ASME SA-36 Equal and Unequal Steel Angles
What is ASME SA-36 Steel Angle?
ASME SA-36 steel angle is a hot-rolled equal-leg or unequal-leg L-shape furnished to the ASME specification SA-36/SA-36M, Carbon Structural Steel. In ASME BPVC Section II, Part A, 2023 edition, SA-36/SA-36M is printed as identical with ASTM A36/A36M-19. The Code edition named on the purchase order is the one that governs acceptance, not a later ASTM year taken on its own.
SHH STEEL supplies these angles for orders that actually name SA-36/SA-36M, the A6/A6M L designation, and the certificate data required for that edition. This page is written for the angle. It is not a data sheet for ASME SA-36 steel plate, for A36 wide-flange beams, or for a channel, and it is not a substitute for the ASTM A36 steel angle page when the order only asks for ASTM A36.
Equal angles have both legs the same length, for example L 4×4×1/2 or L 8×8×1. Unequal angles have a longer and a shorter leg, for example L 5×3×3/8 or L 8×6×1. The third number is the thickness of both legs. The designation is the A6/A6M L-shape, not a bar of the same thickness cut from plate, and not a metric angle that merely looks similar.
The specification’s own scope covers carbon steel shapes, plates and bars of structural quality for riveted, bolted or welded construction of bridges and buildings, and for general structural purposes. These angles are filed under ASME SA-36 in the steel angle profiles category of steel structural profiles. The same specification in plate form is listed separately as ASME SA36 Steel Plate. Do not use the plate page as an angle data sheet.
This page covers Equal and Unequal Steel Angles in ASME SA-36/SA-36M. The Equal Leg Steel Angles and Unequal Leg Steel Angles follow the ASTM A6/A6M L series; the material specification does not by itself define the dimensions.
Code Edition, Certification and What SA-36 Is Not
Ordering “SA-36” means ordering the ASME adopted specification as it appears in Section II, Part A of a named Boiler and Pressure Vessel Code edition. This article follows the 2023 Section II, Part A text, which states that SA-36/SA-36M is identical with ASTM A36/A36M-19. If the construction project is under a different Code year, the SA-36 text in that year’s Section II, Part A is the one that applies. A later ASTM A36 revision is not, by itself, the SA specification in a 2023 book.
An ordinary ASTM A36 certificate does not make the piece SA-36. Material made and documented only to ASTM A36/A36M can be used where the contract calls for A36; it is not SA-36 until it is produced and certified to SA-36/SA-36M as adopted in the named Code edition. Dual marking or a combined A36/SA-36 certificate is legitimate only when every requirement of each named specification is met and the inspection document actually says so. The names are not interchangeable, and a shop should not restamp A36 as SA-36 after the fact.
Listing in Section II, Part A makes the specification available for use where a construction Code — for example Section I, Section III or Section VIII, as the project requires — permits SA-36 for the part in question. That listing is not a blanket approval for every pressure part, every temperature, or every service. SA-36 is a carbon structural steel specification. It is not a pressure-vessel plate specification such as SA-516, and it is not a nuclear-safety default material. Whether an SA-36 angle may be used around a vessel, in a support, or in any other Code-stamped item is decided by the applicable construction Code, the part, the design temperature and the permitted material tables — not by this product page.
The steel shall be killed. Supplementary requirements printed with SA-36/SA-36M — S5 Charpy V-notch, S30 Charpy V-notch for structural shapes with alternate core location, and S32 single-heat bundles — apply only when they are named on the order. They are not default tests for every SA-36 angle.
Material, Dimensions and Tolerances for SA-36 Angles
Keep the material specification and the dimensional standard distinct on the enquiry and on the certificate:
ASME SA-36/SA-36M is the material specification. Chemistry and tensile values on this page are the shapes requirements from SA-36/SA-36M as printed in ASME BPVC Section II, Part A, 2023, identical with ASTM A36/A36M-19. The Code edition named on the order governs material acceptance.
ASTM A6/A6M is the general-requirements and dimensional standard for these rolled L-shapes: dimensions, mass, residual processing of coil (where that route is used), product-analysis tolerances, tension-test orientation, marking and the ordinary shape tolerances. The edition of A6/A6M named on the order governs dimensional acceptance. The size tables below are the standard equal-leg and unequal-leg L series used as a reference; they are not a mill rolling list and not an ASME stock list.
A documented special combination — for example SA-36 on an EN 10056 leg size — is valid only if every requirement of each named standard is met and the certificate identifies both. Matching a nominal 100 mm or 4 in leg is not a substitution method. For an order that only names ASTM A36, use the ASTM A36 steel angle page instead of this one.
ASME SA-36 Equal Leg Steel Angles
The tables below are the standard ASTM A6/A6M equal-leg L series: designation, both leg lengths, thickness and theoretical mass, in inch-pound and SI units. SA-36/SA-36M does not publish a size list of its own. Use the figures to identify a designation and to estimate mass, not as a rolling programme and not as a warehouse list of ASME-certified lengths.
An equal angle has both legs the same length, for example L 4×4×1/2 or L 8×8×1. The third number is the thickness of both legs. Customary fractions are kept, so L 2-1/2×2-1/2×3/16 is not rewritten as a rounded decimal size. Mid-range L 3 to L 8 sizes are the usual enquiry core; 12 in legs and the heaviest 1 in or 1-3/8 in thicknesses should be confirmed line by line, together with the SA-36 certificate and the Code edition named on the order.
Equal-leg angles (61 sizes, L 2×2×1/8 to L 12×12×1-3/8)
L 2 to L 4 equal (28 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 equal (16 sizes)
Swipe horizontally to view all dimensions.
L 8 to L 12 equal (17 sizes)
Swipe horizontally to view all dimensions.
ASME SA-36 Unequal Leg Steel Angles
The tables below are the standard ASTM A6/A6M unequal-leg L series. The longer leg is listed first. L 8×6×1 is an 8 in by 6 in angle, 1 in thick; it is not L 8×8×1, and it is not a European or Chinese unequal angle that happens to have a similar millimetre size. SA-36/SA-36M again supplies the material requirements, not the dimensions.
These rows are reference dimensions and theoretical masses. They are not a list of lengths waiting in a yard under an SA-36 certificate. If the order needs a size outside the tabulated series, that has to be agreed as a special combination and certified accordingly.
Unequal-leg angles (76 sizes, L 2-1/2×1-1/2×3/16 to L 8×6×1)
L 2½ to L 4 unequal (35 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 unequal (22 sizes)
Swipe horizontally to view all dimensions.
L 7 to L 8 unequal (19 sizes)
Swipe horizontally to view all dimensions.
The 137 rows above are the standard equal and unequal L series used for this page. Other special-bar-size or non-standard angles can be reviewed when they are named on the enquiry; they are not invented here. European, Chinese or Japanese angle designations belong to their own dimensional standards, not to these L rows.
SA-36 Chemical Composition for Angles (Shapes Column)
The figures below are heat-analysis limits for SA-36 shapes from Table 3 of SA-36/SA-36M as printed in ASME BPVC Section II, Part A, 2023 (identical with ASTM A36/A36M-19). They are the shapes column for all thicknesses, not a plate-width column, and they are limits, not typical heat results. Product analysis shall conform to the same Table 3 limits, subject to the numeric permitted variations below, taken from Table A of ASTM A6/A6M-19, the general-requirements edition identified with A36/A36M-19 and with this SA-36/SA-36M printing. The A6/A6M edition named on the order governs. Where Table A shows no under-minimum or over-maximum figure, none is applied on this page.
The following product-analysis variations apply to the shapes-column heat-analysis limits above. Manganese has no specified heat-analysis requirement in that column, so no manganese product-analysis limit is invented here.
Do not copy a plate-width chemistry column onto an angle. The plate columns in the same table use different carbon, manganese, phosphorus, sulfur and silicon limits, and they are written for plates, not for L-shapes.
SA-36 Angle Mechanical Properties: Yield, Tensile and Elongation
Tensile properties of SA-36 angles follow the shapes requirements in Table 2 of SA-36/SA-36M as printed in ASME BPVC Section II, Part A, 2023 (identical with ASTM A36/A36M-19), not the plates-and-bars elongation column. The 32 ksi [220 MPa] yield that applies to plates over 8 in does not apply to these sections. The footnote that removes the 80 ksi tensile maximum and lowers the 2 in elongation to 19% applies only to wide-flange shapes with flange thickness over 3 in, not to L-shapes.
