EN 10025-2 S235JR steel angle is a non-alloy equal-leg or unequal-leg L-shape (1.0038) with 235 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Dimensions follow EN 10056-1, with tolerances under EN 10056-2. The ordered edition governs. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.
Keywords
EN 10025-2 S235JR Steel Angle, S235JR equal angle, S235JR unequal angle, EN 10056 L-shape, 1.0038 structural angle
Equivalent Grades:
Near-equivalents only, not automatic substitutes: S355JR is a higher-strength grade, not the same section; Q235B; A36; SS400; S235J0 and S235J2 have colder impact qualities.
Share:
General Description
Material Specification
Available Sizes of EN 10025-2 S235JR Equal Leg Steel Angles
Available Sizes of EN 10025-2 S235JR Unequal Leg Steel Angles
Chemical Composition
Carbon equivalent
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source S235JR Steel Angles from SHH STEEL
FAQ
Conclusion

What is EN 10025-2 S235JR Steel Angle?

EN 10025-2 S235JR steel angle is a hot-rolled equal-leg or unequal-leg L-shape in non-alloy structural steel S235JR (steel number 1.0038). The material standard is EN 10025-2. Nominal dimensions and theoretical masses for these angles are those of EN 10056-1. Shape, dimensional and mass tolerances are those of EN 10056-2. S marks a structural steel, 235 is the minimum yield strength in MPa up to 16 mm, and JR is the impact quality, 27 J at +20 °C. This page is for the angle, not for a UPN, an I or H section, or a plate.

Equal angles have both legs the same length, for example L 150×150×12 or L 200×200×16. Unequal angles have a longer and a shorter leg, for example L 200×100×12. The third number is the thickness of both legs. An L 200×100 is not an L 200×200, and it is not an ASTM L 8×4 or a Chinese unequal angle of a similar millimetre size. The designation is the EN 10056 L-shape, not a bar of the same thickness cut from plate.

These angles are filed under EN 10025-2 steel angle profiles in the steel angle profiles category of steel structural profiles. The same grade in plate form is listed separately as EN 10025-2 S235JR steel plate. Do not use that plate page as an angle data sheet, and do not copy plate chemistry defaults onto an L-shape certificate.

S235JR angles are used for bracing, frames, lintels, clips and general industrial work when the specification names this non-alloy grade in a European L-shape. The grade is not a pressure-vessel or nuclear safety material, and it is not a substitute for S355JR when a 355 MPa yield is what the order requires.

This page covers Equal and Unequal Steel Angles in EN 10025-2 S235JR. The Equal Leg Steel Angles and Unequal Leg Steel Angles follow EN 10056-1; the material standard does not by itself define the dimensions.

Material, Dimensions and Tolerances for S235JR Angles

The order and the inspection certificate should keep material, dimensions and tolerances distinct:

  • EN 10025-2 is the material standard. This article uses ladle chemistry, carbon-equivalent and tensile values for S235JR long products from EN 10025-2:2019. The edition named on the order governs acceptance.
  • EN 10056-1 is the dimensional standard for hot-rolled equal-leg and unequal-leg angles. The size tables below are reference dimensions and theoretical masses from the EN 10056-1:2017 series, limited to the sizes in the verified table set used for this article. They are not a mill rolling list and they are not presented as the complete EN 10056-1:2017 series. The edition of EN 10056-1 named on the order governs dimensional acceptance.
  • EN 10056-2 is the tolerance standard for these angles. This article uses EN 10056-2:1993, which is the current edition. The edition named on the order governs dimensional and mass tolerance acceptance.

A documented special combination — for example S235JR on an ASTM L-shape, or an EN 10056 angle certified to a different material standard — is only valid if every requirement of each named standard is met. Matching a nominal 200 mm or 8 in leg is not a substitution.

EN 10025-2 S235JR Equal Leg Steel Angles

The tables list designation, leg length, thickness, theoretical area and theoretical mass for the equal-leg and unequal-leg sizes in the verified EN 10056-1:2017 set used for this article. Use them to identify and estimate, not as a rolling programme for S235JR, and not as a claim that every EN 10056-1 size is shown here.

EN 10056-1:2017 also covers smaller equal legs and a wider unequal-leg series than the rows below. Those sizes can be reviewed when they are named on the enquiry. This page does not invent dimensions for sizes that were not in the verified table set. Mid-range tabulated rows such as L 150 and L 200 are the usual enquiry core in this set; L 250 and L 300, and the single tabulated L 80 and L 90 thicknesses, should be confirmed size by size.

