LR DH62 marine steel plate per Lloyd's Register (LR) rules at SHH STEEL warehouse

LR DH62 Steel Plate | LR/DH62 Marine Steel Plate

LR LR/DH62 (DH62) extra-high-strength hull structural steel plate, yield 620 N/mm², tensile 720–890 N/mm², Charpy at −20 °C, stamped LR DH62 / LR/DH62 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
LR DH62 steel plate, LR/DH62 marine steel plate, LR DH62 shipbuilding plate, DH62 extra high strength hull steel, Lloyd's Register DH62 plate
Equivalent Grades:
ASTM A131 (no direct); ABS DH62 / DQ63; DNV NV D620; BV/RINA per rules; CCS DH620; NK KD620; KR RD63; GB 712 Grade DH620
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is LR DH62 / LR/DH62 marine steel plate?

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

LR DH62, often written LR/DH62 on mill certificates and plate markings, is an extra-high-strength hull structural steel under Lloyd’s Register Rules for the Manufacture, Testing and Certification of Materials. IACS Unified Requirement W16 covers this strength band (yield 620 N/mm²); LR implements corresponding requirements in its Materials rules. Minimum yield is 620 N/mm², tensile 720–890 N/mm², elongation 15 % min., with Charpy at −20 °C. It sits above the AH–FH 40 higher-strength family (max yield 390 N/mm² under UR W11). Commercial enquiries use LR DH62 or LR/DH62 marine steel plate.

Equivalent grades: LR DH62 ≈ ASTM A131 (no direct grade at this strength) ≈ ABS DH62 / DQ63 ≈ DNV NV D620 ≈ BV D620 ≈ CCS DH620 ≈ NK KD620 ≈ KR RD63 ≈ RINA D620 ≈ GB 712 Grade DH620 (all class-approved, stamped by the issuing society).

Naming note: Lloyd’s Register titles this strength band as DH62 / LR/DH62 (LR uses AH69, not AH70). DNV often titles the same yield as DH620 / DNV NV D620. ABS often titles DH62 (official ABS DQ63). ASTM A131 has no grade at this strength. Write LR/DH62 on the LR purchase order.

LR/DH62 is almost always produced TM or QT by an LR-approved mill to order rather than taken from open stock. SHH STEEL sources extra-high-strength plate from mills with Lloyd’s Register approval for the grade, under Surveyor attendance, with optional multi-class and EN 10204 3.2.

LR LR/DH62 plate: specification summary

ItemLR LR/DH62 / DH62 data
Rule basisLloyd’s Register Rules for Materials (extra-high / high-strength hull steel); IACS UR W16 strength band (see UNCERTAIN for LR paragraph cross-refs without local PDF)
Commercial / stampLR/DH62 (LR DH62)
Yield / tensile / elongation620 / 720–890 N/mm² / 15 % min.
Impact−20 °C; ≈ 62 J L or 41 J T average (IACS UR W16 / aligned tables — confirm on mill certificate)
Deoxidationfully killed, fine grain; N-binding elements per manufacturing specification
Delivery conditionTM or QT (N/CR routes only where specifically approved) — within mill approval thickness limits
MarkingLR DH62 / LR/DH62 (plus delivery-condition / Z / U where ordered)
UTcommonly required for thicker EHS plate (e.g. ≥15 mm) — agree standard (EN 10160 / ASTM A578) on PO
Thickness toleranceIACS UR W13 as adopted by LR (confirm class on PO; see UNCERTAIN)
Certificatemill certificate endorsed by the LR Surveyor; includes Ceq/CET/Pcm as applicable; EN 10204 3.1 / 3.2 on request

Maximum plate thickness depends on delivery condition and the mill’s LR approval sheet — typically TM up to about 100–150 mm and QT higher, but treat the approval limit as governing (UNCERTAIN without local LR PDF). Primary commercial scope we quote is within ~100 mm unless the mill approval and LR survey confirm otherwise.

