ASTM A572 Grade 50 Wide Flange H Beam
What is an ASTM A572 Grade 50 Steel Beam?
An ASTM A572 Grade 50 steel beam is a rolled structural shape whose material conforms to ASTM A572/A572M Grade 50 [345] and whose dimensions and tolerances conform to ASTM A6/A6M. Grade 50 is a high-strength low-alloy columbium-vanadium steel with a minimum yield point of 50 ksi [345 MPa] and a minimum tensile strength of 65 ksi [450 MPa]. The usual product on this page is a W-shape. The “W” designation is the American wide-flange series; it is not a translation of a Chinese HW section or of a European HEA or HEB of a similar nominal depth.
This page covers the rolled shape, not plate. The same grade in plate form is listed separately as ASTM A572 Grade 50 steel plate. Plate chemistry uses the same carbon and manganese maxima, but the default phosphorus and sulphur maxima and some silicon and manganese-minimum rules differ by product form, and the 4 in [100 mm] thickness limit in Table 1 is a plate-and-bar limit. Grade 50 structural shapes are listed with flange or leg thickness “all.” The plate page is not a substitute data sheet for W-shapes.
These beams are filed under ASTM A572 steel beam profiles in the steel beam profiles category of steel structural profiles. Related American beam categories include ASTM A36 and ASTM A992.
A572 also defines Grades 42, 55, 60 and 65. This article is Grade 50, the usual beam grade. Grades 60 and 65 have tighter shape-flange limits (2 in [50 mm]) and are intended, in the specification, for riveted or bolted bridge work, or for riveted, bolted or welded construction in other applications. An enquiry that only says “A572 beam” still needs the grade, the W designation, and any supplementary tests.
Material, Dimensions and Tolerances for A572 Grade 50 Shapes
Two documents should appear, separately, on the purchase order and on the mill test report:
- ASTM A572/A572M is the material specification. This article uses the chemistry, alloy-type and tensile values published in ASTM A572/A572M-21ε1. The edition named on the order governs acceptance. Inch-pound and SI values are official in their own systems and should not be mixed.
- ASTM A6/A6M is the general-requirements standard for rolled structural steel bars, plates, shapes and sheet piling. It sets the W-shape designation system, dimensional and camber tolerances, marking, and the heat-analysis and tension-test rules that A572 refers to. A572 does not itself contain the W-shape size tables.
The steel is killed. A microalloy type — 1, 2, 3 or 5 — is required; the producer selects it unless supplementary requirement S90 names the type on the order. A mill may also certify Grade 50 on a non-W shape, or roll a W-shape to a different material specification, if that combination is in its programme and is fully documented. Do not substitute EN 10025-2 S355JR HEA/HEB/IPE sizes or GB/T 11263 HW/HM/HN sizes by matching a nominal 12 in or 300 mm depth.
A572 Grade 50 W-Shape Sizes and Reference Dimensions
The tables list nominal W-shape reference dimensions: designation, actual depth, width, web and flange thickness in inch and millimetre units, and mass in lb/ft and kg/m. There are 283 designations, grouped by depth. They are reference dimensions for identification and estimating, not a rolling list, and not a claim of guaranteed availability or that every W-shape is produced in A572 Grade 50. Dimensional acceptance, including shape and mass tolerances, follows the edition of ASTM A6/A6M named on the order. Mid-range W12 to W30 beams and the common W8–W14 column sizes are the usual enquiry core; the lightest W4–W6 rows, jumbo column sections, and the deepest W40–W44 rows should be confirmed size by size.
A designation such as W16×26 is a series call: the first number is the nominal depth in inches and the second is the nominal mass in pounds per foot. The actual depth may be slightly less than the nominal value. Root radius is omitted because a single fillet radius is not published as a delivery dimension for these shapes. These W-shape rows are not interchangeable with HW, HM, HN or HEA/HEB/IPE rows of a similar nominal depth.
W4 to W10
The lighter W-shapes, often used as small beams, lintels and miscellaneous members. 41 designations, from W4×13 through the W10 series.
Swipe horizontally to view all dimensions.
W12 and W14
The mid-depth beam and column group, including many of the heavier W12 and W14 column sections. 67 designations.
Swipe horizontally to view all dimensions.
W16 to W21
Common building-beam depths. 55 designations.
Swipe horizontally to view all dimensions.
W24 to W30
Deeper building and industrial beams. 54 designations.
Swipe horizontally to view all dimensions.
W33 to W44
The deepest W-shapes in these reference tables, through W44. 66 designations. Heavier and deeper rows, including wide-flange shapes over 426 lb/ft, should be confirmed size by size against the mill programme.
Swipe horizontally to view all dimensions.
Chinese HW/HM/HN sizes belong to GB/T 11263. European HEA/HEB/IPE sizes are listed on the S355JR H-beam page for that material system, not as A572 dimensions.
A572 Grade 50 Chemical Composition for Shapes
The figures below are heat-analysis requirements for Grade 50 shapes in ASTM A572/A572M-21ε1. They are not a copy of unofficial stockist tables that still show 0.04% phosphorus and 0.05% sulphur as the only limits for every product form, and they are not the wide-plate 0.030% P and S defaults applied without the shape footnote. Product analysis, when required, follows ASTM A6/A6M tolerances.
The required microalloy type is selected from Table 3. Types give the same specified Grade 50 strengths; they are not interchangeable chemistry routes, and the type actually produced belongs on the test report.
A572 Grade 50 Mechanical Properties for Shapes
The tensile requirements below are from ASTM A572/A572M-21ε1 Table 4 for Grade 50. Specimen orientation follows ASTM A6/A6M. The plate-width elongation reduction in footnote D is a plate rule and is not applied to these W-shapes.
A572 Grade 50 specifies minimum yield and tensile values only. It does not cap the actual yield or the yield-to-tensile ratio. Where a project needs those controls — as many building and seismic specifications do — the usual grade to nominate on a W-shape is A992, not an unspoken “A572 will be close enough.”
Impact testing is not a default Grade 50 requirement. For welded bridge work the specification itself says notch toughness is to be negotiated. If a Charpy value is needed, the order should add S5 or S30 and state the test temperature and acceptance value.
Delivery Conditions, Inspection and Identification
A572 Grade 50 shapes are commonly supplied as-rolled and must be killed. The mill test report should show ASTM A572/A572M and its edition, the grade 50 [345], the microalloy type and the applicable alloy contents, the A6/A6M edition, the W designation, the heat number, the heat analysis, the tensile results, and any supplementary requirements that were ordered. When copper steel, S81, S90, S5 or S30 is required, it has to be on the order to appear on the report.
An EN 10204 type 3.1 document is the usual export request when the mill issues one against the ASTM test report; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows ASTM A6/A6M marking practice.
Length is not fixed by the W-shape table. Export lengths in the region of 6–15 m, or other agreed lengths, are a matter for the rolling programme and the order.
Weldability and Surface Condition of A572 Grade 50 Beams
Grade 50 is intended for riveted, bolted or welded structures. The specification points the purchaser to a welding procedure suited to the grade and the service, and to Appendix X3 of ASTM A6/A6M for weldability information. A572 does not specify a carbon-equivalent maximum. The actual heat carbon, manganese and microalloy type, together with a procedure suited to the thickness, are the practical controls. This page does not prescribe a procedure or a preheat chart.
The as-rolled surface is mill scale. A blast class, a paint system, or a hot-dip galvanizing chemistry is an order option, not something implied by the grade name. If galvanizing is planned, the silicon on the heat and the processor’s coating specification should be reviewed before production. Surface quality follows ASTM A6/A6M.
Cutting to length, weld-end preparation, forming or coating can be reviewed when the specification is sent with the enquiry. They are not assumed for every size.
ASTM A6/A6M Shape Tolerances and Theoretical Mass
Dimensional, straightness, camber, sweep, out-of-square and mass tolerances for these W-shapes are those of ASTM A6/A6M, not of ASTM A572/A572M. This article does not reproduce the A6 tolerance tables; acceptance is against the edition named on the order.
The size tables above are nominal W-shape reference dimensions. A delivered W16×26 will measure close to the tabulated depth, width and thicknesses within the tolerances of the ordered ASTM A6/A6M edition, not as a set of exact advertised inches. The lb/ft and kg/m columns are tabulated theoretical masses. Settlement should follow the contract — tabulated theoretical mass or weighed mass — and the ordered A6 mass tolerance.
Applications and Service Limits
A572 Grade 50 beams are used where a 50 ksi [345 MPa] high-strength low-alloy W-shape is accepted and an upper yield limit is not required by the specification:
- Building and industrial frames, platforms and general fabrication that actually name A572 Grade 50.
- Members compared with a 355 MPa European or Chinese grade, provided each line keeps its own standard and shape system.
- Work that does not, by itself, require the A992 yield cap, yield-to-tensile cap or carbon-equivalent cap.
It is not specified here for pressure equipment, for nuclear safety-related components, or for structures whose specification requires A992, A588, or a mandatory impact test that has not been added as a supplementary requirement. Durability comes from the coating or fire-protection system, not from the grade name.
A572 Grade 50 Compared with A992, A36 and S355JR
A572 Grade 50, A992 and A36 can all be rolled as the same W-shape series under ASTM A6/A6M, but they are different material specifications. A992 is the usual modern grade for US building W-shapes; it keeps the 50 ksi minimum yield and adds a 65 ksi yield maximum (70 ksi when the web is the required test location), a 0.85 yield-to-tensile maximum (0.87 from the web), and a carbon-equivalent cap. A36 is a 36 ksi carbon steel. An enquiry that says only “W-beam” is incomplete.
S355JR H-beam is a near-equivalent in yield class, but it carries a 27 J impact requirement at +20 °C and is rolled as HEA, HEB or IPE unless a mill has a documented special combination. Dual certification is possible only when the delivered piece meets every requirement of each named standard.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or a mill certificate.
Sister beam pages in this series (A36, A992, Q355B) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page for the European 355 MPa comparison.
Sourcing A572 Grade 50 Beams from SHH STEEL
SHH STEEL supplies ASTM A572 Grade 50 beams as an export trading house, coordinating mill production and project procurement. The useful part of that model is to align the material edition (ASTM A572/A572M), the grade and microalloy type, the shape standard (ASTM A6/A6M), the exact W designation, any supplementary requirements such as S5, S30, S81 or S90, and the form of the test report before a rolling or allocation programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every W-shape in Grade 50. Mid-range beams and common column sizes are the usual core; jumbo and very deep sections are confirmed per line. Mixed procurement can be used when a take-off spans more than one rolling programme.
The same enquiry can also cover Chinese, European or Japanese designations, provided each line states its material standard, shape standard and size. If cutting, weld-end preparation, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
A572 Grade 50 Beam FAQs
-
Is A572 Grade 50 the same as A992?
- No. Both are 50 ksi classes often rolled as W-shapes, but A992 adds a maximum yield, a maximum yield-to-tensile ratio and a carbon-equivalent cap, and it is a shapes specification in its own right. A572 Grade 50 has minimum yield and tensile values only. Do not treat one as a silent substitute for the other unless the delivered piece is dual-certified to every requirement of both.
-
Which phosphorus and sulphur limits apply to a W-shape?
- Table 2 of ASTM A572/A572M-21ε1 lists 0.030% P and 0.030% S. A footnote permits 0.04% P and 0.05% S for structural shapes, sheet piling, bars, and plates not more than 15 in wide. For Grade 50 beams, those shape allowances apply. Older stockist tables that show 0.04/0.05 for every product, or 0.030/0.030 with no footnote, should be checked against the edition and the product form.
-
Do I need to specify Type 1, 2, 3 or 5?
- A type is required, but the producer may select it unless supplementary requirement S90 names the type on the order. The type used, and the applicable niobium, vanadium, titanium or nitrogen contents, shall be reported on the test report.
-
Is an impact test included with A572 Grade 50?
- Not by default. Charpy testing is added only when the order specifies S5, or S30 for the alternate core location on structural shapes, and states the test temperature and acceptance value. For welded bridge work the specification says notch toughness is to be negotiated.
-
Which standards should appear on the mill test report?
- At least ASTM A572/A572M and its edition, Grade 50 [345], the microalloy type and alloy contents, the ASTM A6/A6M edition, the W designation, the heat analysis, the tensile results, and any supplementary requirements that were ordered.
Request a Quotation for ASTM A572 Grade 50 Wide Flange H Beam
ASTM A572 Grade 50 steel beam is a high-strength low-alloy W-shape with 50 ksi [345 MPa] minimum yield and 65 ksi [450 MPa] minimum tensile strength, and no specified yield maximum. Nominate the W designation to ASTM A6/A6M, name ASTM A572/A572M Grade 50 (or the edition on the order), and add S5, S30, S81 or S90 only if those extras are required. The tables are nominal W-shape reference dimensions, not a rolling list and not a claim of guaranteed availability. Dimensional acceptance follows the ordered edition of ASTM A6/A6M. Send the size list, edition, type or supplementary notes and any processing requirements; SHH STEEL will review the package and quote accordingly.