EN 10297-2 1.4507 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4507 Seamless Stainless Steel Tube

EN 10297-2 1.4507 / X2CrNiMoCuN25-6-3 seamless stainless general-purpose tube (255 / Cu duplex), duplex (austenitic-ferritic), cast analysis per EN table, ambient Rp0.2 min 500 MPa, Rm min 700 MPa, A long. min 20%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4507 / X2CrNiMoCuN25-6-3 (255 / Cu duplex — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4507 Seamless Stainless Steel Tube

EN 10297-2:2005 (BS EN 10297-2:2005) is the European product standard for seamless circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10216-5, and not for welded general-purpose tube under EN 10296-2. Steel number 1.4507 is listed as X2CrNiMoCuN25-6-3 in the austenitic-ferritic (duplex) set. 1.4507 is the Cu-bearing duplex seamless number in EN 10297-2 — order it when Cu is on the chemistry list, not as a catalogue synonym for 2507. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Mill path for 1.4507: specialty duplex seamless OD. SHH STEEL can produce and supply X2CrNiMoCuN25-6-3 under EN 10297-2 1.4507 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex.

On the shop floor people still say “255 / Cu duplex tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4507, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media. Typical duties include chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex. Design caution: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410. Caution thread: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410.

EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4507: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Inside this seamless general-purpose series, compare EN 10297-2 1.4410, EN 10297-2 1.4501, EN 10297-2 1.4462. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4507.

Chemical Composition of EN 10297-2 1.4507

Cast window focus for 1.4507: Buying 255 / Cu duplex-family seamless tube without locking 1.4507 invites silent chemistry drift. Under EN 10297-2 the cast must satisfy X2CrNiMoCuN25-6-3; highlight elements for this grade include C ≤0.030, Cr 24.0–26.0, Ni 5.5–7.5, Mo 2.7–4.0, N 0.15–0.30, Cu 1.00–2.50. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Commercial alias 255 / Cu duplex is body text only. Corrosion thread: duplex plus Cu for selected acid-chloride and seawater-adjacent media.

Below is the BSSA-sourced EN 10297-2 chemistry window for 1.4507 (X2CrNiMoCuN25-6-3). Maxima apply unless a band is printed. SHH STEEL quotes against this window and reports actual cast values on the EN 10204 document — not a rewritten catalogue paraphrase. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Steel C Si Mn P S Cr Mo Ni Cu N
1.4507 / X2CrNiMoCuN25-6-3 ≤0.030 ≤0.70 ≤2.00 ≤0.035 ≤0.015 24.0–26.0 2.7–4.0 5.5–7.5 1.00–2.50 0.15–0.30

Mechanical Properties of EN 10297-2 1.4507

Ambient floors focus for 1.4507: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4507 order. General-purpose Table values for this number read: Rp0.2 min 500 MPa, Rp1.0 min 510 MPa, Rm min 700 MPa, longitudinal elongation min 20%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: duplex (austenitic-ferritic). Caution thread: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 500 510 700 min 20 20 Yes

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4507 / X2CrNiMoCuN25-6-3. Guideline solution/anneal band (Annex B): 1040–1120 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4507

Seamless route narrative for 1.4507: EN 10297-2 1.4507 is seamless only — pierced or extruded hollows are hot-worked and may be cold-finished to size before heat treatment. Duplex X2CrNiMoCuN25-6-3 needs controlled thermomechanical history so the ferrite–austenite balance lands in the ordered window after +AT. For 1.4507, SHH STEEL aligns the Annex A symbol to the duty: descaled HFD/CFD for general mechanical tube, CFA for cleaner bright OD, and CFG/CFP when a measured roughness target is part of the order text. Weld thread: matching Cu-bearing duplex fillers; control heat input.

For duplex 1.4507, solution annealing and rapid cooling are part of the product story, not an optional cosmetic step. Ferritic 1.4507 ships annealed (+A). Annex B points at roughly 1040–1120 °C with water or air cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. NDT Options (eddy current, ultrasonic, leak or hydrostatic) are selected on the order; they are not a substitute for correct duplex heat treatment. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Optional tests under EN 10297-2 for 1.4507 include leak testing, hydrostatic testing, and NDT such as eddy current or ultrasonic methods agreed at enquiry. SHH STEEL records the Options actually performed on the inspection document — we do not claim a test that was not run. Size context for 1.4507: specialty duplex seamless OD. Use thread: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex.

