ASTM B265 Grade 2H Titanium Plate | Grade 2 High Strength (UNS R50400)

ASTM B265 Grade 2H titanium plate is Grade 2 high strength titanium (UNS R50400) supplied annealed. It is specified for 400 MPa minimum tensile strength, 275–450 MPa yield and 20% minimum elongation. Typical uses include pressure vessel shells and heads in chloride service. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
ASTM B265 Grade 2H titanium plate, Grade 2H titanium plate, UNS R50400 plate, Grade 2 high strength titanium plate, ASTM B265 titanium sheet
Equivalent Grades:
UNS R50400, ASME SB-265 Gr.2H
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM B265 Grade 2H titanium plate?

ASTM B265 Grade 2H titanium plate is made to ASTM B265, the ASTM specification for titanium and titanium alloy strip, sheet and plate. It carries the UNS number R50400. Grade 2H has the same chemistry and yield range as Grade 2 but guarantees 58 ksi (400 MPa) minimum tensile strength. The H grades were introduced mainly for pressure vessel design, where the higher guaranteed tensile can support higher design values under the applicable code.

Commercially pure titanium gets its strength from controlled interstitial levels, mainly oxygen and iron, rather than from alloying additions. It has an alpha (hexagonal) structure, cannot be hardened by heat treatment, and is normally used in the annealed condition. A stable, self-healing oxide film gives excellent resistance to seawater, brines, wet chlorine and many oxidizing acids.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

ASTM B265 groups its grades into unalloyed titanium, corrosion-resistant grades with small additions of palladium, ruthenium, nickel or molybdenum, and structural alloys such as Ti-3Al-2.5V and Ti-6Al-4V. Each grade has its own UNS number, and the H grades add a higher guaranteed tensile strength for pressure vessel use.

SHH STEEL handles Grade 2H plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ASTM B265 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASME SB-265 Grade 2H, ASTM B265 Grade 2, ASME SB-265 Grade 2.

Material specification for ASTM B265 Grade 2H

ASTM B265 classifies flat titanium products by thickness and width. The same chemistry and tensile requirements apply to strip, sheet and plate, but dimensional tolerances and bend testing differ by product form.

Ordering item ASTM B265 basis
Standard ASTM B265, Titanium and Titanium Alloy Strip, Sheet, and Plate; state the edition on the order
Grade / UNS Grade 2H, Grade 2 High Strength, UNS R50400
Plate Over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide
Sheet 0.187 in (4.75 mm) and under, 24 in (610 mm) wide or more; state cold or hot rolled
Strip 0.187 in (4.75 mm) and under, less than 24 in (610 mm) wide
Condition Annealed
Certificate Manufacturer’s report with chemical analysis, tensile results and other required tests

Order information listed by the specification includes grade, product limitations, special mechanical properties, marking, finish, packaging, any additional reports and the disposition of rejected material. For ASME Code construction, order to ASME SB-265 Grade 2H and state any dual certification on the purchase order.

Chemical composition of ASTM B265 Grade 2H (UNS R50400)

Single values are maximums; ranges are shown where an element is added. Titanium is determined by difference. Product analysis tolerances cover variation between laboratories and do not broaden the heat analysis limits.

Element Heat analysis, % Permissible variation in product analysis, %
Nitrogen (N) 0.03 +0.02
Carbon (C) 0.08 +0.02
Hydrogen (H) 0.015 +0.002
Iron (Fe) 0.30 +0.15
Oxygen (O) 0.25 +0.03
Other elements, each 0.1 +0.02
Other elements, total 0.4 —
Titanium (Ti) Balance —

Ingot top and bottom are analysed for the listed elements. Hydrogen is tested and reported on at least one final product sample, and a lower hydrogen limit may be negotiated. Other elements need not be reported unless they exceed 0.10% each or 0.40% total, and they may not be added intentionally.

Mechanical properties of ASTM B265 Grade 2H

The values below are the requirements for Grade 2H plate in the annealed condition.

