ASTM A588 Grade A Wide Flange H Beam
What is an ASTM A588 Grade A Wide Flange H Beam?
An ASTM A588 Grade A wide flange H beam is a rolled W-shape whose material conforms to ASTM A588/A588M Grade A and whose dimensions, shape and tolerances conform to ASTM A6/A6M. Grade A is a high-strength low-alloy structural steel written for atmospheric corrosion resistance, with 50 ksi [345 MPa] minimum yield and 70 ksi [485 MPa] minimum tensile for structural shapes. This page is Grade A only. Grade B and Grade K have different chemistry rows and are not covered here.
This page covers the rolled wide-flange shape, not plate and not a channel. A588 plate uses thickness-dependent yield bands (including 46 ksi and 42 ksi values for thicker plates and bars) that do not apply to structural shapes in the way those plate rows are written. The plate data sheet is not a substitute for this W-shape listing. Ordinary 36 ksi carbon W-shapes are ASTM A36 Wide Flange Beam. A 50 ksi non-weathering comparison grade is ASTM A572 Grade 50.
These beams are filed under H Beams and Wide Flange Beams in the steel structural profiles category. The W series is the American wide-flange series, not a Chinese HW or a European HEA of similar depth, and not an S shape.
A588 Grade A W-shapes are used in bridges, exposed frames and other structures where atmospheric corrosion resistance is specified. The specification says that, when properly exposed to the atmosphere, the steel is suitable for many applications in the bare condition. That is not an automatic licence to leave every beam unpainted. Sheltered, wet or chloride-rich details, and surfaces that cannot dry, are poor places to assume a bare finish. The order should say whether the beam is for bare or coated service.
Material, Dimensions and Tolerances for ASTM A588 Grade A W-Shapes
Two documents should appear, separately, on the purchase order and on the mill test report:
- ASTM A588/A588M Grade A is the material specification. This article uses the chemistry and the structural-shape tensile values written for Grade A. The edition named on the order governs acceptance. A Grade B or Grade K certificate does not satisfy a Grade A line unless the order is changed.
- ASTM A6/A6M is the general-requirements standard for the W-shape designation system, dimensions, tolerances, marking, and the heat-analysis and tension-test rules. A588 does not itself contain the W-shape size tables.
Do not treat “A588 beam” as if it automatically meant Grade A or a W12×50, and do not substitute ASTM A572 Grade 50 or a European weathering grade by matching a 50 ksi yield or a similar depth.
ASTM A588 Grade A W-Shape Sizes and Reference Dimensions (ASTM A6/A6M)
The tables list nominal W-shape reference dimensions: designation, nominal depth, mass in lb/ft and kg/m, and actual depth, width, web thickness and flange thickness in both inch and millimetre units. There are 283 designations, grouped by depth so the tables stay readable. They are reference dimensions for identification and estimating, not a rolling list, and not a claim of guaranteed availability or that every W-shape is produced in A588 Grade A. Dimensional acceptance, including shape and mass tolerances, follows the edition of ASTM A6/A6M named on the order. Mid-range W12 to W30 beams and the common W8–W14 column sizes are the usual enquiry core; the lightest W4–W6 rows, jumbo column sections, and the deepest W40–W44 rows should be confirmed size by size.
A designation such as W16×26 is a series call: the first number is the nominal depth in inches and the second is the nominal mass in pounds per foot. The actual depth of a W16×26 is slightly less than 16 in. That is normal. Root radius is omitted because a single fillet radius is not published as a delivery dimension for these shapes, and a radius is not invented here.
Theoretical mass is the tabulated reference value. Settlement should follow the contract — tabulated theoretical mass or weighed mass — and the ordered A6 edition for mass tolerance. These W-shape rows are not interchangeable with HW, HM, HN or HEA/HEB/IPE rows of a similar nominal depth, and they are not S shapes.
W4 to W10
The lighter W-shapes, often used as small beams, lintels and miscellaneous members. 41 designations in this group, from W4×13 to the W10 series.
Swipe horizontally to view all dimensions.
W12 and W14
The mid-depth column and beam group, including many of the heavier W12 and W14 column sections. 67 designations.
Swipe horizontally to view all dimensions.
W16 to W21
Common building-beam depths. 55 designations.
Swipe horizontally to view all dimensions.
