EN 10297-2 1.4460 Seamless Stainless Steel Tube

EN 10297-2 1.4460 / X3CrNiMoN27-5-2 seamless stainless general-purpose tube (329), duplex (austenitic-ferritic), cast analysis per EN table, ambient Rp0.2 min 460 MPa, Rm min 620 MPa, A long. min 20%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4460 / X3CrNiMoN27-5-2 (329 — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4460 Seamless Stainless Steel Tube

EN 10297-2:2005 (BS EN 10297-2:2005) is the European product standard for seamless circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10216-5, and not for welded general-purpose tube under EN 10296-2. Steel number 1.4460 is listed as X3CrNiMoN27-5-2 in the austenitic-ferritic (duplex) set. 1.4460 remains in EN 10297-2 for buyers who still specify 329-class duplex seamless tube — do not auto-substitute 2205 without approval. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Mill path for 1.4460: mechanical seamless OD mid bands. SHH STEEL can produce and supply X3CrNiMoN27-5-2 under EN 10297-2 1.4460 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2.

On the shop floor people still say “329 tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4460, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo. Typical duties include pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2. Design caution: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade. Caution thread: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade.

Scope discipline matters: 1.4460 under EN 10297-2 is seamless general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Role reminder for 1.4460: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Inside this seamless general-purpose series, compare EN 10297-2 1.4462, EN 10297-2 1.4410, EN 10297-2 1.4507. Hub: EN 10297-2. Related pressure seamless chemistry page: EN 10216-5 1.4462.

Chemical Composition of EN 10297-2 1.4460

Cast window focus for 1.4460: Cast analysis for EN 10297-2 1.4460 follows the X3CrNiMoN27-5-2 limits published for this standard’s corrosion- or heat-resisting tables. Key windows on a typical certificate include C ≤0.05, Cr 25.0–28.0, Ni 4.5–6.5, Mo 1.30–2.00, N 0.05–0.20, Si ≤1.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 329 is body text only. Corrosion thread: duplex with Mo for many chloride and mild chemical media.

For 1.4460 / X3CrNiMoN27-5-2, the following chem table is the public EN 10297-2 window SHH STEEL uses at enquiry. Product-analysis Options, when taken, apply the standard’s permitted deviations rather than inventing tighter shop limits. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Steel C Si Mn P S Cr Mo Ni N
1.4460 / X3CrNiMoN27-5-2 ≤0.05 ≤1.00 ≤2.00 ≤0.035 ≤0.015 25.0–28.0 1.30–2.00 4.5–6.5 0.05–0.20

Mechanical Properties of EN 10297-2 1.4460

Ambient floors focus for 1.4460: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4460 order. General-purpose Table values for this number read: Rp0.2 min 460 MPa, Rp1.0 min 470 MPa, Rm min 620 MPa, longitudinal elongation min 20%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: duplex (austenitic-ferritic). Caution thread: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 460 470 620 min 20 — Yes

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4460 / X3CrNiMoN27-5-2. Guideline solution/anneal band (Annex B): 1040–1120 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4460

Seamless route narrative for 1.4460: EN 10297-2 1.4460 is seamless only — pierced or extruded hollows are hot-worked and may be cold-finished to size before heat treatment. Duplex X3CrNiMoN27-5-2 needs controlled thermomechanical history so the ferrite–austenite balance lands in the ordered window after +AT. Annex A process-route symbols for seamless 1.4460 include HFD (hot finished, heat treated, descaled), CFD (cold finished, heat treated, descaled), CFA (cold finished bright annealed), CFG (ground), and CFP (polished). Combinations may be agreed at enquiry. Weld thread: duplex welding practice; ferrite/austenite balance critical.

For duplex 1.4460, solution annealing and rapid cooling are part of the product story, not an optional cosmetic step. Ferritic 1.4460 ships annealed (+A). Annex B points at roughly 1040–1120 °C with water or air cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. NDT Options (eddy current, ultrasonic, leak or hydrostatic) are selected on the order; they are not a substitute for correct duplex heat treatment. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4460. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4460: mechanical seamless OD mid bands. Use thread: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2.

Dimensions and Tolerances for EN 10297-2 1.4460

Dimensional order line for 1.4460: Order EN 10297-2 1.4460 by outside diameter D and wall thickness T for steel name X3CrNiMoN27-5-2. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Mechanical seamless od mid bands. Use thread: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2.

Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4460: mechanical seamless OD mid bands. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Equivalent Grades for EN 10297-2 1.4460

Equivalence talk for 1.4460 starts with X3CrNiMoN27-5-2: 1.4460 / X3CrNiMoN27-5-2 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 329 appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4462, 1.4410, 1.4507. Hook for buyers still using only the 329 alias: lock EN 10297-2 1.4460 on the order line. Caution thread: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade.

Heat Treatment and Delivery Condition for EN 10297-2 1.4460

Ferritic 1.4460 ships annealed (+A). Annex B points at roughly 1040–1120 °C with water or air cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Weld thread: duplex welding practice; ferrite/austenite balance critical.

Fabrication HT reminder for 1.4460 (+AT): For 1.4460, purchasers who need verified IGC after fabrication should say so with the applicable Option and method (EN ISO 3651-2 framing). Mill +AT or +A of the tube does not automatically clear a fabricator’s as-welded joint without procedure control. Delivery framing on the certificate for 1.4460 should match +AT. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Corrosion Resistance of EN 10297-2 1.4460

Corrosion behaviour of EN 10297-2 1.4460 tracks its austenitic-ferritic (duplex) balance: duplex with Mo for many chloride and mild chemical media. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade Corrosion thread: duplex with Mo for many chloride and mild chemical media.

Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4462, 1.4410, 1.4507 when the medium outgrows this number rather than hoping surface finish alone will hold. Family filing for 1.4460 is duplex (austenitic-ferritic). Caution thread: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade.

Applications of EN 10297-2 1.4460 Tube

Applications of EN 10297-2 1.4460 tube centre on mechanical and general engineering rather than PED pressure shells: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2. Role summary: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2.

It is the wrong first choice when a welded product form is mandatory (use EN 10296-2 or EN 10217-7 as applicable), when PED pressure seamless acceptance is locked to EN 10216-5 alone, or when the medium clearly needs a sister such as 1.4462. Primary application sketch: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Weldability of EN 10297-2 1.4460

1.4460 / X3CrNiMoN27-5-2 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: duplex welding practice; ferrite/austenite balance critical. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: duplex welding practice; ferrite/austenite balance critical.

When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Filler/shop note for 1.4460: duplex welding practice; ferrite/austenite balance critical. Caution thread: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade.

Surface Finishes for EN 10297-2 1.4460

Finish selection for 1.4460 on Annex A: For 1.4460, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 329, but the finish symbol still belongs on the EN 10297-2 line. Use thread: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2.

Transit protection for 1.4460 is sized to the Annex A finish: heavier wrap for CFA/CFG/CFP, standard export wrap for HFD/CFD. Open-deck ocean exposure without wrap is refused on bright tube. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Inspection and Testing for EN 10297-2 1.4460

Inspection lot framing for 1.4460 in duplex (austenitic-ferritic): Specific inspection applies to EN 10297-2 1.4460 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Keep 1.4460 heat identity intact from cast through bundle tag. Weld thread: duplex welding practice; ferrite/austenite balance critical.

Purchasers who need witness points on 1.4460 should say so at enquiry. Routine mill inspection still records cast chemistry, tensile results, delivery condition, and dimensions; witness adds scheduling, not a different chemistry table. Use thread: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2.

Packaging and Shipping for EN 10297-2 1.4460

Dispatch note for 1.4460 (329 body alias only): SHH STEEL ships EN 10297-2 1.4460 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled HFD/CFD engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Marking and identity for 1.4460: When cut lengths and special ends are part of the 1.4460 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Finish-sensitive packing for 1.4460 follows the Annex A symbol on the order. Use thread: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2.

Ocean containers loaded with 1.4460 use desiccant and sealed wrap when the route or season warrants it. Inland deliveries may omit container desiccant but never omit end caps on precision OD. Caution thread: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade.

Why Choose SHH STEEL

Why 1.4460 with SHH STEEL — role: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo. SHH STEEL can produce and supply EN 10297-2 1.4460 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “329 tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Grade advice stays practical for 1.4460. If the duty needs a sister chemistry, we point to 1.4462, 1.4410, 1.4507. Design caution for this number: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade Technical clarification on QT level, cold- versus hot-finished rows, or duplex thin-wall footnotes happens before acknowledgement. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade.

Supply Capability

For 1.4460, SHH STEEL can produce and supply seamless tube in the X3CrNiMoN27-5-2 analysis with the Annex A finish you name. Lead time tracks hollow stock and heat-treatment slots; Stock / Available sizes below helps size the first RFQ. Use thread: pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4460 / X3CrNiMoN27-5-2
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Available sizes for 1.4460 follow seamless general-purpose practice: mechanical seamless OD mid bands. Dual size lists against sister grades are welcome on one enquiry sheet. Duty thread: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.

Dual documentation talk for 1.4460 versus 1.4462, 1.4410, 1.4507 is fine at enquiry — each steel number still needs its own cast compliance. SHH STEEL can produce and supply staged deliveries by size priority. Weld thread: duplex welding practice; ferrite/austenite balance critical.

FAQ

What is EN 10297-2 1.4460 seamless stainless steel tube used for?
EN 10297-2 1.4460 (X3CrNiMoN27-5-2) is seamless tube for mechanical and general engineering — pump columns, mechanical process lines, and older European specs that still name X3CrNiMoN27-5-2. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo.
Is EN 10297-2 1.4460 the same as EN 10216-5 1.4460?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4460 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4460 / X3CrNiMoN27-5-2?
Delivery framing for 1.4460 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1040–1120 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4460?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4460 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4460 compare with sister grades 1.4462, 1.4410, 1.4507?
1.4460 / X3CrNiMoN27-5-2 is filed as duplex (austenitic-ferritic). Typical sisters discussed on the same RFQ are 1.4462, 1.4410, 1.4507. Design caution: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4460 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: duplex welding practice; ferrite/austenite balance critical. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4460?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4460?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4460 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: mechanical seamless OD mid bands. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 329 belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 329 in body text and BOM notes, but lock EN 10297-2 and 1.4460 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4460?
Move when chloride pitting, crevice attack, or SCC risk exceeds what duplex (austenitic-ferritic) practice can defend for the temperature and stress state. Caution for this number: modern projects often prefer 1.4462 or superduplex — confirm why 1.4460 is locked before quoting an upgrade Sister pointers: 1.4462, 1.4410, 1.4507. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4460 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4460 is filed as duplex (austenitic-ferritic). If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4460 (X3CrNiMoN27-5-2) is seamless stainless tube for mechanical and general engineering — legacy 25Cr duplex seamless tube (329-class) for mechanical duty needing duplex strength and Mo. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4462, 1.4410, 1.4507. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X