ASTM A572 Grade 50 Equal and Unequal Steel Angles
What is ASTM A572 Grade 50 Steel Angle?
ASTM A572 Grade 50 steel angle is a hot-rolled equal-leg or unequal-leg L-shape in high-strength low-alloy structural steel Grade 50. The material standard is ASTM A572/A572M. Dimensions, mass and general requirements for the rolled section are those of ASTM A6/A6M. The 50 ksi [345 MPa] minimum yield is the same figure used for Grade 50 plates and for Grade 50 W-shapes, but this page is for the angle, not for a W-shape, a channel, or a plate.
Equal angles have both legs the same length, for example L 4×4×1/2 or L 8×8×1. Unequal angles have a longer and a shorter leg, for example L 5×3×3/8 or L 8×6×1. The third number is the thickness of both legs. An L 8×6 is not an L 8×8, and it is not a European or Chinese unequal angle of a similar millimetre size. Grade 50 can use the same L series as A36; the difference is the material, not a second set of designations.
These angles will be filed under an ASTM A572 steel angle term in the steel angle profiles category of steel structural profiles, once that term is created under parent 69. The same grade in plate form is listed separately as A572 Gr.50 structural steel plate. Do not use that plate page as an angle data sheet, and do not copy plate-width chemistry columns onto an L-shape certificate. The A572 channel category is ASTM A572 steel channel profiles; that category is not this product.
Grade 50 angles are used for bracing, frames, clips and general industrial work when the specification names this high-strength low-alloy grade in an L-shape. The grade is not a pressure-vessel or nuclear safety material, and an A36 angle certificate does not fulfil a Grade 50 order.
This page covers Equal and Unequal Steel Angles in ASTM A572 Grade 50. The Equal Leg Steel Angles and Unequal Leg Steel Angles follow the ASTM A6/A6M L series; the material standard does not by itself define the dimensions.
Material, Dimensions and Tolerances for A572 Grade 50 Angles
The order and the inspection certificate should keep material, dimensions and tolerances distinct:
- ASTM A572/A572M is the material standard. This article uses chemistry and tensile values for Grade 50 shapes from ASTM A572/A572M-21ε1. The edition named on the order governs acceptance.
- ASTM A6/A6M is the general-requirements and dimensional standard for these rolled angles. The size tables below are reference dimensions and theoretical masses for the standard equal-leg and unequal-leg L series, not a mill rolling list. The edition of A6/A6M named on the order governs dimensional acceptance.
Grade 50 steel shall be killed. Types 1, 2, 3 and 5 are the types listed for this grade; the type actually supplied should be the one named on the order or agreed with the mill. A documented special combination — for example Grade 50 on an EN 10056 angle, or an L-shape certified to a different material standard — is only valid if every requirement of each named standard is met.
ASTM A572 Grade 50 Equal Leg Steel Angles
The tables list designation, long-leg and short-leg lengths, thickness and theoretical mass, in inch-pound and SI units, for the standard L series under ASTM A6/A6M. The series is the same one used for A36 angles; Grade 50 does not invent a second size list. For equal angles the two legs are the same length. Use the tables to identify and estimate, not as a rolling programme for Grade 50. Mid-range L 3 to L 8 sizes are the usual enquiry core; the 12 in equal legs and the heaviest 1 in or 1-3/8 in thicknesses should be confirmed size by size.
L 4×4×1/2 is a 4 in equal angle, 1/2 in thick. L 8×6×1 is an 8 in by 6 in unequal angle, 1 in thick; it is not L 8×8×1. Designations keep the customary fractions, for example L 2-1/2×2-1/2×3/16. The heaviest tabulated thickness, 1.38 in, is still well below the 3 in flange or leg thickness at which the Grade 50 silicon rule changes.
Equal-leg angles (61 sizes, L 2×2×1/8 to L 12×12×1-3/8)
L 2 to L 4 equal (28 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 equal (16 sizes)
Swipe horizontally to view all dimensions.
L 8 to L 12 equal (17 sizes)
Swipe horizontally to view all dimensions.
ASTM A572 Grade 50 Unequal Leg Steel Angles
Unequal-leg angles (76 sizes, L 2-1/2×1-1/2×3/16 to L 8×6×1)
L 2½ to L 4 unequal (35 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 unequal (22 sizes)
Swipe horizontally to view all dimensions.
L 7 to L 8 unequal (19 sizes)
Swipe horizontally to view all dimensions.
The 137 rows above are the standard equal and unequal L series used for this page. Other special-bar-size or non-standard angles can be reviewed when they are named on the enquiry; they are not invented here. European, Chinese or Japanese angle designations belong to their own dimensional standards, not to these L rows.
A572 Grade 50 Chemical Composition for Angles
The figures below are heat-analysis limits for Grade 50 shapes from ASTM A572/A572M-21ε1. They apply to these L-shapes as structural shapes. They must not be copied from a plate-width column, and they are limits, not typical heat results.
A572 Grade 50 Angle Mechanical Properties
Tensile properties of Grade 50 angles follow the Grade 50 requirements in ASTM A572/A572M-21ε1. There is a 50 ksi [345 MPa] minimum yield and a 65 ksi [450 MPa] minimum tensile strength. The specification does not set a maximum yield for this grade. Those minima are higher than the A36 shapes table, and there is no 80 ksi tensile cap of the kind used for ordinary A36 shapes. The 19% elongation in 2 in that applies to wide-flange shapes over 426 lb/ft [634 kg/m] does not apply to these L-shapes. The small-area tension-test waiver in ASTM A36/A36M clause 8.2 is an A36 rule and is not reused here.
Charpy V-notch testing is not a default Grade 50 requirement. Supplementary requirements such as S5 or S30 apply only when they are named on the order. Do not treat Grade 50 as a weathering steel unless a weathering specification is also named.
Delivery Conditions, Inspection and Identification
A572 Grade 50 angles are commonly supplied as-rolled, in killed steel of the type agreed for the order. The inspection document should show ASTM A572/A572M and its edition, Grade 50, the type where it is required, the A6/A6M L designation, the heat number, the heat analysis, and the tensile results. If a Charpy supplementary or a particular A6/A6M finish is required, that must appear on the order and on the certificate. An A36 angle certificate, or a Grade 50 plate, W-shape or channel certificate, does not, by itself, identify these angles.
An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 20–40 ft or 6–12 m.
Weldability and Surface Condition of A572 Grade 50 Angles
Grade 50 is a weldable high-strength low-alloy structural steel when thickness, joint design and hydrogen control are taken into account. Procedure should be set from the certificate analysis, the type actually supplied, and the applicable welding specification. This page does not prescribe a procedure or a preheat chart, and it does not invent a carbon-equivalent limit that the specification does not table for these as-rolled angles. Fillet welds along both legs, and connections at the heel of an unequal angle, need the detailing that the design actually requires.
The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.
A6/A6M Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these L-shapes are those of ASTM A6/A6M, not of A572/A572M itself. This article does not reproduce the inch or millimetre tolerance tables; acceptance is against the edition named on the order.
A delivered L 4×4×1/2 will measure close to the tabulated legs and thickness within those tolerances, not as a set of exact advertised inches. Out-of-square at the heel and variation of the two legs matter for connections. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
A572 Grade 50 steel angles are used where a 50 ksi high-strength low-alloy grade and an equal or unequal L-shape are specified:
- Bracing, frames, clips, ledgers and general fabrications whose specification names Grade 50 angle rather than A36 or a non-American angle series.
- Export packages that compare the grade with Q355B or with S355JR, provided each line keeps its own material standard, toughness rule and shape system.
It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require a tabulated impact test or a weathering specification that has not been named. Durability comes from the coating or fire-protection system, not from the Grade 50 designation alone.
Grade 50 Angle Compared with A36, Plates and Q355B
An A36 angle can use the same L series at a 36 ksi yield and with a different chemistry table; it does not fulfil a Grade 50 requirement. A572 Gr.50 plate is the same grade in plate form, not an angle, and plate-width chemistry must not be used for these sections. Q355B and S355JR are useful 355 MPa-class comparisons only if chemistry, toughness and the shape standard are also satisfied.
Dual certification requires every requirement of each named standard to be met on the delivered piece. An A572 Grade 50 channel or W-beam page, and an A36 angle page, will be linked here once they are published; those product URLs are not pre-linked.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.
Sourcing A572 Grade 50 Steel Angles from SHH STEEL
SHH STEEL supplies A572 Grade 50 steel angles as an export trading house, coordinating mill production and project procurement. For this product the useful work is to keep Grade 50 from being fulfilled with an A36 certificate, to keep equal and unequal designations from being mixed, and to align type, killed-steel practice, A6/A6M size and the inspection document before a rolling programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every equal or unequal L size in Grade 50. Mid-range L 3 to L 8 sizes are the usual core; 12 in equal legs and the heaviest thicknesses are confirmed per line.
The same enquiry can also cover W-shapes, channels, or Chinese, Japanese or European designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
A572 Grade 50 Steel Angle FAQs
-
Can an A36 angle be supplied against an A572 Grade 50 angle order?
- No, not as a substitute. A36 and Grade 50 can share the same L designation, but Grade 50 has a 50 ksi minimum yield, a different chemistry table, and killed-steel practice. An A36 certificate does not fulfil a Grade 50 requirement.
-
Is an equal Grade 50 angle interchangeable with an unequal angle of the same long-leg length?
- No. L 8×8 and L 8×6 are different sections. The short-leg length, the mass and the connection details are those of the designation that the specification actually names.
-
Which phosphorus and sulfur limits apply to these angles?
- For structural shapes, including L-shapes, footnote I of the Grade 50 chemistry table allows 0.04% phosphorus and 0.05% sulfur, rather than the 0.030% figures that remain tabulated for other product forms.
-
Does the 3 in silicon rule apply to these angles?
- The official wording is 0.40% silicon maximum for shapes with flange or leg thickness 3 in and under. None of the standard L rows tabulated here has a thickness over 3 in; the heaviest tabulated thickness is 1.38 in, so the 0.40% maximum applies to this list.
-
Which standards should appear on the inspection document?
- At least ASTM A572/A572M and its edition, Grade 50, the type where it is required, the L designation to A6/A6M, the heat number, heat analysis, and tensile results. Any impact supplementary should also appear if it was ordered.
Request a Quotation for ASTM A572 Grade 50 Steel Angle
ASTM A572 Grade 50 steel angle is a high-strength low-alloy L-shape with 50 ksi [345 MPa] minimum yield. Nominate the equal or unequal L size to ASTM A6/A6M and the material to ASTM A572/A572M-21ε1 (or the edition on the order). The tables are reference dimensions, not a rolling list. Send the designation list, type, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.