EN 10297-2 1.4749 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4749 Seamless Stainless Steel Tube

EN 10297-2 1.4749 / X18CrN28 seamless stainless general-purpose tube (446 / 28%Cr ferritic heat), ferritic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 280 MPa, Rm min 500 MPa, A long. min 15%, delivery +A. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4749 / X18CrN28 (446 / 28%Cr ferritic heat — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +A as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4749 Seamless Stainless Steel Tube

EN 10297-2 covers seamless stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4749 is the ferritic heat-resisting grade X18CrN28, commercially discussed as 446 / 28%Cr ferritic heat. EN 10297-2 puts ferritic heat-resisting chemistry in 1.4749 alone — do not confuse it with austenitic heat numbers 1.4833/1.4845. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Mill path for 1.4749: heat-service seamless OD with +A delivery. SHH STEEL can produce and supply EN 10297-2 1.4749 seamless stainless steel tube — hot-finished or cold-finished on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, hydrostatic, eddy current, ultrasonic, and related NDT Options). Use thread: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases.

On the shop floor people still say “446 / 28%Cr ferritic heat tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4749, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service. Typical duties include furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases. Design caution: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling. Caution thread: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling.

Scope discipline matters: 1.4749 under EN 10297-2 is seamless general-purpose tube. Sister pages for pressure seamless (EN 10216-5) or welded pressure (EN 10217-7) share chemistry families but not acceptance text. Order the standard that the drawing and regulatory file actually require. Role reminder for 1.4749: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Inside this seamless general-purpose series, compare EN 10297-2 1.4845, EN 10297-2 1.4833, EN 10297-2 1.4016. Hub: EN 10297-2.

Chemical Composition of EN 10297-2 1.4749

Cast window focus for 1.4749: Every 1.4749 heat under EN 10297-2 must meet the cast (ladle) analysis for X18CrN28 in the ferritic heat-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 446 / 28%Cr ferritic heat is body text only. Corrosion thread: high chromium for oxidising scale resistance; not selected for aqueous chloride process duty.

Cast chemistry for seamless 1.4749 must land inside X18CrN28 limits. The table is transcribed from public BSSA EN 10297-2 data for quick comparison with sister grades; always re-check the paid standard when a dispute arises. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Steel C Si Mn P S Cr N
1.4749 / X18CrN28 0.15–0.20 ≤1.00 ≤1.00 ≤0.040 ≤0.015 26.0–29.0 0.15–0.25

Mechanical Properties of EN 10297-2 1.4749

Ambient floors focus for 1.4749: Table mechanical floors for 1.4749 / X18CrN28 are delivery-condition values at room temperature, not elevated-temperature design allowables. Summary: Rp0.2 min 280 MPa, Rm min 500 MPa, longitudinal elongation min 15%. SHH STEEL reports actual tensile results on the EN 10204 3.1 document for the ordered test unit. Family: ferritic heat-resisting. Caution thread: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+A 280 — 500 min 15 15 –

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4749 / X18CrN28. Guideline solution/anneal band (Annex B): 800–860 °C; cooling: water, air or gas.

Seamless Tube Manufacture for EN 10297-2 1.4749

Seamless route narrative for 1.4749: Ferritic seamless 1.4749 (X18CrN28) is produced from pierced or extruded hollows, then annealed (+A) to restore ductility after hot or cold finishing. Grain-growth control during anneal matters for toughness and forming. For 1.4749, SHH STEEL aligns the Annex A symbol to the duty: descaled HFD/CFD for general mechanical tube, CFA for cleaner bright OD, and CFG/CFP when a measured roughness target is part of the order text. Weld thread: ferritic heat-resisting practice; anneal guidance 800–860 °C; watch grain growth.

Ferritic heat-resisting 1.4749 is delivered annealed (+A). Guideline anneal is 800–860 °C; thermal cycling and toughness limits differ from austenitic heat numbers in Table 9. Forming and expansion trials should respect ferritic elongation floors rather than austenitic shop habits. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

When dual documentation against EN 10216-5 is requested for the same 1.4749 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 1.4749: heat-service seamless OD with +A delivery. Use thread: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases.

