DNV FH36 Steel Plate | NV F36 Marine Steel Plate
What is DNV FH36 / NV F36 marine steel plate?
DNV FH36, officially stamped NV F36 on mill-approved plate, is a higher-strength hull structural steel under DNV rules for classification – Ships, which implement IACS UR W11 for the AH–FH 32/36/40 family. Strength level 36 means minimum yield 355 N/mm², tensile 490–630 N/mm² and elongation 21 % min. (A5). The letter FH fixes Charpy V-notch testing at −60 °C. In commercial enquiries it is called DNV FH36 or NV F36 marine steel plate.
Equivalent grades: DNV NV F36 ≈ ASTM A131 Grade FH36 ≈ ABS FH36 ≈ LR FH36 ≈ BV FH36 ≈ CCS F36 / FH36 ≈ NK KF36 ≈ KR RF36 ≈ RINA FH36 ≈ GB 712 Grade FH36 (all class-approved, stamped by the issuing society).
NV F36 is selected when scantlings need the higher yield of the 36 band and the material class assigns −60 °C toughness. Ordinary-strength NV A–E stay at 235 N/mm² yield and cannot replace FH36 without a drawing change. Within the 36 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C; within the FH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².
Plates that pass mill tests under DNV survey are die-stamped or stencilled NV F36 (plus Z or U where through-thickness or ultrasonic requirements apply) and are supplied with a mill certificate the DNV Surveyor endorses. SHH STEEL supplies NV F36 from Chinese mills that hold DNV works approval for the grade, from stock in common sizes or from a mill rolling cycle, with DNV survey arranged at the mill.
DNV NV F36 plate: specification summary
| Item | DNV NV F36 / FH36 data |
|---|---|
| Rule basis | DNV rules for classification – Ships; IACS UR W11 higher-strength Grade FH36 |
| Strength level | higher strength 36, yield 355 N/mm² min., tensile 490–630 N/mm² |
| Toughness class | FH → Charpy at −60 °C |
| Plate thickness primarily covered | up to 100 mm under IACS UR W11 scope for plates; greater thickness by special consideration (see UNCERTAIN) |
| Deoxidation | killed, fine grain practice (UR W11) |
| Impact test | Charpy V at −60 °C; frequency and supply condition per UR W11 tables |
| Marking | NV F36 (commercial “FH36”); plus Z / U / TM where ordered and qualified |
| TMCP Ceq (indicative UR W11 / industry practice) | ≤ 0.38 % for t ≤ 50 mm; ≤ 0.40 % for 50 < t ≤ 100 mm (TM steels) — confirm on mill approval / PO |
| Thickness tolerance | IACS UR W13 as adopted by DNV (minus tolerance commonly 0.3 mm class — confirm on PO; see UNCERTAIN) |
| Certificate | mill certificate endorsed by the DNV Surveyor; EN 10204 3.1 / 3.2 on request |
Size range. Common market thicknesses for FH36 are about 6–80 mm (heavier plates available as per mill approval), widths 1500–3500 mm. Exact maximum thickness for a given delivery condition is as per standard and mill certificate / DNV works approval. Ask for confirmation above 100 mm.
DNV FH36 / NV F36 chemical composition (heat and product analysis)
| Element | Heat (ladle) analysis, % | Product (check) analysis, % | Note |
|---|---|---|---|
| C | 0.16 max. | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | FH group |
| Mn | 0.90–1.60 | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | |
| Si | 0.10–0.50 | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | min. waived if acid-soluble Al ≥ 0.015 % |
| P | 0.025 max. | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | tighter for FH |
| S | 0.025 max. | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | tighter for FH |
| Al (acid soluble) min. | 0.015 min. acid-soluble | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | grain refining |
| Nb | 0.02–0.05 when used singly | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | when used singly; combined minima in UR W11 |
| V | 0.05–0.10 when used singly | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | when used singly |
| Ti | 0.02 max. | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | need not be reported unless intentionally added |
| Cu | 0.35 max. | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | |
| Cr | 0.20 max. | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | |
| Ni | 0.80 max. | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | FH allows higher Ni than AH/DH/EH |
| Mo | 0.08 max. | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | |
| N | 0.009 max. (0.012 if Al present) | numeric tolerance not tabulated in DNV rules – agree on order / mill certificate | FH specifies N max. |
Product (check) analysis column: DNV rules specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.
Source: IACS UR W11 higher-strength chemistry tables (ladle samples) — the chemistry DNV applies to NV F36. AH/DH/EH share one chemistry column; FH is tighter on C, P, S and adds N control with higher Ni allowance. Toughness is differentiated by impact temperature and supply routes, not by separate C/Mn caps within AH/DH/EH. Product (check) analysis numeric tolerances are not tabulated in UR W11; when required, agree tolerances at enquiry. TMCP steels must also meet the applicable Ceq / Pcm limits on the mill approval — ask for Ceq on the certificate.
DNV NV F36 tensile properties
| Property | Requirement (IACS UR W11) |
|---|---|
| Tensile strength Rm | 490–630 N/mm² |
| Yield strength ReH | 355 N/mm² min. |
| Elongation A5 | 21 % min. |
| Impact test temperature | −60 °C |
Alternative flat-specimen elongations by thickness (indicative UR W11 / industry table for strength 36):
| Thickness (mm) | ≤5 | >5–10 | >10–15 | >15–20 | >20–25 | >25–30 | >30–40 | >40–50 |
|---|---|---|---|---|---|---|---|---|
| Elongation min. % | 13 | 15 | 16 | 17 | 18 | 19 | 20 | 21 |
Same tensile band applies to AH/DH/EH/FH 36; only impact temperature and chemistry group (FH vs AH/DH/EH) change across the letter.
DNV NV F36: Charpy at −60 °C and supply condition
| Thickness | Long. avg. at −60 °C | Trans. avg. at −60 °C |
|---|---|---|
| t ≤ 50 mm | 34 J | 24 J |
| 50 < t ≤ 70 mm | 41 J | 27 J |
| 70 < t ≤ 100 mm | 50 J | 34 J |
Source: IACS UR W11 impact table for higher-strength Grade FH36 (full-size; either direction acceptable unless specified). Energies rise with thickness — a 60 mm plate must meet higher values than a 20 mm plate at the same −60 °C. Condition of supply and impact lot size depend on grain-refining practice and thickness (AR/CR/N/TM/QT as permitted). For TMCP FH36, respect Ceq caps ≈ 0.38 % (t≤50) / 0.40 % (50
Thickness tolerance and surface condition
DNV applies IACS UR W13 thickness tolerances unless the PO states otherwise (often 0.3 mm minus class — confirm on PO; see UNCERTAIN). Plus/flatness/width/length per agreed standard (ASTM A6 or EN 10029). Surface quality per EN 10163 or equivalent accepted by DNV; state primer/surface class on receipt if needed.
DNV NV F36 plate stock in China
| Thickness (mm) | Width (mm) | Length (mm) | Condition | Approx. quantity | Location |
|---|---|---|---|---|---|
| 6 | 1800 / 2000 | 6000 / 8000 | AR / CR / N / TM | 100+ t | China |
| 8 | 1800 / 2000 | 8000 / 12000 | AR / CR / N / TM | 200+ t | China |
| 10 | 2000 / 2200 | 8000 / 12000 | AR / CR / N / TM | 200+ t | China |
| 12 | 2000 / 2200 / 2500 | 12000 | AR / CR / N / TM | 200+ t | China |
| 14 | 2000 / 2200 | 12000 | AR / CR / N / TM | 100+ t | China |
| 16 | 2000 / 2500 | 12000 | AR / CR / N / TM | 200+ t | China |
| 20 | 2000 / 2500 | 12000 | AR / CR / N / TM | 100+ t | China |
| 25 | 2200 / 2500 | 12000 | AR / CR / N / TM | 100+ t | China |
| 30 | 2200 | 10000 / 12000 | AR / CR / N / TM | 100+ t | China |
| 40 | 2200 | 10000 | AR / CR / N / TM | 50+ t | China |
| 50 | 2200 | 8000 / 10000 | AR / CR / N / TM | 50+ t | China |
Quantities are approximate and change daily (indicative — confirm before booking); all stock plates carry NV F36 marking and DNV-endorsed mill certificates when sold as DNV class plate. Sizes outside the table (for example 3000 mm width, 60–100 mm thickness, or fixed lengths for a cutting plan) are produced in the next mill rolling cycle, typically 3–6 weeks including DNV survey. Send your size list and we will reply with what is in stock and what must be rolled.
Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and DNV stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.
DNV NV F36 equivalents in other rules and standards
| Standard / society | Designation | Comment |
|---|---|---|
| DNV | NV F36 (DNV FH36) | this page; stamped under DNV survey |
| ASTM A131/A131M | ASTM A131/A131M Grade FH36 | A131 lists AH–FH 32/36/40; product standard only |
| ABS | ABS FH36 | IACS UR W11 higher-strength |
| LR | LR Grade FH36 | IACS UR W11 |
| BV | BV Grade FH36 | IACS UR W11 |
| CCS | CCS FH36 | IACS UR W11 |
| NK (ClassNK) | NK KF36 | ClassNK KF36 |
| KR | KR RF36 | KR RF36 |
| RINA | RINA Grade FH36 | confirm exact designation per RINA rules |
| GB 712 | GB 712 Grade FH36 | not class approval by itself |
| Structural (indicative) | EN 10025-2 S355JR / S355J2 | land structural; no class marking |
These are comparisons, not substitutions. Multi-class stamps require joint survey before rolling.
DNV NV F36 vs other DNV hull grades
Pick FH36 when the drawing specifies higher-strength grade FH36 (or the society equivalent). Do not substitute ordinary Grade A/B unless the designer recalculates scantlings — yield differs (355 vs 235). Within the 36 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Within the FH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².
For yields above 390 N/mm² DNV / IACS move to extra-high strength (UR W16 naming AH420… / NV A420…).
When DNV NV F36 is the right choice: typical uses are low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified. The Charpy temperature (−60 °C) is fixed by the letter, and the strength by the number (ReH 355 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing.
Applications, cutting and welding of DNV NV F36
Typical uses: low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified; weight-saving vs ordinary-strength plate in large tankers, bulkers and container ships. See offshore platform steel plates when primary offshore grades apply.
Welding: higher-strength hull steels need approved higher-strength consumables matched to −60 °C weld-metal toughness; preheat and heat input follow the approved WPS and often track Ceq/Pcm from the mill certificate. TMCP FH36 must respect the Ceq caps noted above. Cutting by oxy-fuel/plasma/laser is routine; thick FH plate may need hydrogen control — follow mill recommendations.
Processing notes for NV F36: cold forming is routine within normal shipyard radii. Line heating and fairing of TMCP plate should stay within the temperature limits recommended by the mill, because overheating can reduce the strength gained in controlled rolling. Check the delivery condition on the certificate before planning hot forming.
Certificates, DNV survey and third-party inspection
Every plate is tested and marked at the mill under DNV survey; the mill certificate lists heat number, ladle chemistry, Ceq where applicable, tensile results (ReH ≥ 355 N/mm², Rm 490–630 N/mm², A ≥ 21 %), Charpy at −60 °C, delivery condition and plate numbers, endorsed by the Surveyor. Optional EN 10204 3.2, UT (U), Z-direction, multi-class.
On receipt: verify NV F36 stamp, −60 °C impact data, energies for the delivered thickness band, thickness within UR W13 / PO tolerance, DNV endorsement present.
Charpy acceptance for NV F36 by thickness (IACS UR W11; actual results as per standard and mill certificate):
| Thickness t (mm) | Test temperature | Average energy, longitudinal (J min.) | Average energy, transverse (J min.) |
|---|---|---|---|
| t ≤ 50 | −60 °C | 34 | 24 |
| 50 < t ≤ 70 | −60 °C | 41 | 27 |
| 70 < t ≤ 100 | −60 °C | 50 | 34 |
If UT or 3.2 was ordered, check the UT report and inspector’s plate list as well.
Common mistakes when ordering DNV FH36 / NV F36
- Ordering “DNV 36” without the letter (FH/…) — toughness class missing
- Accepting ordinary-strength Grade A/B certificates for a FH36 PO
- Ignoring TMCP Ceq caps on TM plate
- FH chemistry (tighter P/S, N) not checked when the PO says FH
- Coil-cut plate without coil approval
- Missing DNV endorsement on the MTC
Write grade, delivery condition, impact temperature and certificate type into the PO.
Sourcing DNV NV F36: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Fake class plate | DNV-approved mills only; traceable NV F36 stamp + certificate; 3.2 on request |
| Payment risk | T/T or L/C; inspection before balance |
| Mixed sizes / grades | FH36 combined with NV A/B/D/E or other AH–FH sizes in one container |
| Lead time visibility | weekly photo updates from dedicated coordinator |
| Prep before ship | cutting, bevelling, drilling, machining in our workshop |
How to order DNV NV F36 plate
Specify DNV FH36 (NV F36), delivery condition (AR/CR/N/TM/QT as applicable), thickness × width × length × qty, Z/U, multi-class, certificate type, port. Send to SHH STEEL.
Sample PO line: “Steel plate to DNV rules for classification – Ships, Grade FH36 (NV F36), delivery condition [AR/CR/N/TM/QT], 20 × 2500 × 12000 mm, 30 pcs, marked NV F36, certificate endorsed by DNV Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].”
FAQ
Conclusion
DNV FH36 / NV F36 is higher-strength hull steel under DNV rules and IACS UR W11: yield 355 N/mm², tensile 490–630 N/mm², Charpy at −60 °C, marking NV F36. Lock on the order: delivery condition, impact lot size, TMCP Ceq if TM, product analysis if needed, multi-class and 3.2.
SHH STEEL supplies NV F36 plate rolled by Chinese mills that hold DNV works approval for the grade, so every plate carries the NV F36 stamp and a Surveyor-endorsed certificate traceable to its heat. Common thicknesses are available from stock; other sizes are scheduled into the mill rolling cycle with DNV survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, BV or another agency) and joint certification with ABS, LR, BV, CCS, NK, KR or RINA.
We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or NV F36 mixed with NV A/B/D/E or other AH–FH sizes, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.
Request a quotation: send SHH STEEL the grade (NV F36 / DNV FH36), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.