L 200×200×16 is a 200 mm equal angle, 16 mm thick, at the boundary of the first yield band. L 200×200×20 is 20 mm thick, so the minimum yield is 225 MPa, not 235 MPa. L 200×100×12 is an unequal 200 mm by 100 mm angle, 12 mm thick; it is not L 200×200×12. L 300×300×35, the heaviest tabulated equal angle here, has a 35 mm leg and remains in the 16–40 mm yield band.

Equal-leg angles (71 verified sizes, L 80×80×8 to L 300×300×35)

L 80 to L 150 equal (15 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 80×80×8 80 8 12.3 9.63
L 90×90×6 90 6 10.6 8.3
L 130×130×10 130 10 25.2 19.8
L 130×130×11 130 11 27.6 21.7
L 130×130×12 130 12 30 23.6
L 130×130×13 130 13 32.3 25.4
L 130×130×14 130 14 34.7 27.2
L 150×150×10 150 10 29.3 23
L 150×150×12 150 12 34.8 27.3
L 150×150×13 150 13 37.6 29.5
L 150×150×14 150 14 40.3 31.6
L 150×150×15 150 15 43 33.8
L 150×150×16 150 16 45.7 35.9
L 150×150×18 150 18 51 40.1
L 150×150×20 150 20 56.3 44.2

L 160 to L 200 equal (28 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 160×160×14 160 14 43.2 33.9
L 160×160×15 160 15 46.1 36.2
L 160×160×16 160 16 49 38.4
L 160×160×17 160 17 51.8 40.7
L 160×160×18 160 18 54.7 42.9
L 160×160×19 160 19 57.5 45.1
L 160×160×20 160 20 60.3 47.3
L 180×180×13 180 13 45.5 35.7
L 180×180×14 180 14 48.8 38.3
L 180×180×15 180 15 52.1 40.9
L 180×180×16 180 16 55.4 43.5
L 180×180×17 180 17 58.7 46
L 180×180×18 180 18 61.9 48.6
L 180×180×19 180 19 65.1 51.1
L 180×180×20 180 20 68.3 53.7
L 180×180×22 180 22 74.9 58.6
L 200×200×15 200 15 58.1 45.6
L 200×200×16 200 16 61.8 48.5
L 200×200×17 200 17 65.5 51.4
L 200×200×18 200 18 69.1 54.2
L 200×200×19 200 19 72.7 57.1
L 200×200×20 200 20 76.3 59.9
L 200×200×21 200 21 79.9 62.8
L 200×200×22 200 22 83.5 65.6
L 200×200×23 200 23 87.1 68.3
L 200×200×24 200 24 90.6 71.1
L 200×200×25 200 25 94.1 73.9
L 200×200×26 200 26 97.6 76.6

L 250 to L 300 equal (28 sizes)

Swipe horizontally to view all dimensions.

Designation Leg h = b (mm) t (mm) A (cm²) Mass (kg/m)
L 250×250×17 250 17 82.1 64.4
L 250×250×18 250 18 86.7 68.1
L 250×250×19 250 19 91.4 71.7
L 250×250×20 250 20 96 75.3
L 250×250×21 250 21 101 78.9
L 250×250×22 250 22 105 82.5
L 250×250×23 250 23 110 86.1
L 250×250×24 250 24 114 89.7
L 250×250×25 250 25 119 93.2
L 250×250×26 250 26 123 96.7
L 250×250×27 250 27 128 101
L 250×250×28 250 28 133 104
L 250×250×29 250 29 137 107
L 250×250×30 250 30 141 111
L 250×250×31 250 31 145 114
L 250×250×32 250 32 150 118
L 250×250×33 250 33 154 121
L 250×250×34 250 34 158 124
L 250×250×35 250 35 163 128
L 300×300×27 300 27 154 121
L 300×300×28 300 28 159 125
L 300×300×29 300 29 165 129
L 300×300×30 300 30 170 133
L 300×300×31 300 31 175 138
L 300×300×32 300 32 181 142
L 300×300×33 300 33 186 146
L 300×300×34 300 34 191 150
L 300×300×35 300 35 197 154

EN 10025-2 S235JR Unequal Leg Steel Angles

Unequal-leg angles (5 verified sizes, L 200×100×10 to L 200×100×16)

Swipe horizontally to view all dimensions.

Designation Long leg h (mm) Short leg b (mm) t (mm) A (cm²) Mass (kg/m)
L 200×100×10 200 100 10 29.2 23
L 200×100×12 200 100 12 34.8 27.3
L 200×100×14 200 100 14 40.3 31.6
L 200×100×15 200 100 15 43 33.7
L 200×100×16 200 100 16 45.7 35.9

American L-shapes, and Chinese or Japanese angle designations, belong to their own dimensional standards, not to these EN 10056 rows.

