833 / X12CrNi23-13 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Enquiry stock map — EN 10297-2 1.4833 / X12CrNi23-13: heat-service seamless OD, HFD/CFD common. SHH STEEL will mark which rows can roll on current hollows versus which need a fresh heat. No invented warehouse tonnages appear on this page. Duty thread: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
Sister comparisons for 1.4833 usually include 1.4845, 1.4878, 1.4835. Dimensional acceptance remains the EN 10297-2 order text, not a peer brochure. SHH STEEL can produce and supply mixed sister bundles when heats and finishes align. Weld thread: 309-class fillers; solution anneal guidance 1050–1150 °C.
FAQ
-
What is EN 10297-2 1.4833 seamless stainless steel tube used for?
- EN 10297-2 1.4833 (X12CrNi23-13) is seamless tube for mechanical and general engineering — furnace parts, heat shields, and high-temperature mechanical tubing in oxidising gases. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty.
-
Is EN 10297-2 1.4833 the same as EN 10216-5 1.4833?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4833 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4833 / X12CrNi23-13?
- Delivery framing for 1.4833 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1050–1150 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4833?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4833 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4833 compare with sister grades 1.4845, 1.4878, 1.4835?
- 1.4833 / X12CrNi23-13 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4845, 1.4878, 1.4835. Design caution: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4833 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: 309-class fillers; solution anneal guidance 1050–1150 °C. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4833?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4833?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4833 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: heat-service seamless OD, HFD/CFD common. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 309S belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 309S in body text and BOM notes, but lock EN 10297-2 and 1.4833 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4833?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: carbon up to 0.15% — distinguish from corrosion-resisting low-C sisters; not for aqueous chloride process as first choice Sister pointers: 1.4845, 1.4878, 1.4835. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4833 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4833 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4833 (X12CrNi23-13) is seamless stainless tube for mechanical and general engineering — 23Cr-13Ni austenitic heat-resisting seamless tube (309S-class) for oxidising elevated-temperature mechanical duty. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4845, 1.4878, 1.4835. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.