ASTM A871 Grade 65 Steel Plate | ASTM A871/A871M Weathering Steel - SHH STEEL

ASTM A871 Grade 65 Steel Plate | A871/A871M Weathering Plate

ASTM A871 Grade 65 is a high-strength low-alloy structural steel plate under ASTM A871/A871M with atmospheric corrosion resistance intended for tubular structures, poles and other suitable applications. Minimum yield is ≥65 ksi [≥450 MPa] with tensile ≥80 ksi [≥550 MPa]. Plate may be furnished as-rolled, normalized or quenched and tempered as required to meet the mechanical package. Guide G101 corrosion-resistance index must be at least 6.0. SHH STEEL supplies A871 Grade 65 plate with EN 10204 3.1 (or 3.2) mill test certificates.
Equivalent Grades:
Approximate talk: ASTM A588 / A709 50W family for weathering role; EN 10025-5 S355J0W / S355J2W / S355K2W; commercial Corten B; GB/T 4171 Q355NH. A871 is a higher-strength pole/tubular plate track (Grade 60 / 65), not an automatic A588 substitute. Confirm against project specs.
Heat Treatment
As-rolled, normalized, or quenched and tempered as required to meet specified mechanical properties. Fine-grain practice.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Atmospheric exposure guidance
Equivalent Material Grade
A871 Grade 65 vs sibling / A588
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A871 Grade 65 steel plate?

ASTM A871/A871M Grade 65 covers HSLA plate for tubular structures and poles (or other suitable applications) with atmospheric corrosion resistance substantially better than carbon structural steels with or without copper addition. When properly exposed to the atmosphere, this steel can be used bare (unpainted) for many applications. Atmospheric corrosion resistance: Guide G101 corrosion-resistance index ≥ 6.0.

Two strength grades are defined: Grade 60 and Grade 65. Chemistry may follow Type I, Type II or Type IV heat-analysis packages. Delivery condition is selected so the ordered mechanical properties are met: as-rolled, normalized or quenched and tempered.

SHH STEEL is a China mill-direct source for A871 weathering plate, with EN 10204 3.1 (or 3.2) mill test certificates and optional third-party inspection. Category hubs: ASTM A871/A871M · Weathering Steel Plates. (Note: the A871 hub may need creating at publish time.)

Sibling grade: ASTM A871 Grade 60. Related weathering pages: ASTM A588 Grade A · ASTM A709 Grade 50W · EN 10025-5 S355J2W · Corten B · GB/T 4171 Q355NH · ASTM A242 Type 1 · JIS G3125 SPA-H.

Material Specification for ASTM A871 Grade 65

Parameter Specification
Standard ASTM A871/A871M (Primary reference ASTM A871/A871M-20; confirm ordered edition on the MTC)
Grade Grade 65
Chemistry type Type I / Type II / Type IV (as ordered)
Family HSLA plate with atmospheric corrosion resistance (poles / tubular structures)
Product form Plate (hot-rolled; coil-to-plate when agreed and fully tested)
Thickness window Typical published tensile window about 0.138-2.00 in [3.5-50.8 mm]; thicker plate by mill inquiry. Confirm ordered thickness on the PO and MTC.
SHH supply focus About 6-50 mm plate (confirm availability for thinner / thicker)
Width / length Width about 1500-3000 mm; length cut-to-size on request
Delivery condition As-rolled, normalized, or quenched and tempered as required to meet the specified mechanical properties. Fine-grain practice.
Corrosion evidence Atmospheric corrosion resistance: Guide G101 corrosion-resistance index ≥ 6.0.
Surface As-rolled or shot blasted
Edge Mill edge or cut edge
Dimensional standard ASTM A6/A6M
Certification EN 10204 3.1 / 3.2
Density 7.85 g/cm³

Chemical Composition of ASTM A871 Grade 65 (Types I / II / IV)

Heat (ladle) analysis limits below follow common ASTM A871/A871M Type I / Type II / Type IV packages used for Grade 60 and Grade 65. Always verify the mill test certificate and ordered type before fabrication or substitution. Atmospheric corrosion resistance: Guide G101 corrosion-resistance index ≥ 6.0.

