ASTM A588 Grade A S Shape I Beams

ASTM A588/A588M Grade A S-shape I-beams use Grade A chemistry and the 50 ksi [345 MPa] minimum yield and 70 ksi [485 MPa] minimum tensile strength specified for A588 structural shapes at all thicknesses. Size tables list the 28 ASTM A6/A6M S-shape reference dimensions, not European IPE or IPN sizes. SHH STEEL reviews the ordered edition and the certificate before quoting.
Keywords
ASTM A588 Grade A S-shape, A588 Grade A I-beam, A588 S-shape I-beam, A588/A588M Grade A American standard beam, A588 Grade A S beam
Equivalent Grades:
Near-equivalents only, not automatic substitutes.
Share:
General Description
Material Specification
Size Chart
Chemical Composition
Mechanical Properties
Applications
Comparison
Equivalent Grades
Sourcing
FAQ
Conclusion

What are ASTM A588 Grade A S-Shape I-Beams?

ASTM A588/A588M covers high-strength low-alloy structural steel shapes, plates and bars of structural quality, intended primarily for use in welded bridges and buildings where weight savings or improved atmospheric corrosion resistance is important. This page is Grade A in the American standard S-shape (I-beam) product form. Wide-flange (W) beams in the same grade remain on ASTM A588 Grade A Wide Flange H Beam. Angles remain on ASTM A588 Grade A Equal and Unequal Steel Angles. Those pages are not this product.

The chemistry and the shape mechanicals follow the same Grade A recitation already used on the live Grade A W-shape page. The edition named on the purchase order governs delivery.

Material, Dimensions and Scope for ASTM A588 Grade A S-Shapes

A588 covers plates, shapes and bars. S-shapes are rolled to the reference dimensions of ASTM A6/A6M. The mechanical requirements cited here are those stated for A588 structural shapes at all thicknesses in the specification: 50 ksi [345 MPa] minimum yield and 70 ksi [485 MPa] minimum tensile strength.

This page does not use European IPE or IPN dimensions for an ASTM grade. Existing A36 and A572 Grade 50 S-shape pages (ASTM A36 S Shape I Beams, ASTM A572 Grade 50 S Shape I Beams) already provide A6 S-shape geometry for those grades. A588 Grade A is added here as its own grade-and-form combination, not as a hybrid of A588 chemistry with an IPE table.

ASTM A588 Grade A S-Shape Sizes: American Standard Beams (ASTM A6/A6M)

The tables list the 28 standard ASTM A6/A6M S-shape reference dimensions, from S24×121 to S3×5.7: designation, actual depth, flange width, web thickness and flange thickness in inch and millimetre units, mass in lb/ft and kg/m, and the companion SI designation from the same AISC Manual, 15th Edition, shape file already used for the live A36 W-shape and S-shape tables. They are reference dimensions for identification and estimating, not a rolling list, and not a claim of guaranteed availability or that every S shape is produced in A588 Grade A. Dimensional acceptance follows the edition of ASTM A6/A6M named on the order. These are American standard S-shapes. They are not European IPE or IPN sizes, and an A588 Grade A enquiry must not be filled from an IPE or IPN table.

A designation such as S12×31.8 is a series call: the first number is the nominal depth in inches and the second is the nominal mass in pounds per foot. The actual depth of some rows is slightly above the nominal inch figure (for example S24×121 is 24.5 in deep). That is normal. Root radius is omitted because a single fillet radius is not published as a delivery dimension for these shapes, and a radius is not invented here. The deepest flange in this standard S series is 1.09 in (S24×121 and S24×106), which is below the 3 in [75 mm] flange-thickness notes that apply to some wide-flange shapes.

Theoretical mass is the tabulated reference value. Settlement should follow the contract — tabulated theoretical mass or weighed mass — and the ordered A6 edition for mass tolerance. These S-shape rows are not interchangeable with W-shapes, with HW, HM or HN, or with IPE, IPN or GB/T 706 I-beams of a similar nominal depth.

S24 to S15

The deeper American Standard S shapes, from S24×121 to S15×42.9. 13 designations in this group.

Swipe horizontally to view all dimensions.

