EN 10297-2 1.4580 Seamless Stainless Steel Tube | EN 10297-2 Stainless Steel - SHH STEEL

EN 10297-2 1.4580 Seamless Stainless Steel Tube

EN 10297-2 1.4580 / X6CrNiMoNb17-12-2 seamless stainless general-purpose tube (316Nb), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 215 MPa, Rm min 510 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4580 / X6CrNiMoNb17-12-2 (316Nb — body alias)
Standard
EN 10297-2
Product form
Seamless tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–20 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10297-2 1.4580 Seamless Stainless Steel Tube

EN 10297-2 covers seamless stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4580 is the austenitic corrosion-resisting grade X6CrNiMoNb17-12-2, commercially discussed as 316Nb. 1.4580 is the Nb-stabilised Mo austenitic seamless number in EN 10297-2 — order the steel number when the list says 316Nb, not a silent swap from 1.4571. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Mill path for 1.4580: process seamless bands with Annex A descaled or bright routes. SHH STEEL can produce and supply X6CrNiMoNb17-12-2 under EN 10297-2 1.4580 as seamless tube for mechanical and general engineering — not as a silent dual of EN 10216-5 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Use thread: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list.

On the shop floor people still say “316Nb tube,” yet that commercial alias does not select cast chemistry, seamless process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10297-2, 1.4580, the Annex A process/surface symbol, and any Options so the mill applies the correct analysis, piercing/drawing route, heat treatment, mechanical floors, and marking. This number’s job on seamless general-purpose duty is: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified. Typical duties include chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list. Design caution: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report. Caution thread: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report.

EN 10297-2 is seamless product only for this series. When a welded general-purpose twin is required, look to EN 10296-2 rather than forcing a seam into a 10297-2 order. When PED pressure seamless acceptance is mandatory, use EN 10216-5 for the same steel number where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Role reminder for 1.4580: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Inside this seamless general-purpose series, compare EN 10297-2 1.4571, EN 10297-2 1.4401, EN 10297-2 1.4550. Hub: EN 10297-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4580.

Chemical Composition of EN 10297-2 1.4580

Cast window focus for 1.4580: Every 1.4580 heat under EN 10297-2 must meet the cast (ladle) analysis for X6CrNiMoNb17-12-2 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Commercial alias 316Nb is body text only. Corrosion thread: Mo plus Nb stabilisation for as-welded aqueous and mildly oxidising services.

Cast chemistry for seamless 1.4580 must land inside X6CrNiMoNb17-12-2 limits. The table is transcribed from public BSSA EN 10297-2 data for quick comparison with sister grades; always re-check the paid standard when a dispute arises. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Steel C Si Mn P S Cr Mo Ni Nb
1.4580 / X6CrNiMoNb17-12-2 ≤0.08 ≤1.00 ≤2.00 ≤0.045 ≤0.015 16.5–18.5 2.00–2.50 10.5–13.5 10×C–1.00

Mechanical Properties of EN 10297-2 1.4580

Ambient floors focus for 1.4580: Do not borrow EN 10216-5 pressure mechanical rows for an EN 10297-2 1.4580 order. General-purpose Table values for this number read: Rp0.2 min 215 MPa, Rp1.0 min 250 MPa, Rm min 510 MPa, longitudinal elongation min 35%. Where cold- and hot-finished rows differ, state the finishing route on the purchase order. Family: austenitic corrosion-resisting. Caution thread: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 215 250 510 min 35 30 Yes

Ambient values from EN 10297-2:2005 Tables 6–9 for 1.4580 / X6CrNiMoNb17-12-2. Guideline solution/anneal band (Annex B): 1020–1100 °C; cooling: water or air.

Seamless Tube Manufacture for EN 10297-2 1.4580

Seamless route narrative for 1.4580: EN 10297-2 does not offer a welded route for 1.4580. Tube in X6CrNiMoNb17-12-2 is made seamless — hot finished and/or cold finished — then heat-treated to the ordered delivery condition. Order EN 10297-2 1.4580 with an Annex A surface/process symbol — HFD or CFD for metallically clean descaled tube, CFA when bright-annealed OD is required, CFG/CFP when ground or polished roughness is written into the purchase order. Weld thread: Nb-bearing Mo austenitic fillers; align procedures with stabilised base metal.

