EN 10025-2 S355JR Equal and Unequal Steel Angles | EN 10025-2 Steel Angles - SHH STEEL

EN 10025-2 S355JR Equal and Unequal Steel Angles

EN 10025-2 S355JR steel angle is a non-alloy equal-leg or unequal-leg L-shape (1.0045) with 355 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Dimensions follow EN 10056-1, with tolerances under EN 10056-2. The ordered edition governs. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.
Keywords
EN 10025-2 S355JR Steel Angle, S355JR equal angle, S355JR unequal angle, 1.0045 structural angle, EN 10056 L-shape
Equivalent Grades:
Near-equivalents only, not automatic substitutes: S235JR is a lower-strength grade, not the same section; Q355B; A572 Grade 50; S355J0 and S355J2 have colder impact qualities.
Share:
General Description
Material Specification
Available Sizes of EN 10025-2 S355JR Equal Leg Steel Angles
Available Sizes of EN 10025-2 S355JR Unequal Leg Steel Angles
Chemical Composition
Carbon equivalent
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source S355JR Steel Angles from SHH STEEL
FAQ
Conclusion

What is EN 10025-2 S355JR Steel Angle?

EN 10025-2 S355JR steel angle is a hot-rolled equal-leg or unequal-leg L-shape in non-alloy structural steel S355JR (steel number 1.0045). The material standard is EN 10025-2. Dimensions and theoretical masses are those of EN 10056-1. Shape and dimensional tolerances are those of EN 10056-2. S marks a structural steel, 355 is the minimum yield strength in MPa up to 16 mm, and JR is the impact quality, 27 J at +20 °C. That impact temperature is the same as for S235JR; what changes on this page is the 355 MPa yield class, the tensile range, and the S355JR chemistry and carbon-equivalent table.

An equal angle is designated by one leg length and the thickness, for example L 200×200×16. An unequal angle is designated by the two leg lengths and the thickness, for example L 200×100×12. L 200×100×12 is not L 200×200×12, and neither is an EN 10365 channel or an HEA of a similar millimetre size. An American L, a Chinese or Japanese angle, or a European channel of similar depth is a different product unless the order documents that combination in full.

These angles are filed under EN 10025-2 steel angle profiles in the steel angle profiles category of steel structural profiles. The same grade as a rolled I or H section is listed as EN 10025-2 S355JR H-beam. The same grade in plate form is listed as EN 10025-2 S355JR steel plate. Do not use either of those pages as an angle data sheet, and do not copy plate chemistry defaults, or channel tolerances from EN 10279, onto an L-shape certificate.

S355JR angles are used for bracing, frames, trim and general fabrications when the specification names this 355 MPa non-alloy grade in a European L-shape. The grade is not a pressure-vessel or nuclear safety material, and it is not a substitute for S355J0 or S355J2 when a colder impact quality is what the order requires, nor for S235JR when a 235 MPa certificate is what was specified.

This page covers Equal and Unequal Steel Angles in EN 10025-2 S355JR. The Equal Leg Steel Angles and Unequal Leg Steel Angles follow EN 10056-1; the material standard does not by itself define the dimensions.

Material, Dimensions and Tolerances for S355JR Angles

The order and the inspection certificate should keep material, dimensions and tolerances distinct:

  • EN 10025-2 is the material standard. This article uses ladle chemistry, carbon-equivalent and tensile values for S355JR long products from EN 10025-2:2019. The edition named on the order governs acceptance.
  • EN 10056-1 is the dimensional standard for these equal-leg and unequal-leg angles. The size tables below are a verified subset of EN 10056-1:2017, not the complete series. They are reference dimensions and theoretical masses. The edition of EN 10056-1 named on the order governs dimensional acceptance.
  • EN 10056-2 is the tolerance standard for these angles. This article uses EN 10056-2:1993 as the known edition. Do not apply EN 10279 channel tolerances, or EN 10034 I- and H-section tolerances, to an L-shape. The edition of EN 10056-2 named on the order governs dimensional and mass tolerance acceptance.

A documented special combination — for example S355JR on an ASTM L-shape, or a European angle certified to a different material standard — is only valid if every requirement of each named standard is met. Matching a nominal 200 mm leg is not a substitution.

EN 10025-2 S355JR Equal Leg Steel Angles

The tables list designation, leg length, thickness, theoretical area and theoretical mass for the equal-leg and unequal-leg sizes in the verified EN 10056-1:2017 set used for this article. Use them to identify and estimate, not as a rolling programme for S355JR, and not as a claim that every EN 10056-1 size is shown here.

EN 10056-1:2017 also covers smaller equal legs and a wider unequal-leg series than the rows below. Those sizes can be reviewed when they are named on the enquiry. This page does not invent dimensions for sizes that were not in the verified table set. Mid-range tabulated rows such as L 150 and L 200 are the usual enquiry core in this set; L 250 and L 300, and the single tabulated L 80 and L 90 thicknesses, should be confirmed size by size.

L 200×200×16 is a 200 mm equal angle, 16 mm thick, at the boundary of the first yield band. L 200×200×20 is 20 mm thick, so the minimum yield is 345 MPa, not 355 MPa. L 200×100×12 is an unequal 200 mm by 100 mm angle, 12 mm thick; it is not L 200×200×12. L 300×300×35, the heaviest tabulated equal angle here, has a 35 mm leg and remains in the 16–40 mm yield band.

Equal-leg angles (71 verified sizes, L 80×80×8 to L 300×300×35)

L 80 to L 150 equal (15 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 80×80×8 80 8 12.3 9.63
L 90×90×6 90 6 10.6 8.3
L 130×130×10 130 10 25.2 19.8
L 130×130×11 130 11 27.6 21.7
L 130×130×12 130 12 30 23.6
L 130×130×13 130 13 32.3 25.4
L 130×130×14 130 14 34.7 27.2
L 150×150×10 150 10 29.3 23
L 150×150×12 150 12 34.8 27.3
L 150×150×13 150 13 37.6 29.5
L 150×150×14 150 14 40.3 31.6
L 150×150×15 150 15 43 33.8
L 150×150×16 150 16 45.7 35.9
L 150×150×18 150 18 51 40.1
L 150×150×20 150 20 56.3 44.2

L 160 to L 200 equal (28 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 160×160×14 160 14 43.2 33.9
L 160×160×15 160 15 46.1 36.2
L 160×160×16 160 16 49 38.4
L 160×160×17 160 17 51.8 40.7
L 160×160×18 160 18 54.7 42.9
L 160×160×19 160 19 57.5 45.1
L 160×160×20 160 20 60.3 47.3
L 180×180×13 180 13 45.5 35.7
L 180×180×14 180 14 48.8 38.3
L 180×180×15 180 15 52.1 40.9
L 180×180×16 180 16 55.4 43.5
L 180×180×17 180 17 58.7 46
L 180×180×18 180 18 61.9 48.6
L 180×180×19 180 19 65.1 51.1
L 180×180×20 180 20 68.3 53.7
L 180×180×22 180 22 74.9 58.6
L 200×200×15 200 15 58.1 45.6
L 200×200×16 200 16 61.8 48.5
L 200×200×17 200 17 65.5 51.4
L 200×200×18 200 18 69.1 54.2
L 200×200×19 200 19 72.7 57.1
L 200×200×20 200 20 76.3 59.9
L 200×200×21 200 21 79.9 62.8
L 200×200×22 200 22 83.5 65.6
L 200×200×23 200 23 87.1 68.3
L 200×200×24 200 24 90.6 71.1
L 200×200×25 200 25 94.1 73.9
L 200×200×26 200 26 97.6 76.6

L 250 to L 300 equal (28 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 250×250×17 250 17 82.1 64.4
L 250×250×18 250 18 86.7 68.1
L 250×250×19 250 19 91.4 71.7
L 250×250×20 250 20 96 75.3
L 250×250×21 250 21 101 78.9
L 250×250×22 250 22 105 82.5
L 250×250×23 250 23 110 86.1
L 250×250×24 250 24 114 89.7
L 250×250×25 250 25 119 93.2
L 250×250×26 250 26 123 96.7
L 250×250×27 250 27 128 101
L 250×250×28 250 28 133 104
L 250×250×29 250 29 137 107
L 250×250×30 250 30 141 111
L 250×250×31 250 31 145 114
L 250×250×32 250 32 150 118
L 250×250×33 250 33 154 121
L 250×250×34 250 34 158 124
L 250×250×35 250 35 163 128
L 300×300×27 300 27 154 121
L 300×300×28 300 28 159 125
L 300×300×29 300 29 165 129
L 300×300×30 300 30 170 133
L 300×300×31 300 31 175 138
L 300×300×32 300 32 181 142
L 300×300×33 300 33 186 146
L 300×300×34 300 34 191 150
L 300×300×35 300 35 197 154

EN 10025-2 S355JR Unequal Leg Steel Angles

Unequal-leg angles (5 verified sizes, L 200×100×10 to L 200×100×16)

Swipe horizontally to view all dimensions.

Designation Long leg h (mm) Short leg b (mm) t (mm) A (cm²) Mass (kg/m)
L 200×100×10 200 100 10 29.2 23
L 200×100×12 200 100 12 34.8 27.3
L 200×100×14 200 100 14 40.3 31.6
L 200×100×15 200 100 15 43 33.7
L 200×100×16 200 100 16 45.7 35.9

S355JR Chemical Composition for Angles (EN 10025-2 Ladle Analysis)

The figures below are ladle-analysis maxima for S355JR long products in EN 10025-2:2019. They should not be copied from S355J0 or S355J2, which use a 0.22% carbon maximum for nominal thickness greater than 30 mm, or from a plate table that uses different phosphorus defaults. They are limits, not typical heat results. For these angles the governing thickness is ordinarily the leg thickness, not the leg length.