Designation d (in) bf (in) tw (in) tf (in) d (mm) bf (mm) tw (mm) tf (mm) Mass (lb/ft) Mass (kg/m) SI designation
S24×121 24.5 8.05 0.8 1.09 622 204 20.3 27.7 121 180 S610×180
S24×106 24.5 7.87 0.62 1.09 622 200 15.7 27.7 106 158 S610×158
S24×100 24 7.25 0.745 0.87 610 184 18.9 22.1 100 149 S610×149
S24×90 24 7.13 0.625 0.87 610 181 15.9 22.1 90 134 S610×134
S24×80 24 7 0.5 0.87 610 178 12.7 22.1 80 119 S610×119
S20×96 20.3 7.2 0.8 0.92 516 183 20.3 23.4 96 143 S510×143
S20×86 20.3 7.06 0.66 0.92 516 179 16.8 23.4 86 128 S510×128
S20×75 20 6.39 0.635 0.795 508 162 16.1 20.2 75 112 S510×112
S20×66 20 6.26 0.505 0.795 508 159 12.8 20.2 66 98.2 S510×98.2
S18×70 18 6.25 0.711 0.691 457 159 18.1 17.6 70 104 S460×104
S18×54.7 18 6 0.461 0.691 457 152 11.7 17.6 54.7 81.4 S460×81.4
S15×50 15 5.64 0.55 0.622 381 143 14 15.8 50 74 S380×74
S15×42.9 15 5.5 0.411 0.622 381 140 10.4 15.8 42.9 64 S380×64

S12 to S3

The mid-range and smaller S shapes, from S12×50 to S3×5.7. 15 designations in this group.

Swipe horizontally to view all dimensions.

Designation d (in) bf (in) tw (in) tf (in) d (mm) bf (mm) tw (mm) tf (mm) Mass (lb/ft) Mass (kg/m) SI designation
S12×50 12 5.48 0.687 0.659 305 139 17.4 16.7 50 74 S310×74
S12×40.8 12 5.25 0.462 0.659 305 133 11.7 16.7 40.8 60.7 S310×60.7
S12×35 12 5.08 0.428 0.544 305 129 10.9 13.8 35 52 S310×52
S12×31.8 12 5 0.35 0.544 305 127 8.89 13.8 31.8 47.3 S310×47.3
S10×35 10 4.94 0.594 0.491 254 125 15.1 12.5 35 52 S250×52
S10×25.4 10 4.66 0.311 0.491 254 118 7.9 12.5 25.4 37.8 S250×37.8
S8×23 8 4.17 0.441 0.425 203 106 11.2 10.8 23 34 S200×34
S8×18.4 8 4 0.271 0.425 203 102 6.88 10.8 18.4 27.4 S200×27.4
S6×17.25 6 3.57 0.465 0.359 152 90.7 11.8 9.12 17.25 25.7 S150×25.7
S6×12.5 6 3.33 0.232 0.359 152 84.6 5.89 9.12 12.5 18.6 S150×18.6
S5×10 5 3 0.214 0.326 127 76.2 5.44 8.28 10 15 S130×15
S4×9.5 4 2.8 0.326 0.293 102 71.1 8.28 7.44 9.5 14.1 S100×14.1
S4×7.7 4 2.66 0.193 0.293 102 67.6 4.9 7.44 7.7 11.5 S100×11.5
S3×7.5 3 2.51 0.349 0.26 76.2 63.8 8.86 6.6 7.5 11.2 S75×11.2
S3×5.7 3 2.33 0.17 0.26 76.2 59.2 4.32 6.6 5.7 8.5 S75×8.5

Wide-flange W-shape dimensions belong on the ASTM A36 Wide Flange Beam page, not in this table. Chinese HW/HM/HN sizes belong to GB/T 11263. European IPE sizes are listed on the EN 10025-2 S235JR IPE and IPN Steel I Beams page for that material system, not as A36 S dimensions.

ASTM A588 Grade A Chemical Composition for Shapes

The table recites the Grade A heat-analysis limits used on the live Grade A W-shape page. Copper is part of the Grade A row, not an optional extra. Grade K, which uses columbium rather than this vanadium band, is not this page.

Swipe horizontally to view all dimensions.

Element Grade A heat analysis Notes
C, max (%) 0.19 See the manganese footnote when carbon is taken below this maximum.
Mn (%) 0.80–1.25 For each 0.01 percentage point reduction below the specified carbon maximum, an increase of 0.06 percentage point manganese above the specified maximum is permitted, up to 1.50 %.
P, max (%) 0.04 Used here as the shapes limit commonly tabulated with this grade.
S, max (%) 0.05 Used here as the shapes limit commonly tabulated with this grade.
Si (%) 0.30–0.65 —
Ni, max (%) 0.40 —
Cr (%) 0.40–0.65 —
Cu (%) 0.25–0.40 Do not treat copper as an optional add-on; it is part of the Grade A row.
V (%) 0.02–0.10 Grade K uses columbium rather than this vanadium band; that is not this page.

ASTM A588 Grade A S-Shape Mechanical Properties: Yield, Tensile and Elongation

For A588 structural shapes, at all thicknesses in the specification, minimum yield point is 50 ksi [345 MPa] and minimum tensile strength is 70 ksi [485 MPa]. Minimum elongation is 18 % in 8 in. [200 mm] and 21 % in 2 in. [50 mm]. Do not replace the 50 ksi yield with a 65 ksi figure; 65 ksi is not the Grade A shape yield on this page.

Swipe horizontally to view all dimensions.

Property Requirement for A588 structural shapes (all thicknesses in the specification)
Minimum yield point 50 ksi [345 MPa]
Minimum tensile strength 70 ksi [485 MPa]
Minimum elongation in 8 in. [200 mm] 18 %
Minimum elongation in 2 in. [50 mm] 21 %

Applications and Service Limits for ASTM A588 Grade A S-Shape I-Beams

A588 Grade A S-shapes are used where an American standard I-beam is wanted in a weathering-grade structural steel. Improved atmospheric corrosion resistance is a purpose of the specification; it is not a substitute for a coating specification unless the order says so. Welding procedures must follow the purchaser’s standard and the named edition.

ASTM A588 Grade A S-Shapes Compared with A588 W-Shapes, A36 S-Shapes and IPE Beams

ASTM A588 Grade A Wide Flange H Beam is the same grade in the W-shape product form. The chemistry and the shape mechanicals match; the geometry does not. ASTM A36 S Shape I Beams and ASTM A572 Grade 50 S Shape I Beams use the same A6 S-shape geometry with different material grades. European IPE and IPN pages already exist under EN 10025-2 on this site and must not be used as A588 S-shape tables.

Near-Equivalents for ASTM A588 Grade A S-Shape I-Beams: Not Automatic Substitutes

Near-equivalents only, not automatic substitutes. Other weathering or 50 ksi shape grades, including other A588 grades and EN 10025-2 S355J0W or S355J2W, have their own chemistry and product-form rules. An A588 Grade A W-shape certificate is not automatic evidence for an S-shape, or the reverse, without a check of the ordered geometry.

Sourcing ASTM A588 Grade A S-Shape I-Beams from SHH STEEL

SHH STEEL reviews the named A588/A588M edition, the Grade A certificate and the ordered S-shape designation before quoting. The A6 S-shape table on this page is not a warehouse list. State the designation (for example S12×31.8) and the length on the enquiry.

FAQ: ASTM A588 Grade A S-Shape I-Beams

Does A588 cover S-shapes?
Yes. A588/A588M covers plates, shapes and bars. This page is Grade A in the A6 S-shape product form. The live Grade A page on this site was previously the W-shape only.
Are the sizes IPE or IPN?
No. The table lists the 28 ASTM A6/A6M S-shape reference dimensions. European IPE and IPN sizes belong on the existing EN 10025-2 I-beam pages, not here.
Is the yield 65 ksi?
No. For A588 structural shapes the minimum yield point is 50 ksi [345 MPa] and the minimum tensile strength is 70 ksi [485 MPa]. A 65 ksi yield figure is not used on this page.

Conclusion

Specify ASTM A588/A588M Grade A S-shapes with Grade A chemistry, the 50 ksi / 70 ksi shape mechanicals, and an A6 S-shape designation. Do not fill the enquiry from a W-shape table or from a European IPE or IPN table.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X