For shapes with a cross-sectional area less than 1 in² [645 mm²], clause 8.2 of the specification provides that the manufacturer need not tension-test the product if the chemistry used is appropriate for obtaining the tensile properties in Table 2. In the standard L series, that area is below 1 in² for these eight sizes: L 2×2×1/8, L 2×2×3/16, L 2×2×1/4, L 2-1/2×1-1/2×3/16, L 2-1/2×1-1/2×1/4, L 2-1/2×2×3/16, L 2-1/2×2-1/2×3/16 and L 3×2×3/16. Larger angles in the tables remain subject to the ordinary tensile test. The rule does not replace Table 2, and this page does not invent a substitute test method.
Charpy V-notch testing is not a default SA-36 requirement. S5 or S30 applies only when it is named on the order. Bearing-plate rules in Section 5 of the specification concern plates, not these L-shapes.
Delivery, Inspection and Identification of SA-36 Angles
SA-36 angles are commonly supplied as-rolled. The inspection document should identify ASME SA-36/SA-36M and the Code edition when the order requires it, the A6/A6M L designation, the heat number, the heat analysis (including reported manganese), and the tensile results where a test is required. If copper steel, a Charpy supplementary, single-heat bundling, or a particular A6/A6M finish is required, that must appear on the order and on the certificate.
An ASTM A36-only mill certificate is not an SA-36 document, even when the chemistry and tensile figures would have satisfied A36-19. An SA-36 plate certificate, or a certificate for an SA-36 W-shape or channel, does not by itself identify an L-shape. An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification or the construction Code requires it. Identification follows the mill’s marking practice under A6/A6M and the SA specification. Length is a matter for the rolling programme and the order, often in the region of 20–40 ft or 6–12 m; those lengths are enquiry ranges, not a stock list.
Weldability and Surface Condition of SA-36 Angles
SA-36 is a weldable carbon structural steel when thickness, joint design and hydrogen control are taken into account. The specification points to Appendix X3 of A6/A6M for weldability information and requires a welding procedure suitable for the grade and the intended use or service. It does not table a carbon-equivalent limit for the grade. Procedure should be set from the certificate analysis and the applicable welding specification, not from an invented CEV figure. This page does not prescribe a procedure or a preheat chart.
Fillet welds along both legs, and connections at the heel of an unequal angle, need the detailing that the design actually requires. The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size, and they do not turn an A36 bar or plate offcut into an SA-36 angle.
A6/A6M Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these L-shapes are those of ASTM A6/A6M, not of SA-36/SA-36M itself. This article does not reproduce the inch or millimetre tolerance tables; acceptance is against the edition of A6/A6M named on the order. A delivered L 4×4×1/2 will measure close to the tabulated legs and thickness within those tolerances, not as a set of exact advertised inches. Out-of-square at the heel and variation of the two legs matter for connections. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
SA-36 steel angles are used where the specification names this carbon structural grade as an equal or unequal L-shape, and where the purchaser needs the material certified to the ASME adopted specification:
Bracing, frames, lintels, clips, ledgers, walkway supports and general fabrications whose purchase order names SA-36/SA-36M rather than ASTM A36 alone, or rather than a higher-strength grade such as ASTM A572 Grade 50 steel angle.
Supporting or attached steel around Code-stamped equipment, but only when the applicable construction Code actually permits SA-36 for that part. This page does not confer that permission, and it does not treat SA-36 angle as a universal pressure-vessel or boiler material.
It is not specified here as a substitute for SA-516 or other pressure-vessel quality plates, for nuclear safety-related components unless the construction Code and the contract expressly accept SA-36 for that use, or for members that actually require a 50 ksi yield or a tabulated impact test. Durability comes from the coating or fire-protection system named on the order, not from the SA-36 designation itself.
SA-36 Angle Compared with A36 Angle, SA-36 Plate and Grade 50
ASTM A36 steel angle uses the same shapes chemistry column and the same 36 ksi yield and 58–80 ksi tensile figures in A36/A36M-19, and it can use the same A6/A6M L series. That overlap does not turn an A36-only delivery into SA-36. The ASME certificate, and the Code edition when it is required, are the difference this page is written to protect.
ASME SA-36 steel plate is the same material specification in a different product form, with plate-width chemistry columns and plate elongation rules that must not be copied onto an L-shape. A36 wide-flange beams likewise share the 36 ksi yield, but they are W-shapes, not angles, and the thick-flange tensile footnote in Table 2 applies to those W-shapes, not to the L series.
An A572 Grade 50 angle can use the same L series at a higher yield and with a different chemistry table. It is not an SA-36 certificate, and SA-36 is not a substitute when the order requires 50 ksi.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade, one certificate or one shape for another on a contract or an inspection document.