For austenitic 1.4580, cold finishing (CFD/CFA/CFG/CFP) is the usual path to tighter OD and surface control after a hot-finished hollow; heavy walls may remain HFD. Austenitic 1.4580 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1020–1100 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

When dual documentation against EN 10216-5 is requested for the same 1.4580 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 1.4580: process seamless bands with Annex A descaled or bright routes. Use thread: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list.

Dimensions and Tolerances for EN 10297-2 1.4580

Dimensional order line for 1.4580: Order EN 10297-2 1.4580 by outside diameter D and wall thickness T for steel name X6CrNiMoNb17-12-2. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Process seamless bands with annex a descaled or bright routes. Use thread: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list.

Tolerance classes on diameter and wall follow the EN 10297-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Size hint for 1.4580: process seamless bands with Annex A descaled or bright routes. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Equivalent Grades for EN 10297-2 1.4580

Equivalence talk for 1.4580 starts with X6CrNiMoNb17-12-2: 1.4580 / X6CrNiMoNb17-12-2 is the EN 10297-2 designation for this chemistry as seamless general-purpose tube. Commercial alias 316Nb appears in body text only — not in the H1. ASTM/ASME pages that share a related chemistry are different product standards with different wall bases, mechanical tables, and tests. Confirm before treating them as interchangeable. Inside this seamless general-purpose series, compare sisters 1.4571, 1.4401, 1.4550. Hook for buyers still using only the 316Nb alias: lock EN 10297-2 1.4580 on the order line. Caution thread: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report.

Heat Treatment and Delivery Condition for EN 10297-2 1.4580

Austenitic 1.4580 is delivered solution annealed (+AT). Public Annex B guidance places solution annealing near 1020–1100 °C with water or air cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Weld thread: Nb-bearing Mo austenitic fillers; align procedures with stabilised base metal.

Fabrication HT reminder for 1.4580 (+AT): Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4580, restore the delivery condition agreed on the order before corrosive or load-bearing service. Delivery framing on the certificate for 1.4580 should match +AT. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Corrosion Resistance of EN 10297-2 1.4580

Corrosion behaviour of EN 10297-2 1.4580 tracks its austenitic corrosion-resisting balance: Mo plus Nb stabilisation for as-welded aqueous and mildly oxidising services. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report Corrosion thread: Mo plus Nb stabilisation for as-welded aqueous and mildly oxidising services.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4580 is filed as austenitic corrosion-resisting — pick tests that match that filing. Family filing for 1.4580 is austenitic corrosion-resisting. Caution thread: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report.

Applications of EN 10297-2 1.4580 Tube

Applications of EN 10297-2 1.4580 tube centre on mechanical and general engineering rather than PED pressure shells: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list. Role summary: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists. Use thread: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list.

Typical BOM language pairs EN 10297-2 1.4580 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “316Nb” substitutions do not creep in. Primary application sketch: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Weldability of EN 10297-2 1.4580

1.4580 / X6CrNiMoNb17-12-2 is welded as a fabricator joint on mechanical assemblies even though the tube product itself is seamless under EN 10297-2. Shop guidance: Nb-bearing Mo austenitic fillers; align procedures with stabilised base metal. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Weld thread: Nb-bearing Mo austenitic fillers; align procedures with stabilised base metal.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report Filler/shop note for 1.4580: Nb-bearing Mo austenitic fillers; align procedures with stabilised base metal. Caution thread: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report.

Surface Finishes for EN 10297-2 1.4580

Finish selection for 1.4580 on Annex A: Surface finish on EN 10297-2 1.4580 is carried by the Annex A symbol: descaled HFD/CFD for general mechanical tube, bright-annealed CFA for cleaner OD appearance, and ground CFG or polished CFP when roughness is agreed at enquiry. Carbon-steel strapping must not contact the stainless surface. Alias reminder: commercial talk may say 316Nb, but the finish symbol still belongs on the EN 10297-2 line. Use thread: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list.

Agree any site-storage constraints for 1.4580 at enquiry. Long inland dwell in winter road-salt regions needs sealed wrap even when ocean freight is not involved. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Inspection and Testing for EN 10297-2 1.4580

Inspection lot framing for 1.4580 in austenitic corrosion-resisting: Specific inspection applies to EN 10297-2 1.4580 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Keep 1.4580 heat identity intact from cast through bundle tag. Weld thread: Nb-bearing Mo austenitic fillers; align procedures with stabilised base metal.