LR LR/DH62 chemical composition (heat analysis envelope)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C (depends on route)0.14–0.21 max. by grade/condition (UR W16 / mill approval)numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificateTM/QT and letter routes may tighten C
Mntypically 1.0–1.70 (route-dependent)numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificateas per mill approval
Sitypically 0.60 max. (QT may differ)numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate
P / Stighter than UR W11 HS; often 0.025 max. or lower on EQ/FQ-style routesnumeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificateconfirm on approval sheet
Al total min.fine-grain practicenumeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificateAl/N control unless other N-binders used
Nb / V / Tilimits per UR W16 / mill approvalnumeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificatecombined microalloy caps apply
Ni / Cu / Cr / Moper approval chemistrynumeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate
Ceq / CET / Pcmmaxima by category and condition on approvalnot applicable (calculated from heat analysis)report on certificate

Product (check) analysis column: LR Rules for Materials specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Source: IACS UR W16 chemistry envelope as implemented by Lloyd’s Register for LR/DH62 — exact ladle limits depend on delivery condition (TM vs QT) and toughness letter. Values above are the rule envelope; the purchase order and mill approval sheet govern. Product analysis: as per standard and mill certificate. All intentionally added elements and Ceq (or CET/Pcm) are to be reported. Flagged UNCERTAIN where a local LR Materials PDF was not available to quote paragraph numbers.

LR LR/DH62 tensile and impact properties

PropertyRequirement (IACS UR W16 aligned)
Yield strength ReH (or Rp0.2)620 N/mm² min.
Tensile strength Rm720–890 N/mm²
Elongation (transverse, 5.65√A)15 % min.
Impact test temperature−20 °C
Impact energy (indicative)62 J L or 41 J T average

Final acceptance values are as per standard and mill certificate under LR survey. For thick plate, additional mid-thickness tensile/impact positions may apply — confirm at enquiry. Test frequency is typically each heat-treatment batch of same cast/condition/thickness.

Delivery condition and toughness for LR/DH62

Charpy temperature is fixed by the grade letter: DH → −20 °C. Indicative average energy 62 / 41 J (L/T) from IACS UR W16 aligned tables — confirm exact figures on the LR-endorsed certificate. Unlike UR W11 higher-strength tables, EHS energies are usually stated as a single pair rather than rising through many thickness bands; thick-plate mid-thickness rules may still apply.

Allowed delivery conditions are primarily TM and QT within the mill’s approved thickness. Vacuum degassing is commonly required for higher categories and for thicker plate — follow the mill approval. State TM or QT on the PO; do not leave delivery condition blank for DH62.

Thickness tolerance and surface condition

Lloyd’s Register applies IACS UR W13 unless the PO states otherwise (confirm minus class on PO; see UNCERTAIN). Surface repair limits follow the applicable LR / UR rules; state primer/surface class on receipt if needed. For QT plate, avoid notching cut edges; follow mill cutting recommendations.

LR LR/DH62 plate — mill-roll supply in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
102000 / 22008000 / 12000TM / QT200+ tChina
122000 / 2200 / 250012000TM / QT200+ tChina
142000 / 220012000TM / QT100+ tChina
162000 / 250012000TM / QT200+ tChina
202000 / 250012000TM / QT100+ tChina
252200 / 250012000TM / QT100+ tChina
30220010000 / 12000TM / QT100+ tChina
40220010000TM / QT50+ tChina
5022008000 / 10000TM / QT50+ tChina

Extra-high grades such as LR/DH62 are rarely held as open stock; the table shows the size bands we quote against scheduled mill rolls. Quantities are indicative. All plates sold as LR class carry LR/DH62 marking and an LR-endorsed mill certificate. Typical mill lead time including LR survey is about 6–10 weeks (commercial estimate — confirm per quote). Send your size list and we will reply with the next available rolling slot.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and LR stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

LR LR/DH62 equivalents in other rules and standards

Standard / societyDesignationComment
LR (Lloyd’s Register)LR/DH62 (LR DH62)this page; LR uses AH69 not AH70
ASTM A131/A131MASTM A131/A131M — no direct Grade DH62A131 stops at FH40
ABSABS DH62 / DQ63commercial DH62 / official DQ63 (ABS uses 70 where LR uses 69)
DNVDNV NV D620DNV titles DH620 for this yield band
BVBV (per rules)EHS name not verified from local BV PDF — write per rules
CCSCCS DH620CCS follows W16-style naming
NK (ClassNK)NK KD620NK KD620
KRKR RD63KR RD63 (KR uses ABS-style category numbers)
RINARINA (per rules)EHS name not verified from local RINA PDF
GB 712GB 712 Grade DH620listed in GB 712 EHS band; not class approval alone

These are comparisons, not substitutions. Always write the LR stamp LR/DH62 on the PO, plus any additional society stamps you need.

LR LR/DH62 vs higher-strength and other EHS grades

Use DH62 when scantlings need yield 620 N/mm². Do not substitute AH40/EH40 (390 N/mm² max under UR W11) without redesign. Within the 62 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Neighbouring strengths are 55 / 69 — swapping strength needs class approval of the drawing change.

When LR LR/DH62 is the right choice: typical uses are higher-strength members that the material class table assigns to −20 °C, such as thicker deck and bottom strakes, sheer strakes and hatch coamings at extra-high yield — weight-critical hull girder strakes, polar and ice-class primary structure, and offshore units where 620 N/mm² is specified. See offshore platform steel plates for related offshore grades.

Applications and welding notes for LR LR/DH62

Typical uses: higher-strength members that the material class table assigns to −20 °C, such as thicker deck and bottom strakes, sheer strakes and hatch coamings at ReH 620 N/mm²; strength deck and shell of large container ships and gas carriers where EHS is specified; ice-belt and polar primary structure; selected offshore members. See offshore platform steel plates.

Welding: LR/DH62 is an extra-high-strength steel supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by LR. Ceq/CET/Pcm from the ladle analysis govern hydrogen control, preheat, interpass and heat-input windows. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits. We do not give generic preheat temperatures.

Processing notes: LR/DH62 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and LR. Cold forming and bending radii should follow the mill’s data sheet. Thermal cutting parameters follow mill recommendations so the cut edge is not damaged.

Certificates, LR survey and third-party inspection

LR survey at the mill; certificate includes ladle chemistry, Ceq/CET/Pcm as applicable, tensile (ReH ≥ 620, Rm 720–890, A ≥ 15 %), Charpy at −20 °C, delivery condition, UT if ordered, and plate identity. Optional EN 10204 3.2 and multi-class.

On receipt: verify LR/DH62 stamp, −20 °C impact data, energies ≥ ordered/certified minima, thickness within tolerance, Surveyor endorsement, UT report if required.

Charpy acceptance for LR/DH62 (IACS UR W16 aligned; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
as per UR W16 / mill approval (typically t/4 position)−20 °C6241

For thickness above ~100 mm, additional mid-thickness rules may apply — confirm at enquiry. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.

Common mistakes when ordering LR DH62 / LR/DH62

  • Ordering “LR 62” without the letter (DH) — toughness missing
  • Writing ABS DH62 or DNV DH620 on an LR-class PO without arranging that society’s survey (wrong stamp)
  • Leaving delivery condition blank (TM vs QT changes price, mill and properties)
  • Expecting ASTM A131 dual-cert at this strength (A131 has no EHS grade)
  • Skipping UT on thick EHS plate when the yard specification requires it
  • Missing LR endorsement / assuming GB 712 Grade DH620 alone is class approval
  • Confusing LR AH69 with ABS AH70 — same yield band, different society title

Write grade, TM/QT, impact temperature, UT level and certificate type into the PO.

Sourcing LR LR/DH62: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateLR-approved mills only; traceable LR/DH62 stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mill minimum / long lead timecombine sizes on one heat where possible; weekly photo updates; clear rolling-slot confirmation before deposit
Welding / heat-input risksend ladle Ceq/CET/Pcm before shipment; support WPS review with mill data
Prep before shipcutting, bevelling, drilling, machining in our workshop (follow mill cutting notes for QT)

How to order LR LR/DH62 plate

Specify LR DH62 (LR/DH62), delivery condition TM or QT, thickness × width × length × qty, Z/U/UT level, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to Lloyd’s Register Rules for Materials, Grade DH62 (LR/DH62), delivery condition [TM/QT], 30 × 2500 × 12000 mm, 10 pcs, marked LR DH62 / LR/DH62, certificate endorsed by LR Surveyor, EN 10204 3.2 [if required], UT [EN 10160 / ASTM A578 level], CIF [port].”

