ABS EH36 shipbuilding steel plate at SHH STEEL

ABS EH36 Shipbuilding Steel Plate Supplier

ABS EH36 higher-strength hull steel plate, yield 355 N/mm², tensile 490–620 N/mm², Charpy at −40 °C, stamped AB/EH36. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
ABS EH36 steel plate, ABS Grade EH36 shipbuilding plate, AB/EH36 plate, AH/DH/EH/FH 36 hull steel
Equivalent Grades:
ASTM A131 Grade EH36; DNV / LR / BV / CCS / NK / KR / RINA Grade EH36; GB 712 Grade EH36
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is ABS EH36 shipbuilding steel plate?

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

Equivalent grades: ABS EH36 ≈ ASTM A131 Grade EH36 ≈ DNV NV E36 ≈ LR EH36 ≈ BV EH36 ≈ CCS E36 / EH36 ≈ NK KE36 ≈ KR RE36 ≈ RINA EH36 ≈ GB 712 Grade EH36 (all class-approved, stamped by the issuing society).

ABS EH36 is a higher-strength hull structural steel under ABS Rules Part 2, Chapter 1, Section 3 (2-1-3). It belongs to the E-class (−40 °C) toughness group at strength level 36: minimum yield 355 N/mm², tensile 490–620 N/mm², elongation 21 % min. Plates are die-stamped AB/EH36 after ABS survey. EH36 is the −40 °C higher-strength grade at 355 N/mm² yield; plate is typically N/TM with each-piece impact in many Table 5 cells.

Thickness coverage for plates: AH/DH/EH 32/36 and AH/DH/EH 40 / FH 32/36/40 are listed up to 150 mm (2-1-3/1). Ordinary-strength ABS Grade A / ABS B / ABS D / ABS E stay at 235 N/mm² yield; EH36 is selected when scantlings need the higher yield of the 36 band.

SHH STEEL supplies ABS EH36 from ABS-approved Chinese mills, stock or mill roll, with optional multi-class and EN 10204 3.2. Related pages: ABS EH32 / ABS EH40; same strength other toughness: ABS AH36 / ABS DH36 / ABS FH36.

Buyer note for EH36: EH plate routes in Table 5 are dominated by N/TM with each-piece impact — plan mill time like ordinary Grade E, not like AH stock. Live reference for ordinary strength: ABS Grade A.

ABS EH36 plate: specification summary

ItemABS EH36 data
RuleABS Rules Part 2, 2-1-3 Higher-strength Hull Structural Steel (2023 checked); general 2-1-2 clauses also apply
Strength levelhigher strength 36, yield 355 N/mm² min., tensile 490–620 N/mm²
Toughness classEH → Charpy at −40 °C
Plate thickness coveredup to and including 150 mm (as listed for this grade family in 2-1-3/1)
Deoxidationkilled, fine grain practice (2-1-3/5)
Impact testCharpy V at −40 °C; frequency and supply condition per 2-1-3/7.3 Table 5
MarkingAB/EH36 (+ Z/U if ordered)
TMCP Ceq (Table 6)≤ 0.38 % for t ≤ 50 mm; ≤ 0.40 % for 50 < t ≤ 100 mm (TM steels)
Thickness toleranceminus 0.3 mm (2-1-1/15.3)
CertificateABS Surveyor-endorsed mill certificate; EN 10204 3.1 / 3.2 on request

Size range. Common market thicknesses for EH36 are about 6–80 mm (heavier plates available as per mill approval), widths 1500–3500 mm. Exact maximum thickness for a given delivery condition is as per standard and mill certificate / ABS works approval.

ABS EH36 chemical composition (heat and product analysis)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C0.18 max.0.22 max. (0.18 + 0.04)AH/DH/EH group
Mn0.90–1.60 (AH ≤12.5 mm may be 0.70 min.)0.81–1.72 (0.90 − 0.09; 1.60 + 0.12)Note 3: AH ≤12.5 mm may use 0.70 % Mn min.
Si0.10–0.500.04–0.56 (0.10 − 0.06; 0.50 + 0.06)min. waived if acid-soluble Al ≥ 0.015 %
P0.035 max.0.045 max. (0.035 + 0.010)
S0.035 max.0.045 max. (0.035 + 0.010)
Al (acid soluble) min.0.015 min. acid-soluble (or total Al per 2-1-3/5)0.015 min. (Al not listed in ASTM A6/A6M Table A – heat limit applies)or total Al per 2-1-3/5; grain refining
Nb0.02–0.05 when used singly0.01–0.06 (0.02 − 0.01; 0.05 + 0.01)when used singly; combined minima in 2-1-3/5
V0.05–0.10 when used singly0.04–0.11 (0.05 − 0.01; 0.10 + 0.01)when used singly
Ti0.02 max.0.03 max. (0.02 + 0.01)need not be reported unless intentionally added
Cu0.35 max.0.38 max. (0.35 + 0.03)may report ≤ 0.02 % if below
Cr0.20 max.0.24 max. (0.20 + 0.04)
Ni0.40 max.0.43 max. (0.40 + 0.03)FH allows higher Ni than AH/DH/EH
Mo0.08 max.0.09 max. (0.08 + 0.01)
N—no heat limit specified – report actual valuenot specified as a max in AH/DH/EH Table 1

Product (check) analysis column = heat (ladle) limit adjusted by ASTM A6/A6M-19 Table A “Permitted Variations in Product Analysis”, as required by ABS Rules Part 2, 2-1-2/5.3 (maximum + “over”, minimum − “under”; row chosen by the specified upper limit); arithmetic shown in brackets.

Source: ABS 2-1-3/7.3 Table 1. Heat (ladle) analysis must meet the table. Product (check) analysis, when required, follows ABS 2-1-2/5.3 → ASTM A6 (or other national) tolerances — ABS itself publishes no numeric product limits. AH/DH/EH share one chemistry column; toughness is differentiated by impact temperature and Table 5 supply routes, not by C/Mn caps. TMCP steels must also meet Table 6 Ceq. Ask for product analysis and Ceq/Pcm on the certificate at enquiry.

ABS EH36 tensile properties

PropertyRequirement
Tensile strength490–620 N/mm²
Yield point355 N/mm² min.
Elongation21 % min. (alt. A flat / C round)

Source: 2-1-3/7.3 Table 2. Alternative B specimen elongations (Table 3) for XH36:

Thickness (mm)≤55–1010–1515–2020–2525–3030–4040–50
Elongation min. %1315161718192021

Same tensile band applies to AH/DH/EH/FH 36; only impact temperature and chemistry group (FH vs AH/DH/EH) change across the letter.

ABS EH36: Charpy at −40 °C and supply condition

ThicknessLong. avg. at −40 °CTrans. avg. at −40 °C
t ≤ 50 mm34 J24 J
50 < t ≤ 70 mm41 J27 J
70 < t ≤ 100 mm50 J34 J
100 < t ≤ 150 mm54 J36 J

Source: 2-1-3/7.3 Table 4 (full-size; either direction acceptable). Condition of supply and impact lot size follow Table 5 and depend on grain-refining element (Nb, V, Al, Al+Ti) and thickness. In brief for plates: AH grades allow “any” condition in thinner bands with 50 t lots; DH often N/TM/CR; EH/FH plate routes are predominantly N/TM with each-piece (P) impact in many cells. Exact route for your thickness is as per standard and mill certificate — state the required delivery condition on the PO.

TMCP EH36: carbon equivalent caps 0.38 % (t ≤ 50) and 0.40 % (50 < t ≤ 100) per Table 6; over 100 mm Ceq agreed with ABS at mill qualification.

Thickness tolerance and surface condition

Minus tolerance 0.3 mm (2-1-1/15.3.2). Plus/flatness/width/length per ASTM A6 or as agreed. Surface repair per 2-1-1/3; state primer/surface class in the order if needed.

ABS EH36 plate stock in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
61800 / 20006000 / 8000N / TM / CR100+ tChina
81800 / 20008000 / 12000N / TM / CR200+ tChina
102000 / 22008000 / 12000N / TM / CR200+ tChina
122000 / 2200 / 250012000N / TM / CR200+ tChina
142000 / 220012000N / TM / CR100+ tChina
162000 / 250012000N / TM / CR200+ tChina
202000 / 250012000N / TM / CR100+ tChina
252200 / 250012000N / TM / CR100+ tChina
30220010000 / 12000N / TM / CR100+ tChina
40220010000N / TM / CR50+ tChina
5022008000 / 10000N / TM / CR50+ tChina

Quantities are approximate and change daily; all stock plates carry AB/EH36 marking and ABS-endorsed mill certificates. Sizes outside the table are produced in the next mill rolling cycle, typically 3–6 weeks including ABS survey (as per standard and mill certificate for exact lead time). Send your size list and we will reply with stock vs roll.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and ABS stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

ABS EH36 equivalents

Standard / societyDesignationComment
ASTM A131/A131MASTM A131/A131M Grade EH36A131 lists AH–FH 32/36/40; product standard only
IACS societiesGrade EH36DNV/LR/BV/CCS/NK/KR/RINA unified UR W11; BV FH36 / BV FH40
GB 712GB 712 Grade EH36not class approval by itself
Ordinary-strength ABSABS Grade A / Grades B, D, E235 N/mm² yield family
Same toughness other strengthABS EH32 / ABS EH40EH family
Same strength other toughnessABS AH36 / ABS DH36 / ABS FH3636 band

Comparisons, not substitutions. Multi-class stamps require joint survey before rolling.

ABS EH36 vs other ABS hull grades

Pick EH36 when the drawing specifies higher-strength grade EH36 (or the society equivalent). Do not substitute ordinary Grade E unless the designer recalculates scantlings — yield differs (355 vs 235). Within the 36 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Within the EH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².

For yields above 390 N/mm² ABS moves to Extra High Strength (2-1-8, AQ43/DQ47…), commercially often titled AH42/AH46 — see ABS AH42 and siblings.

When ABS EH36 is the right choice: typical uses are special and primary category members, crack-arrest strakes, and hull structure for cold-route or ice-strengthened vessels needing −40 °C toughness. The Charpy temperature (−40 °C) is fixed by the letter, and the strength by the number (ReH 355 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing. Swapping to a different letter or strength needs class approval of the drawing change, not just a new purchase order.

Applications and welding notes for ABS EH36

Typical uses: primary hull members at −40 °C with 355 N/mm² yield; Arctic-capable merchant tonnage. See offshore platform steel plates when primary offshore grades apply.

Welding: higher-strength hull steels need approved higher-strength consumables matched to required weld-metal toughness; preheat and heat input follow the approved WPS and often track Ceq/Pcm from the mill certificate (as per standard and mill certificate). TMCP EH36 must respect Table 6 Ceq caps. Cutting by oxy-fuel/plasma/laser is routine; thick QT/FH plate may need hydrogen control — follow mill recommendations.

Within the EH letter, moving 36 → other strengths (ABS EH32, ABS EH40) changes yield/tensile/elongation and Table 4 energies, not the Charpy temperature (−40 °C). Pick strength from the scantling; pick letter from the design temperature.

Processing notes for ABS EH36: cold forming of EH36 is routine within normal shipyard radii. Line heating and fairing of TMCP plate should stay within the temperature limits recommended by the mill, because overheating can reduce the strength gained in controlled rolling. Check the delivery condition on the certificate before planning hot forming.

Certificates, ABS survey and third-party inspection

ABS survey at the mill; certificate includes ladle chemistry, Ceq where applicable, tensile, Charpy at −40 °C, delivery condition and plate identity. Optional EN 10204 3.2, UT (U), Z-direction, multi-class. On receipt: verify AB/EH36 stamp, −40 °C impact data, energies ≥ Table 4, thickness ≥ nominal − 0.3 mm.

Charpy acceptance for ABS EH36 by thickness (from 2-1-3; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
t ≤ 50−40 °C3424
50 < t ≤ 70−40 °C4127
70 < t ≤ 100−40 °C5034
100 < t ≤ 150−40 °C5436

On receipt, check that the test temperature on the certificate is −40 °C and that the energy matches the band for the delivered thickness, not the thinnest band. Also check that the plate number on the stamp matches the certificate line, and that the ABS Surveyor endorsement is present. If UT was ordered (e.g. EN 10160 or ASTM A578 level), check the UT report as well. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.

Common mistakes ordering ABS EH36

  • Ordering “ABS 36” without the letter (AH/DH/EH/FH) — toughness class missing
  • Accepting ordinary-strength Grade E certificates for a EH36 PO
  • Ignoring TMCP Ceq caps (0.38/0.40) on TM plate
  • FH chemistry (tighter P/S, N) not checked when the PO says FH
  • Coil-cut plate without coil approval
  • Missing ABS endorsement on the MTC
  • Stock vs mill roll for ABS EH36?: Common 8–25 mm EH36 is often available from China stock with EH36 marking; thicker or QT/FH routes are usually mill-roll with ABS survey (about 3–6 weeks as a commercial estimate — confirm per order).

Write grade, delivery condition, impact temperature and certificate type into the PO.

Sourcing ABS EH36: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateABS-approved mills only; traceable stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mixed sizes / gradesEH36 combined with A/B/D/E or other AH–FH sizes in one container
Lead time visibilityweekly photo updates from dedicated coordinator
Prep before shipcutting, bevelling, drilling, machining in our workshop

How to order ABS EH36 plate

Specify ABS EH36 (2-1-3), delivery condition (AR/CR/N/TM/QT as applicable), thickness × width × length × qty, Z/U, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to ABS Rules Part 2 2-1-3, Grade EH36, delivery condition [AR/CR/N/TM/QT], 20 × 2500 × 12000 mm, 30 pcs, marked AB/EH36, certificate endorsed by ABS Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].” Each bracketed item changes price, lead time and which mills can supply, so fix them at enquiry stage.

FAQ

What sizes and minimum order quantity can you supply for ABS EH36 plate?
2-1-3/1 lists EH36 plate up to and including 150 mm. Most enquiries we receive for EH36 are 8–60 mm thick, 1800–3000 mm wide and 6000–12000 mm long. Popular sizes can come from China stock carrying the AB/EH36 marking, with no fixed minimum. A mill rolling for a special width, thickness above roughly 60 mm or a Z-grade normally needs a minimum quantity per size, which we confirm per order. We can combine several sizes, or EH36 with other hull grades, to reach a rolling or container quantity.
How is ABS EH36 certified, and can you arrange EN 10204 3.2 witness inspection?
Every plate is made by an ABS-approved mill under ABS survey. It is die-stamped or stencilled AB/EH36 with the heat or plate number, and the mill test certificate is endorsed by the ABS Surveyor. The certificate gives the ladle chemistry, the tensile results (ReH ≥ 355 N/mm², Rm 490–620 N/mm², A ≥ 21 %), the Charpy results at −40 °C, the delivery condition and the plate identity. If your contract asks for EN 10204 3.2, we arrange it before rolling. The witness can be the ABS Surveyor, a second class society (dual or multi-class stamping, e.g. ABS + DNV or LR), or a third-party inspector such as SGS or BV who witnesses the tests and checks the markings. 3.2 cannot be added after the plates have been tested, so please state it on the enquiry.
What is the impact test temperature and energy for ABS EH36, and do thickness limits apply?
ABS EH36 is tested at −40 °C. Required average energies (longitudinal/transverse, J min.) under 2-1-3 Table 4 rise with thickness: ≤50 mm 34/24; 50–70 mm 41/27; 70–100 mm 50/34; 100–150 mm 54/36. This matters when you order thick EH36: a 60 mm plate must meet higher values than a 20 mm plate at the same −40 °C. The test lot size and the permitted delivery condition (AR, CR, N, TM or QT) for each thickness follow 2-1-3 Table 5. Above 100 mm, ABS also asks for tensile and impact data at quarter and mid thickness (2-1-1/16). Results are as per standard and mill certificate.
What welding and preheat guidance applies to ABS EH36?
ABS EH36 needs higher-strength welding consumables approved for −40 °C weld-metal toughness. For TMCP plate, 2-1-3 Table 6 caps the carbon equivalent at 0.38 % (t ≤ 50 mm) and 0.40 % (50 < t ≤ 100 mm); above 100 mm it is agreed at mill approval. N or AR plate of the same grade may have a higher actual Ceq, so the delivery condition affects how easy the plate is to weld. Preheat, interpass temperature and heat input must follow your ABS-approved WPS. We send the mill certificate’s ladle analysis and Ceq before shipment so the welding engineer can confirm the procedure qualifies. We do not give generic preheat temperatures.
What is the delivery time for ABS EH36 plate?
Stock sizes of ABS EH36 can usually be cut, inspected and loaded in about 7–15 days. Mill-rolled orders typically take about 3–6 weeks plus inspection, depending on thickness, delivery condition and the mill schedule. These are commercial estimates, confirmed with each quote. If 3.2 witness or multi-class survey is required, we book the inspector when we place the mill order so testing is not delayed. A dedicated coordinator sends weekly progress photos (rolling, marking, testing, packing, loading) until the bill of lading is issued.
Which payment terms do you accept for ABS EH36, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the AB/EH36 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance, so the plate is verified before most of the money moves. With L/C, payment is tied to the presented documents (commercial invoice, packing list, B/L, mill certificate, and the 3.2 or class certificate if you require one). For first orders we can start with a smaller trial lot. The proforma invoice shows the grade, sizes and certificate type, so the contract and the delivered plate match.
What are the equivalent grades of ABS EH36 among class societies and GB 712?
ABS EH36 corresponds to ASTM A131/A131M Grade EH36, Grade EH36 of DNV / LR / BV / CCS / NK / KR / RINA, and GB 712 Grade EH36. All share yield 355 N/mm², tensile 490–620 N/mm² and a Charpy test at −40 °C under the IACS unified requirements. Even so, a plate is only accepted by the society whose stamp and certificate it carries. Order ABS EH36 for ABS class, or ask for multi-class (e.g. ABS + DNV + LR) when one stock must serve several projects. GB 712 or A131 certificates alone do not replace the ABS stamp.
Can you cut, bevel or machine ABS EH36 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut EH36 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the AB/EH36 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. Shot blasting and shop primer are available on request. Loading photos and a packing list come with each shipment. See SHH STEEL for our processing capabilities.

Conclusion

ABS EH36 is higher-strength hull steel: yield 355 N/mm², tensile 490–620 N/mm², Charpy at −40 °C, marking AB/EH36. Lock on the order: delivery condition per Table 5, impact lot size, TMCP Ceq if TM, product analysis if needed, multi-class and 3.2.

SHH STEEL supplies EH36 from ABS-approved mills with Surveyor-endorsed certificates, stock or roll, optional 3.2 and multi-class.

T/T or L/C with inspection before balance; mixed containers; photo follow-up; in-house cutting/bevelling/drilling/machining.

Request a quotation: send SHH STEEL ABS EH36, sizes, qty, port and any multi-class/Z/U/3.2 needs.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X