Published sister pages for the comparison grades in angle form include GB/T 706 Q235B, JIS G 3101 SS400 and EN 10025-2 S235JR. Use those pages for their own standards; do not treat them as SA-36 equivalents.
Stock and Supply of ASME SA-36 Steel Angles from SHH STEEL
SHH STEEL supplies ASME SA-36 equal-leg and unequal-leg steel angles as an export trading house, coordinating mill production and project procurement. The useful work on this product is to keep the SA specification and the ASTM A36 name from being treated as interchangeable, to keep equal and unequal designations from being mixed, to keep the eight small-area sizes under clause 8.2 from being assumed as ordinary mill tensile specimens, and to align the A6/A6M size, the Code edition and the inspection document before a rolling programme is committed.
Sizes, lengths and certificates are confirmed per enquiry. The tables on this page are the standard L series, not a list of pieces on the floor and not a claim that every tabulated size is available under an SA-36 certificate at short notice. Mid-range L 3 to L 8 sizes are the usual core; 12 in equal legs and the heaviest thicknesses are confirmed per line.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every equal or unequal L size, and an A36 rolling from any of them is not assumed to be SA-36. The order has to state SA-36/SA-36M and the certificate has to follow that specification.
The same enquiry can also cover plates, W-shapes, channels, or Chinese, Japanese or European designations, provided each line states its material standard, shape standard, size and, where it applies, the Code edition. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
SA-36 Steel Angle FAQs
-
Is an ASTM A36 angle automatically certified to ASME SA-36?
- No. In the 2023 Section II, Part A book, SA-36/SA-36M is identical with ASTM A36/A36M-19, so the shapes chemistry and tensile figures match that ASTM edition. That does not make an A36-only product into SA-36. The piece has to be certified to SA-36/SA-36M as adopted in the named Code edition. Dual marking is valid only when both named specifications are met and both appear on the inspection document.
-
Does a listing in ASME Section II mean these angles can be used in any pressure service?
- No. Section II, Part A publishes the material specification. The construction Code, the part, the design temperature and the permitted material tables decide whether an SA-36 angle may be used. SA-36 is a carbon structural steel specification, not a blanket pressure-vessel or nuclear-safety material, and it is not a substitute for SA-516 plate.
-
Can I use an SA-36 plate certificate for an angle?
- No. The plate page and an angle are different product forms. Plate chemistry columns and plate elongation rules in Table 2 and Table 3 are not the shapes requirements. The certificate must identify the L-shape actually supplied.
-
Is an equal angle interchangeable with an unequal angle of the same long-leg length?
- No. L 8×8 and L 8×6 are different sections. The short-leg length, the mass and the connection details are those of the designation that the specification actually names.
-
Which edition should appear on the inspection document?
- Name ASME SA-36/SA-36M and the Code edition required by the order — this article follows the 2023 Section II, Part A text, identical with ASTM A36/A36M-19 — together with the A6/A6M L designation, the heat number, heat analysis including reported manganese, and tensile results where a test is required. Any copper-steel or impact supplementary should also appear if it was ordered. A later ASTM A36 year on its own is not the SA specification in a 2023 book.
-
Which SA-36 angles may skip a mill tension test?
- Clause 8.2 allows the manufacturer not to tension-test shapes with a cross-sectional area less than 1 in² if the chemistry used is appropriate for Table 2. In the standard L series that applies to L 2×2×1/8, L 2×2×3/16, L 2×2×1/4, L 2-1/2×1-1/2×3/16, L 2-1/2×1-1/2×1/4, L 2-1/2×2×3/16, L 2-1/2×2-1/2×3/16 and L 3×2×3/16. Larger angles remain subject to the ordinary tensile test.
Request a Quotation for ASME SA-36 Steel Angle
ASME SA-36 steel angle is a carbon structural L-shape certified to SA-36/SA-36M as adopted in ASME Section II, Part A. This article follows the 2023 edition, which is identical with ASTM A36/A36M-19: 36 ksi [250 MPa] minimum yield and 58–80 ksi [400–550 MPa] tensile strength for shapes. Nominate the equal or unequal L size to ASTM A6/A6M, the material to SA-36/SA-36M, and the Code edition required by the project. An A36-only certificate is not enough. The tables are reference dimensions, not a rolling list. Send the designation list, Code edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.