LR Steel Plates

Product Showcase

LR Steel Plates Carbon Steel Plates

SHH STEEL offers LR Rules-compliant LR AH32/DH32/EH36 steel plates. Lloyd’s Register Rules for Ships cover material manufacture, testing, and certification for hull construction in welded steel vessels. Certified quality, competitive prices, customizable. Trust SHH STEEL!

LR FH40 marine steel plate per Lloyd's Register (LR) rules at SHH STEEL warehouse

LR FH40 Steel Plate | LR/FH40 Marine Steel Plate

LR LR/FH40 (FH40) higher-strength hull structural steel plate, yield 390 N/mm², tensile 510–650 N/mm², Charpy at −60 °C, stamped LR FH40 / LR/FH40 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
LR EH40 shipbuilding steel plate to Lloyd's Register (LR) rules, stacked hull plates

LR EH40 Steel Plate | LR/EH40 Marine Steel Plate

LR LR/EH40 (EH40) higher-strength hull structural steel plate, yield 390 N/mm², tensile 510–650 N/mm², Charpy at −40 °C, stamped LR EH40 / LR/EH40 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
Close view of LR DH40 hull structural steel plate, Lloyd's Register (LR) rules

LR DH40 Steel Plate | LR/DH40 Marine Steel Plate

LR LR/DH40 (DH40) higher-strength hull structural steel plate, yield 390 N/mm², tensile 510–650 N/mm², Charpy at −20 °C, stamped LR DH40 / LR/DH40 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
LR AH40 marine steel plate per Lloyd's Register (LR) rules at SHH STEEL warehouse

LR AH40 Steel Plate | LR/AH40 Marine Steel Plate

LR LR/AH40 (AH40) higher-strength hull structural steel plate, yield 390 N/mm², tensile 510–650 N/mm², Charpy at 0 °C, stamped LR AH40 / LR/AH40 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
LR FH36 shipbuilding steel plate to Lloyd's Register (LR) rules, stacked hull plates

LR FH36 Steel Plate | LR/FH36 Marine Steel Plate

LR LR/FH36 (FH36) higher-strength hull structural steel plate, yield 355 N/mm², tensile 490–630 N/mm², Charpy at −60 °C, stamped LR FH36 / LR/FH36 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
Close view of LR EH36 hull structural steel plate, Lloyd's Register (LR) rules

LR EH36 Steel Plate | LR/EH36 Marine Steel Plate

LR LR/EH36 (EH36) higher-strength hull structural steel plate, yield 355 N/mm², tensile 490–630 N/mm², Charpy at −40 °C, stamped LR EH36 / LR/EH36 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
LR DH36 marine steel plate per Lloyd's Register (LR) rules at SHH STEEL warehouse

LR DH36 Steel Plate | LR/DH36 Marine Steel Plate

LR LR/DH36 (DH36) higher-strength hull structural steel plate, yield 355 N/mm², tensile 490–630 N/mm², Charpy at −20 °C, stamped LR DH36 / LR/DH36 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
LR AH36 shipbuilding steel plate to Lloyd's Register (LR) rules, stacked hull plates

LR AH36 Steel Plate | LR/AH36 Marine Steel Plate

LR LR/AH36 (AH36) higher-strength hull structural steel plate, yield 355 N/mm², tensile 490–630 N/mm², Charpy at 0 °C, stamped LR AH36 / LR/AH36 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
Close view of LR FH32 hull structural steel plate, Lloyd's Register (LR) rules

LR FH32 Steel Plate | LR/FH32 Marine Steel Plate

LR LR/FH32 (FH32) higher-strength hull structural steel plate, yield 315 N/mm², tensile 440–590 N/mm², Charpy at −60 °C, stamped LR FH32 / LR/FH32 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
LR EH32 marine steel plate per Lloyd's Register (LR) rules at SHH STEEL warehouse

LR EH32 Steel Plate | LR/EH32 Marine Steel Plate

LR LR/EH32 (EH32) higher-strength hull structural steel plate, yield 315 N/mm², tensile 440–590 N/mm², Charpy at −40 °C, stamped LR EH32 / LR/EH32 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
LR DH32 shipbuilding steel plate to Lloyd's Register (LR) rules, stacked hull plates

LR DH32 Steel Plate | LR/DH32 Marine Steel Plate

LR LR/DH32 (DH32) higher-strength hull structural steel plate, yield 315 N/mm², tensile 440–590 N/mm², Charpy at −20 °C, stamped LR DH32 / LR/DH32 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More
Close view of LR AH32 hull structural steel plate, Lloyd's Register (LR) rules

LR AH32 Steel Plate | LR/AH32 Marine Steel Plate

LR LR/AH32 (AH32) higher-strength hull structural steel plate, yield 315 N/mm², tensile 440–590 N/mm², Charpy at 0 °C, stamped LR AH32 / LR/AH32 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
View More

LR Steel Plates Carbon Steel Plates

LR FH69 Steel Plate | LR/FH69 Marine Steel Plate LR EH69 Steel Plate | LR/EH69 Marine Steel Plate LR DH69 Steel Plate | LR/DH69 Marine Steel Plate LR AH69 Steel Plate | LR/AH69 Marine Steel Plate
LR FH62 Steel Plate | LR/FH62 Marine Steel Plate LR EH62 Steel Plate | LR/EH62 Marine Steel Plate LR DH62 Steel Plate | LR/DH62 Marine Steel Plate LR AH62 Steel Plate | LR/AH62 Marine Steel Plate
LR FH55 Steel Plate | LR/FH55 Marine Steel Plate LR EH55 Steel Plate | LR/EH55 Marine Steel Plate LR DH55 Steel Plate | LR/DH55 Marine Steel Plate LR AH55 Steel Plate | LR/AH55 Marine Steel Plate
LR FH50 Steel Plate | LR/FH50 Marine Steel Plate LR EH50 Steel Plate | LR/EH50 Marine Steel Plate LR DH50 Steel Plate | LR/DH50 Marine Steel Plate LR AH50 Steel Plate | LR/AH50 Marine Steel Plate
LR FH46 Steel Plate | LR/FH46 Marine Steel Plate LR EH46 Steel Plate | LR/EH46 Marine Steel Plate LR DH46 Steel Plate | LR/DH46 Marine Steel Plate LR AH46 Steel Plate | LR/AH46 Marine Steel Plate
LR FH42 Steel Plate | LR/FH42 Marine Steel Plate LR EH42 Steel Plate | LR/EH42 Marine Steel Plate LR DH42 Steel Plate | LR/DH42 Marine Steel Plate LR AH42 Steel Plate | LR/AH42 Marine Steel Plate
LR FH40 Steel Plate | LR/FH40 Marine Steel Plate LR EH40 Steel Plate | LR/EH40 Marine Steel Plate LR DH40 Steel Plate | LR/DH40 Marine Steel Plate LR AH40 Steel Plate | LR/AH40 Marine Steel Plate
LR FH36 Steel Plate | LR/FH36 Marine Steel Plate LR EH36 Steel Plate | LR/EH36 Marine Steel Plate LR DH36 Steel Plate | LR/DH36 Marine Steel Plate LR AH36 Steel Plate | LR/AH36 Marine Steel Plate
LR FH32 Steel Plate | LR/FH32 Marine Steel Plate LR EH32 Steel Plate | LR/EH32 Marine Steel Plate LR DH32 Steel Plate | LR/DH32 Marine Steel Plate LR AH32 Steel Plate | LR/AH32 Marine Steel Plate
LR Grade E Steel Plate | LR/E Marine Steel Plate LR Grade D Steel Plate | LR/D Marine Steel Plate LR Grade B Steel Plate | LR/B Marine Steel Plate LR Grade A Steel Plate | LR/A Marine Steel Plate

Shipbuilding Steel Plates

SHH STEEL, a premier Shipbuilding Steel Plates exporter, produces and exports shipbuilding steel plates for marine vessels and offshore structures. Our plates, such as AH36 and DH36, provide high strength, toughness, and corrosion resistance, meeting ABS and BV standards. With a 5,000-ton inventory, we guarantee 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for reliable marine-grade steel plates and custom maritime solutions.

Shipbuilding Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *