ASTM A36 Wide Flange H Beam
What is an ASTM A36 Wide Flange Beam?
An ASTM A36 wide-flange beam is a rolled W-shape whose material conforms to ASTM A36/A36M and whose dimensions, shape and tolerances conform to ASTM A6/A6M. A36 is a carbon structural steel with a minimum yield point of 36 ksi [250 MPa] and a tensile-strength range of 58–80 ksi [400–550 MPa] for ordinary thicknesses. The designation “W” is the American wide-flange series; it is not a translation of a Chinese HW section or of a European HEA or HEB of a similar nominal depth.
This page covers the rolled wide-flange shape, not plate. The same specification in plate form is listed separately as ASTM A36 steel plate. Plate chemistry is split by thickness and width in Table 3, plate elongation rules differ, and the 32 ksi [220 MPa] yield reduction applies only to plates over 8 in [200 mm] thick. The plate page is not a substitute data sheet for W-shapes. A related ASME listing is discussed on ASME SA-36 steel plate; this product is ordered and certified to ASTM A36/A36M for shapes.
These beams are filed under ASTM A36 steel beam profiles in the steel beam profiles category of steel structural profiles. Sister categories for higher-strength American shapes include ASTM A572 and ASTM A992.
A36 W-shapes are used in general building and industrial frames, platforms, skids and fabrication where a 36 ksi carbon steel is specified and an impact test is not a default requirement. They are not a 50 ksi grade, not a weathering steel, and not a pressure-vessel or nuclear safety material. If the enquiry only says “A36 beam,” the shape series (W, S, C or MC), the A6 size, and any supplementary tests still need to be confirmed.
Material, Dimensions and Tolerances for A36 W-Shapes
Two documents should appear, separately, on the purchase order and on the mill test report:
- ASTM A36/A36M is the material specification for carbon structural steel. This article uses the chemistry and tensile values published in ASTM A36/A36M-19, the current edition used here. The edition named on the order governs acceptance. Inch-pound and SI values are both official; each system is used as published, not as a converted equivalent mixed into the other.
- ASTM A6/A6M is the general-requirements standard for rolled structural steel bars, plates, shapes and sheet piling. For W-shapes it sets the designation system, dimensional and camber tolerances, marking, and the heat-analysis and tension-test rules that A36 refers to. A36 does not itself contain the W-shape size tables.
A mill may also certify A36 on a non-W shape (S, C, MC, L or a metric H), or roll a W-shape to a different material specification, if that combination is in its programme and is fully documented. Do not treat “A36 beam” as if it automatically meant a W12×50, and do not substitute EN 10025-2 S355JR HEA/HEB/IPE sizes or GB/T 11263 HW/HM/HN sizes by matching a nominal 12 in or 300 mm depth.
A36 W-Shape Sizes and Reference Dimensions
The tables list nominal W-shape reference dimensions: designation, nominal depth, mass in lb/ft and kg/m, and actual depth, width, web thickness and flange thickness in both inch and millimetre units. There are 283 designations, grouped by depth so the tables stay readable. They are reference dimensions for identification and estimating, not a rolling list, and not a claim of guaranteed availability or that every W-shape is produced in A36. Dimensional acceptance, including shape and mass tolerances, follows the edition of ASTM A6/A6M named on the order. Mid-range W12 to W30 beams and the common W8–W14 column sizes are the usual enquiry core; the lightest W4–W6 rows, jumbo column sections, and the deepest W40–W44 rows should be confirmed size by size.
A designation such as W16×26 is a series call: the first number is the nominal depth in inches and the second is the nominal mass in pounds per foot. The actual depth of a W16×26 is slightly less than 16 in. That is normal, just as a European HEA 300 is 290 mm deep. Root radius is omitted because a single fillet radius is not published as a delivery dimension for these shapes, and a radius is not invented here.
Theoretical mass is the tabulated reference value. Settlement should follow the contract — tabulated theoretical mass or weighed mass — and the ordered A6 edition for mass tolerance. These W-shape rows are not interchangeable with HW, HM, HN or HEA/HEB/IPE rows of a similar nominal depth.
W4 to W10
The lighter W-shapes, often used as small beams, lintels and miscellaneous members. 41 designations in this group, from W4×13 to the W10 series.
Swipe horizontally to view all dimensions.
W12 and W14
The mid-depth column and beam group, including many of the heavier W12 and W14 column sections. 67 designations.
Swipe horizontally to view all dimensions.
W16 to W21
Common building-beam depths. 55 designations.
Swipe horizontally to view all dimensions.
W24 to W30
Deeper building and industrial beams. 54 designations.
Swipe horizontally to view all dimensions.
W33 to W44
The deepest W-shapes in these reference tables, through W44. 66 designations. Heavier and deeper rows should be confirmed size by size against the mill programme.
Swipe horizontally to view all dimensions.
Chinese HW/HM/HN sizes belong to GB/T 11263. European HEA/HEB/IPE sizes are listed on the S355JR H-beam page for that material system, not as A36 dimensions.
A36 Chemical Composition for Shapes (Heat Analysis)
The figures below are the heat-analysis limits for shapes in ASTM A36/A36M-19 Table 3, “All” thicknesses. They are not the plate columns of the same table, which split carbon, manganese and silicon by thickness and width. Where the table shows no manganese requirement, manganese still has to be determined and reported on the heat analysis under ASTM A6/A6M.
These limits are heat analysis. Product analysis, when required, follows the permitted variations in ASTM A6/A6M. Unofficial tables that copy a plate carbon of 0.25% or a plate phosphorus of 0.030% into a W-shape enquiry are using the wrong column.
A36 Mechanical Properties for Shapes
The tensile requirements below are from ASTM A36/A36M-19 Table 2. The shapes elongation column is used here, not the plates-and-bars column (which has a 23% minimum in 2 in). Tension-test orientation follows ASTM A6/A6M.
The 36 ksi [250 MPa] yield point applies to shapes at all listed thicknesses. Do not carry the plate-only 32 ksi reduction onto a W-shape certificate. Likewise, the ordinary 80 ksi tensile maximum is waived only for wide-flange shapes with flange thickness over 3 in [75 mm]; most catalogue W-shapes have thinner flanges than that, so the 58–80 ksi range still applies.
A36 does not specify a default Charpy test. If the project needs an impact value, the order should add S5 or, for the alternate core location on structural shapes, S30, and should state the test temperature and the absorbed-energy criterion. Those supplements are not implied by the grade name.
Delivery Conditions, Inspection and Identification
A36 shapes are commonly supplied in the as-rolled condition. The mill test report should show ASTM A36/A36M and its edition, the grade A36, the A6/A6M edition used for dimensions and general requirements, the W designation, the heat number, the heat analysis (including the reported manganese, even where no Mn range is specified), the tensile results, and any supplementary requirements that were ordered.
An EN 10204 type 3.1 document is the usual export request when the mill issues one against the ASTM test report; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification on the product follows ASTM A6/A6M marking practice: typically the designation, mill identification and heat or piece reference.
Length is not fixed by the W-shape table. US mills commonly roll these sections in imperial fixed lengths; export lengths in the region of 6–15 m or other agreed lengths are a matter for the rolling programme and the order.
Weldability and Surface Condition of A36 W-Shapes
A36 is a weldable carbon structural steel when thickness, joint design and hydrogen control are taken into account. The specification itself points the purchaser to a suitable welding procedure. Because A36 does not set a carbon-equivalent maximum for shapes, the actual heat carbon and the reported manganese, together with a procedure suited to the thickness, are the practical controls. This page does not prescribe a procedure or a preheat chart.
The as-rolled surface is mill scale. A blast class, a paint system, or a hot-dip galvanizing chemistry is an order option, not something implied by the grade name. If galvanizing is planned, the silicon on the heat and the processor’s coating specification should be reviewed before production. Surface quality follows ASTM A6/A6M; special finish requirements belong in the enquiry.
Cutting to length, weld-end preparation, forming or coating can be reviewed when the specification is sent with the enquiry. They are not assumed for every size.
ASTM A6/A6M Shape Tolerances and Theoretical Mass
Dimensional, straightness, camber, sweep, out-of-square and mass tolerances for these W-shapes are those of ASTM A6/A6M, not of ASTM A36/A36M. This article does not reproduce the A6 tolerance tables; acceptance is against the edition named on the order.
The size tables above are nominal W-shape reference dimensions. A delivered W16×26 will measure close to the tabulated depth, width and thicknesses within the tolerances of the ordered ASTM A6/A6M edition, not as a set of exact advertised inches. Flange out-of-square and web off-centre matter for end-plate connections.
The lb/ft and kg/m columns are published theoretical masses. Weighed mass may sit above or below those figures and still be within the A6 mass tolerance. Settlement should follow the contract.
Applications and Service Limits
A36 wide-flange beams are used where a 36 ksi [250 MPa] carbon steel W-shape is accepted:
- General building and industrial frames, platforms, skids and miscellaneous fabrication.
- Members that the specification actually names as A36, rather than A572 Grade 50 or A992.
