ASTM A572 Grade 50 S Shape I Beams
What are ASTM A572 Grade 50 S Shape I Beams?
ASTM A572 Grade 50 S-shape I-beams are American Standard Beams in high-strength low-alloy structural steel Grade 50. The material standard is ASTM A572/A572M. Dimensions, mass and general requirements for the rolled section are those of ASTM A6/A6M. The 50 ksi [345 MPa] minimum yield is the same figure used for Grade 50 plates, angles and W-shapes, but this page is for the S-shape only. It is not the live ASTM A36 S-shape page, and it is not a Grade 50 wide-flange, channel, angle or sheet-pile page.
Material, Dimensions and Tolerances for ASTM A572 Grade 50 S Shapes
A complete order has to keep three documents distinct: A572/A572M is the material standard; A6/A6M is the general-requirements and dimensional standard for the S series; the ordered editions of both govern acceptance. The chemistry and tensile figures on this page are the shapes values already verified for Grade 50 angles and channels on this site. They apply to S-shapes as structural shapes. A plate-width chemistry column must not be copied here.
ASTM A572 Grade 50 S Shape Sizes: American Standard Beams (ASTM A6/A6M)
The table lists the same 28 typographical A6/A6M S designations already verified on the A36 S-shape page, from S24x121 to S3x5.7. Grade 50 can use that S series; the difference is the material, not a second set of designations. The table is not a mill rolling list and not a W-shape table. The maximum flange in this series is 1.09 in, well under 3 in.
Swipe horizontally to view all dimensions.
S12 to S3
The mid-range and smaller S shapes, from S12×50 to S3×5.7. 15 designations in this group.
Swipe horizontally to view all dimensions.
Wide-flange W-shape dimensions belong on the ASTM A36 Wide Flange Beam page, not in this table. Chinese HW/HM/HN sizes belong to GB/T 11263. European IPE sizes are listed on the EN 10025-2 S235JR IPE and IPN Steel I Beams page for that material system, not as A36 S dimensions.
ASTM A572 Grade 50 Chemical Composition for S Shapes (Heat Analysis)
For Grade 50 shapes, carbon is 0.23 % maximum. Manganese is 1.35 % maximum, and may be raised to 1.60 % under the carbon trade-off stated in the table, with a 0.50 % manganese minimum and a manganese-to-carbon ratio of not less than 2. Phosphorus 0.04 % and sulfur 0.05 % apply to structural shapes (Footnote I), which includes these S-shapes. Silicon is 0.40 % maximum for flanges 3 in and under. Do not paste a 0.030 % plate phosphorus default onto an S-shape certificate.
Swipe horizontally to view all dimensions.
ASTM A572 Grade 50 S Shape Mechanical Properties
Minimum yield is 50 ksi [345 MPa] and minimum tensile strength is 65 ksi [450 MPa], with no specified yield maximum. Minimum elongation is 18 % in 8 in [200 mm] and 21 % in 2 in [50 mm]. These are the shapes figures, not a plate-width column. A Charpy test is not required unless specified. An A36 S-shape certificate, with its 36 ksi yield and 58-80 ksi tensile range, does not fulfil a Grade 50 order.
Swipe horizontally to view all dimensions.
Applications and Service Limits for ASTM A572 Grade 50 S Shape I Beams
Grade 50 S-shapes are used in frames, bracing and general construction where an American Standard Beam is named in this high-strength low-alloy grade. The grade is not a pressure-vessel or nuclear safety material, and it is not a weathering grade such as A588. If the project needs a W-shape, an A36 S-shape, or a different Grade 50 product form, that product has to be ordered as such.
Near-Equivalents for ASTM A572 Grade 50 S Shapes: Not Automatic Substitutes
ASTM A36 S-shapes use the same A6 series with a lower yield and a different chemistry table. ASTM A992 is a W-shape specification, not an S-shape default. EN 10025-2 S355JR I-beams and GB/T 1591 Q355B I-beams use different shape systems. ASME SA designations are not inferred here.
Sourcing ASTM A572 Grade 50 S Shape I Beams from SHH STEEL
Send the S designation, the length, and the A572/A572M edition, and name Grade 50 explicitly. Do not use the A36 S-shape term, or a Grade 50 W-shape or angle term, for this page. Create and assign only the new ASTM A572 I-beam child term under parent 797; do not tick the H-beam A572 term. SHH STEEL reviews the grade, the designation and the certificate before quoting.
ASTM A572 Grade 50 S Shape FAQs
-
Is this the same as the A36 S-shape page?
- No. The 28 designations are the same A6 S series, but Grade 50 has a 50 ksi yield, a 65 ksi tensile minimum, and a different chemistry table. An A36 certificate does not fulfil this order.
-
May manganese exceed 1.35 %?
- Yes, up to 1.60 %, only under the stated carbon trade-off, and with a manganese minimum of 0.50 % and a manganese-to-carbon ratio of not less than 2.
-
Which phosphorus limit applies?
- 0.04 % phosphorus and 0.05 % sulfur apply to structural shapes, including these S-shapes. Do not paste a 0.030 % plate default here.
-
Should this post use an existing H-beam A572 term?
- No. Create the I-beam child term ASTM A572 (astm-a572-steel-i-beam-profiles) under parent 797, and do not tick H-beam terms or parent 797.
Conclusion
ASTM A572 Grade 50 S-shape I-beams use the 28 typographical A6 S designations with a 50 ksi yield and a 65 ksi tensile minimum. This is not the A36 S-shape page and not a W-shape listing. Confirm the designation, the grade and the certificate on the order, and assign only the new I-beam child term.