ASTM A588 Grade A Equal and Unequal Steel Angles
What is ASTM A588 Grade A Steel Angle?
ASTM A588 Grade A steel angle is a hot-rolled equal-leg or unequal-leg L-shape in high-strength low-alloy structural steel Grade A, furnished for the atmospheric corrosion resistance that the specification is written around. The material standard is ASTM A588/A588M. Dimensions, mass and general requirements for the rolled section are those of ASTM A6/A6M. SHH STEEL supplies these angles to the grade letter, L designation, edition and certificate named on the order.
This page is written for Grade A only. Grades B and K are other A588 grades with their own chemistry, and they are not this data sheet. Do not use ASTM A588 Grade A steel plate, or the Grade B or Grade K plate pages, as an angle data sheet, and do not treat this page as a substitute for ASTM A572 Grade 50 steel angle when weathering performance is not what the order requires.
The official scope of A588/A588M-24 covers high-strength low-alloy structural steel shapes, plates and bars for welded, riveted or bolted construction, intended primarily for welded bridges and buildings where savings in weight or added durability are important. The atmospheric corrosion resistance of this steel in most environments is substantially better than that of carbon structural steels with or without copper. When properly exposed to the atmosphere, the steel is suitable for many applications in the bare (unpainted) condition. The specification is limited to material up to 8 in [200 mm] inclusive. These angles are filed in the steel angle profiles category of steel structural profiles.
This page covers Equal and Unequal Steel Angles in ASTM A588 Grade A. The Equal Leg Steel Angles and Unequal Leg Steel Angles follow the ASTM A6/A6M L series; the material standard does not by itself define the dimensions.
Material, Dimensions and Tolerances for A588 Grade A Angles
Keep the material specification, the grade letter and the dimensional standard distinct:
ASTM A588/A588M is the material standard, and Grade A is the grade on this page. The current ASTM listing used for the official public scope is A588/A588M-24. Grade A heat-analysis limits and the structural-shapes tensile row on this page follow the figures commonly tabulated for that specification. The edition named on the order governs acceptance.
ASTM A6/A6M is the general-requirements and dimensional standard for these rolled L-shapes. The size tables below are the standard equal-leg and unequal-leg L series used as a reference, not a mill rolling list. The edition of A6/A6M named on the order governs dimensional acceptance.
The specification points to Guide G101 for methods of estimating atmospheric corrosion resistance. That guide is not a substitute for naming Grade A, and it does not turn a painted carbon angle into an A588 angle.
ASTM A588 Grade A Equal Leg Steel Angles
The tables below are the standard ASTM A6/A6M equal-leg L series. ASTM A588/A588M does not publish a size list of its own, and the specification as a whole is limited to material 8 in [200 mm] thick or less — well above any standard L thickness. Use the figures to identify a designation and to estimate mass, not as a rolling programme and not as a warehouse list of weathering angles.
An equal angle has both legs the same length, for example L 4×4×1/2 or L 8×8×1. Mid-range L 3 to L 8 sizes are the usual enquiry core; 12 in legs and the heaviest thicknesses should be confirmed line by line, together with the Grade A certificate.
Equal-leg angles (61 sizes, L 2×2×1/8 to L 12×12×1-3/8)
L 2 to L 4 equal (28 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 equal (16 sizes)
Swipe horizontally to view all dimensions.
L 8 to L 12 equal (17 sizes)
Swipe horizontally to view all dimensions.
ASTM A588 Grade A Unequal Leg Steel Angles
The tables below are the standard ASTM A6/A6M unequal-leg L series for the same Grade A material. L 8×6×1 is an 8 in by 6 in angle, 1 in thick; it is not L 8×8×1, and it is not a metric unequal angle of a similar millimetre size.
These rows are reference dimensions and theoretical masses, not a list of bare or painted lengths waiting in a yard.
Unequal-leg angles (76 sizes, L 2-1/2×1-1/2×3/16 to L 8×6×1)
L 2½ to L 4 unequal (35 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 unequal (22 sizes)
Swipe horizontally to view all dimensions.
L 7 to L 8 unequal (19 sizes)
Swipe horizontally to view all dimensions.
The 137 rows above are the standard equal and unequal L series used for this page. Other special-bar-size or non-standard angles can be reviewed when they are named on the enquiry; they are not invented here. European, Chinese or Japanese angle designations belong to their own dimensional standards, not to these L rows.
A588 Grade A Chemical Composition for Angles
The figures below are the Grade A heat-analysis limits commonly tabulated for ASTM A588/A588M. They are limits, not typical heat results, and they are not the Grade B or Grade K rows. The 0.04% phosphorus and 0.05% sulfur maxima are the limits used on this page for structural shapes. A tighter phosphorus or sulfur figure sometimes shown for plate is not applied to these L-shapes. Product analysis, when required, shall conform to those same heat-analysis limits, subject to the numeric permitted variations below, taken from Table A of ASTM A6/A6M-19. Where Table A shows no under-minimum or over-maximum figure, none is applied on this page.
The following product-analysis variations apply to those heat-analysis limits.
Table A footnote A gives a different manganese variation for bars and bar-size shapes: ±0.03% up to 0.90% inclusive, and ±0.06% over 0.90% to 2.20% inclusive. Where a heat-analysis limit is a maximum only, the over-maximum variation is the figure that raises the product-analysis ceiling. The A6/A6M edition named on the order governs.
Do not copy a Grade B or Grade K chemistry row onto a Grade A angle, and do not copy a plate-width exception onto this L-shape unless the ordered edition actually requires it.
A588 Grade A Angle Mechanical Properties: Yield, Tensile and Elongation
For structural shapes, the tensile requirements commonly tabulated for ASTM A588/A588M apply to all thicknesses in the specification: 70 ksi [485 MPa] minimum tensile strength, 50 ksi [345 MPa] minimum yield, 18% minimum elongation in 8 in [200 mm] and 21% minimum elongation in 2 in [50 mm]. The reductions that appear for plates and bars thicker than 4 in [100 mm] are plate-and-bar rules. They are not applied to these L-shapes.
A footnote that lowers the 2 in elongation to 18% applies to wide-flange shapes with flange thickness over 3 in [75 mm], not to these L-shapes. None of the standard L rows tabulated here has a thickness over 3 in. Charpy testing is not treated here as a default A588 requirement; if an impact supplementary is needed, it must be named on the order. Tension-test orientation follows A6/A6M.
Delivery, Inspection and Identification of A588 Grade A Angles
A588 Grade A angles are commonly supplied as-rolled. The inspection document should identify ASTM A588/A588M and its edition, Grade A (not merely “A588”), the A6/A6M L designation, the heat number, the heat analysis and the tensile results. An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request. A Grade A plate certificate does not identify an L-shape, and a Grade B certificate does not satisfy a Grade A line. Length is a matter for the rolling programme and the order, often in the region of 20–40 ft or 6–12 m; those lengths are enquiry ranges, not a stock list.
Weldability, Exposure and Surface Condition of A588 Grade A Angles
A588 Grade A is intended for welded, riveted or bolted construction. The specification requires a welding procedure suitable for the grade and the intended use or service, and points to Appendix X3 of A6/A6M for weldability information. This page does not prescribe a procedure or a preheat chart. Procedure should be set from the certificate analysis and the applicable welding specification.
Bare weathering service depends on proper exposure so that the surface can develop and hold its oxide. The as-rolled surface is mill scale; blast cleaning, painting or another coating system is an order option when the design is not a bare application. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry.
A6/A6M Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these L-shapes are those of ASTM A6/A6M, not of A588/A588M itself. This article does not reproduce the inch or millimetre tolerance tables; acceptance is against the edition of A6/A6M named on the order. Out-of-square at the heel and variation of the two legs matter for connections. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
A588 Grade A steel angles are used where a 50 ksi HSLA L-shape and the atmospheric corrosion resistance of this specification are what the order names: bridge and building work, exposed frames, bracing and details that are intended to stand bare when the exposure is suitable, or to be coated when the design requires it. The 50 ksi yield is the same figure used for A572 Grade 50 steel angle, but that grade is not a weathering specification.
Bare use is not automatic in every climate or in every detail. Sheltered, wet, or chloride-rich exposures, and details that trap moisture, can be poor places to assume an unpainted A588 surface. The grade is not specified here as a pressure-vessel or nuclear-safety material, and it is not a stainless steel. Durability in a coated design comes from the coating system as well as from the grade.
A588 Grade A Angle Compared with A588 Plate, Grade B and Grade 50
ASTM A588 Grade A steel plate is the same grade in a different product form, with plate tensile reductions above 4 in that must not be copied onto an L-shape. Grade B and Grade K plates are other A588 grades; their chemistry is not the Grade A row on this page.
A572 Grade 50 steel angle can use the same L series at a 50 ksi yield, but it is not written as a weathering grade. A36 steel angle is a carbon grade with a 36 ksi yield and no A588 corrosion-resistance claim.
Near-Equivalents: Not Automatic Substitutes
Stock and Supply of A588 Grade A Steel Angles from SHH STEEL
SHH STEEL supplies ASTM A588 Grade A equal-leg and unequal-leg steel angles as an export trading house, coordinating mill production and project procurement. The useful work on this product is to keep the Grade A letter on the certificate, to keep equal and unequal designations from being mixed, and to align the A6/A6M size, the edition and any bare-or-coated finish before a rolling programme is committed.
Sizes, lengths and certificates are confirmed per enquiry. The tables are the standard L series, not a list of weathering pieces on the floor. Mid-range L 3 to L 8 sizes are the usual core; 12 in equal legs and the heaviest thicknesses are confirmed per line.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every equal or unequal L size in Grade A. If cutting, punching, forming, a coating system or a bare-weathering finish is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
A588 Grade A Steel Angle FAQs
-
Why does this page name Grade A instead of just A588?
- A588/A588M is a specification with more than one grade letter, and the chemistry rows are not the same. This article is written for Grade A, which is the grade commonly tabulated for A588 angles. A Grade B or Grade K certificate does not satisfy a Grade A line unless the order is changed.
-
Do these angles use the lower yield values listed for thick A588 plate?
- No. The 46 ksi and 42 ksi yield figures that appear for plates and bars over 4 in are plate-and-bar rules. Structural shapes are commonly tabulated at 50 ksi yield and 70 ksi tensile for all thicknesses in the specification. The standard L series is far below those plate-thickness bands.
-
Can every A588 Grade A angle be left unpainted?
- Not automatically. The specification says that, when properly exposed to the atmosphere, the steel is suitable for many applications in the bare condition. Sheltered, wet or chloride-rich details, and surfaces that cannot dry, are poor places to assume a bare finish. The order should say whether the angle is for bare or coated service.
-
Is an equal angle interchangeable with an unequal angle of the same long-leg length?
- No. L 8×8 and L 8×6 are different sections. The short-leg length, the mass and the connection details are those of the designation that the specification actually names.
-
Is A588 Grade A the same as A572 Grade 50?
- No. Both can be furnished as 50 ksi L-shapes, but A588 Grade A is written for atmospheric corrosion resistance and has its own chemistry, including copper, chromium and vanadium bands that A572 Grade 50 does not share as this grade.
Request a Quotation for ASTM A588 Grade A Steel Angle
ASTM A588 Grade A steel angle is a high-strength low-alloy L-shape with 50 ksi [345 MPa] minimum yield and 70 ksi [485 MPa] minimum tensile strength for structural shapes. Nominate the equal or unequal L size to ASTM A6/A6M and the material to ASTM A588/A588M Grade A (or the edition on the order). Name whether the angle is for bare or coated service. The tables are reference dimensions, not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.