S235JR Chemical Composition for Angles (EN 10025-2 Ladle Analysis)

The figures below are ladle-analysis maxima for S235JR long products in EN 10025-2:2019. They are limits, not typical heat results. Do not mix them with unofficial tables that borrow plate phosphorus figures or that give S235JR a silicon maximum it does not generally have. For these angles, apply the carbon band that matches the governing nominal thickness, ordinarily the leg thickness, not the length of the leg.

Element Ladle analysis, max (mass %) Notes for S235JR long products, angles
C, t ≤ 16 mm 0.17 —
C, 16 mm < t ≤ 40 mm 0.17 —
C, t > 40 mm 0.20 For nominal thickness greater than 100 mm, carbon is subject to agreement.
Si No general maximum A dash in the source table. By agreement, silicon may be set at 0.14–0.25% and phosphorus at ≤0.035% for hot-dip galvanizing category B.
Mn 1.40 —
P 0.040 See the galvanizing agreement above. Do not paste a flat-product 0.035% default onto an angle order unless that is what was agreed.
S 0.040 —
N 0.012 The nitrogen maximum does not apply if total aluminium is at least 0.020%, or if sufficient other nitrogen-binding elements are present and reported.
Cu 0.55 —
Other added elements As reported If other elements are added, they shall be mentioned on the inspection document.

S235JR Carbon Equivalent for Angles

The carbon equivalent is calculated from the ladle analysis by CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Cu + Ni)/15. The EN 10025-2:2019 maxima for S235JR long products are:

Nominal thickness (mm) Maximum CEV (ladle analysis, %)
t ≤ 30 0.35
30 < t ≤ 40 0.35
40 < t ≤ 140 0.38

The third band applies to nominal thicknesses greater than 40 mm and not more than 140 mm. For thicknesses above 140 mm, a carbon-equivalent limit is not tabulated here and must be agreed and verified on the order; no value is invented for that range. Every tabulated leg in the size tables above is 35 mm or thinner, so those rows sit in the first band (0.35%). Clause 7.2.5 of EN 10025-2:2019 addresses special conditions for S275 and S355; those conditions are not applied to S235JR on this page.

S235JR Angle Mechanical Properties: Yield, Tensile and +20 °C Impact

Tensile properties of S235JR are thickness-dependent. The values below are from EN 10025-2:2019 for long products, with elongation based on L0 = 5.65√S0. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed and verified on the order; the 100–150 mm row is the published long-product band and is not an invented extension. No mechanical limits beyond 150 mm are invented here.

Nominal thickness t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A (%)
t ≤ 16 235 360–510 26
16 < t ≤ 40 225 360–510 26
40 < t ≤ 63 215 360–510 25
63 < t ≤ 80 215 360–510 24
80 < t ≤ 100 215 360–510 24
100 < t ≤ 150 195 350–500 22

Apply the band that matches the governing nominal thickness, ordinarily the leg thickness of the angle, not the 150 mm or 200 mm leg length. L 150×150×10 (t = 10 mm) is in the 235 MPa band. L 200×200×20 and L 300×300×35 (t = 20 mm and 35 mm) are in the 225 MPa band, not the 235 MPa band.

Quality JR requires a Charpy V-notch absorbed energy of 27 J at +20 °C. For long products the test is normally longitudinal unless the order specifies otherwise. If the project needs 27 J at 0 °C or at −20 °C, the grade to nominate is S235J0 or S235J2, not S235JR.

Delivery Conditions, Inspection and Identification

S235JR angles are commonly supplied in the as-rolled condition. The inspection document should show EN 10025-2 and its edition, the grade S235JR (1.0038), the EN 10056-1 L designation, the EN 10056-2 edition used for tolerances, the delivery condition, the heat number, ladle analysis, the carbon equivalent, and the tensile and +20 °C impact results. If a galvanizing chemistry has been agreed, that agreement belongs on the document as well. An S235JR H-section or channel certificate, or a plate certificate, does not, by itself, identify an L-shape.

An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 6–15 m or 12 m.

Weldability and Surface Condition of S235JR Angles

S235JR is a weldable non-alloy structural steel when thickness, joint design and hydrogen control are taken into account. The CEV table above is the starting point; the certificate values and a procedure suited to the leg thickness are the practical controls. This page does not prescribe a procedure or a preheat chart. Fillet welds along both legs, and connections at the heel of an unequal angle, need the detailing that the design actually requires.

The as-rolled surface is often specified to EN 10163-3:2004, class C, subclass 1, when that condition is named on the order. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.

EN 10056-2 Shape Tolerances and Theoretical Mass

Dimensional, shape and mass tolerances for these L-shapes are those of EN 10056-2, not of EN 10025-2 and not of EN 10056-1 itself. This article uses EN 10056-2:1993 as the current edition and does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.