- Export packages that compare the grade with Q235B or S235JR, provided each line keeps its own standard and shape system.
It is not specified here for pressure equipment, for nuclear safety-related components, or for structures whose specification requires a 50 ksi grade or a mandatory impact test that has not been added as a supplementary requirement. Durability comes from the coating or fire-protection system, not from the grade name. Weathering or marine exposure needs an agreed protection system, not bare A36.
A36 Compared with A572 Grade 50, A992, Q235B and S235JR
A36, A572 Grade 50 and A992 can all be rolled as the same W-shape series under ASTM A6/A6M, but they are different material specifications. A572 Grade 50 is a 50 ksi (345 MPa) high-strength low-alloy grade. A992 is the usual modern grade for US building W-shapes, with its own tensile window and chemistry. An enquiry that says only “W-beam” is incomplete.
Q235B under GB/T 700, rolled as HW/HM/HN to GB/T 11263, is a 235 MPa carbon steel with a 27 J impact requirement at +20 °C. S235JR in the EN 10025-2 beam family is a 235 MPa European grade, usually supplied as HEA, HEB or IPE. Dual certification is possible only when the delivered piece meets every requirement of each named standard, including chemistry, tests, dimensions and tolerances.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or a mill certificate. Where a project allows an alternative, the substitution should be written into the order and verified on the test report.
Sister beam pages in this series (A572 Grade 50, A992, Q235B, S235JR) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page when a European 355 MPa comparison is needed.
Sourcing A36 Wide Flange Beams from SHH STEEL
SHH STEEL supplies ASTM A36 wide-flange beams as an export trading house, coordinating mill production and project procurement. The useful part of that model is to align the material edition (ASTM A36/A36M), the shape standard (ASTM A6/A6M), the exact W designation, any supplementary requirements such as S5 or S30, and the form of the test report before a rolling or allocation programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every W-shape in A36. Mid-range beams and common column sizes are the usual core; jumbo and very deep sections are confirmed per line. Mixed procurement can be used when a take-off spans more than one rolling programme.
The same enquiry can also cover Chinese, European or Japanese designations, provided each line states its material standard, shape standard and size. If cutting, weld-end preparation, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
A36 Wide Flange Beam FAQs
-
Can I replace a W-shape with an HEA, HEB or HW of the same nominal depth?
- No. W-shapes follow ASTM A6/A6M. HEA/HEB/IPE and HW/HM/HN are different series, with different widths, flange thicknesses, masses and tolerance standards. A W12 is not an HEA 300, an HEB 300 or an HW 300×300. Select the section from the standard named on the drawing, or obtain a formal design change.
-
Does A36 have a 32 ksi yield for thick flanges?
- No. The 32 ksi [220 MPa] yield reduction in ASTM A36/A36M is for plates over 8 in [200 mm] thick. Shapes keep the 36 ksi [250 MPa] minimum. What does change for wide-flange shapes with flange thickness over 3 in [75 mm] is the tensile maximum (the 80 ksi cap does not apply) and the 2 in elongation (19% minimum), together with the manganese and silicon footnotes in Table 3.
-
Is an impact test included with A36?
- Not by default. Charpy testing is added only when the order specifies a supplementary requirement — S5, or S30 for the alternate core location on structural shapes — and states the test temperature and acceptance value.
-
Is A36 the same as A992 or A572 Grade 50?
- No. All three may be rolled as W-shapes, but A572 Grade 50 is a 50 ksi high-strength low-alloy grade and A992 is the usual modern grade for US building W-shapes, with its own chemistry and tensile window. They are not silent substitutes for A36, and A36 is not a silent substitute for them.
-
Which standards should appear on the mill test report?
- At least ASTM A36/A36M and its edition, the grade A36, the ASTM A6/A6M edition used for dimensions and general requirements, the W designation, the heat analysis (including reported manganese), the tensile results, and any supplementary requirements such as S5 or S30 that were ordered.
Request a Quotation for ASTM A36 Wide Flange H Beam
ASTM A36 wide-flange beam is a carbon structural W-shape with 36 ksi [250 MPa] minimum yield and a 58–80 ksi [400–550 MPa] tensile range for ordinary thicknesses. Nominate the W designation to ASTM A6/A6M, and name ASTM A36/A36M (or the edition on the order) as the material specification. Add S5 or S30 only if an impact test is required. The tables are nominal W-shape reference dimensions, not a rolling list and not a claim of guaranteed availability. Dimensional acceptance follows the ordered edition of ASTM A6/A6M. Send the size list, edition, any supplements and processing notes; SHH STEEL will review the package and quote accordingly.