Dimensions and Tolerances for EN 10297-2 1.4507

Dimensional order line for 1.4507: SHH STEEL aligns OD × wall, tolerance class, and process-route symbol for 1.4507 / X2CrNiMoCuN25-6-3 before rolling or drawing slots are locked. Specialty duplex seamless od. Use thread: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex.

Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4507: specialty duplex seamless OD. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Equivalent Grades for EN 10297-2 1.4507

Equivalence talk for 1.4507 starts with X2CrNiMoCuN25-6-3: 1.4507 / X2CrNiMoCuN25-6-3 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 255 / Cu duplex appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4410, 1.4501, 1.4462. Hook for buyers still using only the 255 / Cu duplex alias: lock EN 10297-2 1.4507 on the order line. Caution thread: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410.

Heat Treatment and Delivery Condition for EN 10297-2 1.4507

Ferritic 1.4507 ships annealed (+A). Annex B points at roughly 1040–1120 °C with water or air cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Weld thread: matching Cu-bearing duplex fillers; control heat input.

Fabrication HT reminder for 1.4507 (+AT): For 1.4507, purchasers who need verified IGC after fabrication should say so with the applicable Option and method (EN ISO 3651-2 framing). Mill +AT or +A of the tube does not automatically clear a fabricator’s as-welded joint without procedure control. Delivery framing on the certificate for 1.4507 should match +AT. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Corrosion Resistance of EN 10297-2 1.4507

Corrosion behaviour of EN 10297-2 1.4507 tracks its austenitic-ferritic (duplex) balance: duplex plus Cu for selected acid-chloride and seawater-adjacent media. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410 Corrosion thread: duplex plus Cu for selected acid-chloride and seawater-adjacent media.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4507 is filed as austenitic-ferritic (duplex) — pick tests that match that filing. Family filing for 1.4507 is duplex (austenitic-ferritic). Caution thread: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410.

Applications of EN 10297-2 1.4507 Tube

Applications of EN 10297-2 1.4507 tube centre on mechanical and general engineering rather than PED pressure shells: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex. Role summary: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex.

Typical BOM language pairs EN 10297-2 1.4507 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “255 / Cu duplex” substitutions do not creep in. Primary application sketch: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Weldability of EN 10297-2 1.4507

1.4507 / X2CrNiMoCuN25-6-3 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: matching Cu-bearing duplex fillers; control heat input. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: matching Cu-bearing duplex fillers; control heat input.

Filler selection should match or over-alloy the base X2CrNiMoCuN25-6-3 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, martensitic, duplex, or heat-resisting — not a single shop habit. Filler/shop note for 1.4507: matching Cu-bearing duplex fillers; control heat input. Caution thread: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410.

Surface Finishes for EN 10297-2 1.4507

Finish selection for 1.4507 on Annex A: Surface finish on EN 10297-2 1.4507 is carried by the Annex A symbol: descaled HFD/CFD for general mechanical tube, bright-annealed CFA for cleaner OD appearance, and ground CFG or polished CFP when roughness is agreed at enquiry. Carbon-steel strapping must not contact the stainless surface. Alias reminder: commercial talk may say 255 / Cu duplex, but the finish symbol still belongs on the EN 10297-2 line. Use thread: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex.

Storage guidance for 1.4507: keep bundles off bare concrete in coastal yards, avoid chloride-bearing tarps against CFA OD, and leave end caps fitted until fabrication. Special export crate liners are available when the packing note asks for them. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Inspection and Testing for EN 10297-2 1.4507

Inspection lot framing for 1.4507 in duplex (austenitic-ferritic): Specific inspection applies to EN 10297-2 1.4507 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Keep 1.4507 heat identity intact from cast through bundle tag. Weld thread: matching Cu-bearing duplex fillers; control heat input.

