EN 10297-2 1.4401 Seamless Stainless Steel Tube
What is EN 10297-2 1.4401 Seamless Stainless Steel Tube
EN 10297-2:2005 (BS EN 10297-2:2005) is the European product standard for seamless circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10216-5, and not for welded general-purpose tube under EN 10296-2. Steel number 1.4401 is listed as X5CrNiMo17-12-2 in the austenitic corrosion-resisting set. EN 10297-2 1.4401 carries X5CrNiMo17-12-2 into general-purpose seamless supply — do not treat it as automatic dual with 1.4404 without checking carbon and IGC footnotes. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Mill path for 1.4401: broad seamless mechanical catalogue OD×wall. SHH STEEL can produce and supply EN 10297-2 1.4401 seamless stainless steel tube — hot-finished or cold-finished on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, hydrostatic, eddy current, ultrasonic, and related NDT Options). Use thread: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L.
On the shop floor people still say “316 tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4401, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316. Typical duties include chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L. Design caution: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints. Caution thread: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints.
EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4401: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Inside this seamless general-purpose series, compare EN 10297-2 1.4404, EN 10297-2 1.4436, EN 10297-2 1.4571. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4401. ASTM/ASME related product pages (not interchangeable by default): A269 TP316, A213 TP316.
Chemical Composition of EN 10297-2 1.4401
Cast window focus for 1.4401: Every 1.4401 heat under EN 10297-2 must meet the cast (ladle) analysis for X5CrNiMo17-12-2 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 316 is body text only. Corrosion thread: Mo-bearing chromium-nickel film similar to 316L-family with carbon at the standard ceiling.
Chemical limits for 1.4401 / X5CrNiMo17-12-2 under EN 10297-2 appear in the table underneath. Source priority is BSSA’s EN 10297-2 article cross-checked to the 2005 grade list. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
| Steel | C | Si | Mn | P | S | Cr | Mo | Ni | N |
|---|---|---|---|---|---|---|---|---|---|
| 1.4401 / X5CrNiMo17-12-2 | ≤0.07 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.015 | 16.5–18.5 | 2.00–2.50 | 10.0–13.0 | ≤0.11 |
Mechanical Properties of EN 10297-2 1.4401
Ambient floors focus for 1.4401: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4401 order. General-purpose Table values for this number read: Rp0.2 min 205 MPa, Rp1.0 min 240 MPa, Rm min 510 MPa, longitudinal elongation min 40%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic corrosion-resisting. Caution thread: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 205 | 240 | 510 min | 40 | 30 | Yes* (normally not sensitised) |
Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4401 / X5CrNiMo17-12-2. Guideline solution/anneal band (Annex B): 1020–1100 °C; cooling: water or air.
Seamless Tube Manufacture for EN 10297-2 1.4401
Seamless route narrative for 1.4401: EN 10297-2 does not offer a welded route for 1.4401. Tube in X5CrNiMo17-12-2 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Seamless manufacture for 1.4401 finishes through hot- or cold-finished routes. Pick HFD/CFD for descaled engineering surfaces, CFA for bright anneal, and CFG or CFP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Weld thread: 316/316L fillers depending on carbon strategy; anneal fabricated joints on corrosive duty when required.
For austenitic 1.4401, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4401 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1020–1100 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
State leak-tightness, hydrostatic, eddy-current, or ultrasonic Options explicitly for 1.4401. General-purpose seamless acceptance is not identical to EN 10216-5 TC1/TC2 pressure regimes; copy the Options list you need onto the EN 10297-2 order. Size context for 1.4401: broad seamless mechanical catalogue OD×wall. Use thread: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L.
Dimensions and Tolerances for EN 10297-2 1.4401
Dimensional order line for 1.4401: SHH STEEL aligns OD × wall, tolerance class, and process-route symbol for 1.4401 / X5CrNiMo17-12-2 before rolling or drawing slots are locked. Broad seamless mechanical catalogue od×wall. Use thread: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L.
Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4401: broad seamless mechanical catalogue OD×wall. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Equivalent Grades for EN 10297-2 1.4401
Equivalence talk for 1.4401 starts with X5CrNiMo17-12-2: 1.4401 / X5CrNiMo17-12-2 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 316 appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4404, 1.4436, 1.4571. Hook for buyers still using only the 316 alias: lock EN 10297-2 1.4401 on the order line. Caution thread: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints.
Heat Treatment and Delivery Condition for EN 10297-2 1.4401
Austenitic 1.4401 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1020–1100 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: 316/316L fillers depending on carbon strategy; anneal fabricated joints on corrosive duty when required.
Fabrication HT reminder for 1.4401 (+AT): Hot-working temperature bands in Annex B for X5CrNiMo17-12-2 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Delivery framing on the certificate for 1.4401 should match +AT. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Corrosion Resistance of EN 10297-2 1.4401
Corrosion behaviour of EN 10297-2 1.4401 tracks its austenitic corrosion-resisting balance: Mo-bearing chromium-nickel film similar to 316L-family with carbon at the standard ceiling. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints Corrosion thread: Mo-bearing chromium-nickel film similar to 316L-family with carbon at the standard ceiling.
For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4401 is filed as austenitic corrosion-resisting — pick tests that match that filing. Family filing for 1.4401 is austenitic corrosion-resisting. Caution thread: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints.
Applications of EN 10297-2 1.4401 Tube
Applications of EN 10297-2 1.4401 tube centre on mechanical and general engineering rather than PED pressure shells: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L. Role summary: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L.
Skip 1.4401 when the specification locks a different family — for example forcing ferritic 1.4401 into severe chloride process duty, or forcing a free-machining grade into welded corrosive service. Sister conversation inside EN 10297-2: 1.4404, 1.4436, 1.4571. Primary application sketch: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Weldability of EN 10297-2 1.4401
1.4401 / X5CrNiMo17-12-2 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: 316/316L fillers depending on carbon strategy; anneal fabricated joints on corrosive duty when required. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: 316/316L fillers depending on carbon strategy; anneal fabricated joints on corrosive duty when required.
For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints Filler/shop note for 1.4401: 316/316L fillers depending on carbon strategy; anneal fabricated joints on corrosive duty when required. Caution thread: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints.
Surface Finishes for EN 10297-2 1.4401
Finish selection for 1.4401 on Annex A: For 1.4401, pick CFA when residual scale is unacceptable on visible mechanical assemblies; pick CFG/CFP only with a written OD/ID scope and roughness target. Descaled HFD/CFD remains the workhorse engineering finish. Alias reminder: commercial talk may say 316, but the finish symbol still belongs on the EN 10297-2 line. Use thread: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L.
During delivery of 1.4401, SHH STEEL can add edge guards, VCI paper, or sealed PE wrap when the enquiry lists them. Descaled engineering finishes still need caps; bright and polished finishes need full OD sleeve protection. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Inspection and Testing for EN 10297-2 1.4401
Inspection lot framing for 1.4401 in austenitic corrosion-resisting: Specific inspection applies to EN 10297-2 1.4401 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Keep 1.4401 heat identity intact from cast through bundle tag. Weld thread: 316/316L fillers depending on carbon strategy; anneal fabricated joints on corrosive duty when required.
Inspection documents for 1.4401 list every Optional test that actually ran. Surrogate “typical” NDT language is never printed. Tube marking repeats the steel number 1.4401 so warehouse staff cannot confuse sister heats in the same bundle bay. Use thread: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L.
Packaging and Shipping for EN 10297-2 1.4401
Dispatch note for 1.4401 (316 body alias only): Finished EN 10297-2 1.4401 (X5CrNiMo17-12-2) seamless tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (CFA/CFG/CFP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Marking and identity for 1.4401: When cut lengths and special ends are part of the 1.4401 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Finish-sensitive packing for 1.4401 follows the Annex A symbol on the order. Use thread: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L.
For 1.4401, export documentation includes packing list, certificate, and any third-party release notes agreed at order. Heat segregation rules stay in force when multiple steel numbers share a container. Caution thread: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints.
Why Choose SHH STEEL
Why 1.4401 with SHH STEEL — role: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316. SHH STEEL can produce and supply EN 10297-2 1.4401 as seamless general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “316 tube” label on whatever is in the rack. We keep Part 5 pressure talk honest: when PED seamless pressure acceptance is required, we point you to EN 10216-5 for the same chemistry where it exists. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Grade advice stays practical for 1.4401. If the duty needs a sister chemistry, we point to 1.4404, 1.4436, 1.4571. Design caution for this number: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints If the file later becomes PED pressure seamless, we help retarget EN 10216-5 rather than relabeling a general-purpose MTC. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints.
Supply Capability
SHH STEEL can produce and supply EN 10297-2 1.4401. Ask SHH STEEL for EN 10297-2 1.4401 when you need seamless general-purpose X5CrNiMo17-12-2 with named Options. We can produce and supply trial lengths or production heats once OD, wall, finish symbol, and test Options are clear. See Stock / Available sizes below. Use thread: chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L.
| Item | Capability |
|---|---|
| Standard | EN 10297-2:2005 seamless general-purpose |
| Steel | 1.4401 / X5CrNiMo17-12-2 |
| Product form | Seamless tube (HFD / CFD / CFA / CFG / CFP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–20 mm within family practice (other by agreement) |
Stock / Available sizes
Enquiry stock map — EN 10297-2 1.4401 / X5CrNiMo17-12-2: broad seamless mechanical catalogue OD×wall. SHH STEEL will mark which rows can roll on current hollows versus which need a fresh heat. No invented warehouse tonnages appear on this page. Duty thread: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
Sister comparisons for 1.4401 usually include 1.4404, 1.4436, 1.4571. Dimensional acceptance remains the EN 10297-2 order text, not a peer brochure. SHH STEEL can produce and supply mixed sister bundles when heats and finishes align. Weld thread: 316/316L fillers depending on carbon strategy; anneal fabricated joints on corrosive duty when required.
FAQ
-
What is EN 10297-2 1.4401 seamless stainless steel tube used for?
- EN 10297-2 1.4401 (X5CrNiMo17-12-2) is seamless tube for mechanical and general engineering — chemical process mechanical lines, marine-adjacent utilities, and general engineering that names 316 rather than 316L. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316.
-
Is EN 10297-2 1.4401 the same as EN 10216-5 1.4401?
- Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4401 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4401 / X5CrNiMo17-12-2?
- Delivery framing for 1.4401 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1020–1100 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4401?
- SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4401 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4401 compare with sister grades 1.4404, 1.4436, 1.4571?
- 1.4401 / X5CrNiMo17-12-2 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4404, 1.4436, 1.4571. Design caution: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
Can 1.4401 be welded even though the tube is seamless?
- Yes — fabricator joints are common on mechanical assemblies. Shop guidance: 316/316L fillers depending on carbon strategy; anneal fabricated joints on corrosive duty when required. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4401?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10297-2 1.4401?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4401 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: broad seamless mechanical catalogue OD×wall. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 316 belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 316 in body text and BOM notes, but lock EN 10297-2 and 1.4401 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4401?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: higher carbon than 1.4404 raises as-welded sensitisation risk — prefer 1.4404 or 1.4571 for corrosive as-welded joints Sister pointers: 1.4404, 1.4436, 1.4571. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10297-2 1.4401 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4401 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10297-2 1.4401 (X5CrNiMo17-12-2) is seamless stainless tube for mechanical and general engineering — standard-carbon Mo-bearing austenitic seamless tube for mechanical duty parallel to commercial 316. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4404, 1.4436, 1.4571. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.