Property Requirement
Tensile strength, min 58 ksi (400 MPa)
Yield strength, 0.2% offset 40–65 ksi (275–450 MPa)
Elongation in 2 in or 50 mm, min 20%
Bend test, under 0.070 in (1.8 mm) Mandrel radius 2T, bent 105° without outside fracture
Bend test, 0.070–0.187 in (1.8–4.75 mm) Mandrel radius 2.5T
Bend test, over 0.187 in (4.75 mm) Not applicable to material over 4.75 mm

Tensile tests are made at room temperature. The yield range has an upper limit as well as a lower one. That cap protects formability, so a plate with very high yield can fail the grade even if it is strong. Bend tests apply to sheet and strip up to 0.187 in (4.75 mm); plate over that thickness is not bend tested under the specification.

Elevated-temperature design values are not part of the plate specification. They come from the design code, such as ASME Section II, Part D where the grade is listed.

Delivery condition, finish and marking

ASTM B265 covers material in the annealed condition. Plate must be free of injurious external and internal imperfections. Annealed product may be furnished descaled, sandblasted, ground, or sandblasted and ground; state the finish on the order.

  • Condition: Annealed
  • Surface: descaled, sandblasted or ground, as ordered; minor spot grinding is permitted within the thickness tolerance
  • Marking: specification, grade, heat number, manufacturer’s identification and nominal thickness, in rows that can be removed with hot alkaline cleaning
  • Packaging: boxed, crated, boarded or as the manufacturer’s standard practice unless the order states otherwise

CP titanium is supplied annealed; it is not strengthened by heat treatment, and stress relieving after heavy forming or welding is agreed case by case. If the plate will be formed or welded in your shop, say so at enquiry so the finish and protective packing suit the next process.

Welding and fabrication of Grade 2H titanium plate

Grade 2H is readily weldable by gas tungsten arc, plasma arc and other inert-gas processes. The key condition is shielding: hot titanium picks up oxygen, nitrogen and hydrogen from air, and that contamination embrittles the weld and heat-affected zone.

  • Use trailing shields and back purging so the weld and heat-affected zone stay protected until they cool below about 400 °C
  • Keep joints, filler wire and gloves clean and free of oil, moisture and iron contamination
  • Use matching CP filler metal unless the design engineer specifies otherwise
  • Use weld colour as a quick check of shielding quality, and reject heavily discoloured welds
  • Avoid contact with carbon steel tools during cutting and forming to prevent iron pick-up

Cold forming is practical for the CP grades, with bend radii that increase as oxygen and strength rise. Springback is higher than for stainless steel, so allow for it in tooling.

For machining, use sharp carbide or high-speed steel tools, low cutting speeds, heavy feeds and plenty of coolant. CP titanium is gummy rather than hard, so dull tools cause galling and smeared surfaces. Keep chips clean and separated from other metals, and do not let fine chips accumulate, because titanium fines can ignite.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

Dimensional tolerances are set in the specification’s tables for thickness, width, length, weight and flatness. Plate flatness has its own table for annealed plate. For sheet, cold-rolled tolerances apply unless hot-rolled sheet is ordered.

State the nominal thickness, width, length, quantity and any cutting drawing at enquiry. If a project needs tighter flatness, a specific edge condition or cut-to-size pieces, write it on the order rather than relying on the default tables. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Grade 2H titanium plate

Typical uses of Grade 2H plate include:

  • Pressure vessel shells and heads in chloride service
  • Heat exchanger tube sheets and channel covers
  • Desalination and seawater cooling equipment
  • Chemical process columns where Grade 2 corrosion behaviour is needed with higher guaranteed tensile

Plate certified as Grade 2H may also be certified as Grade 2, but Grade 2 plate cannot be assumed to meet 2H. Unalloyed titanium is not recommended in hydrofluoric acid or fluoride-bearing media, hot reducing acids such as concentrated hydrochloric or sulfuric acid, dry chlorine gas, or red fuming nitric acid. In hot, acidic brines where crevice corrosion is a risk, Pd-, Ru- or Ni-Mo-bearing grades are often considered instead. The design engineer must confirm suitability for the actual medium and temperature.