W24 to W30
Deeper building and industrial beams. 54 designations.
Swipe horizontally to view all dimensions.
W33 to W44
The deepest W-shapes in these reference tables, through W44. 66 designations. Heavier and deeper rows should be confirmed size by size against the mill programme.
Swipe horizontally to view all dimensions.
Chinese HW/HM/HN sizes belong to GB/T 11263. European HEA/HEB/IPE sizes are not A588 dimensions. S shapes are a different A6 series and are not tabulated here. Ordinary carbon W-shapes in the same A6 series are listed on ASTM A36 Wide Flange Beam; that page is not a weathering specification.
ASTM A588 Grade A Chemical Composition for Shapes
The figures below are the Grade A heat-analysis limits commonly tabulated for ASTM A588/A588M. They are limits, not typical heat results, and they are not the Grade B or Grade K rows. The 0.04% phosphorus and 0.05% sulfur maxima are the limits used on this page for structural shapes. A tighter phosphorus or sulfur figure sometimes shown for plate is not applied to these W-shape shapes. Product analysis, when required, shall conform to those same heat-analysis limits, subject to the numeric permitted variations below, taken from Table A of ASTM A6/A6M-19. Where Table A shows no under-minimum or over-maximum figure, none is applied on this page.
The following product-analysis variations apply to those heat-analysis limits.
Table A footnote A gives a different manganese variation for bars and bar-size shapes: ±0.03% up to 0.90% inclusive, and ±0.06% over 0.90% to 2.20% inclusive. Where a heat-analysis limit is a maximum only, the over-maximum variation is the figure that raises the product-analysis ceiling. The A6/A6M edition named on the order governs.
Do not copy a Grade B or Grade K chemistry row onto a Grade A beam, and do not copy a plate-width exception onto this W-shape unless the ordered edition actually requires it.
ASTM A588 Grade A W-Shape Mechanical Properties: Yield, Tensile and Elongation
For structural shapes, the tensile requirements commonly tabulated for ASTM A588/A588M apply to all thicknesses in the specification: 70 ksi [485 MPa] minimum tensile strength, 50 ksi [345 MPa] minimum yield, 18% minimum elongation in 8 in [200 mm] and 21% minimum elongation in 2 in [50 mm]. The reductions that appear for plates and bars thicker than 4 in [100 mm] are plate-and-bar rules. They are not applied to these W-shape shapes.
A footnote that lowers the 2 in elongation to 18% applies to wide-flange shapes with flange thickness over 3 in [75 mm], not to these W-shape shapes. None of the standard W-shape rows tabulated here has a thickness over 3 in. Charpy testing is not treated here as a default A588 requirement; if an impact supplementary is needed, it must be named on the order. Tension-test orientation follows A6/A6M.
Delivery, Inspection and Identification of ASTM A588 Grade A W-Shapes
A588 Grade A W-shapes are commonly delivered in the as-rolled condition unless the order names a different condition. The mill test report should identify ASTM A588/A588M Grade A (or the edition on the order), the W designation, and the heat. Marking should follow ASTM A6/A6M so the piece can be matched to the certificate.
A Grade B or Grade K certificate, or an A588 plate certificate, is not a Grade A W-shape certificate for the designation on this page. If the beam is for bare weathering service or for a coated finish, say so on the order.
Weldability, Exposure and Surface Condition of ASTM A588 Grade A W-Shapes
A588 Grade A is a weldable high-strength low-alloy steel, but this page is not a welding procedure. Procedure qualification, consumables and any weathering-steel welding practice remain the fabricator’s responsibility. Chemistry, including copper, chromium and vanadium bands, is part of what distinguishes this grade from A572 Grade 50.
Bare exposure only performs as intended when the surface can wet and dry in a suitable atmosphere. Sheltered pockets, pack-out at faying surfaces, and chloride-rich or persistently wet details need a deliberate finish decision. Surface condition for painting, if coating is required, should be named on the order.
ASTM A6/A6M Shape Tolerances and Theoretical Mass for ASTM A588 Grade A W-Shapes
Dimensional, straightness, camber, sweep, out-of-square and mass tolerances for these W-shapes are those of ASTM A6/A6M, not of ASTM A588/A588M. This article does not reproduce the A6 tolerance tables; acceptance is against the edition named on the order.