Dimensions and Tolerances for EN 10297-2 1.4749

Dimensional order line for 1.4749: Order EN 10297-2 1.4749 by outside diameter D and wall thickness T for steel name X18CrN28. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Heat-service seamless od with +a delivery. Use thread: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases.

Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4749: heat-service seamless OD with +A delivery. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Equivalent Grades for EN 10297-2 1.4749

Equivalence talk for 1.4749 starts with X18CrN28: 1.4749 / X18CrN28 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 446 / 28%Cr ferritic heat appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4845, 1.4833, 1.4016. Hook for buyers still using only the 446 / 28%Cr ferritic heat alias: lock EN 10297-2 1.4749 on the order line. Caution thread: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling.

Heat Treatment and Delivery Condition for EN 10297-2 1.4749

Ferritic heat-resisting 1.4749 is delivered annealed (+A). Guideline anneal is 800–860 °C; thermal cycling and toughness limits differ from austenitic heat numbers in Table 9. Weld thread: ferritic heat-resisting practice; anneal guidance 800–860 °C; watch grain growth.

Fabrication HT reminder for 1.4749 (+A): Hot-working temperature bands in Annex B for X18CrN28 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4749 should match +A. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Corrosion Resistance of EN 10297-2 1.4749

Corrosion behaviour of EN 10297-2 1.4749 tracks its ferritic heat-resisting balance: high chromium for oxidising scale resistance; not selected for aqueous chloride process duty. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling Corrosion thread: high chromium for oxidising scale resistance; not selected for aqueous chloride process duty.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4749 is filed as ferritic heat-resisting — pick tests that match that filing. Family filing for 1.4749 is ferritic heat-resisting. Caution thread: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling.

Applications of EN 10297-2 1.4749 Tube

Applications of EN 10297-2 1.4749 tube centre on mechanical and general engineering rather than PED pressure shells: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases. Role summary: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases.

It is the wrong first choice when a welded product form is mandatory (use EN 10296-2 or EN 10217-7 as applicable), when PED pressure seamless acceptance is locked to EN 10216-5 alone, or when the medium clearly needs a sister such as 1.4845. Primary application sketch: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Weldability of EN 10297-2 1.4749

1.4749 / X18CrN28 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: ferritic heat-resisting practice; anneal guidance 800–860 °C; watch grain growth. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: ferritic heat-resisting practice; anneal guidance 800–860 °C; watch grain growth.

Filler selection should match or over-alloy the base X18CrN28 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, martensitic, duplex, or heat-resisting — not a single shop habit. Filler/shop note for 1.4749: ferritic heat-resisting practice; anneal guidance 800–860 °C; watch grain growth. Caution thread: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling.

Surface Finishes for EN 10297-2 1.4749

Finish selection for 1.4749 on Annex A: Interior Ra limits, electropolish, or special protection for X18CrN28 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4749 when the mill can measure and report the finish. Alias reminder: commercial talk may say 446 / 28%Cr ferritic heat, but the finish symbol still belongs on the EN 10297-2 line. Use thread: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases.

Agree any site-storage constraints for 1.4749 at enquiry. Long inland dwell in winter road-salt regions needs sealed wrap even when ocean freight is not involved. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Inspection and Testing for EN 10297-2 1.4749

Inspection lot framing for 1.4749 in ferritic heat-resisting: NDT intensity on 1.4749 is Option-driven under EN 10297-2 — eddy current, ultrasonic, leak, or hydrostatic methods are selected at enquiry. That is a different framing from EN 10216-5 TC1/TC2 pressure categories; copy the Options you need. Keep 1.4749 heat identity intact from cast through bundle tag. Weld thread: ferritic heat-resisting practice; anneal guidance 800–860 °C; watch grain growth.

Acceptance marks on 1.4749 reference the inspection lot. If a piece is cut after delivery, retain the marked end or transfer the heat identity under the fabricator’s quality system so traceability survives the saw. Use thread: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases.

Packaging and Shipping for EN 10297-2 1.4749

Dispatch note for 1.4749 (446 / 28%Cr ferritic heat body alias only): Finished EN 10297-2 1.4749 (X18CrN28) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Marking and identity for 1.4749: Marking typically includes manufacturer identity, dimensions, EN 10297-2, steel name or number 1.4749, cast/code, inspection mark, and correlation number; Annex A process-route symbols appear when agreed. SHH STEEL keeps stencil or inkjet marking legible without damaging CFA/CFP surfaces. Finish-sensitive packing for 1.4749 follows the Annex A symbol on the order. Use thread: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases.

Project freight for 1.4749 can be staged by installation sequence when the packing list names priority bundles. That staging is agreed before the saw schedule locks. Caution thread: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling.

Why Choose SHH STEEL

Why 1.4749 with SHH STEEL — role: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service. SHH STEEL can produce and supply X18CrN28 as EN 10297-2 1.4749 seamless tube with honest scope boundaries. General engineering seamless acceptance is what this page sells; pressure, welded-pressure, and welded-general-purpose sisters are separate standards with separate MTCs. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

Grade advice stays practical for 1.4749. If the duty needs a sister chemistry, we point to 1.4845, 1.4833, 1.4016. Design caution for this number: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling Export document packs are assembled to match the heat tags on the bundles you will receive. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling.

Supply Capability

SHH STEEL can produce and supply EN 10297-2 1.4749. SHH STEEL’s EN 10297-2 1.4749 offering is make-to-order seamless tube in X18CrN28. We can produce and supply cut lengths and standard mill lengths. Use the Stock / Available sizes map as a planning aid, then confirm live availability on the quote. Use thread: furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4749 / X18CrN28
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +A
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes note for 1.4749: bring the OD × wall list early. Context: heat-service seamless OD with +A delivery. Bright CFA and polished CFP may add finishing lead time versus descaled CFD/HFD. Duty thread: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.

When 1.4749 shares a project with 1.4845, 1.4833, 1.4016, keep separate heat identity tags. SHH STEEL can produce and supply coordinated size lists so fabrication receives matched OD bands without mixed certificates. Weld thread: ferritic heat-resisting practice; anneal guidance 800–860 °C; watch grain growth.

FAQ

What is EN 10297-2 1.4749 seamless stainless steel tube used for?
EN 10297-2 1.4749 (X18CrN28) is seamless tube for mechanical and general engineering — furnace tubes adjacent hardware, burner components, and high-temperature mechanical parts in oxidising gases. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service.
Is EN 10297-2 1.4749 the same as EN 10216-5 1.4749?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4749 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4749 / X18CrN28?
Delivery framing for 1.4749 is +A under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 800–860 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4749?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4749 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4749 compare with sister grades 1.4845, 1.4833, 1.4016?
1.4749 / X18CrN28 is filed as ferritic heat-resisting. Typical sisters discussed on the same RFQ are 1.4845, 1.4833, 1.4016. Design caution: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4749 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: ferritic heat-resisting practice; anneal guidance 800–860 °C; watch grain growth. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4749?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4749?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4749 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: heat-service seamless OD with +A delivery. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 446 / 28%Cr ferritic heat belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 446 / 28%Cr ferritic heat in body text and BOM notes, but lock EN 10297-2 and 1.4749 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4749?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic heat-resisting practice can defend for the temperature and stress state. Caution for this number: ferritic heat-resisting toughness and thermal cycling limits differ from austenitic heat grades — confirm duty temperature and cycling Sister pointers: 1.4845, 1.4833, 1.4016. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4749 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4749 is filed as ferritic heat-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4749 (X18CrN28) is seamless stainless tube for mechanical and general engineering — the only ferritic heat-resisting grade in EN 10297-2 — high-Cr N-bearing seamless tube for oxidising heat service. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4845, 1.4833, 1.4016. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *