LR EH46 Steel Plate | LR/EH46 Marine Steel Plate
What is LR EH46 / LR/EH46 marine steel plate?
LR EH46, often written LR/EH46 on mill certificates and plate markings, is an extra-high-strength hull structural steel under Lloyd’s Register Rules for the Manufacture, Testing and Certification of Materials. IACS Unified Requirement W16 covers this strength band (yield 460 N/mm²); LR implements corresponding requirements in its Materials rules. Minimum yield is 460 N/mm², tensile 570–720 N/mm², elongation 17 % min., with Charpy at −40 °C. It sits above the AH–FH 40 higher-strength family (max yield 390 N/mm² under UR W11). Commercial enquiries use LR EH46 or LR/EH46 marine steel plate.
Equivalent grades: LR EH46 ≈ ASTM A131 (no direct grade at this strength) ≈ ABS EH46 / EQ47 ≈ DNV NV E460 ≈ BV E460 ≈ CCS EH460 ≈ NK KE460 ≈ KR RE47 ≈ RINA E460 ≈ GB 712 Grade EH460 (all class-approved, stamped by the issuing society).
Naming note: Lloyd’s Register titles this strength band as EH46 / LR/EH46 (LR uses AH69, not AH70). DNV often titles the same yield as EH460 / DNV NV E460. ABS often titles EH46 (official ABS EQ47). ASTM A131 has no grade at this strength. Write LR/EH46 on the LR purchase order.
LR/EH46 is almost always produced TM or QT by an LR-approved mill to order rather than taken from open stock. SHH STEEL sources extra-high-strength plate from mills with Lloyd’s Register approval for the grade, under Surveyor attendance, with optional multi-class and EN 10204 3.2.
LR LR/EH46 plate: specification summary
| Item | LR LR/EH46 / EH46 data |
|---|---|
| Rule basis | Lloyd’s Register Rules for Materials (extra-high / high-strength hull steel); IACS UR W16 strength band (see UNCERTAIN for LR paragraph cross-refs without local PDF) |
| Commercial / stamp | LR/EH46 (LR EH46) |
| Yield / tensile / elongation | 460 / 570–720 N/mm² / 17 % min. |
| Impact | −40 °C; ≈ 46 J L or 31 J T average (IACS UR W16 / aligned tables — confirm on mill certificate) |
| Deoxidation | fully killed, fine grain; N-binding elements per manufacturing specification |
| Delivery condition | TM or QT (N/CR routes only where specifically approved) — within mill approval thickness limits |
| Marking | LR EH46 / LR/EH46 (plus delivery-condition / Z / U where ordered) |
| UT | commonly required for thicker EHS plate (e.g. ≥15 mm) — agree standard (EN 10160 / ASTM A578) on PO |
| Thickness tolerance | IACS UR W13 as adopted by LR (confirm class on PO; see UNCERTAIN) |
| Certificate | mill certificate endorsed by the LR Surveyor; includes Ceq/CET/Pcm as applicable; EN 10204 3.1 / 3.2 on request |
Maximum plate thickness depends on delivery condition and the mill’s LR approval sheet — typically TM up to about 100–150 mm and QT higher, but treat the approval limit as governing (UNCERTAIN without local LR PDF). Primary commercial scope we quote is within ~100 mm unless the mill approval and LR survey confirm otherwise.
LR LR/EH46 chemical composition (heat analysis envelope)
| Element | Heat (ladle) analysis, % | Product (check) analysis, % | Note |
|---|---|---|---|
| C (depends on route) | 0.14–0.21 max. by grade/condition (UR W16 / mill approval) | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | TM/QT and letter routes may tighten C |
| Mn | typically 1.0–1.70 (route-dependent) | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | as per mill approval |
| Si | typically 0.60 max. (QT may differ) | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | |
| P / S | tighter than UR W11 HS; often 0.025 max. or lower on EQ/FQ-style routes | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | confirm on approval sheet |
| Al total min. | fine-grain practice | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | Al/N control unless other N-binders used |
| Nb / V / Ti | limits per UR W16 / mill approval | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | combined microalloy caps apply |
| Ni / Cu / Cr / Mo | per approval chemistry | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | |
| Ceq / CET / Pcm | maxima by category and condition on approval | not applicable (calculated from heat analysis) | report on certificate |
Product (check) analysis column: LR Rules for Materials specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.
Source: IACS UR W16 chemistry envelope as implemented by Lloyd’s Register for LR/EH46 — exact ladle limits depend on delivery condition (TM vs QT) and toughness letter. Values above are the rule envelope; the purchase order and mill approval sheet govern. Product analysis: as per standard and mill certificate. All intentionally added elements and Ceq (or CET/Pcm) are to be reported. Flagged UNCERTAIN where a local LR Materials PDF was not available to quote paragraph numbers.