When selecting Grade 2H, compare it with Grade 1, Grade 2, Grade 3. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Grade 2H with other ASTM B265 grades

The grades below are the closest neighbours of Grade 2H in ASTM B265. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Grade 1 (R50250) 35 ksi (240 MPa) 20–45 ksi (138–310 MPa) 24% Best formability, lowest strength
Grade 2 (R50400) 50 ksi (345 MPa) 40–65 ksi (275–450 MPa) 20% General process equipment
Grade 2H (R50400) 58 ksi (400 MPa) 40–65 ksi (275–450 MPa) 20% Grade 2 with higher guaranteed tensile
Grade 3 (R50550) 65 ksi (450 MPa) 55–80 ksi (380–550 MPa) 18% Higher strength, less formable
Grade 4 (R50700) 80 ksi (550 MPa) 70–95 ksi (483–655 MPa) 15% Highest-strength CP grade

A higher-strength CP grade is not an automatic upgrade. It reduces formability and may change bend radii and welding practice, so a grade change needs engineer approval.

ASTM B265 Grade 2H equivalent grades

The designations below are commonly compared with ASTM B265 Grade 2H. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to ASTM B265 Grade 2H
ASME SB-265 Grade 2H ASME Code adoption of B265; ordered for pressure equipment
ASTM B265 Grade 2 Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified
ASME SB-265 Grade 2 Base grade: same chemistry, lower minimum tensile strength; H material may be dual certified
JIS H4600 Class 2 (TP340) Nearest by role only; composition and properties differ
GB/T 3621 TA2G Nearest by role only; composition and properties differ
UNS R50400 Same unified number; the H suffix is a tensile requirement, not a separate UNS

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Grade 2H titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to the ASTM B265 edition, grade and product form you name, and keep B265 and SB-265 requirements distinct
  • Certificates are checked against the Grade 2H chemistry and tensile limits, including the yield upper limit
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for ASTM B265 Grade 2H plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material ASTM B265 Grade 2H (UNS R50400), edition; add ASME SB-265 if Code use
Product form Plate, sheet or strip; for sheet, cold or hot rolled
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Any special mechanical properties, extra analysis or reports
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Is ASTM B265 Grade 2H the same as ASME SB-265 Grade 2H?
SB-265 is the ASME Code adoption of B265, so Grade 2H requirements normally match. They are separate documents, and ASME may adopt a different edition. For Code work, order SB-265 Grade 2H or dual certification.
What is the tensile strength of ASTM B265 Grade 2H titanium plate?
The requirement is 58 ksi (400 MPa) minimum. The 0.2% proof or yield strength is 40–65 ksi (275–450 MPa). Minimum elongation is 20%. Values apply to the condition and thickness range stated in the standard.
What is Grade 2H mainly used for?
Typical uses include pressure vessel shells and heads in chloride service, heat exchanger tube sheets and channel covers and desalination and seawater cooling equipment. Plate certified as Grade 2H may also be certified as Grade 2, but Grade 2 plate cannot be assumed to meet 2H.
When is a titanium product classed as plate under B265?
Plate is over 0.187 in (4.75 mm) thick and over 10 in (254 mm) wide. Thinner product is sheet if 24 in (610 mm) wide or more, otherwise strip.
What should I send for a quotation?
Send ASTM B265 Grade 2H, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination. Add ASME SB-265 if the plate is for Code construction.

Request a quotation for ASTM B265 Grade 2H titanium plate

ASTM B265 Grade 2H is Grade 2 high strength titanium, UNS R50400, specified for 58 ksi (400 MPa) minimum tensile strength, 40–65 ksi (275–450 MPa) yield or proof strength and 20% minimum elongation in the annealed condition. Typical uses include pressure vessel shells and heads in chloride service and heat exchanger tube sheets and channel covers.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ASTM B265 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *