ASTM A36 Equal and Unequal Steel Angles
What is ASTM A36 Steel Angle?
ASTM A36 steel angle is a hot-rolled equal-leg or unequal-leg L-shape in carbon structural steel A36. The material standard is ASTM A36/A36M. Dimensions, mass and general requirements for the rolled section are those of ASTM A6/A6M. The 36 ksi [250 MPa] minimum yield is the same figure used for A36 plates and for A36 wide-flange beams, but this page is for the angle, not for a W-shape, a channel, or a plate.
Equal angles have both legs the same length, for example L 4×4×1/2 or L 8×8×1. Unequal angles have a longer and a shorter leg, for example L 5×3×3/8 or L 8×6×1. The third number is the thickness of both legs. An L 8×6 is not an L 8×8, and it is not a European or Chinese unequal angle of a similar millimetre size. The designation is the A6/A6M L-shape, not a bar of the same thickness cut from plate.
These angles are filed under ASTM A36 steel angle profiles in the steel angle profiles category of steel structural profiles. The same grade in plate form is listed separately as ASTM A36 steel plate and ASME SA-36 steel plate. Do not use those plate pages as an angle data sheet.
A36 angles are used for bracing, frames, lintels, connection clips and general industrial work when the specification names this carbon grade in an L-shape. The grade is not a pressure-vessel or nuclear safety material, and it is not a substitute for ASTM A572 Grade 50 when a 50 ksi yield is what the order requires.
This page covers Equal and Unequal Steel Angles in ASTM A36. The Equal Leg Steel Angles and Unequal Leg Steel Angles follow the ASTM A6/A6M L series; the material standard does not by itself define the dimensions.
Material, Dimensions and Tolerances for A36 Angles
The order and the inspection certificate should keep material, dimensions and tolerances distinct:
- ASTM A36/A36M is the material standard. This article uses chemistry and tensile values for A36 shapes from ASTM A36/A36M-19. The edition named on the order governs acceptance.
- ASTM A6/A6M is the general-requirements and dimensional standard for these rolled angles. The size tables below are reference dimensions and theoretical masses for the standard equal-leg and unequal-leg L series, not a mill rolling list. The edition of A6/A6M named on the order governs dimensional acceptance.
A documented special combination — for example A36 on an EN 10056 angle, or an L-shape certified to a different material standard — is only valid if every requirement of each named standard is met. Matching a nominal 100 mm or 4 in leg is not a substitution.
ASTM A36 Equal Leg Steel Angles
The tables list designation, long-leg and short-leg lengths, thickness and theoretical mass, in inch-pound and SI units, for the standard L series under ASTM A6/A6M. For equal angles the two legs are the same length. Use the tables to identify and estimate, not as a rolling programme for A36. Mid-range L 3 to L 8 sizes are the usual enquiry core; the 12 in equal legs and the heaviest 1 in or 1-3/8 in thicknesses should be confirmed size by size.
L 4×4×1/2 is a 4 in equal angle, 1/2 in thick. L 8×6×1 is an 8 in by 6 in unequal angle, 1 in thick; it is not L 8×8×1. Designations keep the customary fractions, for example L 2-1/2×2-1/2×3/16, rather than a rounded decimal size.
Equal-leg angles (61 sizes, L 2×2×1/8 to L 12×12×1-3/8)
L 2 to L 4 equal (28 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 equal (16 sizes)
Swipe horizontally to view all dimensions.
L 8 to L 12 equal (17 sizes)
Swipe horizontally to view all dimensions.
ASTM A36 Unequal Leg Steel Angles
Unequal-leg angles (76 sizes, L 2-1/2×1-1/2×3/16 to L 8×6×1)
L 2½ to L 4 unequal (35 sizes)
Swipe horizontally to view all dimensions.
L 5 to L 6 unequal (22 sizes)
Swipe horizontally to view all dimensions.
L 7 to L 8 unequal (19 sizes)
Swipe horizontally to view all dimensions.
The 137 rows above are the standard equal and unequal L series used for this page. Other special-bar-size or non-standard angles can be reviewed when they are named on the enquiry; they are not invented here. European, Chinese or Japanese angle designations belong to their own dimensional standards, not to these L rows.
A36 Chemical Composition for Angles (Shapes Column)
The figures below are heat-analysis limits for A36 shapes from Table 3 of ASTM A36/A36M-19. They are the “All” thicknesses shapes column. They must not be copied from a plate-width column, and they are limits, not typical heat results.
A36 Angle Mechanical Properties: Yield, Tensile and Elongation
Tensile properties of A36 angles follow the shapes requirements in Table 2 of ASTM A36/A36M-19, not the bar elongation column. The 32 ksi [220 MPa] yield that applies to plates over 8 in does not apply to these sections. The footnote that removes the 80 ksi tensile maximum and lowers the 2 in elongation to 19% applies only to wide-flange shapes with flange thickness over 3 in, not to L-shapes.
For shapes with a cross-sectional area less than 1 in² [645 mm²], ASTM A36/A36M clause 8.2 provides that the manufacturer need not tension-test the product if the chemistry is appropriate for Table 2. In the standard L series, that area is below 1 in² for these eight sizes: L 2×2×1/8, L 2×2×3/16, L 2×2×1/4, L 2-1/2×1-1/2×3/16, L 2-1/2×1-1/2×1/4, L 2-1/2×2×3/16, L 2-1/2×2-1/2×3/16, L 3×2×3/16. Larger angles in the tables remain subject to the ordinary tensile test. Charpy V-notch testing is not a default A36 requirement; supplementary requirements such as S5 or S30 apply only when they are named on the order.
Delivery Conditions, Inspection and Identification
A36 angles are commonly supplied as-rolled. The inspection document should show ASTM A36/A36M and its edition, the grade A36, the A6/A6M L designation, the heat number, the heat analysis (including reported manganese), and the tensile results where a test is required. If copper steel, a Charpy supplementary, or a particular A6/A6M finish is required, that must appear on the order and on the certificate. An A36 W-shape or channel certificate does not, by itself, identify an L-shape.
An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 20–40 ft or 6–12 m.
Weldability and Surface Condition of A36 Angles
A36 is a weldable carbon structural steel when thickness, joint design and hydrogen control are taken into account. The specification does not table a carbon-equivalent limit for the grade. Procedure should be set from the certificate analysis and the applicable welding specification, not from an invented CEV figure. This page does not prescribe a procedure or a preheat chart. Fillet welds along both legs, and connections at the heel of an unequal angle, need the detailing that the design actually requires.
The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.
A6/A6M Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these L-shapes are those of ASTM A6/A6M, not of A36/A36M itself. This article does not reproduce the inch or millimetre tolerance tables; acceptance is against the edition named on the order.
A delivered L 4×4×1/2 will measure close to the tabulated legs and thickness within those tolerances, not as a set of exact advertised inches. Out-of-square at the heel and variation of the two legs matter for connections. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
A36 steel angles are used where a 36 ksi carbon grade and an equal or unequal L-shape are specified:
- Bracing, frames, lintels, clips, ledgers and general fabrications whose specification names A36 angle rather than Grade 50 or a non-American angle series.
- Export packages that compare the grade with Q235B or with S235JR, provided each line keeps its own material standard and shape system.
It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require A572 Grade 50 or a tabulated impact test. Durability comes from the coating or fire-protection system, not from the A36 designation.
A36 Angle Compared with A36 Beams, Grade 50 and Q235B
A36 wide-flange beams share the same material standard and the same 36 ksi yield, but they are W-shapes, not L-shapes. An A572 Grade 50 angle can use the same L series at a higher yield and with a different chemistry table. Q235B and S235JR are useful lower-strength comparisons only if chemistry, toughness and the shape standard are also satisfied.
Dual certification requires every requirement of each named standard to be met on the delivered piece. The A36 steel channel page in this series will be linked here once it is published.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.
Sourcing A36 Steel Angles from SHH STEEL
SHH STEEL supplies A36 steel angles as an export trading house, coordinating mill production and project procurement. For this product the useful work is to keep equal and unequal designations from being mixed, to keep the eight small-area sizes under clause 8.2 from being assumed as ordinary mill tensile specimens, and to align the A6/A6M size, the material edition and the inspection document before a rolling programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every equal or unequal L size in A36. Mid-range L 3 to L 8 sizes are the usual core; 12 in equal legs and the heaviest thicknesses are confirmed per line.
The same enquiry can also cover W-shapes, channels, or Chinese, Japanese or European designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
A36 Steel Angle FAQs
-
Is an equal angle interchangeable with an unequal angle of the same long-leg length?
- No. L 8×8 and L 8×6 are different sections. The short-leg length, the mass and the connection details are those of the designation that the specification actually names.
-
Do A36 angles use the bar elongation of 23% in 2 in?
- No. L-shapes are shapes, not bars. The shapes requirements are 20% in 8 in and 21% in 2 in, with 36 ksi minimum yield and 58–80 ksi tensile strength.
-
Which A36 angles may skip a mill tension test?
- ASTM A36/A36M clause 8.2 allows the manufacturer not to tension-test shapes with a cross-sectional area less than 1 in² if the chemistry is appropriate for Table 2. In the standard L series that applies to L 2×2×1/8, L 2×2×3/16, L 2×2×1/4, L 2-1/2×1-1/2×3/16, L 2-1/2×1-1/2×1/4, L 2-1/2×2×3/16, L 2-1/2×2-1/2×3/16 and L 3×2×3/16. Larger angles remain subject to the ordinary tensile test.
-
Does the 3 in flange chemistry note apply to these angles?
- The official wording is for shapes with flange thickness over 3 in. None of the standard L rows tabulated here has a thickness over 3 in; the heaviest tabulated thickness is 1.38 in. This page does not invent a separate 3 in-leg chemistry band.
-
Which standards should appear on the inspection document?
- At least ASTM A36/A36M and its edition, the grade A36, the L designation to A6/A6M, the heat number, heat analysis including reported manganese, and tensile results where a test is required. Any copper-steel or impact supplementary should also appear if it was ordered.
Request a Quotation for ASTM A36 Steel Angle
ASTM A36 steel angle is a carbon structural L-shape with 36 ksi [250 MPa] minimum yield. Nominate the equal or unequal L size to ASTM A6/A6M and the material to ASTM A36/A36M-19 (or the edition on the order). The tables are reference dimensions, not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.