LR LR/EH46 tensile and impact properties
| Property | Requirement (IACS UR W16 aligned) |
|---|---|
| Yield strength ReH (or Rp0.2) | 460 N/mm² min. |
| Tensile strength Rm | 570–720 N/mm² |
| Elongation (transverse, 5.65√A) | 17 % min. |
| Impact test temperature | −40 °C |
| Impact energy (indicative) | 46 J L or 31 J T average |
Final acceptance values are as per standard and mill certificate under LR survey. For thick plate, additional mid-thickness tensile/impact positions may apply — confirm at enquiry. Test frequency is typically each heat-treatment batch of same cast/condition/thickness.
Delivery condition and toughness for LR/EH46
Charpy temperature is fixed by the grade letter: EH → −40 °C. Indicative average energy 46 / 31 J (L/T) from IACS UR W16 aligned tables — confirm exact figures on the LR-endorsed certificate. Unlike UR W11 higher-strength tables, EHS energies are usually stated as a single pair rather than rising through many thickness bands; thick-plate mid-thickness rules may still apply.
Allowed delivery conditions are primarily TM and QT within the mill’s approved thickness. Vacuum degassing is commonly required for higher categories and for thicker plate — follow the mill approval. State TM or QT on the PO; do not leave delivery condition blank for EH46.
Thickness tolerance and surface condition
Lloyd’s Register applies IACS UR W13 unless the PO states otherwise (confirm minus class on PO; see UNCERTAIN). Surface repair limits follow the applicable LR / UR rules; state primer/surface class on receipt if needed. For QT plate, avoid notching cut edges; follow mill cutting recommendations.
LR LR/EH46 plate — mill-roll supply in China
| Thickness (mm) | Width (mm) | Length (mm) | Condition | Approx. quantity | Location |
|---|---|---|---|---|---|
| 10 | 2000 / 2200 | 8000 / 12000 | TM / QT | 200+ t | China |
| 12 | 2000 / 2200 / 2500 | 12000 | TM / QT | 200+ t | China |
| 14 | 2000 / 2200 | 12000 | TM / QT | 100+ t | China |
| 16 | 2000 / 2500 | 12000 | TM / QT | 200+ t | China |
| 20 | 2000 / 2500 | 12000 | TM / QT | 100+ t | China |
| 25 | 2200 / 2500 | 12000 | TM / QT | 100+ t | China |
| 30 | 2200 | 10000 / 12000 | TM / QT | 100+ t | China |
| 40 | 2200 | 10000 | TM / QT | 50+ t | China |
| 50 | 2200 | 8000 / 10000 | TM / QT | 50+ t | China |
Extra-high grades such as LR/EH46 are rarely held as open stock; the table shows the size bands we quote against scheduled mill rolls. Quantities are indicative. All plates sold as LR class carry LR/EH46 marking and an LR-endorsed mill certificate. Typical mill lead time including LR survey is about 6–10 weeks (commercial estimate — confirm per quote). Send your size list and we will reply with the next available rolling slot.
Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and LR stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.
LR LR/EH46 equivalents in other rules and standards
| Standard / society | Designation | Comment |
|---|---|---|
| LR (Lloyd’s Register) | LR/EH46 (LR EH46) | this page; LR uses AH69 not AH70 |
| ASTM A131/A131M | ASTM A131/A131M — no direct Grade EH46 | A131 stops at FH40 |
| ABS | ABS EH46 / EQ47 | commercial EH46 / official EQ47 (ABS uses 70 where LR uses 69) |
| DNV | DNV NV E460 | DNV titles EH460 for this yield band |
| BV | BV (per rules) | EHS name not verified from local BV PDF — write per rules |
| CCS | CCS EH460 | CCS follows W16-style naming |
| NK (ClassNK) | NK KE460 | NK KE460 |
| KR | KR RE47 | KR RE47 (KR uses ABS-style category numbers) |
| RINA | RINA (per rules) | EHS name not verified from local RINA PDF |
| GB 712 | GB 712 Grade EH460 | listed in GB 712 EHS band; not class approval alone |
These are comparisons, not substitutions. Always write the LR stamp LR/EH46 on the PO, plus any additional society stamps you need.
LR LR/EH46 vs higher-strength and other EHS grades
Use EH46 when scantlings need yield 460 N/mm². Do not substitute AH40/EH40 (390 N/mm² max under UR W11) without redesign. Within the 46 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Neighbouring strengths are 42 / 50 — swapping strength needs class approval of the drawing change.
When LR LR/EH46 is the right choice: typical uses are special and primary category members, crack-arrest strakes, and hull structure for cold-route or ice-strengthened vessels needing −40 °C toughness at extra-high yield — weight-critical hull girder strakes, polar and ice-class primary structure, and offshore units where 460 N/mm² is specified. See offshore platform steel plates for related offshore grades.
Applications and welding notes for LR LR/EH46
Typical uses: special and primary category members, crack-arrest strakes, and hull structure for cold-route or ice-strengthened vessels needing −40 °C toughness at ReH 460 N/mm²; strength deck and shell of large container ships and gas carriers where EHS is specified; ice-belt and polar primary structure; selected offshore members. See offshore platform steel plates.
Welding: LR/EH46 is an extra-high-strength steel supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by LR. Ceq/CET/Pcm from the ladle analysis govern hydrogen control, preheat, interpass and heat-input windows. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits. We do not give generic preheat temperatures.
Processing notes: LR/EH46 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and LR. Cold forming and bending radii should follow the mill’s data sheet. Thermal cutting parameters follow mill recommendations so the cut edge is not damaged.
Certificates, LR survey and third-party inspection
LR survey at the mill; certificate includes ladle chemistry, Ceq/CET/Pcm as applicable, tensile (ReH ≥ 460, Rm 570–720, A ≥ 17 %), Charpy at −40 °C, delivery condition, UT if ordered, and plate identity. Optional EN 10204 3.2 and multi-class.
On receipt: verify LR/EH46 stamp, −40 °C impact data, energies ≥ ordered/certified minima, thickness within tolerance, Surveyor endorsement, UT report if required.
Charpy acceptance for LR/EH46 (IACS UR W16 aligned; actual results as per standard and mill certificate):
| Thickness t (mm) | Test temperature | Average energy, longitudinal (J min.) | Average energy, transverse (J min.) |
|---|---|---|---|
| as per UR W16 / mill approval (typically t/4 position) | −40 °C | 46 | 31 |
For thickness above ~100 mm, additional mid-thickness rules may apply — confirm at enquiry. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.
Common mistakes when ordering LR EH46 / LR/EH46
- Ordering “LR 46” without the letter (EH) — toughness missing
- Writing ABS EH46 or DNV EH460 on an LR-class PO without arranging that society’s survey (wrong stamp)
- Leaving delivery condition blank (TM vs QT changes price, mill and properties)
- Expecting ASTM A131 dual-cert at this strength (A131 has no EHS grade)
- Skipping UT on thick EHS plate when the yard specification requires it
- Missing LR endorsement / assuming GB 712 Grade EH460 alone is class approval
- Confusing LR AH69 with ABS AH70 — same yield band, different society title
Write grade, TM/QT, impact temperature, UT level and certificate type into the PO.
Sourcing LR LR/EH46: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Fake class plate | LR-approved mills only; traceable LR/EH46 stamp + certificate; 3.2 on request |
| Payment risk | T/T or L/C; inspection before balance |
| Mill minimum / long lead time | combine sizes on one heat where possible; weekly photo updates; clear rolling-slot confirmation before deposit |
| Welding / heat-input risk | send ladle Ceq/CET/Pcm before shipment; support WPS review with mill data |
| Prep before ship | cutting, bevelling, drilling, machining in our workshop (follow mill cutting notes for QT) |
How to order LR LR/EH46 plate
Specify LR EH46 (LR/EH46), delivery condition TM or QT, thickness × width × length × qty, Z/U/UT level, multi-class, certificate type, port. Send to SHH STEEL.
Sample PO line: “Steel plate to Lloyd’s Register Rules for Materials, Grade EH46 (LR/EH46), delivery condition [TM/QT], 30 × 2500 × 12000 mm, 10 pcs, marked LR EH46 / LR/EH46, certificate endorsed by LR Surveyor, EN 10204 3.2 [if required], UT [EN 10160 / ASTM A578 level], CIF [port].”
FAQ
Conclusion
LR EH46 / LR/EH46 is extra-high-strength hull steel (IACS UR W16 band): yield 460 N/mm², tensile 570–720 N/mm², Charpy at −40 °C, marking LR/EH46. Lock on the order: TM or QT, UT level, Ceq/CET/Pcm reporting, multi-class and 3.2.
SHH STEEL supplies LR/EH46 plate rolled by Chinese mills that hold Lloyd’s Register works approval for the grade, so every plate carries the LR/EH46 stamp and a Surveyor-endorsed certificate traceable to its heat. Sizes are scheduled into the mill rolling cycle with LR survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, BV or another agency) and joint certification with ABS, DNV, BV, CCS, NK, KR or RINA.
We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or LR/EH46 with neighbouring EHS sizes or higher-strength AH–FH 40 where the drawing allows, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.
Request a quotation: send SHH STEEL the grade (LR/EH46 / LR EH46), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.