GB/T 706 Q235B Equal and Unequal Steel Angles
What is GB/T 706 Q235B Steel Angle?
GB/T 706 Q235B steel angle is a hot-rolled Chinese L-section whose material grade is Q235B under GB/T 700 and whose shape, tolerances and theoretical mass are ordered to GB/T 706. Q stands for yield strength, 235 is the minimum upper yield strength in MPa for the thinnest tabulated thickness band, and B is the quality grade, which carries a longitudinal Charpy V-notch requirement of 27 J at +20 °C when impact testing applies.
This page covers the rolled angle, not plate, not a channel and not an H-section. The same grade in plate form is listed separately as GB/T 700 Q235B steel plate. For plates, tensile specimens are taken transverse to the rolling direction and elongation may be two percentage points lower than the Table 2 values used for sections and bars. The plate page is not a substitute data sheet for angles, and neither is GB/T 11263 Q235B H-beam.
These bars are filed under steel angle profiles in the steel structural profiles category. They are Chinese equal-leg and unequal-leg angles. They are not European EN 10056 L-sections, American L-shapes, or Japanese angles of a similar millimetre leg, and they are not channels, I-beams or GB/T 11263 H-sections. A Q235B channel to GB/T 706 is a different product, with its own designation and its own page when that page is published.
Q235B is a general carbon structural steel for building frames, workshops and ordinary fabrication where a +20 °C impact quality is accepted. It is not a 355 MPa grade, not a weathering steel, and not a pressure-vessel or nuclear safety material. If an enquiry only says “Q235 angle,” the quality letter, the dimensional standard and the leg thickness still have to be named.
This page covers Equal and Unequal Steel Angles whose grade is Q235B (GB/T 700) and whose sizes follow GB/T 706. The Equal Leg Steel Angles and Unequal Leg Steel Angles are Table A.3 and Table A.4 series; the material standard does not by itself define the dimensions.
Material, Dimensions and Tolerances for Q235B Angles
Three documents should appear, separately, on the purchase order and on the inspection certificate:
- GB/T 700 is the material standard for carbon structural steels. This article uses ladle-analysis limits and tensile values from GB/T 700-2006, which remains the current edition. The edition named on the order governs acceptance.
- GB/T 706 is the product standard for hot-rolled section steel, including these equal-leg and unequal-leg angles. It sets the size series, dimensional and shape tolerances, theoretical mass and section surface rules, and it points chemistry and mechanical properties to GB/T 700 or GB/T 1591. It is not itself the material certificate. The size tables below are the complete standard series in GB/T 706-2016 Table A.3 (equal-leg) and Table A.4 (unequal-leg). GB/T 706-2016 is used as the numeric basis. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition of GB/T 706 named on the order governs dimensional acceptance.
- Tolerances on leg length, thickness, out-of-square, length, straightness and mass are those of the ordered GB/T 706 edition, not of GB/T 700 and not of GB/T 11263.
A mill may certify Q235B on a European or Japanese angle, or roll a Chinese angle to a different material standard, if that combination is in its programme and is fully documented. Matching a nominal 50 mm or 2 in leg is not a substitution.
GB/T 706 Q235B Equal Leg Steel Angles
The tables list the complete standard angle series in GB/T 706-2016: Table A.3 equal-leg angles, 115 sizes from 20×20×3 to 250×250×35, and Table A.4 unequal-leg angles, 71 sizes from 25×16×3 to 200×125×18. The usual designation is the leg and thickness string, written ∠b×b×d for equal legs (for example ∠200×200×24, often abbreviated ∠200×24) and ∠B×b×d for unequal legs (for example ∠160×100×16). Theoretical mass uses a density of 7.85 g/cm³. The root radii in GB/T 706 are for roll-pass design and are not delivery conditions, so they are not listed in the size tables. Use the tables to identify and estimate, not as a rolling programme for Q235B. Mid-range equal legs such as 50×50×5 and 75×75×8 are the usual enquiry core; the 20×20 families, the 200×200 and 250×250 rows, and the larger unequal legs should be confirmed size by size.
GB/T 706-2016 is used as the numeric basis. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition of GB/T 706 named on the order governs dimensional acceptance. This page does not invent rows that Tables A.3 and A.4 do not list, and it does not treat a Chinese 50×50×5 as interchangeable with a European, American or Japanese 50 mm equal angle.
The governing thickness is ordinarily the leg thickness d, not the leg length. Several of the larger tabulated equal-leg angles, and 200×125×18 among the unequal-leg rows, have a leg thickness over 16 mm and therefore fall into the 225 MPa band.
Equal-leg angles — Table A.3, Models 2 to 6.3 equal (36 sizes)
Swipe horizontally to view all dimensions.
Equal-leg angles — Table A.3, Models 7 to 12.5 equal (41 sizes)
Swipe horizontally to view all dimensions.
Equal-leg angles — Table A.3, Models 14 to 25 equal (38 sizes)
Swipe horizontally to view all dimensions.
GB/T 706 Q235B Unequal Leg Steel Angles
Unequal-leg angles — Table A.4, Models 2.5/1.6 to 10/8 unequal (41 sizes)
Swipe horizontally to view all dimensions.
Unequal-leg angles — Table A.4, Models 11/7 to 20/12.5 unequal (30 sizes)
Swipe horizontally to view all dimensions.
Q235B Chemical Composition for Angles (GB/T 700 Ladle Analysis)
The figures below are ladle-analysis maxima for Q235B in GB/T 700-2006. They are limits, not typical heat results. Product analysis may differ by the deviations in GB/T 222. Do not mix these values with unofficial tables that still quote the withdrawn 1988 manganese range of 0.30–0.70%. Q235B on an angle is the same grade as Q235B on plate or on an H-beam, but the certificate still has to identify the angle.
Q235B does not carry a carbon-equivalent cap in GB/T 700-2006. The grade may be supplied as rimming steel (F) or killed steel (Z); the Z mark is usually omitted when the steel is killed. The concession that carbon, manganese and silicon need not be delivery conditions if the mechanical properties are guaranteed belongs to grade A, not to grade B. Residual chromium, nickel and copper each have a 0.30% maximum and need not be analysed when the supplier guarantees the limit.
Q235B Angle Mechanical Properties: Yield, Tensile and +20 °C Impact
Tensile properties of Q235B are thickness-dependent. The values below are from GB/T 700-2006 Table 2. For sections and bars, tensile and bend specimens are longitudinal. For these angles the governing thickness is ordinarily the leg thickness d, not the leg length. Do not read the 235 MPa figure against the leg length, and do not treat a 16 mm plate rule as if it automatically described a 100 mm or 200 mm leg. Several of the larger tabulated angles have a leg thickness over 16 mm and therefore fall into the 225 MPa band; the later bands remain in the table because still heavier special bars can be agreed.
Tensile strength stays 370–500 MPa in every tabulated band. For a section thicker than 100 mm at the test location, the standard allows the lower tensile limit to be reduced by 20 N/mm²; that concession should appear on the certificate when it is used. Elongation is 26% through 40 mm. The 2006 edition no longer keeps a separate elongation column for thicknesses of 16 mm and under. Plate and strip are tested in the transverse direction and may be two percentage points lower; use the Q235B steel plate page for those figures, not this table.
Q235B requires a 27 J Charpy impact test at +20 °C, longitudinal, for thickness of 12 mm and above (or diameter of 16 mm and above). For Q235B thinner than 25 mm the impact test may be omitted when the supplier guarantees conformity and the purchaser agrees. That is a waiver of inspection, not a deletion of the requirement. Many tabulated angles have a leg thickness of 12 mm or more and still under 25 mm, so the waiver can apply when both parties agree; it is not automatic, and it does not apply once the leg reaches 25 mm.
Delivery Conditions, Inspection and Identification
GB/T 700 states that steel is generally delivered in the hot-rolled, controlled-rolled or normalized condition. These angles are commonly supplied as-rolled unless the order calls for another condition. The inspection document should identify Q235B, the GB/T 700 edition, the GB/T 706 designation and the edition used for dimensions and mass, the delivery condition, the heat number, ladle analysis, and the mechanical results against the thickness at the test location, which for these angles is ordinarily the leg thickness d. Packaging, marks and certificates follow GB/T 2101 in the edition named on the order. A plate certificate, or an H-beam or channel certificate, does not, by itself, identify an angle.
An EN 10204 type 3.1 document is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification on the product follows the mill’s marking practice and the ordered standards. Length is a matter for the rolling programme and the order.
Weldability and Surface Condition of Q235B Angles
Q235B is a weldable carbon structural steel when thickness, joint design and hydrogen control are taken into account. Because GB/T 700 does not set a CEV cap for this grade, the actual ladle carbon and manganese on the certificate, together with a welding procedure suited to the thickness, are the practical controls. This page does not prescribe a procedure or a preheat chart.
The as-rolled surface is mill scale. A blast class, a paint system, or a hot-dip galvanizing chemistry is an order option, not something implied by the grade name. If galvanizing is planned, the silicon and phosphorus on the heat, and the processor’s coating specification, should be reviewed before production. Surface quality also follows the ordered edition of GB/T 706; special finish requirements belong in the enquiry. Cutting to length, punching, forming or coating can be reviewed when the specification is sent with the enquiry. They are not assumed for every size.
GB/T 706 Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these angles are those of GB/T 706, not of GB/T 700 and not of the GB/T 11263 envelope written for H-sections. This article uses GB/T 706-2016 as the numeric size basis and does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order. GB/T 706-2026 is the successor edition, with implementation from 1 December 2026.
A delivered ∠50×50×5 will measure close to 50 × 50 × 5 mm within those tolerances, not as a set of exact advertised millimetres. Out-of-square and leg tilt matter for connections. Settlement on theoretical or weighed mass should follow the contract. Theoretical masses in the size tables use a density of 7.85 g/cm³; they are not a substitute for a weighed-mass agreement if the order requires one.
Applications and Service Limits
Q235B steel angles are used where a 235 MPa yield class, a +20 °C impact quality and a GB/T 706 L-section are accepted:
- Building frames, bracing, lintels, truss work, workshops and general structural fabrication.
- Machinery bases, skids and support steelwork that do not require a 355 MPa grade.
- Export packages that compare the grade with S235JR plate or with SS400 plate, provided each line keeps its own material standard and shape system.
It is not specified here for pressure equipment, for nuclear safety-related components, or for structures whose specification requires a lower impact-test temperature or a fine-grain weldable grade. Durability comes from the coating or fire-protection system, not from the grade name. Weathering or marine exposure needs an agreed protection system, not bare Q235B.
Q235B Angle Compared with Q355B, S235JR, SS400 and A36
Q235B, Q355B, S235JR, SS400 and A36 are often grouped in export discussions, but they are not interchangeable certificates. Q235B is a Chinese 235 MPa carbon steel on the GB/T 706 angle series. Q355B is a 355 MPa grade under GB/T 1591, not a Q235B certificate. S235JR plate carries its own chemistry, CEV and a +20 °C impact test; a European angle in that grade would be an EN 10056 L, not a Chinese ∠50×50×5. SS400 plate is named for a 400–510 N/mm² tensile range and does not publish carbon or manganese maxima. ASTM A36 is an American carbon grade on a different shape system. Q235B H-beam and Q235B plate share the material grade, not the section.
A Q235B channel to GB/T 706, and a later Q355B angle to the same dimensional standard, will be linked here once those pages are published; those product URLs are not pre-linked.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.
Sourcing Q235B Steel Angles from SHH STEEL
SHH STEEL supplies Q235B steel angles as an export trading house, coordinating mill production and project procurement. The useful part of that model is to keep the material edition (GB/T 700) distinct from the shape edition (GB/T 706-2016 as the numeric basis here, or the successor edition when that is what the order names), to apply the yield band to the leg thickness rather than the leg length, and to align the inspection document before a rolling programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every Table A.3 or A.4 size in Q235B. Mid-range equal legs such as 50×50×5 and 75×75×8 are the usual core; the 20×20 families, the 200×200 and 250×250 rows, and the larger unequal legs are confirmed per line.
The same enquiry can also cover channels, H-sections, or European, American or Japanese designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
Q235B Steel Angle FAQs
-
Which edition of GB/T 706 is used for the size tables?
- The size tables use GB/T 706-2016 as the numeric basis and are the complete Table A.3 equal-leg series (115 sizes, 20×20×3 to 250×250×35) and Table A.4 unequal-leg series (71 sizes, 25×16×3 to 200×125×18). GB/T 706-2026 is the successor edition, with implementation from 1 December 2026. The edition of GB/T 706 named on the order governs dimensional acceptance.
-
Does the 235 MPa yield apply to every Q235B angle in the tables?
- No. The governing thickness is ordinarily the leg thickness d, not the leg length. Angles with d ≤ 16 mm sit in the 235 MPa band. Several larger equal-leg sizes, and 200×125×18 among the unequal-leg rows, have a leg thicker than 16 mm and therefore fall into the 225 MPa band. The later bands remain in the mechanical table for still heavier special bars.
-
Is a Chinese 50×50×5 interchangeable with a European or Japanese 50 mm equal angle?
- No. A Chinese ∠50×50×5 is a GB/T 706 section. An EN 10056 L, an American L or a JIS G 3192 50×50 angle of similar millimetre size is a different section, with its own root-radius practice, mass and tolerance envelope.
-
Can the +20 °C impact test be omitted on these angles?
- Q235B requires 27 J at +20 °C, longitudinal, for thickness of 12 mm and above. For Q235B thinner than 25 mm the test may be omitted when the supplier guarantees conformity and the purchaser agrees. That is a waiver of inspection, not a deletion of the requirement, and it is not automatic. Once the leg reaches 25 mm the waiver does not apply.
-
Which standards should appear on the inspection document?
- At least GB/T 700 and its edition, the grade Q235B, the GB/T 706 designation and the edition used for dimensions and mass, the delivery condition, ladle analysis, and mechanical results against the thickness at the test location, ordinarily the leg thickness d. Packaging, marks and certificates follow GB/T 2101. A plate, H-beam or channel certificate does not, by itself, identify an angle.
Request a Quotation for GB/T 706 Q235B Steel Angle
GB/T 706 Q235B steel angle is a Chinese equal-leg or unequal-leg L-section with 235 MPa minimum yield in the first thickness band and a 27 J impact requirement at +20 °C. Nominate the GB/T 706 designation (for example ∠50×50×5, ∠200×200×20 or ∠160×100×16) and the material to GB/T 700-2006 (or the edition on the order). The size tables use GB/T 706-2016 as the numeric basis; GB/T 706-2026 is the successor edition, with implementation from 1 December 2026; the ordered edition governs. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.