JIS G 3101 SS400 Equal and Unequal Steel Angles | JIS G 3101 Steel Angles - SHH STEEL

JIS G 3101 SS400 Equal and Unequal Steel Angles

JIS G 3101 SS400 steel angle is a general-structure L-section named for a 400–510 N/mm² tensile range, not a 400 N/mm² yield. Minimum yield is 245 N/mm² up to 16 mm. Dimensions follow the JIS G 3192 angle series. The ordered edition governs. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.
Keywords
JIS G 3101 SS400 Steel Angle, SS400 equal angle, SS400 unequal angle, JIS G 3192 angle, general-structure angle
Equivalent Grades:
Near-equivalents only, not automatic substitutes: Q235B; S235JR; SM490A and SM490B belong to JIS G 3106 and are not SS400 certificates.
Share:
General Description
Material Specification
Available Sizes of JIS G 3101 SS400 Equal Leg Steel Angles
Available Sizes of JIS G 3101 SS400 Unequal Leg Steel Angles
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source SS400 Steel Angles from SHH STEEL
FAQ
Conclusion

What is JIS G 3101 SS400 Steel Angle?

JIS G 3101 SS400 steel angle is a hot-rolled L-section in rolled steel for general structure, grade SS400. The material standard is JIS G 3101. Dimensions, mass and tolerances for the section itself are those of JIS G 3192. The “400” in the grade name is the lower end of the specified tensile range (400–510 N/mm²). It is not a 400 N/mm² yield. Up to 16 mm, the minimum yield point or proof stress is 245 N/mm², and it steps down as the thickness at the test-piece location increases.

The designation is the leg and thickness string itself: A×A×t for equal-leg angles, A×B×t for unequal-leg angles, and A×B×t1×t2 for the unequal-leg unequal-thickness series — for example 75×75×9, 150×100×12 or 200×90×9×14. JIS G 3192 does not require an ASTM-style L prefix. A 75 mm Japanese equal angle is not a European EN 10056 L 75×75, an American L, or a Chinese GB/T 706 angle of similar millimetre size.

These angles are filed under JIS G3101 steel angle profiles in the steel angle profiles category of steel structural profiles. The same grade in plate form is listed separately as JIS G 3101 SS400 steel plate. Do not use that plate page as an angle data sheet, and do not copy a plate elongation-reduction rule onto an angle certificate. A Japanese channel or H-beam in SS400 is a different product, with its own designation and its own page when that page is published.

SS400 angles are used for building and general industrial framing when the specification names this Japanese general-structure grade. JIS G 3101 does not specify a Charpy test for SS400. The grade is not a pressure-vessel or nuclear safety material, and it is not a substitute for JIS G 3106 SM490 when a welded-structure grade and a defined impact quality are what the order requires.

This page covers Equal and Unequal Steel Angles in JIS G 3101 SS400. The Equal Leg Steel Angles (JIS G 3192 Table 8) and Unequal Leg Steel Angles (Tables 9 and 10) follow JIS G 3192; the material standard does not by itself define the dimensions.

Material, Dimensions and Tolerances for SS400 Angles

The order and the inspection certificate should keep material, dimensions and tolerances distinct:

  • JIS G 3101 is the material standard. This article uses heat-analysis and tensile values for SS400 from JIS G 3101:2024. The edition named on the order governs acceptance.
  • JIS G 3192 is the dimensional, mass and tolerance standard for these hot-rolled angles. The size tables below are the complete tabulated standard series in JIS G 3192:2024 Table 8 (equal-leg), Table 9 (unequal-leg) and Table 10 (unequal-leg unequal-thickness). The tabulated sizes are representative; other section dimensions may be used by agreement. The edition of JIS G 3192 named on the order governs dimensional and mass acceptance.

A documented special combination — for example SS400 on a European L, or a JIS angle certified to a different material standard — is only valid if every requirement of each named standard is met. Matching a nominal 75 mm or 3 in leg is not a substitution.