Acceptance marks on 1.4580 reference the inspection lot. If a piece is cut after delivery, retain the marked end or transfer the heat identity under the fabricator’s quality system so traceability survives the saw. Use thread: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list.

Packaging and Shipping for EN 10297-2 1.4580

Dispatch note for 1.4580 (316Nb body alias only): SHH STEEL ships EN 10297-2 1.4580 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled HFD/CFD engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Marking and identity for 1.4580: For 1.4580, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Finish-sensitive packing for 1.4580 follows the Annex A symbol on the order. Use thread: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list.

Project freight for 1.4580 can be staged by installation sequence when the packing list names priority bundles. That staging is agreed before the saw schedule locks. Caution thread: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10297-2 1.4580 seamless stainless steel tube. Why 1.4580 with SHH STEEL — role: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified. Choose SHH STEEL for EN 10297-2 1.4580 when you need a mill partner who will not blur EN 10297-2 with EN 10216-5 or EN 10217-7 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

Grade advice stays practical for 1.4580. If the duty needs a sister chemistry, we point to 1.4571, 1.4401, 1.4550. Design caution for this number: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report Export document packs are assembled to match the heat tags on the bundles you will receive. Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Caution thread: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report.

Supply Capability

SHH STEEL can produce and supply EN 10297-2 1.4580. SHH STEEL’s EN 10297-2 1.4580 offering is make-to-order seamless tube in X6CrNiMoNb17-12-2. We can produce and supply cut lengths and standard mill lengths. Use the Stock / Available sizes map as a planning aid, then confirm live availability on the quote. Use thread: chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list.

Item Capability
Standard EN 10297-2:2005 seamless general-purpose
Steel 1.4580 / X6CrNiMoNb17-12-2
Product form Seamless tube (HFD / CFD / CFA / CFG / CFP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–20 mm within family practice (other by agreement)

Stock / Available sizes

Stock / Available sizes note for 1.4580: bring the OD × wall list early. Context: process seamless bands with Annex A descaled or bright routes. Bright CFA and polished CFP may add finishing lead time versus descaled CFD/HFD. Duty thread: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.

When 1.4580 shares a project with 1.4571, 1.4401, 1.4550, keep separate heat identity tags. SHH STEEL can produce and supply coordinated size lists so fabrication receives matched OD bands without mixed certificates. Weld thread: Nb-bearing Mo austenitic fillers; align procedures with stabilised base metal.

FAQ

What is EN 10297-2 1.4580 seamless stainless steel tube used for?
EN 10297-2 1.4580 (X6CrNiMoNb17-12-2) is seamless tube for mechanical and general engineering — chemical and elevated-temperature mechanical tubing where 316Nb chemistry is on the material list. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed. Role summary: Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified.
Is EN 10297-2 1.4580 the same as EN 10216-5 1.4580?
Chemistry families may overlap, but acceptance differs. EN 10297-2 is seamless general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10297-2 MTC for 1.4580 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4580 / X6CrNiMoNb17-12-2?
Delivery framing for 1.4580 is +AT under the EN 10297-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1020–1100 °C with water or air cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4580?
SHH STEEL can produce and supply HFD, CFD, CFA, CFG, and CFP routes for EN 10297-2 1.4580 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4580 compare with sister grades 1.4571, 1.4401, 1.4550?
1.4580 / X6CrNiMoNb17-12-2 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4571, 1.4401, 1.4550. Design caution: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
Can 1.4580 be welded even though the tube is seamless?
Yes — fabricator joints are common on mechanical assemblies. Shop guidance: Nb-bearing Mo austenitic fillers; align procedures with stabilised base metal. Mill heat treatment of the seamless tube does not replace a qualified WPS on site welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4580?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10297-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10297-2 1.4580?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4580 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: process seamless bands with Annex A descaled or bright routes. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 316Nb belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 316Nb in body text and BOM notes, but lock EN 10297-2 and 1.4580 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4580?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: not a chloride upgrade beyond Mo austenitic practice; confirm Nb analysis on the cast report Sister pointers: 1.4571, 1.4401, 1.4550. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10297-2 1.4580 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4580 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4749 / 1.4833 / 1.4845 / 1.4835 / 1.4876 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10297-2 1.4580 (X6CrNiMoNb17-12-2) is seamless stainless tube for mechanical and general engineering — Nb-stabilised Mo-bearing austenitic seamless tube parallel to 1.4571 when niobium stabilisation is specified. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4571, 1.4401, 1.4550. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X