FAQ

What sizes and minimum order quantity can you supply for LR DH62 / LR/DH62 plate?
LR/DH62 is ordered as Lloyd’s Register extra-high-strength grade DH62 (IACS UR W16 strength band). The plate is fully killed, and the maximum thickness depends on the delivery condition (TM or QT) and the mill’s LR approval. In practice LR/DH62 is nearly always produced by an approved mill to order rather than taken from stock, so a mill minimum per heat or rolling usually applies. Send thickness × width × length × quantity per size and we will say whether the order fits a scheduled rolling or needs its own heat. Small balance quantities can sometimes ride on another DH62 order.
How is LR LR/DH62 certified, and can you arrange EN 10204 3.2 witness inspection?
Every plate is made by an LR-approved mill under Lloyd’s Register survey. It is die-stamped or stencilled LR DH62 / LR/DH62 with the heat or plate number, and the mill test certificate is endorsed by the LR Surveyor. The certificate gives ladle chemistry, Ceq/CET/Pcm as applicable, tensile (ReH ≥ 620 N/mm², Rm 720–890 N/mm², A ≥ 15 %), Charpy at −20 °C, delivery condition, UT if ordered, and plate identity. If your contract asks for EN 10204 3.2, we arrange it before rolling. Dual or multi-class (e.g. LR + ABS or DNV) must be booked before testing. 3.2 cannot be added afterwards.
What is the impact test temperature and energy for LR DH62 / LR/DH62, and do thickness limits apply?
LR/DH62 is tested at −20 °C with an indicative average of at least 62 J longitudinal or 41 J transverse (IACS UR W16 aligned tables). Impact specimens typically come from the quarter-thickness position (t/4). For thicker plates, LR / UR W16 may require additional positions. Rule maximum thickness depends on whether the plate is TM or QT and on mill approval, so give the delivery condition as well as the thickness, and we will check the approved mill’s range before quoting. Final values are as per standard and mill certificate (see UNCERTAIN).
What welding and preheat guidance applies to LR LR/DH62?
LR/DH62 is an extra-high-strength steel (yield ≥ 620 N/mm²) supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by LR. Ceq is calculated from the ladle analysis and limited by the approval chemistry; the mill may also report CET or Pcm for low-carbon TM/QT steel. Hydrogen control, preheat, interpass temperature and heat-input windows come from the approved WPS and the mill’s recommendations. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits.
What is the delivery time for LR LR/DH62 plate?
LR/DH62 is normally rolled to order. Typical commercial lead time is about 6–10 weeks from confirmed PO and deposit, depending on the mill rolling schedule, QT capacity, UT and any 3.2 witness. Ocean transit comes on top of that. This is a commercial estimate, not a rule value, and we confirm it with each quotation. Every week, your coordinator sends the rolling, heat-treatment, testing and stamping status with photos. Delays are reported as soon as the mill tells us, not at the shipping date.
Which payment terms do you accept for LR DH62, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the LR/DH62 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance. With L/C, payment is tied to the presented documents. For first orders we can start with a smaller trial lot. The proforma invoice shows the grade (LR/DH62 / LR DH62), TM/QT, sizes and certificate type.
What are the equivalent grades of LR LR/DH62 among class societies and GB 712?
Lloyd’s Register lists LR/DH62 for commercial DH62 (LR uses AH69, not AH70). ASTM A131/A131M stops at FH40, so it has no direct equivalent. ABS DH62 / DQ63 is the usual ABS counterpart. DNV NV D620 is the DNV counterpart (DNV titles DH620). CCS DH620, NK KD620 and KR RD63 are the CCS/NK/KR counterparts. BV and RINA EHS names are written “per rules” until verified. GB 712 Grade DH620 is listed in the GB 712 EHS band but is not class approval by itself. Always write LR/DH62 on the PO, plus any additional society stamps you need.
Can you cut, bevel or machine LR LR/DH62 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut DH62 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the LR/DH62 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For QT extra-high-strength plate, thermal cutting parameters follow the mill’s recommendations so the cut edge is not damaged. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. See SHH STEEL for our processing capabilities.

Conclusion

LR DH62 / LR/DH62 is extra-high-strength hull steel (IACS UR W16 band): yield 620 N/mm², tensile 720–890 N/mm², Charpy at −20 °C, marking LR/DH62. Lock on the order: TM or QT, UT level, Ceq/CET/Pcm reporting, multi-class and 3.2.

SHH STEEL supplies LR/DH62 plate rolled by Chinese mills that hold Lloyd’s Register works approval for the grade, so every plate carries the LR/DH62 stamp and a Surveyor-endorsed certificate traceable to its heat. Sizes are scheduled into the mill rolling cycle with LR survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, BV or another agency) and joint certification with ABS, DNV, BV, CCS, NK, KR or RINA.

We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or LR/DH62 with neighbouring EHS sizes or higher-strength AH–FH 40 where the drawing allows, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.

Request a quotation: send SHH STEEL the grade (LR/DH62 / LR DH62), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X