Element Ladle analysis, max (mass %) Notes for S355JR long products, angles
C, t ≤ 16 mm 0.24 The same 0.24% maximum applies in all three carbon columns for S355JR. Do not copy the tighter 0.22% figure used for S355J0 or S355J2 at t > 30 mm.
C, 16 mm < t ≤ 40 mm 0.24 —
C, t > 40 mm 0.24 For nominal thickness greater than 100 mm, carbon is subject to agreement.
Si 0.55 By agreement, silicon may be set at 0.14–0.25% and phosphorus at ≤0.035% for hot-dip galvanizing category B.
Mn 1.60 —
P 0.040 See the galvanizing agreement above. Do not paste a flat-product default onto an angle order unless that is what was agreed.
S 0.040 —
N 0.012 The nitrogen maximum does not apply if total aluminium is at least 0.020%, or if sufficient other nitrogen-binding elements are present and reported.
Cu 0.55 —
Other added elements As reported If other elements are added, they shall be mentioned on the inspection document.

S355JR Carbon Equivalent for Angles

Carbon equivalent (CEV) maxima for S355JR long products follow the table below. The third band is 40 mm < t ≤ 140 mm. A CEV limit between 140 mm and 150 mm is not published here and must be agreed, not assumed. When EN 10025-2:2019 clause 7.2.5 is invoked on the order for S355, the CEV approach may be adjusted under that option; review the clause as written rather than inventing a substitute table. None of the tabulated legs in this set exceeds 40 mm, so they sit in the first CEV band; the later bands are shown because a thicker special section could be agreed.

Nominal thickness (mm) Maximum CEV (ladle analysis, %)
t ≤ 30 0.45
30 < t ≤ 40 0.47
40 < t ≤ 140 0.47

S355JR Angle Mechanical Properties: Yield, Tensile and +20 °C Impact

Tensile properties of S355JR long products follow EN 10025-2:2019, with elongation based on L0 = 5.65√S0. For these angles the nominal thickness is ordinarily the leg thickness t. L 200×200×16 remains in the 355 MPa band; L 200×200×20 and L 300×300×35 (t 35 mm) are in the 345 MPa band. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed; the 100–150 mm row is the published long-product band, not an invented extension. No mechanical limits beyond 150 mm are given here.

Nominal thickness t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A (%)
t ≤ 16 355 470–630 22
16 < t ≤ 40 345 470–630 22
40 < t ≤ 63 335 470–630 21
63 < t ≤ 80 325 470–630 20
80 < t ≤ 100 315 470–630 20
100 < t ≤ 150 295 450–600 18

The JR impact requirement is 27 J at +20 °C, longitudinal unless the order states otherwise. Sharing that test temperature with S235JR does not make the two grades interchangeable on yield, tensile strength, chemistry or carbon equivalent.

Delivery Conditions, Inspection and Identification

S355JR angles are commonly supplied in the as-rolled condition. The inspection document should show EN 10025-2 and its edition, the grade S355JR (1.0045), the EN 10056 designation, the EN 10056-2 edition used for tolerances, the delivery condition, the heat number, ladle analysis, the carbon equivalent, and the tensile and +20 °C impact results. If a galvanizing chemistry has been agreed, or if clause 7.2.5 has been invoked, that agreement belongs on the document as well. An S355JR H-section certificate, a channel certificate, or a plate certificate does not, by itself, identify an angle.

An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 6–15 m or 12 m.

Weldability and Surface Condition of S355JR Angles

S355JR is a weldable non-alloy structural steel when thickness, joint design and hydrogen control are taken into account. The CEV table above is the starting point; the certificate values and a procedure suited to the leg thickness are the practical controls. This page does not prescribe a procedure or a preheat chart.

The as-rolled surface is often specified to EN 10163-3:2004, class C, subclass 1, when that condition is named on the order. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.

EN 10056-2 Shape Tolerances and Theoretical Mass

Dimensional, shape and mass tolerances for these equal-leg and unequal-leg angles are those of EN 10056-2, not of EN 10025-2, not of EN 10279, and not of EN 10034. This article uses EN 10056-2:1993 as the known edition and does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.

A delivered L 200×200×16 will measure close to the tabulated legs and thickness within those tolerances, not as a set of exact advertised millimetres. Out-of-square and loose or tight included angle matter for connections. Settlement on theoretical or weighed mass should follow the contract.

Applications and Service Limits

S355JR steel angles are used where a 355 MPa non-alloy grade and an EN 10056 L-shape are specified:

  • Bracing, frames, trim, lintels and general fabrications whose specification names S355JR angle rather than S235JR or a non-European angle series.
  • Export packages that compare the grade with Q355B or with A572 Grade 50 plate, provided each line keeps its own material standard and shape system.

It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require S355J0, S355J2 or a defined lower-temperature quality. Durability comes from the coating or fire-protection system, not from the S355JR designation.

S355JR Angle Compared with S235JR, Q355B and A572 Grade 50

S355JR H-beams share the same material grade at the same yield class, but they are I or H sections, not L-shapes, and they use EN 10034 rather than EN 10056-2 for tolerances. Q355B H-beams and A572 Grade 50 plate are useful 345–355 MPa comparisons only if chemistry, toughness and the shape standard are also satisfied. S355JR plate is the same grade in plate form, not an angle. S235JR plate illustrates the lower-strength JR quality in this family; it is not an angle data sheet and it is not an S355JR certificate.

Dual certification requires every requirement of each named standard to be met on the delivered piece. An S355JR channel page, or an S235JR angle page, in this series will be linked here once it is published; those product URLs are not pre-linked.

Near-Equivalents: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to S355JR angle Caution
S235JR section EN 10025-2; dimensions EN 10056 or EN 10365 according to the shape A lower-strength grade in the same material family, with the same +20 °C JR impact quality. S235JR has its own chemistry, CEV and 235 MPa yield table. It is not an S355JR certificate. An H-section and an L-shape of a similar millimetre size are different products.
Q355B / A572 Grade 50 GB/T 1591 or ASTM A572/A572M; different shape standards Common 345–355 MPa comparisons in export enquiries. A Chinese or American angle follows GB/T 706 or ASTM A6/A6M, not the EN 10056 L designation. A shared 50 ksi or 355 MPa discussion is not a substitution method.
S355J0 / S355J2 angle EN 10025-2 The same 355 MPa class with a colder impact quality and tighter phosphorus and sulphur in the J2 quality. JR is 27 J at +20 °C. J0 is 27 J at 0 °C and J2 is 27 J at −20 °C. Those qualities are not implied by an S355JR certificate, and JR carbon at t > 30 mm is not the J0/J2 figure.

Sourcing S355JR Steel Angles from SHH STEEL

SHH STEEL supplies S355JR steel angles as an export trading house, coordinating mill production and project procurement. For this product the useful work is to keep equal and unequal designations from being mixed, to keep the size tables labelled as a verified subset rather than the complete EN 10056-1 series, to apply the yield band to the leg thickness rather than the leg length, and to align the EN 10056 designation, the material edition and the inspection document before a rolling programme is committed.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every tabulated L size in S355JR. Mid-range L 150 and L 200 rows are the usual core in this set; L 250, L 300 and the single tabulated L 80 and L 90 thicknesses are confirmed per line.

The same enquiry can also cover channels, I or H sections, or Chinese, Japanese or American designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

S355JR Steel Angle FAQs

Are the size tables the complete EN 10056-1:2017 series?
No. The tables are a verified subset: 71 equal-leg sizes (L 80, L 90, L 130, L 150, L 160, L 180, L 200, L 250 and L 300 in the thicknesses listed) and five unequal-leg sizes, all L 200×100. Smaller equal legs and a wider unequal series exist in EN 10056-1:2017 but are not invented here. They can be reviewed when named on the enquiry.
Does the 355 MPa yield apply to every S355JR angle in the tables?
No. 355 MPa is the minimum yield for nominal thickness up to 16 mm. For these angles the governing thickness is ordinarily the leg thickness, not the leg length. L 200×200×16 is in the 355 MPa band; L 200×200×20 is in the 345 MPa band.
Is an equal angle interchangeable with an unequal angle of the same long-leg length?
No. L 200×200×12 and L 200×100×12 share a 200 mm long leg but are different sections, with different short-leg width, area and mass. Nominate the full designation.
Which tolerance standard applies to these angles?
EN 10056-2, not EN 10279 and not EN 10034. This article uses EN 10056-2:1993 as the known edition; the edition named on the order governs.
Which standards should appear on the inspection document?
At least EN 10025-2 and its edition, the grade S355JR (1.0045), the EN 10056 designation, the EN 10056-2 edition used for tolerances, the delivery condition, ladle analysis, the carbon equivalent, tensile results by thickness, and the +20 °C impact result.

Request a Quotation for EN 10025-2 S355JR Steel Angle

EN 10025-2 S355JR steel angle is a non-alloy equal-leg or unequal-leg L-shape (1.0045) with 355 MPa minimum yield up to 16 mm. Nominate the designation to EN 10056-1, the tolerances to EN 10056-2, and the material to EN 10025-2:2019 (or the editions on the order). The tables are a verified subset of EN 10056-1:2017, used as reference dimensions, not a rolling list and not the complete series. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X