EN 10155 Weathering Steel Overview | Superseded by EN 10025-5
What is EN 10155 and why is it superseded?
EN 10155 (commonly EN 10155:1993) specified structural steels with improved atmospheric corrosion resistance. BS EN 10025-5:2004 together with BS EN 10025-1:2004 supersedes BS EN 10155:1993, which is withdrawn. Current purchasing, mill dual-certification and steelspecs product content live under EN 10025-5.
This is a light overview only. It is not a full grade farm. If an RFQ still says EN 10155 S355J2G2W or Fe 510 D2 KI, map it with the table below and quote the matching EN 10025-5 plate.
Category hubs: EN 10155 · EN 10025-5 · Weathering Steel Plates.
Primary live grade pages: EN 10025-5 S355J2W · EN 10025-5 S355J0W · EN 10025-5 S355K2W · EN 10025-5 S355J2WP · EN 10025-5 S355J0WP · EN 10025-5 S235J2W · EN 10025-5 S235J0W.
Material Specification note for EN 10155 (historical)
| Parameter | Specification |
|---|---|
| Historical standard | EN 10155 (withdrawn; commonly cited as EN 10155:1993) |
| Superseding standard | EN 10025-5 (+ EN 10025-1) |
| Page type | Overview / mapping only (not a grade SKU farm) |
| Product form | Hot-rolled structural plate / sections historically; follow EN 10025-5 for current supply |
| Preferred order text | EN 10025-5 + modern grade (e.g. S355J2W), unless the project forces a legacy designation on documents |
| Certification today | EN 10204 3.1 / 3.2 to EN 10025-5; legacy EN 10155 marking only by special agreement |
| Density | 7.85 g/cm³ |
Chemical Composition: use EN 10025-5 mapped grade
Do not maintain a separate EN 10155 chemistry farm on this site. Chemistry for current supply follows EN 10025-5 for the mapped grade.
W-family reference: see S355J2W / S355J0W / S235J2W.
WP-family (elevated phosphorus) reference: see S355J2WP / S355J0WP.
Always verify the mill test certificate against the ordered (usually EN 10025-5) edition.
Mechanical Properties: use EN 10025-5 mapped grade
Delivery Conditions under EN 10025-5
Follow EN 10025-5 delivery conditions for current orders (+AR / +N as applicable). See the linked EN 10025-5 grade pages for condition notes. Do not invent a separate EN 10155 delivery matrix on this overview.
Dimensional Tolerances via current EN package
Dimensional tolerances for current plate supply follow the dimensional standards cited by the EN 10025-5 order package (for example EN 10029 for plate), not a separate EN 10155 tolerance farm.
Applications and service limits (legacy RFQs)
Legacy EN 10155 citations still appear on older drawings, bridge archives and some international RFQs. Typical end uses are the same as EN 10025-5 weathering plate: bridges, facades, outdoor structures, vehicles and containers.
Route the inquiry to the matching live page: S355J2W · S355J0W · S355J2WP · S355J0WP · S235J2W · Corten B · Corten A.
Atmospheric exposure guidance (same intent as EN 10025-5)
Atmospheric exposure guidance is identical in intent to EN 10025-5 weathering steels. Use the table as a selection aid; final coating or grade choice follows the project specification.
| Environment | Typical fit for bare EN weathering plate | Note |
|---|---|---|
| Rural / mild industrial | Usually suitable | Needs wet/dry cycles for patina |
| Urban / general industrial | Often suitable | Check local pollution and design details |
| Coastal / marine splash with moderate chloride | Use with caution | May need coating or another grade |
| Sheltered pockets that stay wet | Not preferred bare | Design out traps or coat locally |
| Continuous immersion / aggressive chloride | Not recommended bare | Select coated carbon steel or another material |
EN 10155 → EN 10025-5 mapping table
Old → new mapping (informative). Based on EN 10025-5 Annex A style correspondence tables widely published with the 2004 transition. Confirm any substitution against the project specification.
| EN 10155:1993 (legacy) | EU 155-80 (older) | EN 10025-5 (use this) | Note |
|---|---|---|---|
| S235J0W | Fe 360 C KI | S235J0W | Same modern name already in EN 10155 |
| S235J2W | Fe 360 D KI | S235J2W | Same modern name already in EN 10155 |
| S355J0WP | Fe 510 C 1 KI | S355J0WP | WP track; same modern name |
| S355J2WP | Fe 510 D 1 KI | S355J2WP | WP track; same modern name |
| S355J0W | Fe 510 C 2 KI | S355J0W | W track; same modern name |
| S355J2G1W / S355J2G2W | Fe 510 D 2 KI (for G1W) | S355J2W | EN 10155 split G1W/G2W; EN 10025-5 unified as S355J2W |
| S355K2G1W / S355K2G2W | – | S355K2W | EN 10155 split G1W/G2W; EN 10025-5 unified as S355K2W |
Related non-EN pages: Corten A · Corten B · ASTM A242 Type 1 · GB/T 4171 Q355NH · JIS G3125 SPA-H · ISO 630-5.
How to convert an EN 10155 RFQ to EN 10025-5
How to handle an RFQ that still says EN 10155.
| RFQ wording | What to do | Live page |
|---|---|---|
| EN 10155 S355J2W / S355J2G2W / S355J2G1W | Quote EN 10025-5 S355J2W | S355J2W |
| EN 10155 S355K2G1W / S355K2G2W | Quote EN 10025-5 S355K2W | S355K2W |
| EN 10155 S355J0WP / S355J2WP | Quote the same modern WP grade under EN 10025-5 | S355J0WP · S355J2WP |
| EN 10155 S235J0W / S235J2W | Quote EN 10025-5 S235J*W | S235J0W · S235J2W |
| Only Fe 510 / Fe 360 weathering names | Map via EU 155 column, then EN 10025-5 | EN 10025-5 hub |
Why choose SHH STEEL for EN 10155 / EN 10025-5 weathering inquiries
- Clear supersession messaging: EN 10155 → EN 10025-5, without SEO spam grade farms
- Direct links to live EN 10025-5 product pages already on steelspecs.com
- China mill-direct EN 10025-5 weathering plate with EN 10204 3.1 / 3.2
- Help converting legacy RFQs into current order text
- Hubs: EN 10155 · EN 10025-5 · Weathering Steel Plates
Supply and inspection when an RFQ still cites EN 10155
| Item | SHH STEEL supply note |
|---|---|
| What we supply | EN 10025-5 weathering plate mapped from legacy EN 10155 RFQs |
| Preferred cert | EN 10025-5 on EN 10204 3.1 / 3.2 MTC |
| Legacy marking | EN 10155 designation on documents only by special agreement |
| Processing | Cutting, beveling, shot blasting available |
| Third-party inspection | SGS, TUV, BV or ABS can be arranged |
| Quotation needs | Legacy EN 10155 name (if any) + preferred EN 10025-5 grade, thickness × width × length, quantity, delivery condition, inspection level |
FAQ
-
Is EN 10155 still valid?
- No for new European specification work. It is superseded by EN 10025-5 (with EN 10025-1). Use the EN 10025-5 hub.
-
What happened to S355J2G1W and S355J2G2W?
- Under EN 10025-5 they are unified as S355J2W (with +N when normalized delivery is required).
-
Can you still mark EN 10155 on the MTC?
- Only by special agreement when a project forces the legacy designation. Default supply and certification are EN 10025-5.
-
Where are the chemistry and tensile tables?
- On the live EN 10025-5 grade pages linked above. This overview intentionally avoids duplicating a full grade farm.
-
How does this relate to ISO 630-5?
- ISO 630-5 is a parallel international weathering standard with strong EN overlap. See ISO 630-5.
Request a quotation
Send the legacy EN 10155 designation (if present), the preferred EN 10025-5 grade, thickness × width × length, quantity, delivery condition and any inspection requirement. SHH STEEL will map the grade, confirm mill dual-cert options and return a quotation.
Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097
More options: EN 10025-5 · S355J2W · S355J2WP · EN 10155 · Weathering Steel Plates · Structural Steel Plates