JIS G 3101 SS400 Equal Leg Steel Angles

The tables list the complete tabulated standard angle series in JIS G 3192:2024: Table 8 equal-leg angles, 40 sizes from 25×25×3 to 250×250×35; Table 9 unequal-leg angles, 13 sizes from 90×75×9 to 150×100×15; and Table 10 unequal-leg unequal-thickness angles, 7 sizes from 200×90×9×14 to 400×100×13×18. Each table carries footnote a: the listed sizes are representative, and sizes other than those listed are agreed between the purchaser and the supplier. Use the tables to identify and estimate, not as a rolling programme for SS400. Mid-range equal legs such as 75×75 and 100×100 are the usual enquiry core; the 25×25 and 30×30 families, the 250×250 rows, and the Table 10 series should be confirmed size by size.

Table 10 is a separate series and is not a subset of Table 9. Root and toe radii r1 and r2 are tabulated standard dimensions in these JIS series and are shown. Theoretical mass uses a density of 7.85 g/cm³. This page does not invent rows that Tables 8, 9 and 10 do not list.

75×75×9 has a 9 mm leg, so the 245 N/mm² yield band applies. 150×150×15 remains in that first band. 150×150×19 and 200×200×20 have 19 mm and 20 mm legs, so the minimum yield is 235 N/mm², not 245 N/mm². On Table 10 the usual thickness basis is the thicker leg t2. Annex JA of JIS G 3101 applies only to sections whose leg length is under 40 mm: in Table 8, only the 25×25 and 30×30 families. Review those bars against Annex JA in the edition named on the order; the numeric JA values are not restated here. Annex JA does not apply to the 40×40 family or to any Table 9 or Table 10 size.

Equal-leg angles — Table 8, 40 sizes

Swipe horizontally to view all dimensions.

Designation (A×A×t) A (mm) t (mm) r1 (mm) r2 (mm) Area (cm²) Mass (kg/m)
25×25×3 25 3 4 2 1.427 1.12
30×30×3 30 3 4 2 1.727 1.36
40×40×3 40 3 4.5 2 2.336 1.83
40×40×5 40 5 4.5 3 3.755 2.95
45×45×4 45 4 6.5 3 3.492 2.74
45×45×5 45 5 6.5 3 4.302 3.38
50×50×4 50 4 6.5 3 3.892 3.06
50×50×5 50 5 6.5 3 4.802 3.77
50×50×6 50 6 6.5 4.5 5.644 4.43
60×60×4 60 4 6.5 3 4.692 3.68
60×60×5 60 5 6.5 3 5.802 4.55
65×65×5 65 5 8.5 3 6.367 5.00
65×65×6 65 6 8.5 4 7.527 5.91
65×65×8 65 8 8.5 6 9.761 7.66
70×70×6 70 6 8.5 4 8.127 6.38
75×75×6 75 6 8.5 4 8.727 6.85
75×75×9 75 9 8.5 6 12.69 9.96
75×75×12 75 12 8.5 6 16.56 13.0
80×80×6 80 6 8.5 4 9.327 7.32
90×90×6 90 6 10 5 10.55 8.28
90×90×7 90 7 10 5 12.22 9.59
90×90×10 90 10 10 7 17.00 13.3
90×90×13 90 13 10 7 21.71 17.0
100×100×7 100 7 10 5 13.62 10.7
100×100×10 100 10 10 7 19.00 14.9
100×100×13 100 13 10 7 24.31 19.1
120×120×8 120 8 12 5 18.76 14.7
130×130×9 130 9 12 6 22.74 17.9
130×130×12 130 12 12 8.5 29.76 23.4
130×130×15 130 15 12 8.5 36.75 28.8
150×150×12 150 12 14 7 34.77 27.3
150×150×15 150 15 14 10 42.74 33.6
150×150×19 150 19 14 10 53.38 41.9
175×175×12 175 12 15 11 40.52 31.8
175×175×15 175 15 15 11 50.21 39.4
200×200×15 200 15 17 12 57.75 45.3
200×200×20 200 20 17 12 76.00 59.7
200×200×25 200 25 17 12 93.75 73.6
250×250×25 250 25 24 12 119.4 93.7
250×250×35 250 35 24 18 162.6 128

JIS G 3101 SS400 Unequal Leg Steel Angles

Unequal-leg angles — Table 9, 13 sizes

Swipe horizontally to view all dimensions.

Designation (A×B×t) A (mm) B (mm) t (mm) r1 (mm) r2 (mm) Area (cm²) Mass (kg/m)
90×75×9 90 75 9 8.5 6 14.04 11.0
100×75×7 100 75 7 10 5 11.87 9.32
100×75×10 100 75 10 10 7 16.50 13.0
125×75×7 125 75 7 10 5 13.62 10.7
125×75×10 125 75 10 10 7 19.00 14.9
125×75×13 125 75 13 10 7 24.31 19.1
125×90×10 125 90 10 10 7 20.50 16.1
125×90×13 125 90 13 10 7 26.26 20.6
150×90×9 150 90 9 12 6 20.94 16.4
150×90×12 150 90 12 12 8.5 27.36 21.5
150×100×9 150 100 9 12 6 21.84 17.1
150×100×12 150 100 12 12 8.5 28.56 22.4
150×100×15 150 100 15 12 8.5 35.25 27.7

Unequal-thickness angles — Table 10, 7 sizes

Swipe horizontally to view all dimensions.

Designation (A×B×t1×t2) A (mm) B (mm) t1 (mm) t2 (mm) r1 (mm) r2 (mm) Area (cm²) Mass (kg/m)
200×90×9×14 200 90 9 14 14 7 29.66 23.3
250×90×10×15 250 90 10 15 17 8.5 37.47 29.4
250×90×12×16 250 90 12 16 17 8.5 42.95 33.7
300×90×11×16 300 90 11 16 19 9.5 46.22 36.3
300×90×13×17 300 90 13 17 19 9.5 52.67 41.3
350×100×12×17 350 100 12 17 22 11 57.74 45.3
400×100×13×18 400 100 13 18 24 12 68.59 53.8

SS400 Chemical Composition for Angles (JIS G 3101 Heat Analysis)

SS400 on an angle is the same grade as SS400 on plate, but the certificate still has to identify the angle, not a plate heat that happens to share the name. JIS G 3101:2024, issued 20 February 2024, tabulates only phosphorus and sulphur maxima for SS400. It does not set carbon, silicon or manganese maxima for this grade, and it does not publish a carbon-equivalent cap. A mill may still report those elements on the inspection document; they are recorded values, not SS400 limits, unless the purchase order adds them. Elements shown as dashes, and elements not listed, may be added as necessary and shall be reported if they are.

Element Heat analysis, max (mass %) Notes for SS400 angles
C No tabulated maximum The carbon column for SS400 is a dash, not a zero-carbon requirement. Carbon and other unlisted elements may be added as necessary, and if they are added they shall be reported.
Mn No tabulated maximum The manganese column for SS400 is also a dash. Do not copy an SS540 manganese maximum (1.60%) onto an SS400 order.
Si Not a tabulated column JIS G 3101:2024 Table 2 does not list a silicon maximum for SS330, SS400 or SS490.
P 0.050 This is a heat-analysis maximum, not a typical result.
S 0.050 This is a heat-analysis maximum, not a typical result.

A deoxidation practice is not prescribed for SS400 angles. What the heat actually was — rimmed, killed or something in between — belongs on the certificate when it is reported. Do not assume a fully killed route from the grade letters alone.

SS400 Angle Mechanical Properties: Yield, Tensile, Elongation and Bend

Tensile properties of SS400 sections follow Table 3 of JIS G 3101:2024 (plates, strips, flats and sections). Thickness is that at the test-piece location. For these angles that thickness is ordinarily the leg thickness t, or the thicker leg t2 on the Table 10 series. Do not read the 245 N/mm² figure against the longer leg length, and do not treat a 16 mm rule written for plate as if it automatically described a 75 mm or 150 mm leg.

Thickness at the test-piece location (mm) Minimum yield point or proof stress (N/mm²) Tensile strength (N/mm²)
t ≤ 16 245 400–510
16 < t ≤ 40 235 400–510
40 < t ≤ 100 215 400–510
t > 100 205 400–510

The 205 N/mm² band is the standard’s fourth yield step. It applies only when the test-location thickness is over 100 mm, which none of the tabulated JIS G 3192 angle series reach. It is kept here so a heavier special bar is not read against the 215 N/mm² line by habit.

Elongation in SS400 depends on both thickness and the tensile-test piece. The first three tabulated rows use the No. 5 or No. 1A pieces named in the standard. The last row uses test piece No. 4. The further No. 4 reduction that applies when plate thickness exceeds 90 mm is a plate rule; it is not extended to these angles unless the ordered edition of JIS G 3101 is shown to apply that reduction to the section.

Thickness (mm) Test piece Minimum elongation (%)
t ≤ 5 No. 5 21
5 < t ≤ 16 No. 1A 17
16 < t ≤ 40 No. 1A 21
40 < t ≤ 50 No. 1A 21
t > 50 No. 4 23

SS400 is bent 180° around a pin of 1.5 t. The bend uses the same thickness basis as the tensile test. The bend test may be omitted unless the purchaser specifies it; the steel still has to satisfy the bendability requirement. The 2024 edition does not require a Charpy impact test for SS400, on angles or on any other product form. If a project specification calls for an impact test, that requirement has to be written into the order; it is not supplied by the grade name.

Delivery Conditions, Inspection and Identification

SS400 angles are commonly supplied as-rolled. The inspection document should show JIS G 3101 and its edition, the grade SS400, the JIS G 3192 size designation (A×A×t, A×B×t or A×B×t1×t2), the delivery condition, the heat number, the heat analysis (including any added elements), and the tensile results by thickness. If not otherwise specified at the time of order, the inspection document is a JIS G 0415 inspection certificate 3.1. A toughness result cannot be inferred from an SS400 certificate. A plate certificate, or an H-section or channel certificate, does not, by itself, identify an angle.

Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order.

Weldability and Surface Condition of SS400 Angles

SS400 is widely welded in general-structure work when thickness, joint design and hydrogen control are taken into account. Because the grade does not publish carbon or manganese maxima, the heat analysis on the certificate, rather than an assumed CEV table, is the practical starting point. This page does not prescribe a procedure or a preheat chart, and it does not invent a carbon-equivalent limit that JIS G 3101 does not table for SS400.

Cutting, punching, forming, blast, paint or galvanizing can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.

JIS G 3192 Shape Tolerances and Theoretical Mass

Dimensional, shape and mass tolerances for these angles are those of JIS G 3192, not of JIS G 3101. This article uses JIS G 3192:2024 as the known edition and does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.

A delivered 75×75×9 will measure close to the tabulated legs and thickness within those tolerances, not as a set of exact advertised millimetres. Out-of-square and leg tilt matter for connections. Settlement on theoretical or weighed mass should follow the contract. Theoretical masses in the size tables are the tabulated values; they are not a substitute for a weighed-mass agreement if the order requires one.

Applications and Service Limits

SS400 steel angles are used where this Japanese general-structure grade and a JIS G 3192 L-section are specified:

  • Building and industrial frames, bracing, lintels, truss work and general fabrications whose specification names SS400 angle rather than a welded-structure grade or a European, American or Chinese angle series.
  • Export packages that compare the grade with Q235B or with S235JR plate, provided each line keeps its own material standard and shape system.

It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require a defined Charpy test. Durability comes from the coating or fire-protection system, not from the SS400 designation.

SS400 Angle Compared with Q235B, S235JR and SM490

SS400, Q235B and S235JR are often grouped in a 235 MPa discussion, but they are not interchangeable certificates. SS400 is named for its 400–510 N/mm² tensile range and does not publish carbon or manganese maxima, nor a Charpy test. Q235B is a Chinese 235 MPa grade on a different shape system. S235JR plate carries tabulated carbon and manganese and a +20 °C impact test; a European angle in that grade would be an EN 10056 L, not a JIS G 3192 designation. SS400 plate is the same grade in plate form, not an angle.

SM490A and SM490B can use the same JIS angle series, but they belong to JIS G 3106, with a higher tensile class and, for B and C, specified impact tests. Dual certification requires every requirement of each named standard to be met on the delivered piece. A Japanese SS400 channel or H-beam page in this series will be linked here once it is published; those product URLs are not pre-linked.

Near-Equivalents: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to SS400 angle Caution
Q235B GB/T 700; dimensions GB/T 706 for angles A common Chinese 235 MPa comparison used in export enquiries, often discussed alongside SS400. Q235B has its own chemistry table, including tabulated carbon and manganese limits that SS400 does not publish. The shape names follow GB/T 706, not the JIS G 3192 A×A×t or A×B×t designation.
S235JR EN 10025-2; dimensions EN 10056 A 235 MPa European general-structure comparison, usually as an equal-leg or unequal-leg L when the product is an angle. S235JR has tabulated carbon, manganese and a +20 °C impact test. Those requirements are not implied by an SS400 certificate, and an EN 10056 L is not a JIS angle of similar leg length.
SM490A / SM490B JIS G 3106; the same JIS G 3192 angle series may be used Welded-structure grades in a higher tensile class, with specified impact tests for B and C. SM490 is not SS400. An SS400 certificate does not carry a JIS G 3106 impact quality. Dual certification requires every requirement of each named standard to be met on the delivered piece.

Sourcing SS400 Steel Angles from SHH STEEL

SHH STEEL supplies SS400 steel angles as an export trading house, coordinating mill production and project procurement. For this grade the useful work is to keep the tensile-named SS400 designation from being read as a 400 N/mm² yield, to keep equal, unequal and unequal-thickness series from being mixed, to apply the yield band to the leg thickness rather than the leg length, and to align the inspection document with the edition named on the order before a rolling programme is committed.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every Table 8, 9 or 10 size in SS400. Mid-range 75×75 and 100×100 equal legs are the usual core; the 25×25 and 30×30 families, the 250×250 rows and the Table 10 series are confirmed per line.

The same enquiry can also cover channels, H-sections, or Chinese, European or American designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

SS400 Steel Angle FAQs

Does SS400 have a 400 N/mm² yield?
No. The 400 in the grade name is the lower end of the 400–510 N/mm² tensile range. The minimum yield point or proof stress is 245 N/mm² up to 16 mm, then 235, 215 and 205 N/mm² in the thicker bands. For these angles the governing thickness is ordinarily the leg t, or the thicker leg t2 on the unequal-thickness series, not the leg length.
Does JIS G 3101 specify an impact test for SS400?
No. There is no Charpy requirement for SS400 in JIS G 3101. A toughness value must not be inferred from the grade name. If a defined impact test is required, nominate a standard and quality that actually table it, such as a JIS G 3106 grade.
Which angle series are listed, and what does footnote a mean?
The tables are the complete tabulated standard series in JIS G 3192:2024: Table 8 equal-leg (40 sizes), Table 9 unequal-leg (13 sizes) and Table 10 unequal-leg unequal-thickness (7 sizes). Footnote a states that the listed sizes are representative and that other section dimensions may be used by agreement. Table 10 is a distinct series, not a subset of Table 9.
Does Annex JA apply to every small SS400 angle?
Annex JA of JIS G 3101 applies only to sections whose leg length is under 40 mm. In the Table 8 series that means only the 25×25 and 30×30 families. It does not apply to 40×40 or to any Table 9 or Table 10 size. Review those two families against Annex JA in the ordered edition; this page does not restate the numeric JA values.
Which standards should appear on the inspection document?
At least JIS G 3101 and its edition, the grade SS400, the JIS G 3192 designation, the delivery condition, heat analysis including any added elements, and tensile results by thickness. If not otherwise specified, the inspection document is a JIS G 0415 inspection certificate 3.1.

Request a Quotation for JIS G 3101 SS400 Steel Angle

JIS G 3101 SS400 steel angle is a general-structure L-section with a 400–510 N/mm² tensile range and 245 N/mm² minimum yield up to 16 mm. Nominate the JIS G 3192 designation (A×A×t, A×B×t or A×B×t1×t2) and the material to JIS G 3101:2024 (or the edition on the order). The tables are the standard Table 8, 9 and 10 series, used as reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X