A delivered L 150×150×12 will measure close to the tabulated legs and thickness within those tolerances, not as a set of exact advertised millimetres. Out-of-square at the heel and variation of the two legs matter for connections. Settlement on theoretical or weighed mass should follow the contract.

Applications and Service Limits

S235JR steel angles are used where a 235 MPa non-alloy grade and an equal or unequal L-shape are specified:

  • Bracing, frames, lintels, clips, ledgers and general fabrications whose specification names S235JR angle rather than S355JR or a non-European angle series.
  • Export packages that compare the grade with Q235B or with A36, provided each line keeps its own material standard and shape system.

It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require S235J0, S235J2 or S355JR. Durability comes from the coating or fire-protection system, not from the S235JR designation.

S235JR Angle Compared with S355JR, Q235B and A36

S355JR H-beams share the same material standard family at a higher yield, but they are I or H sections, not L-shapes, and they use EN 10365 and EN 10034 rather than EN 10056. Q235B and A36 are useful lower-strength comparisons only if chemistry, toughness and the shape standard are also satisfied. S235JR plate is the same grade in plate form, not an angle.

Dual certification requires every requirement of each named standard to be met on the delivered piece. An S235JR H-beam or channel page in this series will be linked here once it is published; those product URLs are not pre-linked.

Near-Equivalents: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to S235JR angle Caution
S355JR section EN 10025-2; dimensions EN 10056 or EN 10365 according to the shape A higher-strength grade in the same material family. S355JR has its own chemistry, CEV and 355 MPa yield table. It is not an S235JR certificate. An H-section and an L-shape of a similar millimetre size are different products.
Q235B / A36 / SS400 GB/T 700 or ASTM A36/A36M or JIS G 3101; different shape standards Common lower-strength comparisons in export enquiries. A Chinese, American or Japanese angle follows GB/T 706, ASTM A6/A6M or JIS G 3192, not the EN 10056 L designation. A shared 235 MPa or 36 ksi discussion is not a substitution method.
S235J0 / S235J2 angle EN 10025-2 The same 235 MPa class with a colder impact quality. JR is 27 J at +20 °C. J0 is 27 J at 0 °C and J2 is 27 J at −20 °C. Those qualities are not implied by an S235JR certificate.

Sourcing S235JR Steel Angles from SHH STEEL

SHH STEEL supplies S235JR steel angles as an export trading house, coordinating mill production and project procurement. For this product the useful work is to keep equal and unequal designations from being mixed, to apply the yield band to the leg thickness rather than the leg length, to be clear when a requested size is outside the verified EN 10056-1 table set used here, and to align the EN 10056 designation, the material edition and the inspection document before a rolling programme is committed.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every equal or unequal L size in S235JR. Mid-range tabulated L 150 and L 200 sizes are the usual core; L 250 and L 300, and sizes outside the tables below, are confirmed per line.

The same enquiry can also cover channels, I or H sections, or Chinese, Japanese or American designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

S235JR Steel Angle FAQs

Are the size tables the complete EN 10056-1:2017 series?
No. The tables are the equal-leg and unequal-leg sizes in the verified EN 10056-1:2017 set used for this article: 71 equal rows from L 80×80×8 to L 300×300×35, and five unequal rows in L 200×100. Smaller equal legs and a wider unequal-leg series exist in EN 10056-1:2017 and can be reviewed when they are named; this page does not invent those dimensions.
Does the 235 MPa yield apply to every S235JR angle in the tables?
No. 235 MPa is the minimum yield for nominal thickness up to 16 mm. For these angles the governing thickness is ordinarily the leg thickness, not the leg length. L 150×150×10 is in the 235 MPa band; L 200×200×20 and L 300×300×35 are in the 225 MPa band.
Is an equal angle interchangeable with an unequal angle of the same long-leg length?
No. L 200×200 and L 200×100 are different sections. The short-leg length, the mass and the connection details are those of the designation that the specification actually names.
Which tolerance standard applies to these angles?
EN 10056-2, not EN 10056-1 itself and not EN 10034 or EN 10279. This article uses EN 10056-2:1993 as the current edition; the edition named on the order governs.
Which standards should appear on the inspection document?
At least EN 10025-2 and its edition, the grade S235JR (1.0038), the L designation to EN 10056-1, the EN 10056-2 edition used for tolerances, the delivery condition, ladle analysis, the carbon equivalent, tensile results by thickness, and the +20 °C impact result.

Request a Quotation for EN 10025-2 S235JR Steel Angle

EN 10025-2 S235JR steel angle is a non-alloy L-shape (1.0038) with 235 MPa minimum yield up to 16 mm. Nominate the equal or unequal L size to EN 10056-1, the tolerances to EN 10056-2, and the material to EN 10025-2:2019 (or the editions on the order). The tables are a verified EN 10056-1:2017 size set, not the complete series and not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X