Element Type I Type II Type IV
C ≤0.19 ≤0.20 ≤0.17
Mn 0.80-1.35 0.75-1.35 0.50-1.20
P ≤0.030 ≤0.030 ≤0.030
S ≤0.030 ≤0.030 ≤0.030
Si 0.30-0.65 0.15-0.50 0.25-0.50
Ni ≤0.40 ≤0.50 ≤0.40
Cr 0.40-0.70 0.40-0.70 0.40-0.70
Cu 0.25-0.40 0.20-0.40 0.30-0.50
V 0.02-0.10 0.01-0.10 –
Mo – – ≤0.10
Nb (Cb) – – 0.005-0.05

Type I / II use vanadium micro-alloying; Type IV uses columbium (niobium) with optional molybdenum. Do not mix type chemistries on one heat without mill agreement. Product-analysis tolerances follow ASTM A6 practice as applicable.

Mechanical Properties of ASTM A871 Grade 65

Tensile requirements for ASTM A871 Grade 65. Tension tests are typically transverse. For plates wider than 24 in [600 mm], elongation may be reduced by two percentage points; further adjustments follow ASTM A6.

Grade Yield min Tensile min Elongation in 2 in [50 mm] Elongation in 8 in [200 mm]
Grade 65 ≥65 ksi [≥450 MPa] ≥80 ksi [≥550 MPa] ≥17% ≥15%

Charpy V-notch impact testing is part of A871 mechanical practice; temperature and energy levels follow the purchase order / ASTM A6 supplementary requirements. A common published practice is longitudinal average ≥15 ft-lbf [20 J] at -20 °F [-29 °C]; always confirm the ordered CVN package on the MTC.

Sibling strength class: ASTM A871 Grade 60 (YS ≥60 ksi / TS ≥75 ksi).

Density is approximately 7.85 g/cm³.

Delivery Conditions for ASTM A871 Grade 65

As-rolled, normalized, or quenched and tempered as required to meet the specified mechanical properties. Fine-grain practice.

Hot-rolled weathering plates for poles are often supplied as-rolled when the strength package allows. Normalizing or quenching and tempering is used when thickness, toughness or the ordered mechanical package requires it. SHH STEEL supplies the delivery condition named on the order and reports it on the MTC.

Weldability of ASTM A871 Grade 65

Grade 65 is an HSLA weathering plate. When the steel is to be welded, use procedures suitable for the grade, chemistry type, thickness and intended service (see ASTM A6 Appendix X3 weldability guidance). Common processes include SMAW, GMAW and SAW. Prefer low-hydrogen consumables and consumables selected for weathering service when bare weld exposure is intended.

Preheat and interpass follow thickness, carbon equivalent, joint restraint and the approved WPS. Matching or undermatching filler must be chosen so weld-metal atmospheric behaviour and strength meet the design intent. Q&T heats need extra care on heat input and HAZ toughness.

Related fabrication pages: S355J2W · Q355NH · A588 Grade A.

Dimensional Tolerances for ASTM A871 Grade 65

Dimensional tolerances for A871 plate follow ASTM A6/A6M unless the order cites another dimensional agreement. Flatness, width and length classes should be stated on the purchase order for pole and tubular fabrication packages.

Respect the ordered thickness window and delivery condition. Coil-to-plate product is only A871-qualified after all required processing, inspection and testing are completed.

Applications and service limits for ASTM A871 Grade 65

Typical applications for Grade 65:

  • Transmission and lighting poles
  • Tubular structures and mast sections
  • Outdoor structural members where higher yield than A588-class plate is specified
  • RFQs that cite ASTM A871 Grade 60 / Grade 65 weathering plate

The self-protecting patina can lower long-term maintenance versus painted carbon steel in many rural and industrial atmospheres. It is not a universal coating substitute: sheltered pockets that stay wet, aggressive chloride splash, and continuous immersion often need coating or another material.

Related pages: Grade 60 · A588 Grade A · A709 50W · S355J2W · Corten B · Q355NH · A242 Type 1 · Weathering Steel Plates.

Atmospheric exposure guidance for ASTM A871 Grade 65

Bare Grade 65 is intended for atmospheres where a stable patina can form and dry periodically. Use the table as a selection aid; final coating or grade choice still follows the project specification.

Environment Typical fit for bare A871 plate Note
Rural / mild industrial Usually suitable Needs wet/dry cycles for patina
Urban / general industrial Often suitable Check local pollution and design details
Coastal / marine splash with moderate chloride Use with caution May need coating, higher-Ni practice, or another grade
Sheltered pockets that stay wet Not preferred bare Design out traps or coat locally
Continuous immersion / aggressive chloride Not recommended bare Select coated carbon steel or another material

Equivalent and related grades for ASTM A871 Grade 65

These grades are commonly compared with ASTM A871 Grade 65. They are approximate, not automatic substitutes. Match chemistry type, mechanical properties, toughness, thickness limits and the project specification before replacing one grade with another.

Standard / family Grade Relation Product page
ASTM A871/A871M Grade 65 This page –
ASTM A871/A871M Grade 60 Sibling strength class Grade 60
ASTM A588 / A709 50W Related weathering role; usually lower yield class A588 Gr.A · A709 50W
EN 10025-5 S355J2W / S355J0W / S355K2W Approximate W-family talk S355J2W · S355J0W · S355K2W
Commercial Corten B Common purchasing talk Corten B
GB/T 4171 Q355NH / Q415NH Related NH talk; confirm strength class Q355NH · Q415NH
ASTM A242 Type 1 / Type 2 High-P / lower-P A242 tracks A242 Type 1 · A242 Type 2
JIS G3125 SPA-H High-P sheet/plate talk (different form focus) SPA-H
Category A871 / weathering hubs Family navigation ASTM A871/A871M · Weathering Steel Plates

ASTM A871 Grade 65 vs Grade 60 vs A588 / S355J2W (selection aid)

These grades are often discussed together in purchasing. They are related weathering steels, not automatic substitutes.

Item Grade 65 Grade 60 A588 / S355J2W talk
Yield class ≥65 ksi ≥60 ksi Typically 50 ksi / 355 MPa class
Primary use talk Poles / tubular HSLA plate Poles / tubular HSLA plate Bridges / general weathering structures
Chemistry Type I / II / IV Type I / II / IV Per A588 / EN edition
G101 ≥ 6.0 ≥ 6.0 Per each standard
Pages This page Grade 60 A588 · S355J2W

Why choose SHH STEEL for ASTM A871 Grade 65

Supply, cutting and inspection for ASTM A871 Grade 65

Item SHH STEEL supply note
Thickness About 6-50 mm focus; confirm thinner / thicker against A871 window and mill practice
Size Width about 1500-3000 mm; length cut-to-size on request
Delivery condition As-rolled / normalized / quenched and tempered as ordered
Chemistry type Type I / Type II / Type IV as ordered
Processing Cutting, beveling, shot blasting available
Mill certificate EN 10204 3.1 standard; 3.2 on request
Third-party inspection SGS, TUV, BV or ABS can be arranged
Quotation needs Grade (Grade 65), chemistry type, thickness × width × length, quantity, delivery condition, CVN package, inspection level

FAQ

What is the difference between A871 Grade 60 and Grade 65?
Grade 60 targets ≥60 ksi yield / ≥75 ksi tensile. Grade 65 targets ≥65 ksi yield / ≥80 ksi tensile. See Grade 60 for the sibling page.
What chemistry types are available?
Type I, Type II and Type IV heat-analysis packages. All support the G101 index ≥ 6.0 requirement when correctly produced.
Is A871 the same as A588 or Corten B?
Not automatically. A871 is a higher-strength pole/tubular plate specification. It is often compared with A588, Corten B and S355J2W, but substitution needs project approval and MTC review.
Can A871 be used bare (unpainted)?
Yes, when properly exposed to the atmosphere, A871 steel can be used bare for many applications. Sheltered wet pockets, aggressive chlorides and immersion still need design review or coating.
What delivery conditions are allowed?
As-rolled, normalized, or quenched and tempered as required to meet the specified mechanical properties. Confirm the condition on the order and MTC.

Request a quotation

Send ASTM A871 Grade 65, chemistry type (I / II / IV), thickness × width × length, quantity, delivery condition (AR / normalized / Q&T), CVN package and any inspection requirement. SHH STEEL will return mill availability, certification scope and a quotation.

Contact: admin@steelspecs.com · +86-18939509537 · +86-021-62716097

More options: ASTM A871/A871M · Grade 60 · Weathering Steel Plates · A588 Grade A · S355J2W · Structural Steel Plates

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X