The size tables above are nominal W-shape reference dimensions. A delivered W16×26 will measure close to the tabulated values within those tolerances, not as a set of exact advertised inches. The lb/ft and kg/m columns are published theoretical masses. Settlement should follow the contract.
Applications and Service Limits for ASTM A588 Grade A Wide Flange H Beams
A588 Grade A W-shapes are used in bridges, exposed building frames and other structures where a 50 ksi weathering shape is specified. They are not an automatic unpainted solution for every atmosphere, and they are not a plate, a channel, or a Grade B or Grade K data sheet.
If the project only needs 50 ksi without a weathering chemistry, ASTM A572 Grade 50 may be the specification to nominate. If a 36 ksi carbon W-shape is enough, use ASTM A36 Wide Flange Beam. This page is not a design guide and does not give corrosion-loss tables.
ASTM A588 Grade A Compared with A588 Plate, Grade B and Grade 50
A588 Grade B and Grade K are different grade letters in the same specification, with different chemistry. A certificate for those letters does not satisfy a Grade A line unless the order is changed. A588 plate may carry the same grade letter but is a different product form, and the lower yield values listed for thicker plates and bars are plate-and-bar rules, not the structural-shape row used here (50 ksi yield and 70 ksi tensile for shapes).
ASTM A572 Grade 50 can also be furnished as a 50 ksi W-shape, but it is not written for atmospheric corrosion resistance and does not share this Grade A chemistry. S355J2W and Q355NH are different systems. Dual certification is possible only when the delivered piece meets every requirement of each named standard.
Near-Equivalents for ASTM A588 Grade A Wide Flange H Beams: Not Automatic Substitutes
Sourcing ASTM A588 Grade A Wide Flange H Beams from SHH STEEL
SHH STEEL reviews enquiries for ASTM A588 Grade A W-shapes against a named A6 designation list and a named edition. We check the grade letter, the W designation, and whether the beam is for bare or coated service before quoting. We do not treat Grade B, Grade K, A588 plate, or A572 Grade 50 as the same item, and we do not invent unofficial sizes.
Send the W designation list, the A588/A588M edition, Grade A, the finish requirement, and delivery notes. Images on this page stay empty; photographs can be provided with a quotation when they are available.
A588 Grade A Wide Flange H Beam FAQs
-
Why does this page name Grade A instead of just A588?
- A588/A588M is a specification with more than one grade letter, and the chemistry rows are not the same. This article is written for Grade A, which is the grade commonly tabulated for A588 shapes. A Grade B or Grade K certificate does not satisfy a Grade A line unless the order is changed.
-
Do these W-shapes use the lower yield values listed for thick A588 plate?
- No. The 46 ksi and 42 ksi yield figures that appear for plates and bars over 4 in are plate-and-bar rules. Structural shapes are commonly tabulated at 50 ksi yield and 70 ksi tensile for all thicknesses in the specification.
-
Can every A588 Grade A beam be left unpainted?
- Not automatically. The specification says that, when properly exposed to the atmosphere, the steel is suitable for many applications in the bare condition. Sheltered, wet or chloride-rich details, and surfaces that cannot dry, are poor places to assume a bare finish. The order should say whether the beam is for bare or coated service.
-
Is A588 Grade A the same as A572 Grade 50?
- No. Both can be furnished as 50 ksi W-shapes, but A588 Grade A is written for atmospheric corrosion resistance and has its own chemistry, including copper, chromium and vanadium bands that A572 Grade 50 does not share as this grade.
-
Is this page also an S-shape or channel listing?
- No. This article tabulates ASTM A6 W-shapes. S shapes and C or MC channels are different A6 series and are not published in these tables.
Request a Quotation for ASTM A588 Grade A Wide Flange H Beams
ASTM A588 Grade A wide flange H beams are high-strength low-alloy W-shapes written for atmospheric corrosion resistance, with 50 ksi [345 MPa] minimum yield and 70 ksi [485 MPa] minimum tensile for structural shapes. Nominate the W-shape to ASTM A6/A6M, the material to ASTM A588/A588M Grade A (or the edition on the order), and whether the beam is for bare or coated service. The tables are reference dimensions, not a rolling list. Send the designation list, grade letter, edition, certificate type and any processing notes; SHH STEEL will review them before quoting.