Technological tests on 1.4507 follow the order matrix — they are not assumed. IGC, when required, cites EN ISO 3651-2. Stencil or inkjet marking stays light on polished OD so the finish remains acceptable after receipt inspection. Use thread: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex.

Packaging and Shipping for EN 10297-2 1.4507

Dispatch note for 1.4507 (255 / Cu duplex body alias only): Finished EN 10297-2 1.4507 (X2CrNiMoCuN25-6-3) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Marking and identity for 1.4507: When cut lengths and special ends are part of the 1.4507 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Finish-sensitive packing for 1.4507 follows the Annex A symbol on the order. Use thread: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex.

Packing lists for 1.4507 map bundle IDs to heats and sizes so receiving inspection can clear documents without unpacking every crate. Damaged wrap discovered at destination is reported with photos before the material is issued to fabrication. Caution thread: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410.

Why Choose SHH STEEL

Why 1.4507 with SHH STEEL — role: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media. SHH STEEL can produce and supply X2CrNiMoCuN25-6-3 as EN 10297-2 1.4507 seamless tube with honest scope boundaries. General engineering seamless acceptance is what this page sells; pressure, welded-pressure, and welded-general-purpose sisters are separate standards with separate MTCs. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

Grade advice stays practical for 1.4507. If the duty needs a sister chemistry, we point to 1.4410, 1.4501, 1.4462. Design caution for this number: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410 Quotes state scope boundaries in plain language so purchasing and engineering share the same acceptance standard. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410.

Supply Capability

Supply capability for EN 10297-2 1.4507 / X2CrNiMoCuN25-6-3 starts with your OD × wall list and delivery-condition choice. SHH STEEL can produce and supply against that list with EN 10204 3.1 documents; the Stock / Available sizes block frames enquiry sizes rather than a public warehouse catalogue. Use thread: chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4507 / X2CrNiMoCuN25-6-3
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Available sizes conversation for 1.4507 starts with your OD × wall matrix. Typical note: specialty duplex seamless OD. Send preferred delivery condition (+A / +AT / +QT as applicable) and any eddy-current or hydrostatic Options with the size list. Duty thread: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.

On 1.4507, Options and sister duals (1.4410, 1.4501, 1.4462) belong on the same enquiry as the size list. SHH STEEL can produce and supply production heats after a short pilot when forming or polish trials are required. Weld thread: matching Cu-bearing duplex fillers; control heat input.

FAQ

What is EN 10297-2 1.4507 seamless stainless steel tube used for?
EN 10297-2 1.4507 (X2CrNiMoCuN25-6-3) is seamless tube for mechanical and general engineering — chemical process mechanical lines, seawater-adjacent duties short of superduplex, and specs naming Cu duplex. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media.
Is EN 10297-2 1.4507 the same as EN 10216-5 1.4507?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4507 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4507 / X2CrNiMoCuN25-6-3?
Delivery framing for 1.4507 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1040–1120 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4507?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4507 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4507 compare with sister grades 1.4410, 1.4501, 1.4462?
1.4507 / X2CrNiMoCuN25-6-3 is filed as duplex (austenitic-ferritic). Typical sisters discussed on the same RFQ are 1.4410, 1.4501, 1.4462. Design caution: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410 Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4507 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: matching Cu-bearing duplex fillers; control heat input. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4507?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4507?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4507 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: specialty duplex seamless OD. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 255 / Cu duplex belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 255 / Cu duplex in body text and BOM notes, but lock EN 10297-2 and 1.4507 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4507?
Move when chloride pitting, crevice attack, or SCC risk exceeds what duplex (austenitic-ferritic) practice can defend for the temperature and stress state. Caution for this number: Cu changes corrosion behaviour — do not treat as silent dual of 1.4410 Sister pointers: 1.4410, 1.4501, 1.4462. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4507 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4507 is filed as duplex (austenitic-ferritic). If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4507 (X2CrNiMoCuN25-6-3) is seamless stainless tube for mechanical and general engineering — Cu-bearing duplex seamless tube for improved localised corrosion in certain reducing/chloride media. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4410, 1.4501, 1.4462. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *